Selection of most aggressive test fungi for modified wood - Practical laboratory experience
2016 - IRG/WP 16-20579
One main objective of wood modification processes is the improvement of the durability against wood destroying organisms. Therefore, investigations of the resistance against wood destroying fungi have been one of the main focus within the last years. For the interpretation of the durability results, the selection of suitable test fungi is one of the main questions. A “wrong” fungus species may...
A Gellerich, S Bollmus


Bundle tests - Simple alternatives to standard above ground field test methods
2016 - IRG/WP 16-20581
Within this study we applied different new above ground test set ups to untreated Norway spruce (Picea abies Karst.) and Scots pine sapwood (Pinus sylvestris L.) which are frequently used as reference or control species in wood durability field tests. The overall aim of this study was to find a simple alternative method to the few standardized above ground field test methods, such as the L-joint a...
C Brischke, L Meyer-Veltrup


Modelling the performance of bio-based building materials
2016 - IRG/WP 16-20582
The ‘bio-based economy’ represents a growing area of development globally and covers a wide range of building materials including wood and wood-based products. A ‘bio-based’ material is intentionally made from substances derived from living (or once-living) organisms. In this context it means that the materials and products are made from renewable resources, with the criteria that a renewa...
C Brischke


Decay of wood in outdoor above ground applications: Preview of results on the effect of climate and species in Spain
2017 - IRG/WP 17-20600
Within the framework of the Project BIA-42434R titled ‘Evaluation of the functional performance of wood in outdoor above ground applications’, seven trials containing seven pieces of sawn wood measuring 750x100x20mm3, belonging to seven different wood species (Scots pine, Radiata pine, Laricio pine, sweet chestnut, eucalyptus, Thermo-treated radiata pine and Spruce), were exposed to unprotecte...
J I Fernández-Golfin Seco, M Conde García, M R Diez Barra, M Conde García, L Acuña Rello, E Torres Álvarez, E Perea Alonso, M T Troya


Development of decay hazard maps based on decay prediction models
2016 - IRG/WP 16-20588
Durability plays a very central role in timber engineering, especially when working with wood in use class 3 and above where the risk of decay is high. As one of the primary decay influencing factors, the external condition, i.e. the local climate, is often graded by some type of climate index value. Predominately, climate indices are based on a direct relationship between weather data and decay. ...
J Niklewski, E Frühwald Hansson, C Brischke, D Kavurmaci


Durability of a willow/plastic composite mat
2016 - IRG/WP 16-20592
Developing uses for wood wastes could enhance utilization of low value renewable materials while creating opportunities for rural development. Small diameter willow stems have little use in China, but they could be combined with high density polyethylene to create wood plastic composite mats for decorative applications. These mats could be used in exterior, above ground exposures, but would still ...
Li Yan, Haiyan Duan, Beizhan Quan, J Cappellazzi, J J Morrell


Evaluation of field test data
2016 - IRG/WP 16-20594
The resistance against fungal decay and insect attack of wood can be highly variable, between boards and even within boards. The variability in durability is not always an issue, but for high demanding applications information about its reliability is required. This comprises the variability of outdoor performance. Durability testing in laboratory and outdoor exposures can provide a good basis to ...
F Bongers, C Brischke, J Van den Bulcke, W Gard, I De Windt, H Militz


Effects of Bio-oil Obtained from Laurel (Laurus nobilis) Residues on Biological, Physical, and Mechanical Properties of Treated Wood
2016 - IRG/WP 16-30692
In this study, the effects of bio-oil obtained from Laurel (Laurus nobilis) residues on biological (decay, insect, termite resistance), physical (water absorption, tangential and radial swelling), and mechanical properties (MOE, MOR and CSPG) of treated wood samples were studied. The bio-oil used in this paper was produced by the help of fixed bed reactor type pyrolyzer. GC/MS analysis showed that...
S Akbas, A Temiz, N Terziev, M H Alma, S Palanti, E Feci


Decay resistance of wood treated with bio-friendly preservative systems
2016 - IRG/WP 16-30698
Due to more restrictive toxicological requirements and increased ecological awareness of consumers, wood preservatives containing biocides are no longer desired on the market. Therefore, research on new environmentally friendly formulations is of great importance. One of the possible solutions is to develop new preservatives based on natural substances, which are harmless to humans, animals and th...
B Mazela, G Cofta, W Perdoch, L Ross Gobakken, P Kwaśniewska-Sip


