IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 768 documents. Displaying 25 entries per page.


The Effect of Flavonoids on Colour and Spectral Changes of the Wood Surface Caused by Heat Treatment or Ultra-violet Irradiation
2006 - IRG/WP 06-40341
Both heat treatment and UV irradiation can cause discolouration and change in the spectral properties of wood surface. Some of the characteristic flavonols have significant role on colour and spectral changes, despite of their relative small quantities in wood. Colour changes and spectral properties of natural and extracted black locust (Robinia pseudoacacia L.) and poplar (Populus nigra L.) were...
R Csonka-Rákosa, L Molnár-Hamvas, E Börcsök, J Molnár, K Németh


Photo-degradation of modified and non-modified wood, coated with water borne acrylic coatings during artificial light exposure
2007 - IRG/WP 07-30416
A series of experiments were carried out to investigate photo-degradation of thermally modified (at 210oC and – 0.9 bars for two hours) and non-modified spruce wood (Picea abies L (Karst)), coated with transparent and semitransparent (with 3% pigment content) acrylic coatings during artificial UV light irradiation for 200 hours. Photo-degradation was evaluated in terms of colour changes througho...
M Deka, M Tomažic, M Petric


Construction of an ITS sequence database for the identification and classification of wood rot fungi
2007 - IRG/WP 07-10626
Developing a database that contains information about wood rot fungi is important in improving technologies about wood preservation as well as advances in understanding wood decay. On the other hand, with rapid spread of the Internet, establishment of a system for the swift precise access to information are required for the computerization of the research information. In the present study, genetic...
S Horisawa, Y Honda, S Itakura, S Doi


Genome-wide survey of cellulase related genes of white rot fungus,Pleurotus ostreatus
2007 - IRG/WP 07-10627
A white rot fungus, Pleurotus ostreatus, which is a important edible mushroom, has received much attention to apply to bioremediation and bioconversion because it has both cellulase and ligninase. To confirm copy number of cellulase-related genes encoded in P. ostreatus genome, we attempted to genomic Southern hybridization of P. ostreatus. The draft genome sequence and a large quantity of EST and...
T Tamenori, S Horisawa


White Rot in Eucalyptus Wood: Anatomical Changes and Density Variation by X-Ray Densitometry
2007 - IRG/WP 07-10631
Wood samples of the hybrid Eucalyptus grandis x urophylla attacked by white rot fungi were characterized. Microscopically, the colonization of the fungi was observed in the vessels and radial parenchyma, however the cell walls of the some fibers were attacked, indicating susceptibility to this fungi. Zone lines were observed as a result of interaction and compartmentalization of the fungi. Microsc...
M Tomazello Fo, S Brazolin, M P Chagas


Detection of Anti-Fungal Sapwood Extractives in Non-Durable Scots Pine (Pinus sylvestris), Rubberwood (Hevea brasiliensis) and Jelutong (Dyera costulata)
2007 - IRG/WP 07-10634
A general laboratory bioassay method of Woodward and Pearce (1985) was adopted to detect anti-fungal activity of sapwood or heartwood extractives of 5 Malaysian hardwoods [dark red meranti heartwood (Shorea spp.), red balau heartwood (Shorea spp.), kulim heartwood (Scorodocarpus borneensis), jelutong sapwood (Dyera costulata) and rubberwood sapwood (Hevea brasiliensis), including the temperate Pin...
A H H Wong, R B Pearce


Decay resistance of propionylated Iranian beech against the white rot fungus Tramets versicolor
2008 - IRG/WP 08-30449
In this study, the decay resistance of propionylated beech was investigated against the white rot fungus Trametes versicolor. Iranian beech (Fagus orientalis) was modified with propionic anhydride at different temperatures, concentrations and times without using any catalyst. Different weight percentage gains (WPGs) were obtained under different conditions. The decay resistance of the esterifed wo...
M R M Farahani, S M Hosseini


Soft Rot Determines Service Life of L-joints with Low Borate Loading
2008 - IRG/WP 08-30470
As part of a research program on the potential use of borates by the Canadian wood products industry, Forintek set up an L-joint test of untreated and borate-diffusion treated hem-fir (western hemlock and amabilis fir) in 1990. The treated material had a low initial retention of only 0.2% boric acid equivalent and analysis after 5 years revealed no detectable borate close to the tenon. Nev...
P I Morris, J Wang, J K Ingram


