Soft rot fungi as possible sources of odor in impregnated wood in buildings
1993 - IRG/WP 93-20013
Wood preservatives are frequently used inside houses. In several cases impregnated wood, particularly when used in crawlspaces or other near-ground constructions, has been found to be a source of odor. Mold fungi, soft rot fungi actinomycetes or bacteria growing on impregnated wood are possible producers of the odor. Analyses of volatile emissions from impregnated wood with odor and pure cultures ...
J Bjurman, J Kristensson


Bioassays for rapid assessment of heavy metal toxicity in seawater
1998 - IRG/WP 98-50112
In evaluating the effect of CCA leachate on the establishment of fouling communities on wood exposed in the sea, three organisms were assessed as biological indicators of heavy metal toxicity. These were two macroalgae, Fucus serratus and Undaria pinnatifida. and the motile protist thraustochytrid, Schizochytrium aggregatum. The choice of these organisms for the tests carried out was based on the ...
C J Brown, R L Fletcher, R A Eaton


Modelling the control of decay in freshly felled pine poles
1997 - IRG/WP 97-10206
In a recent study investigating control of decay in freshly felled pine utility poles, it became apparent that the efficacy of different treatment methods was strongly related to the size of the material being treated. A topical application of 5% w/v disodium octaborate tetrahydrate (DOT), brush applied to the cut surfaces of logs with otherwise intact bark was just as effective at excluding white...
M W Schoeman, W Van der Werf, J F Webber, D J Dickinson


Ultrastructure of degraded, CCA-treated Pinus radiata wood from a marine pile
1990 - IRG/WP 1461
During an inspection of marine piles, 12 years after installation, severe degradation was noted on one of them in the vicinity of a corroded eye-bolt. The wood was dark brown in colour and tended to crumble easily. Wood fragments were examined by light microscopy and scanning and transmission electron microscopy and were also analysed for carbohydrates and lignin. Light microscopy showed numerous ...
A P Singh, M E Hedley


Investigation of microwave as a means of eradicating dry rot attack in buildings
1992 - IRG/WP 92-1545
A microwave-apparatus developed for treatment of building-structures infested by dry rot was tested in the laboratory. The test-conditions simulated treatment of either infested timber or infested brickwork. Sawdust samples, both wet and dry, infested by viable mycelium of Serpula lacrymans were packed in glass-tubes. The tubes were then placed in the middle of either 20 cm thick wooden beams or 3...
C Kjerulf-Jensen, A P Koch


Movement and persistence of Dazomet and pellected methylisothiocyanate in wrapped Douglas fir and southern pine timbers
1991 - IRG/WP 1496
The movement and persistence of Dazomet (tetrahydro-3,5-dimethyl-2 H-1,3,5 thiadiazine-6-thione) and pelleted methylisothiocyanate (MIT) was evaluated in wrapped Douglas-fir and Southern Pine timbers. MIT pellets did not impart a fungistatic effect to any of the timbers. Failure of MIT was probably due to loss of MIT from pellets prior to application. Fungistatic effect of Dazomet was consistently...
T L Highley


Development on Damage Functions of Wood Decay for Building Envelope Design
2005 - IRG/WP 05-10556
For the hygrothermal analyses of building envelope systems for insulation design, we tried a natural decay test of wetted wood specimens without any inoculation of fungi. Three principal experimental types: under steady-state conditions (Experiment A), at a cyclic water dripping under Non-steady conditions (Experiment B) and at a cyclic water dipping under-steady conditions (Experiment C), were ca...
H Suzuki, Y Kitadani, K Suzuki, A Iwamae, H Nagai


A Soil Bed Test of the Effect of CCA Penetration on the Performance of Hem-fir Plywood
2004 - IRG/WP 04-30332
An accelerated decay test was set up to compare the performance of CCA-treated Western hemlock/amabilis fir plywood treated to meet the preserved wood foundation (PWF) retention standard with various patterns of preservative penetration. Short lengths of treated plywood and comparable untreated material were installed in a soil bed. After eleven years of exposure, the CCA treatments were all sou...
P I Morris, J K Ingram