Effect of Nano-Silane on Permeability in MDF as a Result of Susceptibility to Moulds and Fungi
2016 - IRG/WP 16-40716
Effects were studied of vapor chamber on specific gas permeability of nanosilane-treated medium-density fiberboards (MDF). Size range of nanoparticles was 20 – 80 nm. Nano-silane (NS) was used at four consumption levels of 0, 50, 100, and 150 g/kg dry wood fibers. Density of all treatments was kept constant at 0.67 g/cm3. Specimens were kept for 18 weeks in vaporized chamber; their specific gas ...
H R Taghiyari, J Norton, A Moradiyan, M Sadegh Taher Tolou Del, H Siahposht, B Moradi-Malek, M Noferesti


The durability of manufactured structural building materials
2016 - IRG/WP 16-40718
The projected market potential for Engineered Wood Products such as CLT (cross laminated timber) is very positive however, potential prolonged rain leakage or moisture exposure during construction and in-service could pose considerable concern for its durability and reputation. This research was conducted to assess the decay resistance of CLT and OSB (oriented strand board) in an accelerated trial...
T Singh, D Page


How intraspecific radial variability of the European Oak’s may influence mild pyrolysis process and durability of the material
2016 - IRG/WP 16-40725
Last decades wood is promoted as building material. Unprotected wood exposed to outdoor conditions undergoes a variety of degradation induced essentially by fungi attacks. Heat treatment of wood by mild pyrolysis (180°C T 240°C under inert atmosphere) is a preservation process with a weak environmental impact, and therefore, is viewed as an interesting alternative to the chemical impregnation me...
J Hamada, A Pétrissans, F Mothe, M Pétrissans, P Gérardin


Incorporation of raw boron minerals to protect particleboard against decay and mold fungi, termites and insects
2016 - IRG/WP 16-40729
This paper evaluated the biological performance of particleboards incorporated with the raw boron minerals ulexite and colemanite against decay, mold fungi, termites and insect larvae in comparison with that of particleboards with zinc borate, or boric acid plus a borax mixture. The results showed that ulexite and colemanite were highly effective against the decay fungi and termite attack in labor...
S N Kartal, E Terzi, P Gerardin, C M Ibanez, T Yoshimura


The durability of natural and thermomodified black poplar wood and Scots pine sapwood after two years of external exposition
2016 - IRG/WP 16-40730
Natural biological durability of many European wood species is considered to be relatively small, particularly in a ground contact conditions. This is due to the exposure of the wood to the range of biological and atmospheric destructive factors. This may to limit the scope of application of the wood of these species, particularly in construction. The biocides are often used for wood protection in...
A Fojutowski, A Kropacz, A Noskowiak


New perspectives for wood protection: enzyme-based treatments
2016 - IRG/WP 16-40742
Wood protection research is continuously looking for more benign and effective treatments. One of the main concerns deals with the toxicity of the active compounds employed in the formulations of the preservatives, since they could become a health and environmental issue. Secondly, long-lasting treatments are preferred in order to increase the service life of the treated wood. Weathering condition...
C Fernández-Costas, S Palanti, M Á Sanromán, D Moldes


Exterior birch plywood: potentiality of the thermo-hydro treatment
2016 - IRG/WP 16-40743
It has been found in the present study that, in laboratory fungi tests after leaching with water (EN 84), exterior birch (Betula spp.) plywood, as birch solid wood, is subjected to degradation by rot fungi. This limits the use of such plywood outdoors or in building structures in high humidity conditions. The possibility to improve the birch plywood fungal resistance was investigated in two ways: ...
B Andersons, I Andersone, A Meija-Feldmane, I Irbe, A Janberga, J Grinins


Durability of Thermally Modified Engineered Wood Products
2016 - IRG/WP 16-40745
In this study, rated plywood, oriented strand board (OSB), laminated strand lumber (LSL), and laminated veneer lumber (LVL) were thermally modified as a post-treatment at 140 °C, 150 °C, 160 °C, 170 °C, and 180 °C using a closed, pressurized treatment method. Eastern larch OSB manufactured from heartwood and sapwood was also thermally modified as a post-treatment at 160 °C and 180°C. All ...
H M Barnes, M D Aro, A Rowlen


