Your search resulted in 879 documents. Displaying 25 entries per page.


The Effects of Natural Weathering on the Properties of Heat Treated Alder Wood
2010 - IRG/WP 10-40484
Heat treatment is an effective method to improve the dimensional stability and biological durability of wood. The heat treatment technology and the heat treated wood products were recently introduced to Turkey. However, only a few studies have been reported on the effect of natural weathering on the properties of heat treated wood in both Turkey and the world. In this study, heat treated alder (Al...
S Yildiz, Ü C Yildiz, E D Tomak


Development of markers to predict decay durability of heat treated wood
2010 - IRG/WP 10-40496
Effect of heat treatment temperature on elemental composition of Scots pine sapwood (Pinus sylvestris) has been investigated in the range of temperatures between 220 and 250°C. Results revealed an important increase of carbon content, while oxygen content significantly decreases. Independently of the heat treatment temperature, elemental composition is strongly correlated with the mass losses due...
Ž Šušteršic, A Mohareb, M Chaouch, M Pétrissans, M Petric, P Gérardin


TMT–Interlab–Test to establish suitable quality control techniques - Structure and first results
2010 - IRG/WP 10-40503
As a result of growing quality demands from manufacturers and end-consumers of thermally modified timber (TMT) recent scientific research activities are increasingly focussed on modification mechanisms and by this on the development of suitable quality control methods. To deepen the knowledge in modification mechanisms and to obtain a larger variety of scientific data for TMT depending on the trea...
C R Welzbacher


Durability of heat treated Malaysian bamboo Gigantochloa scortechinii strips
2010 - IRG/WP 10-40514
Bamboo is one of the fastest growing plants and can be used for various products. In tropical countries such as Malaysia bamboo is abundantly available at reasonable prices, therefore it is used for numerous purposes. However, bamboo (as a lignocellulosic material) is susceptible to fungal and insect attack and it is difficult to protect by preservative treatment. Heat treatment is an option to im...
N Kamarudin, K Sugiyanto


Impact of wood species on the performance of exterior wood coatings
2010 - IRG/WP 10-40519
To prolong the service life of a wooden construction the protective function of a coating is of utmost importance. The chemical composition as well as the wood-coating interface affects the performance of this protective layer and obviously wood species have an impact too. This paper discusses the influence of wood species on the overall coating performance. Therefore, a range of opaque waterborne...
I De Windt, J Van den Bulcke, J Van Acker


Moisture dynamics of WPC as basis for biological durability
2010 - IRG/WP 10-40520
The largest market for wood-polymer composites (WPCs) is currently decking. Although many products are commercially available, a proper standard for the assessment of the biological durability of WPC does not exist. Recommended standards for testing resistance against basidiomycetes should be completed with a method to bring the specimens in a worst case situation, obtaining a moisture level high ...
N Defoirdt, J Van Acker, J Van den Bulcke


Biological degradation of acetylated wood after 18 years in ground contact and 10 years in marine water
2010 - IRG/WP 10-40522
This paper addresses the resistance to biological degradation of acetylated wood. Firstly, it presents results from an EN 252 test after 18 years’ exposure. The test is still running in Nordic NWPC test fields, Simlångsdalen in Sweden and Viikki in Finland. Results from this test were presented after 5 years’ exposure ( IRG/WP 97-30139), and showed that the resistance of acetylated wood wit...
P Larsson Brelid, M Westin


Effect of borax-boric acid Treatment of simul (Bombax ceiba) Veneers on Glue-Bond Quality of Plywood
2010 - IRG/WP 10-40525
The glue-bond quality of plywood made of treated simul (Bombax ceiba) veneers was investigated. The veneers were treated with cold and hot water solution of borax-boric acid (BB) of different concentrations and treatment durations. The plywoods were made at three different pressures in hot press using urea formaldehyde glue. The glue-bond strength of untreated plywood in dry shear-test was found t...
K Akhter, Md Abul Hashem, S Akhter


Effect of Coatings on the Durability of Birch and Spruce Plywood. Part 2: Biological Durability
2010 - IRG/WP 10-40527
Several different coated birch and spruce plywood types were investigated in Finland using the combination of outdoor weathering and decay test EN 12038. The most important factor to affect on the biological performance of birch plywood, coated and uncoated, was edge sealing. For spruce plywood edge sealing had a smaller effect. However, in spite of positive effect against decay, edge sealing did ...
A Nurmi, H Viitanen


