Removal of heavy metals from treated wood using biological methods
2005 - IRG/WP 05-50226
Heavy metals were removed from wood treated with copper based preservatives using brown-rot fungus Fomitopsis palustris. The amount of effective elements removed by treatment methods was examined. The relationship between oxalic acid concentration and the amount of heavy metals removed from each treated wood was also investigated. The relationship between fungus weight and removal rate was also in...
Dong-won Son, Dong-heub Lee


On the Influence of Wood Destroying Fungi on the Feeding Intensity of Termites
2017 - IRG/WP 17-10893
The baiting and feeding stimulating effect of wood attacked by fungal isolates of the species Coniophora, Lentinus, Poria and Gloeophyllum on termites Reticulitermes santonensis is examined. There are significant relationships between the activity of fungal isolates and the feeding behaviour of termites. The most active isolates can be used for increase the attractiveness of wood to wood-destroyin...
W Unger, T L Woods


Electronic noses for detection of rot in wood
1996 - IRG/WP 96-20098
In an ongoing project an electronic nose is being studied and developed for detection of volatile organic compounds (VOC) emitted from wood colonised and decayed by fungi. The electronic nose consists of an array of gas sensors with different selectivity patterns for different groups of volatile organic compounds (VOC). The use of pattern recognition routines implemented by artificial neural netwo...
K Nilsson


Potential toxicants for controlling soft rot in preservative treated hardwoods. Part 4: Evaluation of combined diffusion and toxicity
1979 - IRG/WP 2129
A large number of inorganic and organic preservatives were evaluated as potential soft rot control chemicals, by their degree of inhibition of fungal growth after allowing them to diffuse through a 6 mm thick wood slab. The tests were inoculated with wood powder from soft-rotted CCA treated poles. Pentachlorophenol was unable to diffuse quickly through the wood slab, although formulations with hex...
E W B Da Costa, O Collett


Degradation of the normal fibre walls of rubberwood (Hevea brasiliensis) by the tropical blue-stain fungus Botryodiplodia theobromae
1998 - IRG/WP 98-10286
Rubberwood was examined by light microscopy and transmission electron microscopy (TEM) after exposure to the common tropical sapstain fungus Botryodiplodia theobromae for four weeks to study hyphal colonisation of wood cells and to determine if this fungus also degraded lignified normal fibre cell walls in addition to the walls of non-lignified elements. Light microscopy revealed relatively large ...
A A H Wong, A P Singh


Fungi associated with groundline soft rot decay in copper/chrome/arsenic treated heartwood utility poles of Malaysian hardwoods
1992 - IRG/WP 92-1567
Copper-chrome-arsenic treated heartwood from Malaysian hardwood utility poles in service for 8-23 y at two localities in the wet tropical Peninsula Malaysia were surveyed for soft rot in the ground-contact region. Soft rot decay was detected in all the poles. Isolation studies indicated the ability of a variety of microfungi and basidiomycetes to colonize treated heartwood. Most isolates exhibited...
A H H Wong, R B Pearce, S C Watkinson


Decay patterns observed in butylene oxide modified ponderosa pine after exposure in unsterile soil
1982 - IRG/WP 3211
Small blocks of ponderosa pine (Pinus ponderosa Laws) chemically modified with butylene oxide to three different weight gains were exposed for 6 weeks in unsterile soil. Severe surface decay caused by soft rot fungi and tunnelling bacteria was observed in blocks with 8 weight percent gain. The soft rot attack was restricted to the outer parts of the radial walls in the latewood tracheids. Bacteria...
T Nilsson, R M Rowell


The use of image analysis to quantify soft rot decay
1992 - IRG/WP 92-2410
Image analysis techniques can provide quantitative information from visual images. As part of a wider interest in decay assessment methods we have investigated the application of image analysis techniques for quantifying soft rot decay by Chaetomium globosum in transverse sections of birch wood and bamboo. A method for reducing contamination of the section (and image) by the fungal hyphae and of s...
P J Wickens, R J Murphy


A new laboratory technique devised with the intention of determining whether, related to practical conditions, there should be a relationship between growth rate and decay capacity (of different strains) of Serpula lacrymans
1989 - IRG/WP 1384
Most laboratory techniques for the determination of growth rate not only use a medium (agar) unrelated to practice, but also yield values that are often far less than those found in practice. Also, most laboratory techniques for the determination of decay capacity ensure that the whole of a small test block becomes fully surface-colonised within the first few days; whereas in Australian practice S...
J D Thornton


