The effect of different concentrations of polesaver rods on the survival of selected decay fungi in liquid culture
1998 - IRG/WP 98-30166
An in-vitro method was developed to determine the effect of solutions of Polesaver Rods on the survival of selected decay fungi. Polesaver Rods are a diffusing preservative treatment containing fluorine and boron designed for the internal remedial treatment of power poles. Two white-rot fungi, Perenniporia tephropora and Trametes versicolor, and two brown-rot fungi, Polyporus verecundus and Gloeo...
M A Powell, T Deldot, C McEvoy


Commercial potential of the four-cycle method for the impregnation of green beech sleepers in Yugoslavia
1975 - IRG/WP 347
This paper was presented to the Conference on Wood Protection held in Sarajevo (Yugoslavia) in 1973. The paper was based partially on the report prepared by J. Struhar and G. F. Franciosi, who were appointed in 1972 as FAO consultants to demonstrate the new impregnation process for green beech sleepers in Yugoslavia. The so-called 4-cycle method was developed at the State Forest Research Institute...
N Vidovic


Laboratory evaluation of metallic naphthenates as wood preservatives
1991 - IRG/WP 3654
Fungicidal and termiticidal efficacy of copper and zinc naphthenates was appraised according to Japanese standardized laboratory testing methods. Copper and zinc naphthenates succeeded in protecting wood from decay fungi at retentions of 0.5 and 1.0 kg/m³ as metal, respectively. [JIS A 9302 (1976)] when they were applied to vacuum/soak impregnation [JIS A 9301 (1976)]. With respect to the fungici...
K Tsunoda, M Sakurai


Influencia de la impregnación con soluciones tánicas en la estabilidad dimensional de la madera de Pinus pinaster Ait. procedente de España
1992 - IRG/WP 92-3686
En virtud de la importancia que presenta la madera de Pinus pinaster Ait. en el sector constructivo español, se ha sometido a esta a tratamientos en autoclave con distintas soluciones tánicas naturales y artificiales a fin de estudiar su incidencia en la estabilidad dimensional frente a exposiciones exteriores. En el estudio se pone de manifiesto el efecto creado por el tratamiento protector en ...
J A Rodríguez Barreal, J Cubillo Jordan de Urries, L Garcia Esteban


The influence of copper (II) chemicals on the weathering of treated wood. Part 1: ACQ treatment of wood on its weathering
1994 - IRG/WP 94-30040
Wood weathering can be accelerated by alkylammonium compound (AAC) treatment, and slowed by ammoniacal copper quat (ACQ) treatment. This study aims at investigating the influence of ACQ treatment of wood, especially the present of copper (II), on its weathering. ACQ, CCA and DDAC treated microtomed sections of southern yellow pine earlywood were prepared and naturally weathered for five periods, t...
Ruiying Liu, J N R Ruddick, L Jin


Thermal modification of non-durable wood species 1. The PLATO technology: thermal modification of wood
1998 - IRG/WP 98-40123
The PLATO technology is an innovative upgrading technology with low environmental impact, which can be applied to fast grown and non-durable wood species. This technology is based on a thermal modification of solid wood without the addition of chemicals (e.g. preservatives), consisting of a hydrothermal treatment, followed by drying and curing. The PLATO technology results in a substantial improve...
M J Boonstra, B F Tjeerdsma, H A C Groeneveld


Fumigant movement in Canadian wood species
1984 - IRG/WP 3296
Pole sections prepared from seven Canadian wood species (Thuja plicata, Thuja occidentalis, Pinus contorta, Pinus resinosa, Pinus banksiana, Pseudotsuga menziesii, southern yellow pine) were fumigated with chloropicrin, methylisothiocyanate and Vapam and the rates of fumigant penetration determined. All three fumigants were applied directly into holes bored radially into the pole sections. Analysi...
J N R Ruddick


Improvements of stability and durability of beechwood (Fagus sylvatica) by means of treatment with acetic anhydride
1991 - IRG/WP 3645
In the present investigations, beechwood (Fagus sylvatica) was treated with non-catalysed acetic anhydrid at 120°C and some physical- and biological parameters of the treated wood were compared with those of non-treated wood. The radial and tangential shrinkage and swelling, respectively, and the absorption capacity of the acetylated wood against moisture is considerably lower. The durability aga...
H Militz


