IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 811 documents. Displaying 25 entries per page.


Method of embedding and staining of wood after biological testing to support the identification of decay type
1998 - IRG/WP 98-20131
A method for preparing wood for microscopic analysis after decay testing is described, with special regard to a novel fast simultaneous staining, which helps to identify different types of decay. The novel staining process is explained as well as the embedding of heavily decayed samples in polyethylene glycol (PEG) and picking up of sections by transparent adhesive tape. Special feature of the int...
A O Rapp


Genetic Engineering in tree breeding
1998 - IRG/WP 98-10294
The genetic improvement of forest trees by classical breeding is a slow process in comparison with that of annual crops. Tree breeding however is of great importance and has led to trees with better growth characteristics and better disease resistance. An important wood characteristic which has been neglected in breeding programs is wood durability. The durability of the wood will determine for wh...
J Van Doorsselaere, H Beeckman, M Van Montagu, W Boerjan


Effects of chemical pretreatment of Douglas-fir heartwood on efficacy of potential bioprotection agents
1990 - IRG/WP 1440
Biological protection against wood decay fungi represents an environmentally attractive alternative to the use of chemicals; however, the process of identifying suitable candidates and the conditions that ensure successful protection pose major challenges. One critical aspect of this problem is to identify organisms that can rapidly and uniformly colonize the wood. Wood contains low levels of nutr...
B Dawson-Andoh, J J Morrell


The durability of wood polymer composites against fungi and insects
2000 - IRG/WP 00-40161
New materials such as wood polymer composites are used more in France. These materials are obtained by mixing wood and thermoplastics in different ratios. These kind of material must be considered as new materials and some characteristics such as durability must be evaluated for outdoor applications. On the other hand, some recycled fibers from wood waste could be used as raw materials. Some woodp...
G Labat, I Le Bayon, J Gerard, F Amin


Information from the COIPM Wood Group
1988 - IRG/WP 4146
Abstract from the COIPM minutes: Wood in marine environment: Mrs Gambetta stated that the main item discussed by the Group was the collaborative work to test the durability of heat shrinkable polyolephin sheating materials for the protection of wood against marine organisms. The work began last year when wood samples were sent out to the participants. Three samples of Pinus sylvestris wrapped in ...
A Gambetta


Wood durability in the light of recent trends and research on the durability of building materials and components
2000 - IRG/WP 00-20195
Building-related research of today demonstrates a clear shift in focus from the design and production phases to usage and to the entire life time. A consequence is that the performance criteria of materials, components and of the entire building must be regarded over the life time rather than at the time of production or delivery. As one example can be mentioned the Building Construction Directive...
K Ödeen


Biological resistance of electrolessly plated wood (1). Preliminary report
1994 - IRG/WP 94-40024
Surface metal coating is considered to improve biological resistance of wood as some metal ions are fungitoxic. Six wood species (three softwoods: Cryptomeria japonica, Tsuga heterophylla and Larix spp; three hardwoods: Fagus crenata, Acer mono and Betula platyphylla) were electrolessly plated with nickel or copper, and those were served for laboratory evaluation of their resistance against decay ...
M Hasegawa, K Tsunoda, T Yoshimura


Survey of conditioning treatment practices in the Philippines
1975 - IRG/WP 349
The wood preservation industry in the Philippines is at present beset by many problems. An association of the industry similar to those existing in other countries has only been initiated last year by FORPRIDECOM. It is hoped that the formal organisation of this association will bring into focus the importance of this particular industry in the economic and industrial development of the country. L...
R F Casin


Biological and chemical investigations for the assessment of the environmental impact of wood preservative components
1999 - IRG/WP 99-50127
This study was carried out in order to investigate the suitability of biological and chemical techniques to evaluate the environmental impact of wood preservatives depleted from impregnated wood. Small specimens (15*25*50 mm3) of Scots pine sapwood (Pinus sylvestris) were treated with a CCB salt. After fixation the treated and untreated samples were washed-out according EN 84, and the different le...
E Melcher, H-W Wegen