Effect of wood polymers degradation during heat treatment on extracellular enzymatic activities involved in beech degradation by Trametes versicolor
2008 - IRG/WP 08-40392
Effect of heat treatment on extracellular enzymes involved in wood degradation by Trametes versicolor was investigated. Heat-treated and untreated beech blocks were exposed to T. versicolor on malt agar medium and extracellular enzymatic activities investigated. A strong ABTS oxidizing activity has been detected during the first stage of colonization in both cases, while cellulase activities are m...
S Lekounougou, G Nguila Inari, M Pétrissans, S Dumarçay, J P Jacquot, E Gelhaye, P Gérardin


The susceptibility of hardwood plywood to white rot
2008 - IRG/WP 08-40397
The subject of the tests was resistance of veneer hardwood plywood to activity of pure culture of white rot fungus Trametes versicolor. The tested plywood was made with the use of the following glues: urea-formaldehyde (UF), melamine-urea-formaldehyde (MUF) or phenol-formaldehyde (FF). 4, 12 and 15 mm thick plywood was tested. External veneer of the plywood was mostly alder and the inner veneer (c...
A Fojutowski, A Kropacz


Heat treatment, thermal treatment, thermal degradation of wood, carbon nanotubes and Damascus steel swords. What do they all have in common?
2008 - IRG/WP 08-40399
Thermal degradation of wood is a well known phenomenon. Yet heat-treatment of wood can also provide protection for wood against certain environmental hazards. This paper explores some of the aspects of thermal degradation of wood fiber at relatively low temperatures with a surprising result. Carbon nanotubes (CNTs) were produced when a specific heating regime was used to carbonize the wood fiber. ...
Xinfeng Xie, B Goodell, Yuhui Qian, G Daniel


Effect of a biological treatment on below ground decay of Douglas-fir pole sections
2008 - IRG/WP 08-40433
The use of exogenous sugars to accelerate microbial growth and eventually limit available oxygen in soil surrounding wood in soil contact was investigated on untreated Douglas-fir poles exposed over a 3 year period in Western Oregon. Isolation frequencies differed markedly between treated and untreated poles and the treatment did appear to shift the frequency of some basidiomycetes. The treatment ...
C Freitag and J J Morrell


Effect of different ASAs (alkenyl succinic anhydrides) on the treatment of biological protection of wood in use class 4
2008 - IRG/WP 08-40440
The alkenyl suscinic anhydrides (ASAs) used in this work are adducts resulting from the maleinization reaction of fatty acid alkyl esters. Various products with different alkyl groups were synthesized from rapeseed (Brassica napus) oil esters, rich in oleic acid. The liquids obtained showed a viscosity similar to that of vegetable oils and a brown color. When applied into wood, a thermal treatment...
C Vaca-Garcia, O Pignolet


Antinomic natural self-protection mechanism in long-lasting woods: a case study with three tropical species from French Guiana
2009 - IRG/WP 09-10696
We demonstrate in this work through 3 examples that Amazonian trees may specialize long-lasting woods by means of at least to different approaches. Wallaba impregnates its wood with large amounts of weakly antifungal compounds acting in synergy, while tatajuba and louro vermelho woods are naturally impregnated with antifungal agents. Comparison of biological activities in vitro and concentrations ...
A Rodrigues, M Royer, N Amusant, J Beauchêne, G Herbette, V Eparvier, A Thibaut, L Salmen Espíndola, B Thibaut, D Stien


Effects of cold treatment on wood destroying fungi important in cultural heritage
2009 - IRG/WP 09-10706
The dry rot fungus Serpula lacrymans (Wulfen:Fr.) Schroeter is notorious in building environments for its vitality, destructive potential, and the huge costs associated with remediation of damage caused to wood of cultural heritage. Due to the potentially adverse of effects of chemical treatment methods such as have been attempted in the past, more benign physical methods of treatment, e.g. heat t...
M Lüdicke, W Unger, G Binker


Assessment of decay risk of airborne wood-decay fungi
2012 - IRG/WP 12-10787
The decay risk of airborne wood-decay fungi was investigated by using an air sampler. Japanese cedar disks measuring about 8 cm in diameter and 3 mm in thickness with moisture content at about 100 % were placed in a “BIOSAMP” air sampler and exposed to 1000 liters of air. Air sampling was carried out from June to September at the same sampling site in Tsukuba, Japan. The exposed disks were the...
I Momohara, Y Ota, K Sotome, T Nishimura


