Controlling the sapstain fungus Ceratocystis coerulescens by metabolites obtained from Bjerkandera adusta and Talaromyces flavus
1993 - IRG/WP 93-10024
Sapstain causes severe damage to wood and wood products, posing a major economic problem for the wood industry. The purpose of this study was to determine if metabolites from Bjerkandera adusta and Talaromyces flavus would (1) decolorize stain in wood caused by Ceratocystis coerulescens and (2) prevent sapstain by Ceratocystis coerulescens. We studied the interaction of the sapstain fungus Ceratoc...
S C Croan, T L Highley


Test of N-tritylmorpholine in combination with synthetic pyrethroids against marine borers in tropical Australia and Panama
1991 - IRG/WP 4168
Test blocks ol Pinus sylvestris sapwood were pressure impregnated with white spirit solutions of N-tritylmorpholine, either alone or in combination with permethrin, deltamethrin or cypermethrin. They were exposed in the intertidal zone at Mourilyan Harbour, North Queensland, Australia and subtidally at either end of the Panama Canal. After 5 months' exposure at Naos Island at the Pacific ...
S M Cragg, J D Bultman


Field test results for the elimination of subterranean termite (Coptotermes formosanus) colonies by a bait system containing the IGR hexaflumuron
1997 - IRG/WP 97-10222
Field studies were conducted at Chichijima (Ogasawara Islands, Tokyo) to determine the effectiveness of a termite bait system (commercial name: Sentricon* system) containing hexaflumuron (Insect Growth Regulator: IGR) in the elimination of subterranean termite (Coptotermes formosanus) colonies. The level of subterranean termite activity on Ogasawara Islands is high resulting in extensive damage to...
K Suzuki, Y Morita, K Yamauchi


Experiences from a Danish large scale test by means of a new method of treatment by attack of true dry rot fungus (Serpula lacrymans) in buildings
1994 - IRG/WP 94-10064
Experiences from a new and epoch-making method of treatment in connection with the repair of attack of the true dry rot fungus, Serpula lacrymans (Fr.) S.F. Gray, are described. The paper presents the background of a large scale test comprising repair of more than 150 Danish buildings over a period of approximate 5 years. The method being both gentle to the building and presenting savings of at le...
O Munck, H Sundberg


Properties of hot oil treated wood and the possible chemical reactions between wood and soybean oil during heat treatment
2005 - IRG/WP 05-40304
Thermal treatment with hot oil as the heating media based on the original idea from oil-heat treatment in Germany was investigated. The treatment was mainly carried out at 200ºC and 220ºC for 2 hours and 4 hours, and the wood species were mainly spruce and fir. This paper focuses on the difference between soybean oil and palm oil and the possible chemical reactions between wood and soybean oil. ...
Jieying Wang, P A Cooper


Soft rot test of copper/chrome/arsenic treated heartwood of three Malaysian timbers
1991 - IRG/WP 2381
Standardized heartwood blocks of kempas (Koompassia malaccensis), keruing (Dipterocarpus sp.) and tualang (Koompassia excelsa) were impregnated with 0 to 6.3% (w/v) CCA and challenged to decay by a mixed inocula of Chaetomium globosum, Glenospora graphii, Humicola grisea, Petriella setifera and Trichurus spiralis in a containerized vermiculite-burial decay system according to draft CEN/TC 38 WG 4....
A H H Wong, R-D Peek


Contradiction between uptake of preservative in practical situation and laboratory testing
1992 - IRG/WP 92-2392
By brush treatment water- and solvent-based products were applied on boards of Scots pine and Norway spruce to achieve an uptake of 100 and 200 g/ml. In addition the scope of work to achieve the required uptake of preservative was determined under practical conditions for both product groups. EN 113 (RAL-GZ 830) tests were carried out to test the biological efficacy of products. After 18 months ex...
R Gründlinger, O Janotta, M Melzer


Effect of angle of exposure on degradation of radiata pine during weathering trials
1988 - IRG/WP 2301
The importance of angle of exposure on the degree of weathering of materials has not been adequately resolved. In conventional tests, specimens are exposed at an angle of 45° facing the equator, but more recently experiments on polymeric materials have suggested that an angle of 0° may be preferable since this angle maximises levels of received ultra-violet radiation. In this paper the degradati...
P D Evans


