The role of oxidation in wood degradation by brown-rot fung
1992 - IRG/WP 92-1562
Brown-rot fungi are suggested to degrade cellulose by oxidation with hydrogen radicalsformed eg. in the conversion of hydrogen peroxide in the Fenton type reactions. The stuctural changes in the holocellulose in wood induced by Fenton's reaction on wood components are very similar to those caused by brown-rot fungi. In this work the effect of the Fenton reaction on wood components was stu...
A-C Ritschkoff, J Pere, J Buchert, L Viikari


Identification of brown rot fungi on wood in above ground conditions by PCR, T-RFLP and sequencing
2004 - IRG/WP 04-10512
Fungi selected in test fields in Germany and Estonia and fungi (Coniophora puteana) cultivated on medium have been identified by the molecular methods PCR (Polymerase Chain Reaction), T-RFLP (Terminal Restricted Fragment Length Polymorphism) and sequenced to species level. The samples from the German field test showed that the fruit body sample was a different fungus than from the mycelium sample....
U Råberg, N Högberg, C J Land


Determination methods of phytotoxic effect of wood preservatives
1990 - IRG/WP 2349
The phytotoxic effect of wood preservatives so widely used plays a considerable role in the protection of natural environment. A review was made of the existing methods with which to assess the phytotoxicity of the above chemicals and some suggestions were given concerning the methods most appropriate for their unification. Two areas of research are proposed: 1) estimating the direct effect on ind...
A Kundzewicz, J Wazny


Sampling and analysis of NeXgen-treated timber
1998 - IRG/WP 98-20134
Green sawn timber surfaces of the softwood Caribbean pine and the hardwood white cheesewood were treated by dipping, spraying, and precise spiking with the antisapstain product NeXgen. After storing for either two hours or two weeks, the treated surfaces were sampled by one of four alternative protocols, which included two involving a square wad sampling punch (one hit or six hits), one involving ...
M J Kennedy, D E Ferlazzo, T L Woods, M H Freeman


Cytoplasmic and extracellular localization of manganese II dependent peroxidase(s) in white rot fungi during degradation of woody materials
1989 - IRG/WP 1416
The manner by which lignin is degraded in-situ in natural substrates by white rot fungi still remains a controversial issue particularly the distribution and role(s) played by lignin degrading enzymes (i.e. manganese II peroxidase and lignin peroxidase). In the present study, use was made of anti-manganese II peroxidase and immunolabelling techniques in conjunction with transmission electron micro...
G F Daniel, B Pettersson, T Nilsson, J Volc


Preliminary studies of the performance of iron chelators as inhibitors of brown rot (Coniophora puteana) attack
1996 - IRG/WP 96-10185
This paper describes experiments to examine the proposal that the presence of iron is essential for brown rot fungi to utilize hydroxyl radicals remote from the hyphae as a means of converting the wood into a food source. reliminary test results are presented from trials using three different iron chelators impregnated into Scots pine (Pinus sylvestris) sapwood blocks. Their relative effects on th...
E D Suttie, R J Orsler, P M Wood


Differences in pH, electrical resistance, cation composition and NIR spectra of red spruce wood during early stages of brown rot degradation
2002 - IRG/WP 02-10449
Red spruce sapwood was exposed to degradation by the brown rot fungi Coniophora puteana, Postia placenta, Gloeophyllum trabeum and Serpula lacrymans for 0, 1, 2 or 3 weeks using a modified soil block assay design. Average weight losses over time ranged from 0-8.9% during this time period. Detectable changes in pH, electrical resistance and cation compostion were observed in the wood as early as 1 ...
J Jellison, S Kelley, B Goodell, D Hui, A Ostrofsky


Synergistic combination of an antioxidant and wood preservative: a preliminary study
1998 - IRG/WP 98-30172
We previously proposed that extractives in highly durable angiosperm heartwood may protect wood against white-rot fungal colonization and subsequent degradation by a dual mechanism: extractives have some fungicidal activity and are also free radical scavengers (antioxidants) and thus interfere with the fungal free radical degradative mechanisms. We tested this hypothesis using the commercial bioci...
T Schultz, D D Nicholas, J Minn, K D McMurtrey, T H Fisher


Regulation of hyphal sheath formation iron-chelator production by the brown rot fungi Gloeophyllum trabeum and Postia placenta
1994 - IRG/WP 94-10074
Hyphal sheath formation and iron-chelator production by liquid cultures of the brown rot fungi Gloeophyllum trabeum and Postia placenta were monitored over time. The effects of incubation at various temperatures, pH's and concentrations of iron, manganese and nitrogen were determined. Hyphal sheath production was observed microscopically and quantified with JAVA video analysis. The hyphal...
Y Chen, J Jellison