Isolation of the dry rot fungus, Serpula lacrymans, from the forests of the Himalayan Foothills
1995 - IRG/WP 95-10129
Previous expeditions to the Himalayas (Singh 1993, 1994) have reported on the presence in this area of the dry rot fungus Serpula lacrymans. However, attempts to isolate the organism from material brought back from these expeditions were not successful. In this paper we report on the isolation of Serpula lacrymans from spores and cord material brought back from the Narkanda region of the Himalayas...
N A White, J W Palfreyman, J Singh, S Singh


The preliminary characterization of ß-1,4-xylanase of the brown-rot fungus Gloeophyllum trabeum
1990 - IRG/WP 1447
The extracellular ß-1,4-xylanase of the brown-rot fungus, Gloeophyllum trabeum, was isolated from crude extract by chromatofocusing method (PBE 94 column chromatography). The isoelectric point was estimated to 4.2-4.8 by cromatofocusing and 4.5 by isoelectric focusing (IEF). The molecular weight of the enzyme was estimated to 37,000 dalton by SDS-PAGE. The optimal temperature for the crude extrac...
A-C Ritschkoff, M Rättö, L Viikari


The use of the Pilodyn for detecting soft-rot decay in CCA treated eucalypt poles
1986 - IRG/WP 2251
A 6 Joule Pilodyn unit with 2.5 mm diameter pin was used to inspect CCA treated eucalypt poles, suspected of suffering groundline soft-rot decay. Pole plugs were removed at the inspection region and the amount of soft-rot decay present determined microscopically. High correlation (R² = 0.73) was obtained between the amount of soft-rot and Pilodyn pin penetration. The Pilodyn is recommended as a u...
L E Leightley, G A Willoughby


How to keep coated wood structures sufficiently dry to avoid damage caused by rot
1991 - IRG/WP 2376
During the last ten years, a new type of problems with wood rot has emerged in Scandinavia. Thousands of houses have been damaged by wood rot attaching to the exterior wood panel. This paper provides an overview of finished and ongoing work in order to identify the cause of these problems. In field tests, the moisture conditions were measured in panels coated with different paint systems. The infl...
S Hjort


Suppression of aerial hypha formation by spent culture filtrate of a non-degradative strain of Postia placenta
1991 - IRG/WP 1498
ME20, a wild-type monokaryotic strain of the brown-rot fungus Postia placenta, does not cause significant weight losses in standard soil-wood block decay tests and fails to form aerial hyphae in liquid and agar culture. This abnormal morphological feature may be caused by the same aberrant physiology that prevents the strain from degrading wood efficiently. ME20 releases elevated levels of the aut...
J A Micales


The Relationship of Fiber Cell Wall Ultrastructure to Soft Rot Decay in Kempas (Koompassia malaccensis) Heartwoo
2004 - IRG/WP 04-10541
The ultrastructure of fiber walls in kempas (koompassia malaccensis) heartwood was examined in relation to soft rot cavity formation. The fibers consisted of middle lamella and thick secondary wall. The secondary wall was differentiated in to a S1 layer, and a unique multi-lamellar S2 layer. Two distinct forms of lamellae were recognisable, one type being considerably thicker than the other. They ...
A P Singh, A H H Wong, Yoon Soo Kim, Seung-Gon Wi


The use of TCMTB in applications other than sapstain prevention: A review
1990 - IRG/WP 3606
The efficacy of TCMTB against staining fungi and surface moulds has been thoroughly investigated during the last decade. As a result, the chemical is used as an alternative to the chlorinated phenols in various parts of the world for the preservation of freshly sawn timber. Less known are the data obtained against brown rot, white rot and soft rot fungi. The termite repellent and bactericidal prop...
R Van der Eynde


Wood degradation mechanisms by the brown rot fungus Gloeophyllum trabeum
1997 - IRG/WP 97-10229
A mechanism for the degradation of wood by the brown rot fungus Gloeophyllum trabeum is outlined. The mechanism includes the function of redox-cycling, low molecular weight phenolic derivatives which sequester and reduce iron in acidic environments. The role of oxalate for the sequestration of iron (hydr)oxides and the pH dependent transfer of iron to the G. trabeum phenolic chelators, as well as ...
B Goodell, J Jellison


