IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 477 documents. Displaying 25 entries per page.


Strategies for enhancing usage of treated wood in Indian context
2005 - IRG/WP 05-40305
India constitutes 2% of the world’s forest area but it has to support over 15% of the human and nearly 14% of the cattle population and therefore forests in India are under immense biotic pressure. The main concern today is the rate at which avoidable factors or man made threats accelerate the process of forest degradation and to evolve measures to check the same. Man made threats include expl...
P K Aggarwal, S C Gairola


Antifeedant activities of flavonoids and their related compounds against the subterranean termite, Coptotermes formosanus Shiraki
1999 - IRG/WP 99-10305
Antifeedant activities of some flavonoids and their related compounds against the subterranean termite, Coptotermes formosanus Shiraki were examined with no-choice and two-choice tests. The activities of these compounds were considered in relation to their chemical structures. All flavonoids tested showed antifeedant activities whereas catechinic acid without A-ring and pyran ring in the molecule ...
W Ohmura, S Doi, M Aoyama, S Ohara


Tunnelling bacteria
1983 - IRG/WP 1186
The micromorphology of decay in wood caused by a certain group of single-cell bacteria, called tunnelling bacteria (TB), is described. TB are characterised by their tunnelling ability within the secondary cell walls of wood fibres. Pure cultures of TB have not yet been obtained although the typical decay patterns can be reproduced using mixed bacterial cultures. Some indications of lignin degradin...
T Nilsson, G F Daniel


Wood kiln drying. Simple process of material treament or soft method of preservation? (Le séchage arificiel du bois. Simple opération de traitement du metériau ou méthode douce de préservation?)
1993 - IRG/WP 93-50001-14
Among the processes enabling to extend wood durability, kiln drying can be considered as a treatment and soft preservation method. Dry woods are naturally durable provided they are not subject to important retaking of the moisture. Drying thanks to the application of temperatures from 50 to120°C enable to execute a thermic treatment which kills grubs and mushrooms to ensure a sterilization that c...
F More-Chevalier


The identification of organic compounds in wood using thermal desorption GC-MS - possibilities and limitations
2001 - IRG/WP 01-20224
There is a clear need for the analytical characterisation and identification of organic compounds and their derivatives in different phases especially in timber. In this context the paper describes a rapid and powerful gas chromatographic method for the determination of insecticides, biocides and "other" organic substances in treated and/or modified wood. The main advantage of this procedure is th...
P Jüngel, E Melcher


Adequate preservative treatment of kiln dried Eucalyptus camaldulensis and Acacia mangium for tropical and subtropical wood poles
1996 - IRG/WP 96-40075
The Eucalyptus camaldulensis and Acacia mangium round timbers kiln-dried at EMC and full cell pressure treated with CCA-C ensured requisite penetration and adequate dry retention (30 kg/m³ or 4% w/w). The sufficient inherent strength, seasoning property, treatability of sapwood and heartwood equivalent to 44% of radius, natural durability of heartwood, and field investigation on service performan...
A K Lahiry


Some aspects of testing water repellents
1998 - IRG/WP 98-40113
Several test methods are used to determine the efficiency of water repellent treatments on wood. The most common are: contact angle measurement, swelling rate of samples immersed under water and, the increase in mass of wood samples with time or after a fixed period of time either fully immersed under, or partially immersed in or floating on water. In this paper, some fundamental aspects of the l...
D Lukowsky, M Farnow, T Rypstra


Accelerated diffusion treatment of sawn Sitka spruce grown in the UK
1986 - IRG/WP 3395
The treatment of 'green' sapwood and heartwood of Sitka spruce by diffusion methods was investigated. Steam/dip treatment processes gave increased solution uptakes and depths of penetration of copper in comparison with a simple dip treatment. Further investigation is required to reduce diffusion gradients with copper based formulations and to improve the penetration of '...
R J Murphy, D J Dickinson


Clean creosote - its development, and comparison with conventional high temperature creosote
1983 - IRG/WP 3235
Pigment emulsified creosote (PEC) is presently being tested and shows considerable stability in terms of water content, pigment level, pH, viscosity, rheological behaviour and microscopy. Timber samples from several eucalypt species have been treated with PEC and side matched samples treated with conventional high temperature creosote (HTC). The PEC treated specimens showed higher weight retention...
C W Chin, J B Watkins, H Greaves


