The copper-transporting ATPase pump and its potential role in copper-tolerance
2016 - IRG/WP 16-10859
Copper-tolerant brown-rot decay fungi exploit intricate mechanisms to neutralize the efficacy of copper-containing preservative formulations. The production and accumulation of oxalate is the most widely recognized theory regarding the mechanism of copper-tolerance in these fungi. The role of oxalate, however, may be only one part of a series of necessary components required for this complex mecha...
K M Ohno, C A Clausen, F Green III, G Stanosz


Laboratory evaluations of woods from Pakistan and their extractives against Postia placenta and Trametes versicolor
2016 - M Mankowski, B Hassan, A Bishell, G Kirker
Natural durable wood species are those which exhibit innate tolerance to wood decay organisms such as fungi and termites. The goal of this study was to evaluate 4 wood species (Dalbergia sissoo, Cedrus deodara, Morus alba and Pinus roxburghii) from Pakistan in order to determine their resistance to both a model brown (Postia placenta) and white (Trametes versicolor) rot fungus compared to a durabl...
M Mankowski, B Hassan, A Bishell, G Kirker


High-frequency monitoring of mass loss due to brown rot degradation of modified wood
2016 - IRG/WP 16-10862
Fungi growing in liquid culture undergoes three separate phases in which they i) adapt to the new environment, ii) grow unrestrictedly and exponentially, and iii) are inhibited to increase in number/mass due to lack of nutrients etc. Filamentous fungi have been shown to exhibit similar growth phases in a solid food substrate and have been modelled to grow in this way also in solid wood. In modifie...
R Ringman, A Pilgård, K Richter


Susceptibility of wood substrates to Aurebasidium pullulans at different temperatures
2016 - IRG/WP 16-10863
There is an increasing awareness of how the aesthetical performance of wood exposed outdoors changes over time and especially in the first few years after installation. Mould and blue stain fungi are biological agents that contribute to the weather grey colour on a wooden façade, and the blue stain fungi Aureobasidium pullulans is commonly identified as colonizer on coated and uncoated wood expos...
L Ross Gobakken, G Alfredsen


Exudate production: a detoxification strategy of wood decaying fungi
2016 - IRG/WP 16-10868
Even often observed, the exudate production in fungi remains mainly unstudied. During growth on oak wood, the white-rot fungus Trametes versicolor produces droplets of a red-brown liquid, this phenomenom being observed with nine studied strains. One of these strains secretes a similar exudate on rich medium even in the absence of wood. This secretion seems to be linked to the formation of special...
A Deroy, J G Berrin, S Dumarçay, P Gérardin, A Kohler, D Navarro, C Rose, R Sormani, M Morel-Rouhier, E Gelhaye


Real-Time PCR Assays for the detection of the dry rot fungus Serpula lacrymans and its close relative Serpula himantioides
2016 - IRG/WP 16-10867
Prevention of wood decay by fungi of the phylum Basidiomycota is an important issue of wood protection. The most destructive fungus in buildings in Central Europe is the dry rot fungus Serpula lacrymans, which needs more extensive restauration measures than all other wood decay fungi. Its close relative S. himantioides occurs more frequently in outdoor environment. The assessment and remediation o...
K Jacobs, N Rangno


Identification of the key factors influencing development of the blue stain fungi
2016 - IRG/WP 16-10872
Service life of wood is more and more frequently affected by aesthetic requirements than functional ones. In order to elucidate various aspects of service life, model house with façade elements made of 22 materials was built on the field test site at Department of Wood Science and Technology in Ljubljana. Colour and fungal disfigurement is among other parameters monitored on this house. In parall...
D Kržišnik, B Lesar, N Thaler, M Humar


Selection of most aggressive test fungi for modified wood - Practical laboratory experience
2016 - IRG/WP 16-20579
One main objective of wood modification processes is the improvement of the durability against wood destroying organisms. Therefore, investigations of the resistance against wood destroying fungi have been one of the main focus within the last years. For the interpretation of the durability results, the selection of suitable test fungi is one of the main questions. A “wrong” fungus species may...
A Gellerich, S Bollmus