Determination of total fluoride and boron in preservative-treated wood fluoride by ion selective electrode without steam distillation, and boron colorimetrically using azornethine-h
1998 - IRG/WP 98-20135
An analytical method was developed to determine total fluoride and boron in wood treated with aqueous or solid diffusing fluoride or borate-fluoride formulations. Ground wood was mixed with 30% sodium hydroxide solution and oven-dried for 2 hours before furnacing at 600° C for 1 hour. The cool fused product was dissolved in hot water, transferred to a plastic beaker and neutralised. Fluoride was ...
P A Collins, M J Kennedy


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 1: Treatment of reference samples
1977 - IRG/WP 426
It was agreed in Wildhaus on 15 May 1976 that preparations for the test detailed in Document No: IRG/WP/414 should commence immediately, but that initially only two water-borne preservatives should be used - a copper/chrome/arsenic (CCA) and a copper/chrome/boron (CCB) formulation respectively. PRL, England (R Cockcroft) would be responsible for supplying samples of the reference timbers treated w...
R Cockcroft, T B Dearling, W O Schulz, H V Borck


Preliminary results of the treatment of wood with chlorosilanes
1981 - IRG/WP 3172
It is clear from the initial data reported here that the treatment of pine sapwood with chlorosilanes under the reaction conditions employed did not significantly reduce the decay by both white rot and brown rot fungi. Only the dichlorosilane compounds showed to possess some protective action against fungal attack. Before drawing conclusions on the application of organosilicon compounds as potenti...
M Stevens


Is there a need for re-sealing cut ends of envelope-treated softwood framing timber to protect against attack from Coptotermes spp. (Isoptera)?
2004 - IRG/WP 04-10524
The claim that Australian Coptotermes acinaciformis (Froggatt) do not appear to initiate attack on timber from the end grain, thereby negating the need for treating exposed cut ends of softwood framing material (35 x 90mm) which has a Tanalith™ T envelope, was investigated. Specimens of commercial Pinus radiata framing timber (untreated) and Pinus elliottii (untreated, envelope-treated) were pa...
M Lenz, J W Creffield, S Runko


In situ timber treatments by spraying. Distribution of preservative in wood
1991 - IRG/WP 3678
This study was carried out in order to make the Pest Control Operators able to achieve correct treatments and enhance their efficacy. It was carried out in two steps: 1) in laboratory, to learn the influence of various parameters like spraying pressure, use of repeated applications, distance from nozzle to wood; 2) in situ on roof timber of five buildings. In this case, the applications of the pre...
C Defoin, G Dupont, M Lamour, H Sageot, M-M Serment


Bending & tensile properties of vapor boron-treated composites
2002 - IRG/WP 02-40228
North American composites including laminated veneer lumber, oriented strandboard, and medium density fiberboard were treated by vapor boron technology and subsequently tested in static bending. Tensile properties were also determined for the two composite boards. The study was designed as 3 x 2 factorial with three treatment levels and two mill locations for each composite type. In general, mil...
H M Barnes, R J Murphy, B K Via


Comparison of the effects of borate, germanate and tellurate on fungal growth and wood decay
1992 - IRG/WP 92-1533
The tetra-hydroxy borate ion is known to undergo complexation with polyols and has been shown to inhibit dehydrogenase enzymes in this way. It has been previously suggested that this complexation is responsible for the inhibition of fungal growth and the protection of boron treated timber. Other ions that have the ability to complex with polyols have also been shown to inhibit dehydrogenase activi...
J D Lloyd, D J Dickinson


Technical viability of deltamethrin as a pre-treatment wood preservative
1993 - IRG/WP 93-30012
This paper presents the results of tests conducted on freshly-cut logs and lumber during the seasoning period to verify the effectiveness of Deltamethrin on insect control. The tests were carried out in Quedas do Iguaçú, Paraná (southern region of Brazil) and Breves, Pará (northern region of Brazil) during the-dry and rainy seasons, and used different species of wood and insecticide/fungicide ...
A M F Oliveira, S Milano, J L A Bahia, F Teleginski


