IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 454 documents. Displaying 25 entries per page.


Occurrence of manganese deposits in test stakes exposed in groung contact situations
1996 - IRG/WP 96-10182
Dark spots and flecks were frequently recognized on the surface and within non-preservative treated hard- and softwood test stakes placed in soil contact. Energy dispersive X-ray microanalysis in conjunction with electron microscopy showed the flecks to be composed primarily of manganese dioxide. Detailed transmission electron microscopy observations indicated intrusion of manganese into the wood ...
G F Daniel, T Nilsson, J Volc


Laboratory evaluation of organophosphates as termiticides
1985 - IRG/WP 3330
In accordance with Japan Wood Preserving Association Standard 11(1) laboratory evaluations of five organophosphate insecticides and chlordane were conducted. Superficially treated sapwood of Pinus densiflora Sieb. et Zucc. (10 x 10 x 20 mm³) was compulsorily exposed to the attacks of 150 workers and 15 soldiers of Coptotermes formosanus Shiraki for 21 days at 28±2°C in the dark. Percentage weig...
K Tsunoda, K Nishimoto


Investigation of some technical properties of heat-treated wood
2003 - IRG/WP 03-40266
The objective of this study was to investigate some technical properties of heat-treated wood. Wood heat-treated according to a process intended for wood in above-ground end-uses (European hazard class 3) was subject to the following: · A delamination test according to EN 391 with glulam beams made of heat-treated pine (Pinus sylvestris) and spruce (Picea abies) laminations, assembled with PR...
C Bengtsson, J Jermer, A Clang, B Ek-Olausson


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 9: Report of third inspection (2 years) in Italy
1980 - IRG/WP 461
The wood samples were submerged in the sea at Follonica, Italy, in April 1977. Follonica, latitudine 42°55' North and longitude 10°45' East, is situated on the Tyrrhenian sea. The recorded temperature varies between 13°C to 25°C, salinity 37-38% and pH about 8. The inspections were carried out after 6 months (10/1977), 1 year (4/1978) and 2 years (4/1979)....
A Gambetta, E Orlandi


Life cycle analysis of utility poles. A Swiss case study
1995 - IRG/WP 95-50040-05
Use of preservative-treated wood products faces increasing public and political pressure because of environmental concerns regarding the chemicals used to protect the wood. However, critics usually focus only on one single aspect of the whole life cycle of treated wood products, disregarding other environmental effects of timber utilization. To evaluate the ecological consequences of wooden utilit...
T Künniger, K Richter


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 7: Second report on the samples in Papua New Guinea
1980 - IRG/WP 459
This report presents the findings to date regarding specimens installed in Papua New Guinea, as part of a world-wide marine trial of certain timbers treated with CCA or CCB preservatives. The details of the trial are set out in document number IRG/WP/414. The report discusses the findings in the context of the conditions prevailing at the trial site and of the properties of the trial timbers. The ...
S M Cragg, C R Levy


Aspergillus fumigatus Fresenius resistance to chemical preservatives in piles of pine and birch wood chips
1981 - IRG/WP 1146
Investigation has been carried out on the communities of fungi developing in birch and Scots Pine chip piles in the Ostroleka Pulp and Paper Mill in the North-East of Poland The species composition or fungal communities and their development in a dozen of chip piles during storage was investigated. Untreated and chemically treated birch and pine wood chips were investigated. In all samples the gre...
M H Zielinski


The use of TCMTB in applications other than sapstain prevention: A review
1990 - IRG/WP 3606
The efficacy of TCMTB against staining fungi and surface moulds has been thoroughly investigated during the last decade. As a result, the chemical is used as an alternative to the chlorinated phenols in various parts of the world for the preservation of freshly sawn timber. Less known are the data obtained against brown rot, white rot and soft rot fungi. The termite repellent and bactericidal prop...
R Van der Eynde