Positive dosage response of CCA in hardwood power poles to soft rot indicated from New South Wales soft rot survey dat
1983 - IRG/WP 3233
Experience and observation have shown that retentions of less than 16 kg/m³ in the sapwood of individual hardwood poles are unlikely to delay its deterioration sufficiently to ensure an economic performance in some instances. The higher retentions of current practice should do so subject to adequate inspection and maintenance. Increases in retentions requirements up to 35 kg/m³ more or less, dep...
A J Witheridge


Mapping soft rot decay distribution using image analysis
1993 - IRG/WP 93-20011
Image analysis has been shown to be a useful technique for the assessment of soft rot decay caused by Chaetomium globosum in birch and bamboo (Wickens and Murphy, 1992). The technique can permit assessment of decay in individual or small groups of cells and this has been used to undertake soft rot decay mapping in thin sections of bamboo. Assessments were made of the extent of soft rot decay with ...
P J Wickens, R J Murphy, G F M Watts


Effects of artificial UV weathering and soft rot decay on heat treated wood
2005 - IRG/WP 05-40302
Oil and inert gas oven heat treated pine wood strips 100 µm thick were mildly heat treated (200°C, 30 mins linseed oil, 120 mins oven). Following treatment, specimens were exposed to UV weathering (300 hours) and decay by the soft rot fungus, Chaetomium globosum. The effects of each treatment were assessed by zero span tensile testing, microscopy and by FTIR. Tensile testing of heat treated s...
M D C Hale, S C Ghosh, M J Spear


Relative performances of DNBP and CCA wood preservatives in accelerated decay tests
1988 - IRG/WP 3496
The effectiveness of 2-sec-butyl-4,6-dinitrophenol (DNBP) was compared with that of CCA. Test blocks of Pinus patula and Eucalyptus grandis were impregnated to precisely known retentions of approximately 3, 6, and 10 kg/m³ CCA and solvent-borne DNBP respectively. They were then challenged in decay tests comprising soil burial and exposure to monocultures of Chaetomium globosum, Coriolus versicolo...
W H Schnippenkoetter, L D Abraham, A A W Baecker


Movement and persistence of chloropicrin, Vapam, Dazomet and methylisothiocyanate in red and white oak timbers
1992 - IRG/WP 92-3728
This study describes the movement and persistence of four fumigants in sawn red and white oak timbers exposed out of ground contact for 2 years. Chloropicrin moved the furthest from the point of application, and was the most persistent. Vapam was next best, followed by Dazomet. Methylisothiocyanate (MIT), applied as pellets, was not effective, probably because MIT was lost from pellets prior to tr...
T L Highley


Iron in stone wool - one reason for the increased growth and decay capacity of Serpula lacrymans
1992 - IRG/WP 92-1537
The chemical compositions of stone wool and glass wool were analysed. There was more iron in the stone wool than in the glass wool. It was found that iron present in stone wool was easily dissolved by oxalic acid that Serpula lacrymans is able to produce. The stone wool promoted the decay of pine wood by Serpula lacrymans. The glass wool had no effect on the decay capacity of Serpula Iacrymans. Th...
L Paajanen, A-C Ritschkoff


Physiologic response of Phanerochaete chrysosporium to exposure to triazole fungicides
1994 - IRG/WP 94-10066
Triazoles are increasingly important fungicides which are employed for a variety of applications included wood protection. Several recent studies suggest that white rot fungi are more tolerant of triazole compounds than other wood degrading fungi. Cultural studies using a white rot fungus, Phanerochaete chrysosporium, and 0.2 or 0.8 ppm of tebuconazole or propiconazole suggested that mycelial dry ...
J J Morrell, R K Velicheti


Soft rot decay of Eucalyptus maculata Hook. in different soils from Queensland, Australia
1980 - IRG/WP 1113
In the present work, different Queensland soils were chosen and their gross effects on the decay of treated and untreated Eucalyptus maculata examined. The soils were also amended with various levels of phosphate to study the response of the wood decay mycota to an increasing supply of this nutrient. Phosphate amendment was chosen because of the wide-scale use of superphosphate on Queensland soils...
L E Leightley, I W Russell