Treatment details for the field experiment to determine the performance of preservative treated hardwoods with particlar reference to soft rot
1977 - IRG/WP 384
These notes are compiled to complement and supplement Document No: IRG/WP/367 which described the plan for the treatment of the stakes, using a CCA preservative, for the field experiment. This document gives extra details of the treatment characteristics of the different timber species and as such may give IRG members useful information on the sapwood permeability of a range of hardwoods. The repo...
F W Brooks, M R Gayles


Inorganic preservatives in wood dust - Cause of nasal cancer?
1997 - IRG/WP 97-50085
Since 1985 dust particles from beech and oak trees have been classified by the Senate Commission of the German Research Council (DFG) as being ,,working materials which are definitely carcinogenic to humans". All other wood dusts, including those from softwoods, are classified as being materials ,,with reasonable suspicion of carcinogenic potential". The carcinogenic principle of action continues ...
A O Rapp, K Brandt, R-D Peek, U Schmitt


Leaching characteristics, decay and termite resistance of treated wood with boron compounds, N'-N-(1,8-Naphthalyl) hydroxylamine (NHA-Na), and hydroxynaphthalimide (NHA-H)
2003 - IRG/WP 03-30307
Despite many advantages of boron wood preservatives, boron itself does not adequately protect wood in ground contact and exterior applications because its natural diffusibility and susceptibility to leaching. As a result of previous studies to limit or decrease boron leaching, several fixation systems have been developed. In this study, we evaluated the effects of N'-N-(1, 8-Naphthalyl) h...
S N Kartal, Y Imamura


Selective chromate elimination from the storage-drainage-water of a wood impregnation plant
1980 - IRG/WP 3153
With the Enviro-Chrom-Ex process it is possible to eliminate ecologically and economically hexavalent chromium (chromate) from water selectively. The process which is based on the principle of selective ion exchange works with different chromate concentrations and under the presence of other ions, irrespective of the water hardness. The values of water-offtake reach 0.1 mg CrVI at maximum, causing...
O Wälchli, R Ott, R Hugener, E Graf, B Lieberherr


Relative performance of copper/chrome/boron (CCB) and copper/chrome/arsenate (CCA) in ground contact
1992 - IRG/WP 92-3694
The performance of four retentions each of an oxide CCA formulation and a salt formulation of CCB in radiata pine and European beech was compared after 18 years' field exposure. In radiata pine CCA oxide was more effective (4 failures out of 40) than CCB (9 failures out of 40). However, in European beech CCB was substantially more effective (22 failures) than CCA oxide (all failed). Analy...
M E Hedley


Strength properties of preservative treated pine and spruce wood after super-heated steaming
1984 - IRG/WP 3313
Possible changes of strength properties of CCF pressure impregnated pine and spruce with subsequent steaming at 110°C respective 120°C for 30 min were examined. For spruce analysis of variance indicated that none of the processes had a significant effect on bending strength, compression strength and the corresponding modulus of elasticity as well as on impact bending strength and shear strength ...
R-D Peek


Efficiency of wood impregnation processes
1980 - IRG/WP 3151
Many wood impregnation processes have been in use for a very long time, up to 150 years, but they have not been progressively modified. This paper considers impregnation processes in relation to current requirements, particularly impregnation efficiency and energy consumption. The term 'pore' is used throughout in its physical sense and is not confined to botanical 'pore...
B A Richardson


Interim report on the use of borate rods for the in-situ treatment of joinery
1980 - IRG/WP 3159
In the U.K. in recent years, it has been recognised that there is a major need for in-situ treatment of joinery at risk from or showing the early signs of decay. Several techniques have been developed to provide such a treatment, one of which is based on the insertion of anhydrous borate glass rods. The tests in hand are long term and this report is confined to the mycological isolation data from ...
D J Dickinson


Observations on the performance of copper-based wood preservatives in fungal cellar (soil-bed) tests
1994 - IRG/WP 94-20047
Fungal cellar (soil-bed) tests are considered to be an important tool for the evaluation of the performance of ground contact wood preservatives. Facilities of this type have been established world wide although caution has been exercised in their introduction into standard testing methods for the approval of wood preservatives. This is the result of concerns over the variability in the biological...
G R Williams, D Rudolph, M E Hedley, J A Drysdale, R F Fox


Previous Page | Next Page