Long-term protection of stored lumber against mould, stain, and specifically decay: A comparative field test of fungicidal formulations
1984 - IRG/WP 3281
The problem of decay in packaged, unseasoned lumber stored for many months has become of major importance in recent years. Large financial claims have resulted from decay in Canadian lumber stored at length in seaports and storage yards of distributors. For decades acceptable protection from moulds and sapstain was readily achieved with chlorinated phenols applied at appropriate treating levels. H...
A J Cserjesi, A Byrne, E L Johnson


The evaluation of the occurrence of soft rot in creosoted wooden poles
1988 - IRG/WP 1368
The occurrence of soft rot decay in creosoted wooden poles for overhead power lines was investigated by collection of field samples, their subsequent microscopic examination and statistical analysis of the data collected. Examination of samples collected from 296 poles revealed that approximately 15% of the pole population studied (Eastern Electricity Board) showed the presence of soft rot decay. ...
A Wylde, D J Dickinson


Kinetic of the wood degradation produced by wood decay fung
1993 - IRG/WP 93-20016
The degradation degree of a wooden structure has a direct influence on its loss of mechanical strength. It's necessary to deepen in non destructive techniques which permit to extrapolate the results obtained in laboratory to structural timber used in the building's construction. This work studies the relationship existing between the pulse velocity of ultrasonic waves and the wei...
M T De Troya, A M Navarrete, A Sanchez, V Bucur


Screening of lignin peroxidase from white-rot fungi
1998 - IRG/WP 98-10274
Since lignin peroxidase was first found in the ligninolytic culture of Phanerochaete chrysosporium, it has been regarded as an enzyme responsible for the lignin biodegradation and studied comprehensively. As the results of these studies its unique characteristics have been revealed. On the other hand, the features of lignin peroxidase produced by other white-rot fungi have not been studied so much...
I Momohara


Bending creep test of plywoods under long term exposure to fungal attack
1981 - IRG/WP 2163
Bending creep test and decay test were coupled in order to evaluate the durability of structural plywoods and preservative efficacy. Experimental blocks, 5.0 x 1.2 cm² section x 35.0 cm length, were impregnated with distilled water and inoculated with mycelial fragments of test fungus. Polyethylene bags stretched with metal frame were used as decay chambers. The chambers containing inoculated blo...
M Takahashi


Premature decay of CCA-treated pine posts in horticultural soils - An overview
1984 - IRG/WP 1241
The recent discovery in New Zealand of early decay in CCA-treated pine posts set in horticultural soils led to the establishment of a comprehensive research programme. The objectives and outline of this programme are presented together with an overview of research progress to date. Results suggest that premature decay of CCA-treated timber is restricted to material placed in highly cultivated soil...
J A Butcher


High CCA retentions and the protection of eucalypt power poles
1983 - IRG/WP 3226
Tasmanian power pole material treated to high retentions, was analysed to accurately determine the amount of CCA preservative in the timber. Material from the same disc was subsequently exposed in unsterile soil in order to determine the effectiveness of treatment. Results showed that even at high retention levels, soft-rot attack was not prevented. Fourteen further poles were sampled, but this ti...
L E Leightley, J Norton


Soft rot tests
1983 - IRG/WP 2206
At the IRG meeting in Turkey it was proposed that developments in testing preservative-treated wood in unsterile soil according to techniques variously described as "fungus cellar", "soil-bed", or "accelerated field simulation" be considered along with conventional laboratory procedures as the basis for a standard test. Before formulating any co-operative test programme it is essential to examine ...
J A Butcher


The influence of gaseous oxygen concentration on fungal growth rates, biomass production and wood decay
1998 - IRG/WP 98-10283
The effects of air and several levels of oxygen balanced with nitrogen (% oxygen (v/v) nitrogen to 100%) on growth rates, biomass production and wood decay were investigated. The best technique for measuring daily growth rates in anaerobic jars was found to be by using 40 mm petri dishes which were attached to the walls of the jars. At the end of the test period the same petri dishes were also use...
S M Kazemi, D J Dickinson, R J Murphy