Sawn timber of fir (Abies alba Mill.) - Treatability and usability for the Hazard Classes 3 and 4
1999 - IRG/WP 99-40147
Within a national research project, tests on the treatability on sawn timber of fir (Abies alba Mill.) in oscillation pressure, vacuum pressure and double-vacuum processes have been worked out with 95 trunks taken from 3 different altitude levels (up to a height of 590 metres, 600 to 990 metres and over 1000 metres) and from 4 different regions of Switzerland. As the treatability of round wood can...
E Graf, T Bör


The Effect on Biological and Moisture Resistance of Epichlorohydrin Chemically Modified Wood
2002 - IRG/WP 02-40224
Southern pine solid wood and fiber were chemically modified with epichlorohydrin to help in understanding the role of moisture in the mechanism of biological effectiveness of chemically modified wood. The solid wood had weight gains from 11% to 34%, while the fiber had weight gains from 9% to 75%. After modification, part of the specimens were water leached for 2 weeks or extracted for 2 hours ...
R E Ibach, B-G Lee


The influence of drying and chemical stress on the lignin degradation in aspen by Phanerochaete chrysosporium
1992 - IRG/WP 92-1573
Wood wafers of Populus tremuloides sapwood were incubated on common media with the white rot fungus Phanaerochaete chrysosporium (wild isolate) and subjected to cyclic drying or chemical agents (low levels of borate or trifluoperazine [a calmodulin antagonist]). After a mass loss of approximately 5.5%, wafers were dried and analyzed for acid-insoluble lignin. Those wafers containing chemical agent...
E L Schmidt, Y-L Lin


Utilization of coconut timber from north Sulawesi, Indonesia. Part 2: Treatability
1994 - IRG/WP 94-40025
Under tropical conditions coconut wood is quickly degraded by mold and blue stain fungi. Low density wood in ground contact is commonly decomposed by wood destroying fungi within a period of only a few months, higher density wood from the outer stem regions within 24 to 30 months (MOSTEIRO, CASIN, SERIBAN 1976; McQUIRE 1975). Moreover, according to McQUIRE (1975) green wood of lower density is hig...
R-D Peek


IPBC - A new fungicide for wood protection
1984 - IRG/WP 3295
3-iodo-2-propynyl butyl carbamate (IPBC) is presented as a potential low toxic alternative to pentachlorophenol and the sodium chlorophenoxides. Data on its effect against basidiomycetes is shown. Tests according to both the European standard method, EN-113, and American, ASTM D-413, have shown its potential. The chemical gives protection against both the wood destroying fungi, blue stain, mould and algae. It is possible to have it formulated in both water-based and organic solvent-based products. Treatment of wood out of ground contact (vac-vac products, pretreatment products, primers, stains, etc.) and sapstain control are some of the most potential end use areas within wood protection. Besides wood protection, the IPBC is used as a fungicide in paint, adhesives, caulks and sealants, cement, leather, paper, cutting oil, ink and in different roofing materials.
J Hansen


Potential for using dip/supercritical fluid treatments for wood impregnation
2004 - IRG/WP 04-40276
While supercritical fluid impregnation offers tremendous potential for impregnating wood species that resist conventional liquid preservative treatments, the resulting treatments are often not uniform among samples in a charge or between charges. One factor that influences treatment is the dynamic change in pressure that occurs during introduction of the biocide laden supercritical fluid into the ...
Sung-Mo Kang, J J Morrell


Deterioration of wood viewed from iron nail
1991 - IRG/WP 2368
Deterioration of nail was graded by a five - rank numerical - rating. The rating of nail moisture content and decay of wood were inspected in a mortal-wall of 34-year-old house. The wood was mostly in decay, when the rating of the nail was above about 4, and the moisture content was above about 20%. Nailed wood specimens kept in several humidity room of 20°C for 4 years showed that the rating of ...
H Imamura