Effects of the specimen position on fungal colonisation and wood decay by en 113 test fungi
1998 - IRG/WP 98-20136
For testing wood preservatives according to EN 113 it is common practice to plant the test blocks on neutral supports in order to prevent (1) a diffusion of chemicals into the agar medium and (2) an excessive moistening of the specimens. The procedure was employed in EN 350-1 for testing the natural durability of solid wood. It turned out to be of problematic nature because of the individual requ...
G Kleist, M-T Lenz, R-D Peek


Biological resistances of wood-metaborate composites using the borax solution system
2001 - IRG/WP 01-30259
Combinations of wood and metaborate composite were prepared from sapwood specimens of Japanese cedar (Cryptomeria japonica) and the borax and metallic salts system using the diffusion-penetrated process. Wood-metaborate composites were produced as follows: water-saturated specimens were first impregnated by a saturated borax solution and then diffuse-penetrated with Zn2+, Ca2+, or Pb2+ solution. B...
Liang Lin, T Furuno


A new concept for the evaluation of wood durability for out of ground contact using accelerated L-joint testing
1997 - IRG/WP 97-20123
Since the wood preservation sector is developing in favour of defining exactly the utilization of wood products and preservation techniques as a function of the envisaged hazard class, more in particular the hazard classes 3 and 4 (EN 350) there is obviously a need for a test method evaluating natural durability for out of ground contact applications. Based on the L-joint test as described in the ...
J Van Acker, M Stevens


Antagonistic properties of Gliocladium virens against wood attacking fungi
1996 - IRG/WP 96-10162
Gliocladium virens has shown good antagonism against decay fungi in agar medium and in wood blocks. Gliotoxin produced by Gliocladium virens is associated with biocontrol of some plant diseases, but its importance to biocontrol of wood-attacking fungi is unknown. We investigated the ability of gliotoxin-producing (GLT+) isolates of Gliocladium virens and gliotoxin-deficient (GLT-) mutants of Glioc...
T L Highley, H S Ananthapadmanabha, C R Howell


Biological durabilityof cement-bonded particleboard
1997 - IRG/WP 97-20115
Cement-bonded particleboard (CBP) is a panel product manufactured from a combination of wood particle and cement with various ratio. The wood particle is used as reinforced material and the cement as an inorganic binder. Because of its many excellent properties, such as high weathering resistance, sound attenuation, and good acceptance for a range of surface treatments, CBP is widely used as a fac...
Qiao Wang, M Takahashi


Biological test, AAS and EPR study of copper monoethanolamine complex with quaternary ammonium compounds as a wood preservative
2003 - IRG/WP 03-30321
Experiments were carried out on the wood preservative with a strong fungicidal activity based on Cu(II) carbonate, 2-aminoethanol (monoethanolamine) and quaternary ammonium compound (QAC). The object of the performed investigations was sapwood of Scots pine (Pinus sylvestris L.) treated with Cu-EA-QAC formulation. Mycological investigations were carried out according to EN 113 and EN 84 standards....
B Mazela, I Polus, S K Hoffmann, J Goslar


Laboratory trials of biological control agents against subterranean termites
1991 - IRG/WP 1475
To screen for potential termite control by microorganisms, 17 mold fungi included 3 pathogenic fungi and 7 basidiomycetes, were used to challenge the test termite species, Coptotermes formosanus and Reticulitermes speratus. Test fungi were allowed grow and completely in Petri dishes. To screen for potential termite control by microorganisms, 17 mold fungi included 3 pathogenic fungi and 7 basidiom...
K Suzuki


Categories in wood preservation hazard, risk, and use
1994 - IRG/WP 94-20048
In various countries hazard-, risk-, or use-categories have been established. The different terms seem to be only a sophisticated language problem, but they are rather a basic principle of the philosophy of wood preservation which is going to obtain importance with respect to the low reputation of chemical wood preservatives in an increasing number of countries. Whilst hazard signifies the fact th...
H Willeitner