The Effect on Biological and Moisture Resistance of Epichlorohydrin Chemically Modified Wood
2002 - IRG/WP 02-40224
Southern pine solid wood and fiber were chemically modified with epichlorohydrin to help in understanding the role of moisture in the mechanism of biological effectiveness of chemically modified wood. The solid wood had weight gains from 11% to 34%, while the fiber had weight gains from 9% to 75%. After modification, part of the specimens were water leached for 2 weeks or extracted for 2 hours ...
R E Ibach, B-G Lee


Microscopic analysis of southern pine utility pole core segments
1992 - IRG/WP 92-1542
Fifteen macroscopic core descriptive categories were evaluated by microscopic analysis for accuracy in detecting decay and judging decay severity. Five categories were good indicators of decay as decay was detected in 28 of 48 samples. Five categories were possible indicators of early decay as decay was detected in 6 of 40 core segments and an additional 18 contained hyphae. The remaining five cat...
S E Anagnost, C J K Wang, M Wright


Performance of Tuff Brite C™ and other formulations against blue-stain, mold and brown-stain in freshly-sawn rubberwood (Hevea brasiliensis) in the humid tropics of Peninsular Malaysia
1997 - IRG/WP 97-30163
The relative anti-sapstain and anti-mold efficacies, including brown-stain development in freshly-sawn rubberwood (Hevea brasiliensis) in the Malaysian tropics, between selected water-based product concentrations of formulations Tuff Brite CTM without/with added Borax (at 1.5/0, 1/1.5, 1.5/1.5 and 2%/1.5%), PQ8TM without/with added Borax (at 2.5/0, 1.5/1.5, 2/1.5 and 2.5%/1.5%) and NeXgenTM/NeX-Br...
A H H Wong, T L Woods


The Copper Tolerance of Mycelium vs. Spores for Two Brown Rot Fungi
2002 - IRG/WP 02-10422
The copper tolerance of two brown rot fungi, Gloeophyllum sepiarium and Oligoporus placentus, has been tested using both mycelia and basidiospores as inoculum sources. Mycelial growth of O. placentus on agar medium was shown to be much more tolerant to copper (as copper sulfate) than that of G. sepiarium. However, there was no difference in copper tolerance of basidiospores between the two specie...
S Choi, J N R Ruddick, P I Morris


Properties of cellulose degraded by the brown rot fungus, Postia placenta
1988 - IRG/WP 1350
To gain further understanding of the nature of the cellulose depolymerizing agent or agents of brown-rot fungi, brown-rotted cellulose was chemically and physically characterized. Various culture conditions, such as low nitrogen and elevated oxygen levels, did not induce degradation of cellulose by Postia placenta in liquid cultures. Therefore, brown-rotted cellulose for analysis was prepared by a...
T L Highley, R E Ibach, T K Kirk


Dimensional stabilization and decay resistance of wood treated with brown-rotted lignin and copper sulfate
1990 - IRG/WP 3608
The objective of this study was to evaluate the potential usefulness of brown-rotted lignin (BRL) as a dimensional stabilization and copper complexing agent for wood treatment. For dimensional stabilization, aqueous solutions of the lignin extract were combined with either copper sulfate, glyoxal or other additives. Anti-shrink efficiency (ASE) values as high as 42% were obtained with wood treated...
L Jin, D D Nicholas, T Schultz


Reduction of kiln brown stain in radiata pine lumber after log fumigation with methyl bromide
1997 - IRG/WP 97-30129
Methyl bromide fumigation of freshly felled radiata pine log sections effectively killed living cells in parenchyma to at least 75mm into sapwood. Lumber cut from logs (fumigated and control) stored 1 month outdoors (dry) showed slightly reduced brown stain when kiln dried at conventional temperatures. A more dramatic reduction and elimination of brown stain was noted in lumber cut from fumigated ...
E Schmidt, M E Hedley, D R Page, D Cross


Mechanistic aspects of the reactions of copper complexes with lignin in the presence of hydrogen peroxide and lipid hydroperoxide model compounds as proposed for white rot fungi
2001 - IRG/WP 01-10399
The structural principles and the oxidative reactions of the catalytic system consisting of copper, hydroperoxides, and copper coordination compounds that contain aromatic nitrogen atoms are similar to those of catalytic centers of oxidative enzymes involved in delignification reactions of white rot fungi. The system is capable of selectively degrading lignin and its low molecular weight would all...
K Fackler, P Lamaipis, E Srebotnik, M Humar, C Tavzes, F Pohleven, M Sentjurc, T Watanabe, K Messner