Dimensional stability and decay resistance of wood upon modification with some new type chemical reactants
1994 - IRG/WP 94-40028
Solid wood of home grown species can be upgraded by chemical modification with environmentally acceptable chemicals. The best kwown example of modification reaction is acetylation with acetic anhydride. A continued search for reactive chemicals other than acetic anhydride is ongoing, aiming at the improvement of technical properties of wood. This contribution deals with the results of a screening ...
P Goethals, M Stevens


Assessing the bioresistance conferred to solid wood by chemical modification
1997 - IRG/WP 97-40099
The chemical modification of wood using straight chain alkyl anhydrides can considerably enhance its durability. This paper presents an assessment of the effectiveness of these modifiers in improving the biological resistance of a susceptible softwood when exposed to four different basidiomycete fungi, soft rots and the larvae of the house longhorn beetle (Hylotrupes bajulus). It was clear that so...
E D Suttie, C A S Hill, D Jones, R J Orsler


Soft rot decay in CCA treated eucalypts in Queensland - A comment
1986 - IRG/WP 1301
A survey has been completed concerned with the distribution and severity of groundline soft rot decay in the CCA treated sapwood of eucalypt poles in Queensland. The survey encountered some 1000 poles of which 55% were slightly, 28% moderately and 17% severely decayed. Soft rot decay was more severe in urban than rural locations. Embedment of poles in concrete resulted in severe soft rot. No signi...
L E Leightley


New principles for the protection of wood: Impregnation with waterborne resins
1995 - IRG/WP 95-40047
The environmental impact of classical wood preservatives as well as the use of tropical wood species with high natural durability is regarded increasingly critically in the public. Therefore other partially new principles for the protection of wood, like chemical modification, or treatment with resins were examined especially in USA, Japan and in Europe with promising results predominantly in the ...
A O Rapp, R-D Peek


New ways of chemical wood preservation
1997 - IRG/WP 97-40087
Synergistic effects pertaining to wood preservation have been investigated by combining different polymerizing agents with modifying chemicals, modifying chemicals with known preservatives and new types of preservative chemicals with each other. One of the investigated methods is the use of impregnating solutions based on furfuryl alcohol (produced from biomass), in which the chemicals polymerizes...
M Westin, T Nilsson, B Ohlsson, R Simonson


Silafluofen: Novel chemistry and versatility for termite control
1995 - IRG/WP 95-30069
A novel silicon - containing insectizide, HOE 084498 ('Silafluofen'), with a favourable toxicological profile, has shown activity against a broad spectrum of agricultural and environmental health pests. Results from laboratory and field studies around the world have demonstrated that silafluofen is effective at protecting timber from attack by various species of termite and wood-...
A J Adams, A Jermannaud, M-M Serment


Evaluation of the effectiveness of defence anti-stain in the control of sapstain in laboratory and field tests
1990 - IRG/WP 3593
The anti-sapstain product Defence Anti-stain (DAS) has been evaluated internationally in laboratory and field tests during the years 1988 and 1989. Results of tests carried out by institutes and by own companies in countries like Indonesia, Ivory Coast, Japan, Portugal, Belgium, The Netherlands and Spain will be presented. In the several tests Defence Anti-stain showed a high fungicidal activity t...
G Rustenburg, C J Klaver


A novel chemical barrier system, KORDON® TMB, for the protection of buildings against subterranean termites using a synthetic matrix as carrier for the chemical
1998 - IRG/WP 98-10264
Kordon TMB is a new chemical barrier system for installation beneath concrete slab-on-ground constructions using a matrix other than soil as carrier for the termiticide. The product consists of a synthetic foraminous web (blanket) carrying the synthetic pyrethroid deltamethrin. The blanket is laminated on the upper side to a standard 0.2mm thick moisture vapour membrane of low density polyethylene...
M Lenz, P Morrow, S Runko


Step-wise pressure process for reducing surface roughness in Japanese cedar timber
2003 - IRG/WP 03-40256
Sixteen dried sawn-timber (10.5 x 10.5 x 360 cm) were cut into half. The half of them was treated by step-wise pressure process with 2.5 MPa maximum, and the other half was treated by conventional pressure process with 2.5 MPa maximum. Average DDAC preservative absorption was 461 kg/m3 in the former and 525 kg/m3 in the later. Surface roughness was expressed as the profile element height of collap...
K Yamamoto, M Nozoki