Preservative Treatment of simul (Bombax ceiba) Veneers with Hot and Cold Water Solution of borax-boric acid by Soaking Process
2010 - IRG/WP 10-40528
Veneers of simul (Bombax ceiba) were treated with different concentrations of water- borne preservatives borax-boric acid (BB) by soaking process for different time periods. In the case of hot water treatment, it was found that the average retention of preservative chemicals increased gradually with the increasing treatment period from 20 minutes to 60 minutes. Similar trend was observed in the ca...
K Akhter, Md Abul Hashem, S Akhter


Effect of Nano-Silver Treatment on Densified Wood Properties. Part One: Swelling, Recovery Set, Bending Strength
2010 - IRG/WP 10-40533
In this research the effect of Nano-Silver treatment on compressed wood properties, was studied. Wood specimens were cut from Popolus alba (poplar) and impregnated with Nano-Silver and water. Then the saturated samples were compressed through radial direction in a hot press under pressure of 6 MPa, for 1 and 4 hours. The temperatures of press were 150°C and 175°C. Swelling (24h), recovery set ...
G Rassam, H Reza Taghiyari, B Jamnani, M Ali Khaje


Biological resistance of acetylated particleboards exposed to white (Trametes versicolor (and brown (Coniophora puteana) rot fungi
2010 - IRG/WP 10-40534
This research was conducted to investigate the effect of acetylation on bioresistance of particleboard produced from acetylated wood chips of Fagus orientalis exposed to white (Trametes versicolor (and brown (Coniophora puteana) rot fungi. After 12 hours soaking in acetic anhydride, in order to achieve three level of weight gains, 5, 9 and 16%, acetylated particles were heated in an oven at 120 c...
M Ghorbani kokandeh, K Doosthoseini, A N Karimi, B Mohebby, H Asghari


Deterioration of wooden heritage in outdoor exposure in Romania
2010 - IRG/WP 10-40535
The paper contains a study of the deterioration of wooden heritage in Romania, in outdoor exposure. Romania belongs to the few countries having a rich heritage of this kind. A quantitative image of this heritage reveals the 1,350 objectives transferred and reconstructed in 16 open-air museums, over 1,500 wooden churches, more than 4,000 buildings and technical facilities, historical monuments ...
L Bucşa, C Bucşa


Comparative Study of Heat Treatment of Beech Wood in Hot Water and Steam Medium
2010 - IRG/WP 10-40536
Heat treatment of wood is an effective method to improve the dimensional stability and durability against biodegradation. Heat treatments of beech wood in 2 different mediums (hot water and steam) in 180ºC were compared in physical, mechanical and anatomical properties. Mass loss in hydrothermally treated wood was higher than hygrothermally treated samples. Mechanical properties (MOR, MOE and CS)...
A Talaei, K Yaghoobi, A N Karimi


Combined Effect of Boric Acid and Waste Oil Treatment on Boron Leaching
2010 - IRG/WP 10-50268
In this study it was aimed to investigate the boron leaching amounts in Scots pine wood samples treated with boric acid (BA) and waste oil (WO) alone or by dual treatment. The level of water absorption and water repellent efficiency were determined with cyclical wetting tests, total of 336 hours. Wood samples that have both covered and uncovered transversal section were impregnated with 3% boric a...
Ü C Yildiz, E Dizman


Chapter 7 - Treatment processes of bamboo
2010 - IRG/WP 07-10635-07
For adequate penetration and retention of preservatives in woody bamboos at green, dry, solid and sliced conditions different possible and applied treatment processes have been described along with their classifications. The treated bamboo can be used as building materials; the sufficient treatability ensures its long-term best utilization at ground contact and indoor. All the processes descr...
A K Lahiry


Chapter 11 - Preservation of talla bamboo
2007 - IRG/WP 07-10635-11
Researches revealed that the talla bamboo (Bambusa tulda Roxb.)) in Bangladesh could be full-cell pressure treated with CCA in green and dry conditions. The dry bamboo gives higher loading absorptions than green one when impregnated at same treating conditions. Also higher absorptions are obtained at nodes rather than internodes. Adequate penetration and retention results for ground and wate...
A K Lahiry