Fruitbody formation and basidiosporogenesis by the white rot fungus Pycnoporus cinnabarinus
1988 - IRG/WP 1348
Conditions for fruitbody formation by the white rot fungus Pycnoporus cinnabarinus in vitro were outlined. A marked difference in substrate requirements in comparison to previously tested brown rot fungi was revealed. Agar media containing Walseth cellulose and NH4 tartrate at 1 g/l permit profound production of basidiospores particularly at 15°C but only under light treatment. Higher NH4 tartrat...
J Bjurman


Extracellular hydrogen peroxide-producing and one-electron oxidation system of brown-rot fungi
1990 - IRG/WP 1445
Wood-component-degrading compounds involved in the initial degradation of the cellulose and lignin in wood were isolated from wood-containing culture of brown-rot fungi, Gloeophyllum trabeum and Tyromyces palustris and partially purified by gel filtration on Sephadex G-25 and DEAE-Sepharose ion-exchange chromatography. The compounds were glycoproteins. The molecular weights of the glycoproteins as...
A Enoki, S Yoshioka, H Tanaka, G Fuse


Growth of the copper tolerant brown rot fungus Antrodia vaillantii on different substrates
1995 - IRG/WP 95-10121
In recent years the copper tolerant brown rot fungus Antrodia vaillantii caused severe damages on impregnated wood in ground contact. The pattern of decay gave the impression that impregnated wood was even more severely attacked than unimpregnated. To investigate this question more closely laboratory tests were carried out. In a "choice test" Antrodia vaillantii grew preferably towards CC-impregna...
H Leithoff, I Stephan, M-T Lenz, R-D Peek


Targeted inhibition of wood decay fungi: degradation of cotton cellulose
1999 - IRG/WP 99-10321
Brown-rot decay is responsible for 80% of the damage and replacement of wood in service. For nearly thirty years, researchers have postulated a one-electron oxidase system combining Fe+2 oxalic acid, and H2O2 in the production of hydroxy radicals which ultimately oxidize cellulose in situ. Recently, researchers have been investigating antioxicants, in combination with biocides (Schultz, et al.,199...
F Green III, T A Kuster


Decay resistance of Siberian larch wood against brown rot fungus. - Part 3. The variation between plus trees and their grafted clones
2000 - IRG/WP 00-10350
The aim of the study was to estimate the variation in the decay resistance of Siberian larch (Larix sibirica Ledeb.) wood using mature plus trees and their grafted clones. Samples were collected with an increment core borer from 11 original plus trees and their 25-year-old grafted seed orchard clones. A typical brown rot fungus, Coniophora puteana (Schum. ex Fr.) Karst. (BAM Ebw. 15), was used as ...
H Viitanen, L Paajanen, M Venäläinen, A Harju, P Velling


The effect of a chelator mediated fenton system on activation of TMP fibres and decolorization of synthesized dyes
2004 - IRG/WP 04-50223
The purpose of this work is to improve our current knowledge of the non-enzymatic mechanisms involved in the brown rot degradation of wood, but also to study the potential applications of a chelator-mediated Fenton system in activation of wood fibers and decolorization of synthesized dyes. In this work, Electron Spin Resonance (ESR) spin-trapping techniques were used to study the generation of hyd...
Yuhui Qian, B Goodell, J Jellison


Natural durability of larch heartwood against decay
1997 - IRG/WP 97-10201
Larch heartwood has been promoted in Sweden and in other European countries as an alternative to preservative treated timber. It has even beeen stated that larch heartwood is more durable than preservative treated timber. This paper presents a compilation of facts from scientific reports on the durability of larch heartwood. Some recent data from this department are also reported. All data suggest...
T Nilsson


Solid state NMR study on pine wood degraded by brown rot fungus Gloeophyllum trabeum
1994 - IRG/WP 94-10067
Blocks of Pinus koraiensis wood were degraded by Gloeophyllum trabeum and examined by solid-state 13C NMR spectroscopy. Chemical compositions were estimated from relative signal aras. There was no evidence for preferential degradation of the noncrystalline cellulose which accounted for about 4% by weight of the wood. Loss of partly ordered cellulose on crystal surfaces exceeded the loss of crystal...
Yoon Soo Kim, R Newman