The resistance of thermo-oil modified wood against decay and mould fungi
2009 - IRG/WP 09-40448
Thermally modified wood in comparison to natural wood demonstrates some advantageous functional properties like decreased hygroscopicity, higher dimensional stability. It also has increased durability and improved resistance to fungal decay. However thermal modification of wood may lead to reduced strength properties what may limit the use of wood in mechanically beared constructions. The changes ...
A Fojutowski, A Kropacz, A Noskowiak


Glutathione transferases as functional biomarkers of wood degradation?
2010 - IRG/WP 10-10735
The recent release of several fungal genome sequences allows the report of an overview of fungal glutathione transferases (GSTs) focused on their function in the wood-degrading basidiomycete Phanerochaete chrysosporium. A genomic and phylogenetic analysis of GST classes in various sequenced fungi –zygomycetes, ascomycetes and basidiomycetes- revealed some specificity in GSTs distribution, in com...
E Gelhaye, M Morel


Decay Resistance of Maple (Acer Insigne) Wood Against White Rot
2010 - IRG/WP 10-10740
In this study, the decay resistance of maple (Acer insigne) in natural state and treated with ACC (Acid copper chromate) was investigated against the white rot fungus (Coriolus versicolor). ACC is a kind of water borne preservatives that was used in this study for treating specimens under vacuum and pressure (Bethell procedure) with 3 percent concentration. In conducting mentioned evaluation, koll...
V Tazakor Rezaei


Simulation and Investigation of Wood Degradation by Erosion Bacteria in Laboratory Experiments
2010 - IRG/WP 10-20431
A Microcosm experiment was successfully set up to establish, monitor and manipulate bacterial wood degradation under low oxygen conditions. Sound pine sticks were placed in waterlogged sediment from a heavily decayed pine pile foundation site in Amsterdam. The system was subject to different gassing treatment regimes in order to investigate the role of oxygen in the bacterial degradation process o...
J Gelbrich, E I Kretschmar, N Lamersdorf, H Militz


The Use of Micro-Tensile Testing to Assess Weathering Decay and Oxidative Degradation of Wooden Items
2010 - IRG/WP 10-20433
This paper presents a method to study the weathering performance of wooden items and to assess the oxidative degradation of wood via the Fenton reaction. Weathering resistance and photo-stability of wood was tested using pine wood (Pinus sylvestris) veneer strips measuring approximately 60 µm in thickness. The veneer strips were treated using a reactive chemical to impart surface protection. The ...
C Mai, Yanjun Xie, Zefang Xiao, P D Evans, H Militz


Degradation of Carbon-Based Preservatives by Black-stain Fungi
2010 - IRG/WP 10-30533
Some black-stain fungi are known to exhibit resistance to carbon-based preservatives. However, the cause of this resistance is unclear. The fungi may have mechanisms to tolerate these chemicals, or they may be able to degrade and detoxify them. Fungi capable of degrading carbon-based preservatives are of interest for possible bioremediation of carbon-based preservative-treated wood at the end of i...
R Stirling, P I Morris


A Comparison of the Performance of Related Copper Based Preservatives against Soft Rot
2010 - IRG/WP 10-30540
The performance of pine and beech wood treated with either a soluble copper + quat (ACQ type D) preservative system or a particulate copper + quat system was evaluated in unsterile soil using the European standard ENV 807 soft rot decay test procedure. In addition, to compare soft rot performance of soluble and particulate copper directly without the influence of co-biocides, beech and pine test...
M Ray, D Dickinson, K Archer


Biological degradation of acetylated wood after 18 years in ground contact and 10 years in marine water
2010 - IRG/WP 10-40522
This paper addresses the resistance to biological degradation of acetylated wood. Firstly, it presents results from an EN 252 test after 18 years’ exposure. The test is still running in Nordic NWPC test fields, Simlångsdalen in Sweden and Viikki in Finland. Results from this test were presented after 5 years’ exposure ( IRG/WP 97-30139), and showed that the resistance of acetylated wood wit...
P Larsson Brelid, M Westin


Wood protection by nano silver against white rot
2011 - IRG/WP 11-30554
This research was done with the aim of investigation on the natural durability of poplar (populous deltoides) in natural situation and treated with nano silver against the white rot. Testing samples was treated with the method of modified soaking and nano silver in 3 treating level of 0,200 and 400ppm. In this study effect of coriolus versicolor fungus (identificated as white rot) on populous del...
V Tazakor Rezai, A Usefi, M Soltani


Previous Page | Next Page