Biological resistance of aldehyde-treated wood
1994 - IRG/WP 94-40018
Biological resistance of wood treated with aldehyde cross-linking agents such as glyoxal, glutaraldehyde and dimethylol dihydroxy ethyleneurea (DMDHEU) were investigated. Sapwood blocks of Japanese cedar and Japanese beech, measuring 20 x 20 x 10 mm³ (T x R x L), were vacuum-impregnated at room temperature with 5-25% of aldehyde solutions. Blocks were kept in the solution for 1 week to gain the o...
S Yusuf, Y Imamura, M Takahashi, K Minato


Biological detoxification processes - A check list for assessments
1998 - IRG/WP 98-50120
The number of scientific publications on the biological purification of preservative treated wood implies that the biological treatment of wood wastes becomes more and more important. But an information about a successful industrial application is almost missing in all cases. Therefore the applicability of the proposed purification processes is often uncertain. The feasability of such a biological...
H Leithoff, R-D Peek


An attempt to develop a direct and reliable method for testing the preventive action of preservation treatments of wood against fungal decay
1980 - IRG/WP 2139
In wood preservation there are two classical ways for assessing the reliability of preventive treatments against wood decay: the laboratory tests in which the various parameters are evaluated independently and the field tests or service tests in which those parameters are acting together in the natural environment. One has always tried to build bridges between the two types of experiments and to e...
M Fougerousse


Glulaminated poles - Progress report after 7 years' testing
1987 - IRG/WP 3444
In 1979 a number of glulaminated poles with various preservative treatments were placed in a greenhouse at Uppsala, at the Simlångsdalen test field in southern Sweden and under a power line just south of the Arctic circle in order to study their resistance against biological degradation. The tests have shown that the comparatively best performance will be obtained if each lamination is treated wi...
J Jermer, Ö Bergman


Environmentally benign biological wood preservatives by Streptomyces rimosus, SC-36
1997 - IRG/WP 97-10196
Microbiocides obtained from mutant culture Streptomyces rimosus SC-36 were evaluated for their abilities to inhibit the growth of brown-rot, soft-rot, white-rot, and sapstain fungi on wood. The test fungi were the brown-rot fungi Antrodia carbonica, Gloeophyllum trabeum, Neolentinus lepideus, and Postia placenta; soft-rot fungi Chaetomium globosum, Paecilomyces variotti, Phialocephala dimorphospor...
S C Croan


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 1: Treatment of reference samples
1977 - IRG/WP 426
It was agreed in Wildhaus on 15 May 1976 that preparations for the test detailed in Document No: IRG/WP/414 should commence immediately, but that initially only two water-borne preservatives should be used - a copper/chrome/arsenic (CCA) and a copper/chrome/boron (CCB) formulation respectively. PRL, England (R Cockcroft) would be responsible for supplying samples of the reference timbers treated w...
R Cockcroft, T B Dearling, W O Schulz, H V Borck


A below-ground exposure method for determining the resistance of woody and non-woody materials to attack by subterranean termites
1993 - IRG/WP 93-10012
With existing field test procedures, in which specimens are installed vertically to some of their length into the ground and spaced out from each other ("grave-yard" tests), variations in the rate of contact by termites between replicates can be common. Mechanical damage to specimens during inspection and re-installation may also be difficult to avoid. A new field test method, evaluated in Austral...
M Lenz, J W Creffield


Field testing of alkylammonium wood preservatives
1983 - IRG/WP 3248
The field test performance of five alkylammonium wood preservatives is described. The relative effectiveness of three unmodified formulations was determined by calculation of a Performance Index. Of the three, didecyldimethylammonium chloride was found to be superior to octyldecyldimethylammonium chloride, and both were more effective than alkyltrimethylammonium chloride. However, none were consid...
J N R Ruddick