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 20: Report on the inspection of specimens at Sekondi, Ghana after 48 months
1985 - IRG/WP 4116
The results of the second inspection of CCA- and CCB-treated test panels exposed at Sekondi, Ghana, in June 1980, are presented. The panels of Pinus sylvestris treated with 3% CCA are stil unattacked after 48 months. Panels treated with 10% CCA and still in test (Fagus sylvatica, Pinus sylvestris and Alstonia scholaris) are still free of attack. Locol species treated with 3% CCB have all been dest...
F F K Ampong, N Asare-Nyadu


Bifenthrin, a new insecticide for the control of termites and wood-boring insects
1995 - IRG/WP 95-30076
Bifenthrin, a new insecticidal compound Bifenthrin has been extensively tested, to determine its potential use to control termites and other wood destroying insects. Bifenthrin is effective at extreme low rates which can minimize human and environmental exposure to the product. Results of tests carried out by several research institutes and by FMC in different countries will be presented. The phys...
G Rustenburg


The distribution of introduced acetyl groups and a linseed oil model substance in wood examined by microautoradiography and ESEM
2000 - IRG/WP 00-40169
Microautoradiography, a photographic method that shows the localization of substances labelled with radioactive isotope, and Environmental Scanning Electron Microscopy (ESEM) were combined to enhance sensitivity, resolution and reliability for examination of the distribution of introduced substances in wood. The preparation of microautoradiographs is less complicated when investigated with ESEM an...
M Rosenqvist


Analysis of degradation observed on ancient wooden objects buried underground
2001 - IRG/WP 01-10403
Ancient wooden objects were sometimes excavated from the moat of mounded tombs in Japan. Such wooden objects were in the shape of a sunshade, bird, shield, pole, yugi(a bag that holds arrows) among others. Archaeologists discussed the usage of such shaped objects, but no one could clearly explain their use. Some objects were observed using an ordinary microscope. Deterioration by bacteria was foun...
H Sakai


Mapping soft rot decay distribution using image analysis
1993 - IRG/WP 93-20011
Image analysis has been shown to be a useful technique for the assessment of soft rot decay caused by Chaetomium globosum in birch and bamboo (Wickens and Murphy, 1992). The technique can permit assessment of decay in individual or small groups of cells and this has been used to undertake soft rot decay mapping in thin sections of bamboo. Assessments were made of the extent of soft rot decay with ...
P J Wickens, R J Murphy, G F M Watts


Effects of a formaldehyde and sulphur dioxide treatment on decay and mechanical properties of aspen waferboard
1983 - IRG/WP 3242
Aspen wafers were sequentially treated under vacuum with formaldehyde and sulfur dioxide gas and pressed into waferboard bonded with powdered phenol formaldehyde resin. Decay resistance and strength properties were determined before and after simulated weathering. The water resistance of the phenol bonding system was lost in board made from the gas-treated wafers. This white rot fungus Coriolus ve...
E L Schmidt


Chemical analyses of IRG/COIPM INTERNATIONAL MARINE TEST (to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water) samples
1987 - IRG/WP 4114
Chemical analysis of CCA and CCB treated timber was carried out after exposure at tropical and temperate marine sites. Results indicated that losses of all elements had occurred. In particular, losses of boron were severe. Arsenic and copper were also lost. The chromium components in both formulations was the most dominant metal remaining. The results suggest that chromium modification was importa...
L E Leightley


Comparative environmental impact analysis of telecommunication utility poles: Treated wood and fibreglass
1999 - IRG/WP 99-50136
This study is aimed at providing the information necessary to assess the main environmental implications of different materials utilised in construction of utility poles. The study was performed on fibreglass and CCA treated poles timber. The work has been carried out by identifying and quantifying energy and materials used and wasted released during the entire life of the pole. The interactions w...
A Cugliandolo, M Onofrio, A Quaglino


A potential anti-sapstain chemical for sawmills
1984 - IRG/WP 3300
Several biocidal formulations were tested under laboratory conditions in order to discover an alternative antisapstain chemical to chlorophenoxides. The formulations tested were experimental water solutions containing a quaternary ammonium chloride, a commercial fungicide and/or a sodium salt of some carboxylic acids. The effect of sodium carbonate and borax decahydrate in mixture with a quaternar...
I A Linderborg