Biological degradation resistance of wood acetylated with thioacetic acid
1983 - IRG/WP 3223
Chemically, modification of wood is being considered as an alternative to conventional preservation by toxic chemicals. Acetylated wood has been reported to be quite resistant to most biodegrading organisms at weight percent gains (WPG) around 15-19. The conventional acetylation techniques with acethic anhyrdride result in generation of acetic acid. However, acetylation with thioacetic acid overco...
S Kumar, S C Agarwal


Accelerated testing for out of ground contact using natural biological preconditioning
1996 - IRG/WP 96-20088
Small blocks made of Scots pine sapwood were treated, buried in vermiculite and exposed to natural microbial colonisation during outdoor exposure prior to laboratory decay testing. Periodic microbial isolations, moisture content, permeability and weight loss tests were also conducted. Bacteria and moulds colonised the vermiculite and miniblocks well. Aureobasidium pullulans was common on TnBTO tre...
S Molnar, D J Dickinson, R J Murphy


Tropical In-Ground Durability of Structural Sarawak Hardwoods Impregnated to High Retention with CCA-salts, CCA-oxide and FCAP after 20 Years Exposure
2005 - IRG/WP 05-30384
Statistical analysis (ANOVA) was conducted on durability (termite and decay combined) rating data collected over 20 years exposure period of over 140 species of Sarawak timbers with altogether 30,000 stake specimens, at the Forest Department’s Sibu “graveyard” stake test sites from 1977. About 20 replicated stakes were pressure-treated to refusal with 10% g/ml concentration of up to 3 CCA-sa...
Wang Choon Ling, A H H Wong


Variation in biological performance of CCA caised by preservative application method
1996 - IRG/WP 96-40072
A series of laboratory studies to investigate the influence of treatment application method on CCA performance in Cosican pine has been completed. Biological decay tests, such as serial exposures, were used to induce decay in wood at preservative retentions of up to 10 kg/m³ CCA salts. Significant differences in performance of the preservative against either brown, white or soft rot decay fungi w...
P R Newman, R J Murphy


The influence of extractives on the natural durability of selected Ghanaian hardwoods
2004 - IRG/WP 04-10530
A study of the durability of Nauclea diderrichii, Nesogordonia papaverifera, Corynanthe pachyceras and Glyphaea brevis in laboratory and field tests showed the first three species performed well against a range of fungi and termites. Sapwood of C. pachyceras also performed well against these biodeteriogens. The role of extractives in conferring natural durability was assessed. Total extractive con...
C Antwi-Boasiako, A J Pitman, J Barnett


A trial of "sour" felling to prevent bluestain by depletion of sapwood nutrients
2001 - IRG/WP 01-10404
Discoloration of conifer wood caused by bluestain causes large economic losses in Canada. Most deep stain develops in the log stage during storage or transport. In a search for control strategies that will not disrupt woodlands productivity we tested "sour" felling, termed "hagarashi" in Japan. The practice involves delaying the delimbing of freshly harvested trees. The tree continues to transpire...
A Byrne, A Uzunovic, D Minchin, C Breuil


Specifying preservative-treated resistant timber: Conforming to European Standards
2001 - IRG/WP 01-20235
The most common construction timbers used in the UK are of low natural durability and, generally, resistant to preservative treatment. These include species of spruce, hemlock and fir. However, their characteristically limited and non-uniform uptake of preservatives may still confer sufficient protection to give satisfactory durability performance in terms of biological resistance. This paper desc...
E D Suttie, A F Bravery, T B Dearling


Cleistanthus collinus (Roxb.) Benth. ex Hook. f. and Wrightia tinctoria (Roxb.) R. Br. -- two timbers with promising durability under marine conditions
2005 - IRG/WP 05-10552
During the course of natural durability studies on indigenous timber at Visakhapatnam harbour, two species, namely, Cleistanthus collinus (Karada) and Wrightia tinctoria (Dudhi) were found to resist marine borer attack for reasonably longer periods. The panels of C. collinus completely resisted borer attack for 9 months but became susceptible to teredinid attack thereafter. The teredinids gradua...
M V Rao, M Balaji, V Kuppusamy, K S Rao


Previous Page | Next Page