Marine Borer Resistance of Acetylated and Furfurylated Wood – Results from up to 16 years of Field Exposure
2016 - IRG/WP 16-40756
Furfurylated and acetylated Scots pine sapwood has been tested since 1999 in a marine field with high marine borer activity. In 2004, two test groups with acetylated southern yellow pine (product later known as Perennial Wood™) were put out and over the whole test period differently furfurylated wood (later marketed as Kebony®) test groups have been started. Furthermore, some combinations of mo...
M Westin, P Larsson Brelid, T Nilsson, A O Rapp, J P Dickerson, S Lande, S Cragg


Development of a new method for wood hydrophobizing and fixation of copper compounds by chemical hardening of vegetable based modified oils
2016 - IRG/WP 16-40754
Wood products with ground and direct water contact, but without sufficient biological durability, have to be protected against biological degradation by fungi and other microorganisms. Due to European legislation (Biocidal Products Regulation 528/2012), the selection of possible chemical agents, which are still allowed to be used, is diminishing rapidly. The use of previously widely applied, very ...
C Swaboda, M Fischer, K Jacobs


Chemical, physical-mechanical characterization and durability of thermally modified beech and ash wood by thermo-vacuum process (Termovuoto)
2016 - IRG/WP 16-40758
The paper illustrates part of the results from the CIP Eco-innovation project “Thermo-vacuum: new process for new generation of thermally modified wood”. The project is part of the 7th Framework Programme for European Research and Technological Development, and thermo-vacuum modified wood is already on the European market. The project was selected by the European Commission, EASME Agency, as "...
M Jebrane, I Cuccui, O Allegretti, N Terziev


Fire retardant treated wood products – Properties and uses
2016 - IRG/WP 16-30701
Wood is combustible, but can still perform very well in fire, especially for load bearing structures. However, visible wood surface may not fulfil the fire requirements in building codes and fire retardant treatments may be an option. The highest reaction to fire classification for combustible products may then be reached. However, the excellent fire performance of the virgin fire retardant treate...
B Östman, L Tsantaridis


Effects of wollastonite nanofibers on biological resistance of historical paper against Aspergillus niger
2017 - IRG/WP 17-10878
Effect of wollastonite nanofibers on biological resistance of historical paper against Aspergillus niger was studied. Specimens from A4 papers were also prepared for comparison purposes. Paper specimens were dipped in aqueous nanowollastonite (NW) with 10, 20, 30, and 40% concentrations and compared with control specimens. In order the nanofibers be fixed on paper specimens, 5% of polyvinyl acetat...
H R Taghiyari, A Kalantari, A Ershad-Langroudi, A Kalantari


Durability Testing of a Cattail (Typha spp.) based Insulation Material against Termite Attack
2017 - IRG/WP 17-10879
The use of insulating materials is particularly important in the construction industries, especially with regard to the use of wood and naturally occurring substances. The use and durability of natural materials as insulating materials is of keen interest to many construction experts, and continues to be a topic of intense investigation. It is generally agreed that the use of natural substances ...
M Dass, W Unger, T L Woods


Comparative studies on the durability of English oak (Quercus robur L.) under in-service, field and laboratory conditions
2017 - IRG/WP 17-10881
The durability of many wood species varies due to differences in extractive content, anatomical features, growth conditions, and not at least in dependence of the respective exposure conditions either under test or in real life applications. And so does the durability of English oak (Quercus robur L.), which has recently been considered in the revised European standard EN 350 (2016) and is now cla...
C Brischke, L Meyer-Veltrup, A Soetbeer, M Höpken, E Melcher, J Trautner


Assessing the natural durability for different tropical timber species using the mini-block test
2017 - IRG/WP 17-10886
The Xylarium in the Royal Museum for Central Africa (RMCA, Tervuren, Belgium) contains over 60,000 wood-samples, comprising over 12,000 species. These samples are of great historical and scientific value yet have a random format, which complicates standard testing. The wood-durability against Coniophora puteana and Trametes versicolor was tested for 36 species. Due to the random sample sizes the s...
V Deklerck, I De Windt, N Defoirdt, J Van den Bulcke, H Beeckman, E Espinoza, J Van Acker