Determination of total fluoride in preservative-treated wood by ion selective electrode, without steam distillation
1996 - IRG/WP 96-20086
An analytical method was developed to determine total fluoride in wood treated with aqueous fluoride or borate-fluoride formulations. Ground wood was mixed with 60% sodium hydroxide solution and oven-dried overnight before furnacing at 600°C. The cool fused product was dissolved in warm water before adding a powerful complexant/buffer solution containing sulphosalicylic acid and EDTA. Fluoride wa...
M J Kennedy


Chemical, physical and biological factors affecting wood decomposition in forest soils
2003 - IRG/WP 03-20281
Organic matter (OM) decomposition is an important variable in determining the potential of forest soils to sequester atmospheric CO2. Studies using OM from a particular location gives site-specific decomposition information, but differences in OM type and quality make it difficult to compare results among soils and forest ecosystems. By using a “standard” OM in decomposition studies, OM qual...
M Jurgensen, P Laks, D Reed, A Collins, D Page-Dumroese, D Crawford


The dip diffusion treatment of tropical building timbers in Papua New Guinea
1972 - IRG/WP 310
In Papua New Guinea a dip diffusion process using a multi salt preservative developed by C.S.I.R.0. has been in commercial use for 8 years. Over 200 million super feet (236,000 m³ ) of timber has been treated during this period and current rate of treatment is 34 million super feet (80,400 m³ ) of timber per year in 70 licenced treatment plants. The process has been found to be simple to apply, ...
C R Levy, S J Colwell, K A Garbutt


Summarized comparison of four techniques for detecting defects in poles
1979 - IRG/WP 2126
Since our discussions in open session of Working Group II at Peebles, a number of workers in Australia have collaborated in comparing the efficacy of X-ray, sonic testing, or resistivity measurements for detecting internal defects in poles. The purpose of this circular is to draw to your attention some of the results, in summary form. No attempt has been made to compare techniques. More detailed a...
H Greaves


Characterization of tropical wood-decaying fungi by RFLP analysis of PCR amplified rDNA
1998 - IRG/WP 98-10251
Five brown-rot fungi (Tyromyces palustris, Gloeophyllum trabeum, Antrodia sp., Poria placenta, Coniophora puteana) and three white-rot fungi (Coriolus versicolor, Pycnoporus sanguineus, Lentinus squarrosulus) registred as representative wood-decaying fungi for international standards of wood durability tests have been characterized using molecular tools (PCR/RFLP). The Internal Transcribed Spacer ...
A Zaremski, M Ducousso, Y Prin, D Fouquet


Bioefficacy of boric acid grafted onto wood
1999 - IRG/WP 99-30202
The use of borate treated wood in outdoor is limited because of the migration of borate. The objective of this study is to investigate the fixation of boric acid in wood using polyethylene glycol (PEG-400) to form polyester borate and isocyanato group as coupling agent. FT-IR was used to monitor the reaction between boric acid and PEG. Elemental analysis was conducted to evaluate the C, H, and N v...
Weining Cui, D P Kamdem


Albumin borate: A new non-toxic, wide-spectrum, long-term wood preservative
1998 - IRG/WP 98-30167
Boron, widely recognized for its broad range of activity towards both fungi and insects and for its low mammalian toxicity, can not provide long term protection to treated timber due to its high leachability. Boron, in the form of boric acid, can be partially fixed to timber by the formation of an association with egg albumin, which is insolubilized by heat-induced coagulation. Chemical investiga...
M-F Thévenon, A Pizzi, J-P Haluk


Evaluation of chlorpyrifos as an insecticidal component of a wood preservative
1984 - IRG/WP 3301
After two years of laboratory and field testing, chlorpyrifos is showing excellent potential as an insecticidal treatment to wood. In laboratory termite tests, retentions as low as 1-2 parts-per-million or approximately 0.0008 kg/m³ (0.00005 lbs/ft³) are effective against the Coptotermes formosanus. Laboratory leaching tests have shown no significant effect on the concentration of the retained c...
K Rose, J Kozuma, P Sparrow


Previous Page | Next Page