IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 454 documents. Displaying 25 entries per page.


Image analysis for mould and sapstain detection on wood
2013 - IRG/WP 13-20519
Laboratory tests for mould growth on wood products are time consuming and rely on visual assessments of specimens utilizing subjective rating systems. Accelerated laboratory methods are needed that can provide rapid, quantitative assessment of mould and sapstain growth on solid and composite wood products. Image analysis of scanned spore imprints from southern pine or oriented strandboard (OSB) sp...
C A Clausen, V W Yang


Extraction and analysis of DNA from green and seasoned timber as basic methods for determination of wood species and origin
2013 - IRG/WP 13-20523
Against the background of the European timber trade regulation EUTR, commenced to law by March 2013, the determination of wood species and tracing of its origin is getting a great importance. A promising approach for establishing fast and reliable tracking systems for wood products is DNA analysis. A critical point is the extraction of analysable DNA from the wood and its lignified cell walls. Thu...
K Jacobs, H Mende, W Scheiding


Cell wall properties of softwood deteriorated by fungi: combined chemical analyses, FT-IR spectroscopy, nanoindentation and micromechanical modelling
2013 - IRG/WP 13-20527
Mechanical properties of wood are determined by its inherent hierarchical microstructure, starting at the nanometer scale, where the elementary components cellulose, hemicelluloses, and lignin build up the wood cell wall material. Fungi cause degradation and decomposition of these components and, thus, alter the mechanical properties of wood. The aim of this study is to gain new insight into these...
L Wagner, T K Bader, K de Borst, T Ters, K Fackler


Effect of the nature of the inert atmosphere used during thermal treatment on chemical composition, decay durability and mechanical properties of wood
2013 - IRG/WP 13-40625
Wood heat treatment is an attractive alternative to improve decay resistance of low natural durability wood species. Nowadays, several types of thermal treatments of wood exist. These treatments differ mainly by the nature of the inert atmosphere used to avoid wood combustion which may correspond to: nitrogen, vacuum, steam or oil. Decay resistances as well as mechanical properties are strongly co...
K Candelier, S Dumarçay, A Pétrissans, M Pétrissans, P Gérardin


Study of UV resistance and natural weathering of coatings on chemically modified wood
2013 - IRG/WP 13-40629
In this study, UV resistance and weathering performance of rubberwood (Hevea brasiliensis) and radiata pine (Pinus radiata) modified with benzoyl chloride and acetic anhydride was studied. Performance of polyurethane based wood coatings on modified wood was also evaluated. Unmodified and chemically modified specimens were exposed to accelerated and natural weathering. Modified and unmodified woo...
K K Pandey, K Srinivas


Characterization of wood modification prepared by in situ polymerization with pre-polymer and the mechanism of modification
2013 - IRG/WP 13-40633
Chemical modification of wood is a potential way to obtain high quality wood. In this study, the fast-growing poplar was impregnated with modifier using a pulse-dipping machine by in situ polymerization. Fungal decay analysis, mechanical properties and dimension stability of the natural and modified woods were investigated. The wood samples were also characterized by X-ray diffraction (XRD) Therma...
Qian Lang, Zeng Bi, Junwen Pu


Identification of soft-rot fungi existed in the samples from the galley excavated at Yenikapi
2014 - IRG/WP 14-10833
The shipwrecks of the Middle Byzantine period were excavated during the construction of the Marmaray railway and metro station in Yenikapı between 2004 and 2012. This has become the largest investigations because of the size and the number of the shipwrecks and its associated artifacts. In the previous report, the electron micrographs of the samples revealed that a wide range in the degree of...
T Wada, C Köse, K Igarashi


Microbial Community Analysis of Naturally Durable Wood in an Above Ground Field Test
2014 - IRG/WP 14-10826
This paper presents preliminary results of an above ground field test wherein eight naturally durable wood species were exposed concurrently at two sites in North America. Surface samples were taken at regular intervals from non-durable controls and compared to their more durable counterparts. Terminal Restriction Fragment Length Polymorphism was performed to characterize the microbial (bacteria, ...
G T Kirker, S V Diehl, P K Lebow