Wood biodeterioration monitoring using molecular fluorescence
2016 - IRG/WP 16-20589
Wood is an extremely complex and heterogeneous biological material, susceptible to biodeterioration by wood-destroying organisms. This process can be evaluated by natural resistance tests or non-destructive techniques, such as molecular fluorescence. The fluorescence of wood can be attributed to the presence of fluorophores groups or extractives, as a characteristic of some species. This study aim...
E Meneses Oliveira, A Florian da Costa, J W Batista Brag


Assessment of the biological durability of wood treated with organosilicon compounds
2016 - IRG/WP 16-30685
The European wood construction market is in need of environmentally friendly wood-based products whose service life meets the expectations of end users. Non-biocidal silicon-based water repellents, which can be applied to different materials, help minimize their vulnerability/susceptibility to liquid water. Consequently, they have the potential of increasing wood’s resistance against decay fungi...
M Kutnik, M Montibus, S Derocker, S Salivati, J-P Lecomte


Protection of bamboo against fungi by Laccase-Catalyzed Iodination
2016 - IRG/WP 16-30694
This paper investigated the effectiveness of bamboo treated by laccase-catalyzed oxidation of potassium iodide. Hence, the indoor and outdoor mold fungi resistances were carried out according to the AWPA (2007) Standard E24–06. According to the results, after 35days good resistances against the fungi were in the order of Trichoderma viride > Penicillium citrinum >Aspergillus niger. It was also o...
K P Nayebare, Shaoyong Zhang, Fangli Sun, B Goodell


Activity of wood preservatives against mould fungi
2016 - IRG/WP 16-30695
The resistance of experimental and commercial wood preservatives to mould fungi was determined using a method recommended by the Building Research Institute Instruction. The research of the inhibiting actions of the growth of fungi was carried out on the Scots pine wood Pinus sylvestris L. and beech Fagus sylvatica L. The most active compounds against mould were experimental herbicidal ionic li...
J Zabielska-Matejuk, A Stangierska


Effect of Nano-Silane on Permeability in MDF as a Result of Susceptibility to Moulds and Fungi
2016 - IRG/WP 16-40716
Effects were studied of vapor chamber on specific gas permeability of nanosilane-treated medium-density fiberboards (MDF). Size range of nanoparticles was 20 – 80 nm. Nano-silane (NS) was used at four consumption levels of 0, 50, 100, and 150 g/kg dry wood fibers. Density of all treatments was kept constant at 0.67 g/cm3. Specimens were kept for 18 weeks in vaporized chamber; their specific gas ...
H R Taghiyari, J Norton, A Moradiyan, M Sadegh Taher Tolou Del, H Siahposht, B Moradi-Malek, M Noferesti


Incorporation of raw boron minerals to protect particleboard against decay and mold fungi, termites and insects
2016 - IRG/WP 16-40729
This paper evaluated the biological performance of particleboards incorporated with the raw boron minerals ulexite and colemanite against decay, mold fungi, termites and insect larvae in comparison with that of particleboards with zinc borate, or boric acid plus a borax mixture. The results showed that ulexite and colemanite were highly effective against the decay fungi and termite attack in labor...
S N Kartal, E Terzi, P Gerardin, C M Ibanez, T Yoshimura


Superhydrophobic treatment of Norway spruce wood for improvement of its resistance against brown rot and moulds
2016 - IRG/WP 16-40734
Water repellence of wood can be increased and its some other properties influenced by introduction of hydrophobic chemicals into and on cell walls without affecting the wood’s bulk density due to lumen filling. Herein, a simple dipping method to insert octadecyltrichlorosilane (OTS) into cell walls and to deposit the self-assembled hydrophobic monolayers (SAMs) of OTS is reported. It was found o...
A Kumar, P Ryparová, P Hajek, B Kričej, M Pavlič, A S Škapin, M Šernek, J Tywoniak, J Žigon, M Petrič


Role of cell wall specific moisture content on the brown-rot fungal attack on wood
2016 - IRG/WP 16-40736
Wood is a hydroscopic resource because the cell wall polymers contain hydroxyl and other oxygen-containing groups that attract moisture through hydrogen bonding. Moisture content varies with changing moisture content in its environment. The moisture content in wood is responsible for many of the performance properties we observe. The strength properties of wood are dependent on the moisture con...
R M Rowell