The use of the Shigometer® and Pilodyn® as non-destructive test methods for detecting decay in CCA treated eucalypt poles
1981 - IRG/WP 2153
The groundline condition of sixty C.C.A. treated eucalypt poles comprising six different species was examined using the Pilodyn® and Shigometer®. Although sensitive to the presence of soft-rot decay, the Shigometer® would seem to offer little practical advantage in the eucalypt soft-rot decay situation, since a comparable visual examination could reveal the presence and extent of decay. Initial...
L E Leightley


Influence of sampling on the composition of test solutions
1985 - IRG/WP 2235
For four commercial products of CCB-salts the influence of the kind of sampling on the composition of test solutions has been tested. For each product several 5 g samples have been taken at random, after careful mixing the content of each bottle, and after grinding the whole content. With each sample a 5% test solution was made and analyzed on the content of chromium, copper and boron. Altogether ...
H Willeitner, K Brandt


Modified Wood – Methods, testing and applications: Outcomes of the EU-Thematic Network
2003 - IRG/WP 03-40268
In the last decade, interest in the development of wood modification systems has increased in Europe. Alongside several industrial initiatives for heat treatments, there have also been scaling up and pilot plant projects for chemical wood modification. Between 2000 and 2003, the European Commission funded the "Thematic Network on Wood Modification". This paper will feature the modification process...
D Jones, W Homan, J Van Acker


Fixation of copper-chrome-arsenic treated timber: A comparison of leaching methodologies
1996 - IRG/WP 96-50075
Five packs of kiln dried radiata pine heartwood were treated with copper-chrome-arsenic preservative treated, utilising a modified Bethell treatment schedule. Two methods of determining the level of preservative fixation were compared. These included the diphenylcarbazide method and simulated rainfall testing. The fixation levels were generally higher for tests involving simulated rain leaching. F...
S Walley, P R S Cobham, P Vinden


The natural durability of wood in different use classes
2003 - IRG/WP 03-10457
The natural durability of important European wood species has been tested on 3970 specimen in field trials. The wood was exposed at five test fields in Germany with different climates at each site in European hazard class 4 and 3 (with and without soil contact). Within EHC 3 it was distinguished between tree different expositions (end grain sheltered, unsheltered and with water trap). The test is...
U Augusta, A O Rapp


Which fungi should be included in the laboratory evaluation of anti-stain chemicals?
2001 - IRG/WP 01-20236
Test fungi for efficacy tests of anti-stain formulations were selected based on the assumptions that test fungi should be fungicide-tolerant antagonists and fungi resistant to both fungicides and fungicide- tolerant antagonists, and such fungi should be re-isolated from treated samples with the highest fungicidal concentration used for laboratory evaluation of fungicides. This paper discusses the ...
Hyung-Jun Kim, Jae-Jin Kim, Gyu-Hyeok Kim


Monitoring the potential biological control agent Cartapip
2000 - IRG/WP 00-10365
Attempts to biocontrol woodstain caused by Ophiostoma species led to the development of an O. piliferum colorless mutant - Cartapip (AgraSoL). The mutant's ability to prevent sapstain of stored logs and lumber is tested in a variety of field trials in Germany, England, Canada and New Zealand. To carry out biocontrol field trials, users have to obtain a permit from a regulatory agency and ...
S Schröder, K Sterfinger, Seong Hwan Kim, C Breuil


Blue Stain Testing of Alkyd and Acrylic Stains
2003 - IRG/WP 03-20273
Resistance against blue stain of semi-transparent alkyd and acrylic stains was tested by both EN 152 and the so-called reverse exposure test methods. Comparison of the results, obtained by both methods was the most important aim of this study. As expected, performance of the water-borne acrylic paint was lower compared to protective effectiveness of the alkyd stain. This difference was even more p...
M Petric, M Pavlic, B Kricej, M Humar, F Pohleven


The full guideline for the “double layer test method” - A field test method for determining the durability of wood out of ground
2004 - IRG/WP 04-20290
This guideline describes a test method for wood to be exposed to the weather out of ground contact. The main objective of the method is to evaluate the durability of wood in above ground exposure as shifted overlaid stakes, which form the so called double layer. The method is applicable to the testing of untreated, treated and modified wood. Initially it was developed and found to be most useful ...
A O Rapp, U Augusta


Previous Page | Next Page