The Chelator Mediated Fenton System in the Brown Rot Fungi: Details of the Mechanism, and Reasons Why it has Been Ineffective as a Biomimetic Treatment in some Biomass Applications – a Review
2014 - IRG/WP 14-10828
The chelator-mediated Fenton (CMF) reaction requires the action of two types of chelating compounds. The first chelator, oxalate, solubilizes and then sequesters iron, and the second chelator reduces iron. Iron reduction must be controlled near the fungal hyphae to prevent damaging Fenton chemistry from occurring in that location. Similarly, iron reduction must be promoted within the wood/plant ce...
B S Goodell, M Nakamura, J Jellison


Changes in mechanical and chemical properties of wood exposed outdoors
2014 - IRG/WP 14-20550
The aim of this study was to investigate differences in certain mechanical and chemical properties of three different wood species (common beach (Fagus sylvatica), Norway spruce (Picea abies), and copper-ethanolamine (CuE) impregnated Norway spruce (Picea abies)) that were exposed in use class 3 (CEN, 2006) for periods between 4 and 30 months. The results show, that changes in the investigated me...
N Thaler, C Brischke, D Žlindra, V Vek, M Humar


Statistical analysis of 40 years of preservative in-ground stake testing in Australia
2014 - IRG/WP 14-20552
Wood is widely recognized as a valuable material, yet the natural durability of some wood species limits its use for certain outdoor purposes. For decades, a wide range of methods and chemicals have been developed to increase the resistance of wood against degrading microorganisms and termites. Preservative treatment has a long and widespread tradition in wood protection. Proper testing of the eff...
J Van den Bulcke, L J Cookson, I De Windt, W Li, J Van Acker


Scanning Transmission X-ray Microscopy as a tool for examining chemical changes in wood cell walls due to enzymatic activity
2014 - IRG/WP 14-20556
As development of techniques for examining enzymatic activity on solid, complex biological materials, is considered to be an important factor in further development of enzyme applications and for understanding the decay of plant materials, this study explores applicability of Scanning Transmission X-ray Microscope (STXM) for determining chemical changes in enzymatically treated samples at the cell...
D Jeremic, R Goacher, R Yan, C Karunakaran, E R Master


Resistance to Decay Fungi of Scots Pine Impregnated with Natural and Chemical Preservatives
2014 - IRG/WP 14-30650
In this study, heart-wood and sap-wood specimens of the Scots pine which is naturally grown in Turkey were treated with natural (valex) and some chemical preservatives such as CCA - C (Copper / Chrome / Arsenic), CBA - A (Copper / Boron / Azole). The wood protective efficacies of these preservatives were investigated by means of fungi decay test (EN 113). As a result of the study it was found t...
S Yildiz, U B Şimşek


Dynamic mechanical analysis (DMA) of nano cupric oxide (CuO) modified aqueous phenol formaldehyde (PF) resin
2014 - IRG/WP 14-40654
Phenol formaldehyde (PF) resins, modified by nano CuO incorporating alkane surfactant and polyvinyl alcohol (PVA) 17-99, were analyzed by dynamic mechanical analysis (DMA). The mechanical properties of its bonded plywood including tensile strength, modulus of rupture (MOR), modulus of elasticity (MOE) and shear strength under five test conditions were evaluated. Results indicated that the incorpor...
Wei Gao, Guanben Du


Modern Instrumental Methods to Investigate the Mechanism of Biological Decay in Wood Plastic Composites
2014 - IRG/WP 14-40674
Various instrumental techniques were used to study the fungal decay process in wood plastic composite (WPC) boards. Commercial boards exposed near Hilo, Hawaii (HI) for eight years in both sun and shadow locations were inspected and tested periodically. After eight years of exposure, both boards were evaluated using magnetic resonance imaging (MRI), while a selected area of the board exposed in sh...
G Sun, R Ibach, M Gnatowski, J Glaeser, M Leung, J Haight


Compatibility of Acetylated Wood and Wet Concrete
2014 - IRG/WP 14-40673
One of the newer commercial technologies to provide stability and durability to wood and wood composites is the process of acetylation (the reaction of acetic anhydride with wood). Wood is often used in contact with concrete, although only a very limited amount of species are suitable for this type of application because of durability issues. From this perspective durability class 1 timber such ...
R Rowell, C Lankveld, J Alexander


Chemical composition of extractives of different wood compartments of Pinus merkusii and their potential implication in wood durability
2015 - IRG/WP 15-10841
Amounts and nature of extractives differ strongly according to the compartment of wood and to the nature of the wood species. Previous studies reported that knotwood of several European Pinus sp. contains extractives contents much higher than stemwood consisting mainly of lignans which may find valuable applications in cosmetic, nutraceutic or pharmaceutic sectors. Different explanations have been...
A Wijayanto, S Dumarçay, R Kartika Sari, W Syafii, P Gérardin, C Gérardin-Charbonnier