Biocontrol and bioprotection of wood decay and sapstain fungi
2003 - IRG/WP 03-10474
The most serious damages caused in the wood industries by decay and sapstain fungi, and the growing international pressures on the use of biocides products with toxic active ingredients harmful to human health and the environment, have made it necessary to search for alternative chemical products to protect the wood, and for the possibility to use micro-organisms as biological controllers. This la...
M T De Troya, F Rubio, M Villarreal, F Arenal, F Llinares, V Rubio, D Muñoz-Mingarro, N Acero


Summarized comparison of four techniques for detecting defects in poles
1979 - IRG/WP 2126
Since our discussions in open session of Working Group II at Peebles, a number of workers in Australia have collaborated in comparing the efficacy of X-ray, sonic testing, or resistivity measurements for detecting internal defects in poles. The purpose of this circular is to draw to your attention some of the results, in summary form. No attempt has been made to compare techniques. More detailed a...
H Greaves


Calculation of preformance index of Bardac 20 (an alkylammonium compound) evaluated in a field stake test
1982 - IRG/WP 3206
Bardac 20 treated stakes have been in test for three years at the Westham Island test site near Vancouver, B.C. The Performance Index for the preservative was calculated and found to be 0.009 which infers that, at the standard retention, Bardac 20 added 0.9 y to the life of the stake. It may be concluded that when tested using a standard field stake test using ponderosa pine (Pinus ponderosa Laws)...
J N R Ruddick


Natural durability of Iranian saxual wood (Haloxylon persicum) against the fungal decay
1991 - IRG/WP 1515
Haloxylon persicum is vidly planted in the deserfic region of Iran. At the present time, in the age of 30, these small trees are ready for cutting for the different uses, specially for rural buildings. But there's any knowledge about its durability. In this study the laboratory tests were carried out in accordance to European Standard. 5 fungi were used as: Trametes versicolor, Coniophora...
D Parsapajouh, F H Schweingruber, K Richter


Leachability And Decay Resistance of Copper-Treated Wood
2004 - IRG/WP 04-30337
Samples of scots pine sapwood (Pinus sylvestris L.) were treated with solutions of (Copper II sulfat-5 hydro + fluoroboric acid) and (Copper II sulfat-5 hydro + fluoroboric acid + boric acid) in order to determining to leachability and decay resistance against brown rot fungus (Postia placenta) and white rot fungus (Coriolus versicolor). Results indicated that the copper in treated wood is less s...
A Temiz, T Nilsson, I Deemirtas, Ü C Yildiz


Decay Resistance and Bonding Properties of Structural Flakeboard
2002 - IRG/WP 02-40233
Experimental structural flakeboard panels consisting of differing furnishes and resins were produced and tested for internal bond, linear expansion, thickness swell, and decay resistance. One group of panels was produced with recycled CCA-treated wood as the furnish and commercial phenol formaldehyde (PF) resin as the binder. Other groups of panels were produced with either mixed hardwoods or so...
T F Shupe, Chung-Yun Hse


The possible significance of the lignin content and lignin type on the performance of CCA-treated timber in ground contact
1988 - IRG/WP 1357
The lignin in wood samples of Alstonia scholaris, Octomeles sumatrana and a Simaruba species have been analysed. These timbers are characterised by a high lignin content and low syringyl:guaiacyl ratios. Decay tests with two soft rot fungi showed that the timbers were less susceptible than timbers with a low lignin content and higher syringyl:guaiacyl ratios. Numerous data for field performance of...
T Nilsson, J R Obst, G F Daniel


Wood decay of Pinus sylvestris L. by marine fungi
1990 - IRG/WP 1463
Waterlogged wood decay by marine microorganisms represents a major problem for the conservation of wood structures of historic value. It is important to know which kind of decay affects the wood from a conservation point of view. Enzyme activities of 14 marine fungi belonging to several localities were studied. Also, the weight loss and the rot type suffered by the wood at a microscopic level were...
M C Escorial, M T De Troya, J E Garcia de los Rios