Decontamination of sludges, liquids and soils polluted by “class 1, 2 & 3a” and “temporary” wood treatment products from dipping tanks
2016 - IRG/WP 16-50315
Wood is one of the most widely used building materials as it is easy to find and process. As an organic material, time leads to a degradation of its substance, and even more so when it is exposed to pathogens such as fungi, bacteria and insects. In order to try and inhibit this phenomenon, several preservation treatments have been developed and applied thanks to the production of chemical biocides...
A Zaremski, E Wozniak, S Maman, C Zaremski, S Morel


Effects of climatic factors and material properties on mould growth on untreated wooden claddings
2017 - IRG/WP 17-10884
Mould growth is an important contributor to colour change of untreated wood exposed outdoors. Predicting the development of mould growth is therefore important to ensure successful use of untreated wood as a façade material. More knowledge about the factors affecting mould growth on outdoor exposed wood is required to give better predictions. In this study, climatic factors and material propertie...
S Karlsen Lie, G I Vestøl, O Høibø, L Ross Gobakken


Monitoring of wood biodeterioration by infrared spectroscopy
2017 - IRG/WP 17-20607
The susceptibility of wood to deterioration by rotting fungi is intrinsically related to its chemical composition and the environmental conditions at its place of use, and if not detected in time, can cause enormous financial losses. The process of wood biodeterioration by decay fungi can be evaluated through laboratory accelerated test, in specific field tests, or through non-destructive techniqu...
E Meneses Oliveira, A Florian da Costa, J W Batista Braga


Bio-deterioration of Southern Pine Stakes at Geographically Different Testing Sites
2017 - IRG/WP 17-20609
Southern pine (SP) sapwood is commonly used in preparing the standardized stakes for performance testing as referenced in the American Wood Protection Association (AWPA) Book of Standards. For example, the standardized above ground test methods E16/E18 and the standardized ground contact test method E7 all use sapwood of SP as the preferred wood species for preservative performance test. In this...
Jun Zhang, J Horton


Monitoring Diversity and Colonization Patterns of Wood-Inhabiting Fungi Using Field Stake Tests
2017 - IRG/WP 17-20614
Advances in molecular identification of microbial communities enabling rapid microorganism determination have allowed ecological data to be increasingly incorporated into standardized wood performance tests. Combining standard field tests with molecular methods to study wood-associated microflora can help to better understand fungal colonization and decay processes of wood in service. The potentia...
P Torres-Andrade, J Cappellazzi, J J Morrell


Activity of Two Strobilurin Fungicides Against Three Species of Decay Fungi in Agar Plate Tests
2017 - IRG/WP 17-30704
The objective of this study was to examine the toxicity of strobilurin fungicides against wood decay fungi in order to assess their potential to act as a co-biocide for copper-based wood protection. Two strobilurin fungicides, Heritage (50% azoxystrobin active ingredient) and Insignia (20% pyraclostrobin active ingredients), and copper sulfate pentahydrate were tested against one white rot fungus...
J D Tang, T Ciaramitaro, M Tomaso-Peterson, S V Diehl


The Protective Effect of Different Tree Bark Extractives against Decay Fungi
2017 - IRG/WP 17-30707
There are various modification methods which increase the resistance of wooden materials. Due to recent environmental regulations, there is a need for new and environmentally-friendly wood preservatives. In this study, six different tree bark extractives were evaluated for their wood resistance against fungal degradation. For this purpose, the white rot fungi (Tramates versicolour) and brown rot f...
Ö Özgenç, S Durmaz


Liquefaction of woody waste: A novel approach in wood protection from CNSL based liquefied wood polyols
2017 - IRG/WP 17-30711
Liquefaction of lingo-cellulosic biomass is one of the thermo-chemical conversion processes for developing new materials, adhesives, preservatives and energy systems. The process also provides an opportunity to utilize waste wood such as saw-dust, woody wastes, branches and twigs for the development of value added products. Thus, this research paper deals with an investigation of antifungal and a...
A Kumar, G B.Nagarajappa, S Singh Chauhan


Bio-friendly wood protection systems - resistance to mould and blue-stain fungi
2017 - IRG/WP 17-30713
With stricter restrictions on the use of biocides and increasing environmental awareness there is a pronounced need for effective bio-friendly protection systems in the wood preservative and wood coating industry. One of the possible pathways is to exploit and utilize natural substances with active biological effects. Silanes, caffeine, natural oils and potassium carbonate were chosen as compounds...
L Ross Gobakken, W Perdoch, B Mazela, P Kwaśniewska-Sip, G Cofta