Development of methodologies to evaluate tanning blocking coatings
2016 - IRG/WP 16-40760
In Europe an increased interest in using home-grown hardwoods as sustainable and renewable construction materials started a few years ago. Amongst these species oak and chestnut are two interesting candidates as their heartwood contain a significant amount of tannins which contribute to their natural durability. To avoid wood greying and dimensional variations, oak and chestnut must be protected b...
C Reynaud, L Podgorski


Effects of climatic factors and material properties on mould growth on untreated wooden claddings
2017 - IRG/WP 17-10884
Mould growth is an important contributor to colour change of untreated wood exposed outdoors. Predicting the development of mould growth is therefore important to ensure successful use of untreated wood as a façade material. More knowledge about the factors affecting mould growth on outdoor exposed wood is required to give better predictions. In this study, climatic factors and material propertie...
S Karlsen Lie, G I Vestøl, O Høibø, L Ross Gobakken


Fungal growth on coated wood exposed outdoors: influence of coating pigmentation, cardinal direction and inclination of wood surfaces
2017 - IRG/WP 17-10896
The objective of the SERVOWOOD project was to develop and establish European Standards that will facilitate the prediction of service life for exterior wood coatings. One of the objective of this project was to study fungal growth of the field exposed panels. Two coatings applied in 2 and 3 coats were exposed for one year outdoors at 45° south: one solventborne (alkyd based) and one waterborne (a...
L Podgorski, C Reynaud, M Montibus


Bio-friendly wood protection systems - resistance to mould and blue-stain fungi
2017 - IRG/WP 17-30713
With stricter restrictions on the use of biocides and increasing environmental awareness there is a pronounced need for effective bio-friendly protection systems in the wood preservative and wood coating industry. One of the possible pathways is to exploit and utilize natural substances with active biological effects. Silanes, caffeine, natural oils and potassium carbonate were chosen as compounds...
L Ross Gobakken, W Perdoch, B Mazela, P Kwaśniewska-Sip, G Cofta


Bacterial adhesion to selected wood finishes
2017 - IRG/WP 17-40793
A new generation of furniture, including antibacterial surfaces, should adjust to the changing needs of an ageing population. Respectively, determination of bacterial adhesion on wooden surfaces, finished with various wood finishes or coating is an important topic. The main aims of our work were of a preliminary character. We wanted to state if the existing methods for testing of bacterial adhesio...
M Petrič, D Kekec, J Žigon, K Godič Torkar, K Bohinc


Plasma-assisted bleaching of blue-stain from lodgepole pine wood
2017 - IRG/WP 17-40799
We hypothesize that plasma will etch wood and fungal hyphae in blue-stained lodgepole pine, and increase the ability of hypochlorite bleach to remove discolouration from blue-stained wood. Blue-stained lodgepole pine wood was exposed to a glow-discharge plasma derived from water, and the surface wettability, permeability and colour of the treated wood was measured. Plasma-treated wood was dipped i...
A Jamali, P D Evans


Bio-preservative properties of technical lignins from South African pulp mills: An investigation towards a conceptualized development of natural compound-based wood preservatives
2018 - IRG/WP 18-30724
The depletion of naturally durable timber and the risk posed by some of the conventional wood preservatives to human health and the environment continue to drive research efforts towards developing new formulations that are benign. Furthermore, the global concept of environmental sustainability aims at optimal use of resources and to comprehensively include conversion of waste to value added produ...
A Alade, L Tyhoda, M Meincken


Visual appearance of unpainted wooden claddings during the first year of outdoor exposure: Evaluation of surface mould growth, lightness (L*) and wasp attack
2018 - IRG/WP 18-40841
This study addresses changes in visual appearance of unpainted wood materials exposed outdoors. Specimens of Norway spruce (Picea abies) Scots pine (Pinus sylvestris), aspen (Populus tremula), acetylated Radiata pine (Pinus radiata) and DMDHEU-modified Scots pine sapwood were exposed facing south in Ås, Norway for 60 weeks. During this period, surface mould growth development and wasp attack were...
S Karlsen Lie, L Ross Gobakken, G I Vestøl, O Høibø


Performance of a water-borne stain on beech, spruce, MDF and OSB improved by plasma pre-treatment
2020 - IRG/WP 20-40897
Coatings are an important part of wood protection, especially for outdoor applications. In order to provide a good protection, protective coatings need to exhibit good adhesion, mechanical resistance, and weathering resistance. Plasma pre-treatments are an established method to increase the performance of existing coatings including those on wood and wood-based substrates. Moreover, plasma deposit...
S Dahle, J Žigon, I Uranjek, M Petrič


Influence of weathering of wood surfaces before and after treatment with iron(II) sulphate
2023 - IRG/WP 23-30786
Outdoor wood is exposed to various factors that cause the wood to grey or age. The ageing processes can vary greatly depending on the exposure. Parts of the wood that are not exposed to external factors, e.g. under the eaves, are less exposed and the ageing process is therefore slower. This can be accelerated by solutions based on iron ions. In this way, the wood greys quickly and evenly. However,...
B Lesar, M Humar, F Osvald


Fungicidal properties of black liquor from the waste MDF board digestion in terms of wood protection
2023 - IRG/WP 23-50379
The aim of the work was to determine the fungicidal properties of black liquor as a product of the chemical digestion of waste MDF board. The resistance of wood treated with black liquor from MDF waste pulping process was compared with the resistance of wood treated with black liquor from the pulping process of a by-product from agricultural production. The control material consisted of non-treate...
B Mazela, W Perdoch, A Szulc, I Sieminska


The durability and mechanical properties of 40 years old Black locust poles
2024 - IRG/WP 24-11042
This study investigates the durability and mechanical properties of 40-year-old black locust (Robinia pseudoacacia) poles harvested from a vineyard in Slovenia. Wood from these poles was compared to recently harvested black locust wood to determine possible reuse options. Visual inspection, hyperspectral imaging, and laboratory tests were conducted to assess decay, density, mechanical properties, ...
M Humar, J Malik, J Levanic, D Krzisnik, E Kerzic, B Lesar