The whitening cause of Korean wooden heritage by flame retardant treatment
2015 - IRG/WP 15-20560
Korean wooden heritage used to treat by flame retardants in order to protect fire. There are 2 types flame retardant using for wooden heritage. These flame retardants treatment are basic measure that apply to wooden heritage along with other fire protection. The flame retardants cause white stains by reacting with Korean traditional wood painting (Dancheong) and increase wood humidity. The Korean ...
Jin Qyu Kim, Gyu-Seong Han, Yong Jae Chung, Hwa Soo Lee, Dong Won Son


Durability of Fence Posts of Four Wood Species After 20 Years in Field Test
2015 - IRG/WP 15-30670
In the past years, wood consumption from native forests has drastically reduced the availability of wood. Fast-growing species such as Pinus and Eucalyptus suitably impregnated with chemicals may show a service life equal or higher than hardwood with high natural durability. The field tests have been an alternative widely used to evaluate the durability of wood and the efficiency of preservatives....
A Florian da Costa, A C Salgado de Freitas, E Meneses Oliveira


Effect of natural variability of European Oak wood on heat treatment process and potential implication on wood durability
2015 - IRG/WP 15-40693
Environmental pressures appeared in France and in most European countries during the last decade has led to the development of more environmentally acceptable preservation methods. In this context, wood heat treatment has been one of the most investigated alternative method during the last years. Treated at temperatures ranging between 180 and 220°C, wood components undergo more or less important...
J Hamada, A Pétrissans, F Mothe, M Pétrissans, P Gérardin


Foundation piles: analysis of beech wood decay in service life conditions
2016 - IRG/WP 16-10858
Wood piles foundation system was largely used over decades. Thus, numerous buildings over the world are based on this constructive system. In the context of reduction of CO2 emissions in the building field of constructions, substitution of concrete by wood as material for foundation piles seems to be a promising alternative. However, fluctuation of the water table level in soil may promote fungal ...
Q Kleindienst, A Besserer, M-L Antoine, C Perrin, J-F Bocquet, L Bléron


Studying fungal growth using automated image analysis and computer simulations
2016 - IRG/WP 16-20590
Wooden materials are prone to fungal attack resulting in damage and economic losses. Therefore many efforts have been made to understand the degradation of wood and to avoid the adverse effect of fungi. Even though the extent of degradation of a material is inversely proportional to the extension of the fungi attacking it, most researchers focus mainly on the former, leaving the study of the latte...
G Vidal-Diez de Ulzurrun, J M Baetens, J Van den Bulcke, B De Baets


Preparation of Calibration Standards for the Analysis of Pentachlorophenol in Treated Wood by X-ray Fluorescence
2016 - IRG/WP 16-20591
The primary purpose of this project was to develop a method for preparing calibration standards that can be used by the wood treating industry to calibrate X-ray fluorescence instrumentation. Calibration standards of penta/P9-oil in southern yellow pine that cover the retention range of 0.2 to 0.9 pcf (0.6 to 1.9 %) were successfully prepared. A detailed procedure for mixing penta in treating sol...
L L Ingram Jr, H M Barnes, R Shmulsky, D Jeremic


Combustion and thermal characteristics of Korean wood species
2016 - IRG/WP 16-40727
This study examined the combustion and thermal characteristics of domestic woods in Korea. Wood was confirmed by a cone calorimeter according to the KS F ISO 5660-1 standard. The combustion properties of the wood were measured in terms of the heat release rate (HRR), total heat released (THR), mass lose rate (MLR), and ignition time (time to ignition; TTI). Also, the thermal properties were measur...
Huyun Jeong Seo, Jung-eun Park, Dong Won Son, Won-Joung Hwang


Dynamic mechanical analysis of viscoelastic properties of heat treated glycerol-impregnation poplar wood
2016 - IRG/WP 16-40732
The viscoelastic properties of glycerol-impregnated poplar wood after heat treatments at various temperatures were examined by dynamic-mechanical analysis. The spectra of storage modulus (E’) and loss tangent (tgδ) in the frequency at 10 Hz were measured at the temperature range from -100 to 300℃. Compared to no peak in E’ spectra and two relaxation processes in tanδ spectra of...
Li Yan


Previous Page | Next Page