Chapter 12 - Treatment Groups of Bamboo
2007 - IRG/WP 07-10635-12
Study on distribution of CCA in three major bamboo species in Bangladesh, full-cell pressure treated at green and dry conditions revealed two treatment groups and some treating principles. Higher adequate treatment for ground and water contact use is only possible by treating problematic bamboo species pre-kiln dried up to half of its FSP and non-problematic species pre-dried up to FSP (20% ...
A K Lahiry


Methods of field data evaluation - time versus reliability
2011 - IRG/WP 11-20466
Field testing of wood and wood-based products is so far the most reliable way to get information on performance with respect to durability and expected service life. However, field trials are extremely time and cost consuming. The main objective of the present study was to investigate possible correlations between early stages of decay, preferably during the first 5 years, and the actual service l...
P Larsson Brelid, C Brischke, A O Rapp, M Hansson, M Westin, J Jermer, A Pilgård


LOSP for glulam, when should the treatment be applied?
2011 - IRG/WP 11-30555
Treatment options for outdoor above-ground (H3) exposed glulam of Pinus radiata and P. elliottii were examined. Beams were treated with azole LOSP (containing a zinc tracer) aiming for retentions of 35-40 l/m3 or 70-80 l/m3. Treatment was conducted either before or after gluing. TBTN LOSP and CCA were included as comparative treatments. Test specimens for exposure were cut after treatment, while w...
L J Cookson


ISPM No. 15 and the Incidence of Wood Pests: Recent Findings, Policy Changes, and Current Knowledge Gaps
2011 - IRG/WP 11-30568
Largely as a result of international trade, hundreds of species of bark- and wood-infesting insects have become established in countries outside their native range. Many of these exotic insects have caused severe economic and environmental impact to urban and forest trees in the receiving countries. Most bark- and wood-infesting insects have been transported to new countries by means of the wood...
R A Haack, E G Brockerhoff


Protective Levels of Borates in timber Foundation Piles 5 – 18 Years after In-situ Remedial Treatment in Areas with Wet Clay Ground Conditions. The Jerbor and Eurobor Protocol, Part 1.
2011 - IRG/WP 11-30571
Timber has been used as foundation piles and grillages for decades or even centuries. Since the late 1970s a method for investigate, analyze and treat building timber foundations in soft clay grounds against decay fungus with a biocide have been developed and used by the late professor Allan Jerbo. Settling of buildings in soft clay grounds is continuously monitored and if damages to the building ...
M Theorin, K-M Bandh


The potential of silicone-based formulations to enhance wood properties through industrial treatment for outdoor use
2011 - IRG/WP 11-30578
High hygroscopicity is one of the main weaknesses of wood as far as its susceptibility to biodegradation, and specifically to fungal decay. New wood preservation technologies are constantly entering the wood protection market, competing with traditional, biocide-based preservation. Silicones are commercially used as hydrophobic agents on stones and concrete. They belong to the restricted number of...
F Simon, F Marchal, F Pochon, M Kutnik, I Le Bayon


Biological and mechanical performances of particleboard panels made from maritime pine (Pinus pinaster) and glued with cornstarch-mimosa tannin-urea formaldehyde adhesive
2011 - IRG/WP 11-40542
The objective of this work was to demonstrate the utility of cornstarch-mimosa tannin-based resins designed for application as an adhesive in the particleboard production. Bond qualities of cornstarch-mimosa tannin- urea formaldehyde (UF) (10:4:86, weight ratios) resins and commercial UF resin were assessed by using an automatic bonding evaluation system, prior to production of particleboard panel...
A Moubarik, F Charrier, A Pizzi, A Allal, B Charrier


Biological properties of Pinus radiata veneers modified with hexamethoxymethyl melamine
2011 - IRG/WP 11-40552
An investigation of the effects on decay and termite resistance of a wood modification process involving prepolymers of hexamethoxymethyl melamine (HMMM) was conducted using LVL as a model engineered wood product. Dry Pinus radiata veneers were vacuum-impregnated with a wood modification formulation containing a mixture (P-H:S-H) of two separate prepolymerisation reactions containing polyvinyl al...
A Siraa, S Millward, C Molloy