IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 826 documents. Displaying 25 entries per page.


Effects of polyvinyl alcohol on leachability and efficacy of boron wood preservatives against fungal decay and termites attack
2010 - IRG/WP 10-30526
In this study, the use of polyvinyl alcohol (PVA) as boron fixative agent was investigated. Two levels of PVA (2.5 and 4%) were evaluated with disodium octaborate tetrahydrate (DOT) at three concentrations (1, 2 and 4% boric acid equivalent (BAE) using a double vacuum impregnation processes on Scots pine sapwood specimens. Leaching was performed according to a laboratory leaching procedure. Boron ...
A Mohareb, M F Thévenon, E Wozniak, P Gérardin


A comparison of the chemistry of alkaline copper and micronized copper treated wood
2010 - IRG/WP 10-30528
This paper discusses the chemistry of the reaction of alkaline copper and micronized copper with wood. The objective of this study is to examine the copper species produced in wood during the fixation reaction using electron paramagnetic resonance (EPR) spectroscopy. The initial experiments (phases 1 to 2) were designed to confirm the effect of time of treatment and solution concentration on the s...
Wei Xue, P Kennepohl, J N R Ruddick


Assessment of Boracol 200RH (FrameSaver) as a remedial treatment to control decay in pre-decayed model timber frame units
2010 - IRG/WP 10-30529
Model timber frame units constructed from untreated radiata pine were pre-wetted to approximately 40% moisture content and inoculated with Coniophora puteana and Oligoporus placenta. Units were transferred to a controlled environment room maintained at 25°C and 95% RH for 7 and 10 weeks to allow two levels of decay to become established in units. Following pre-decay, units were disassembled, clea...
Mick Hedley, Dave Page, Jackie van der Waals


Treatment of Scots pine wood with oil in water and water in oil emulsion systems: Effects on boron leaching and water absorption
2010 - IRG/WP 10-30535
The aim of this study was to investigate the water absorption and water repellent efficiency of oils and oil water emulsions [oil-in-water (O/W) and water-in-oil (W/O)] and possibilities of reducing the amount of boron leaching from treated wood. Scots pine wood samples treated with waste or sunflower oil and water formulations contained 3%BA. The level of water absorption and water repellent effi...
E D Tomak, Ü C Yildiz, A Can


Distribution and availability of preservative components in ACQ treated wood - effects of coatings and weathering
2010 - IRG/WP 10-30537
Copper and quaternary ammonium compound (quat) distributions across lumber (gradients) and availability, as measured by amount removed by intensive leaching of wood flour, were measured in ACQ treated southern pine lumber. Samples were evaluated just after treatment and stabilization, or after 3 years of laboratory storage, or after 3 years of natural weathering exposure. The objective was to in...
T Ung, M Nejad, P Cooper


Copper preservative systems: A rapid investigation into effects of co-biocides and used treating solutions
2010 - IRG/WP 10-30541
The efficacy of various micronized and amine copper preservative systems was evaluated using soil block testing with the copper tolerant brown rot fungi, Postia placenta. The American Wood Protection Association E22 protocol was used to compare the relative efficacy of preservatives by monitoring compressive strength losses of the systems in southern pine wood. As information, the weight losses ...
T F Shupe, K Ragon, Q Wu, M H Freeman, C R McIntyre


Antifungal and wood preservative efficacy of IPBC is enhanced by α - aminoisobutyric acid
2010 - IRG/WP 10-30544
There is currently a need to reduce the biocide content of wood preservatives, without decreasing efficacy. The nonmetabolised amino acid analogue α-aminoisobutyric acid (AIB) acts as a translocated inhibitor of mycelial spread in basidiomycete wood decay fungi, although it does not kill the organism. Factorial combinations of AIB with either the azole fungicide tebuconazole, or 3-iodo-2-...
P Bota, E Baines, A Mead, S C Watkinson


Copper nanoparticles in southern pine wood treated with a micronised preservative: Can nanoparticles penetrate the cell walls of tracheids and ray parenchyma?
2010 - IRG/WP 10-30547
This study tests the hypothesis that copper nanoparticles can penetrate the cell walls of southern pine wood treated with a micronised preservative. We examined the nanodistribution of particles in tracheid and ray parenchyma cell walls using state-of-the-art HR (High Resolution)-TEM and HR-STEM (Scanning Transmission Electron Microscope)-EDX. These devices are capable of atomic-scale resolution. ...
H Matsunaga, Y Kataoka, M Kiguchi, P Evans


Fungal decay resistance and mechanical properties of plywood panels made from maritime pine (Pinus pinaster) and bonded with cornstarch-quebracho tannin-phenol formaldehyde adhesive
2010 - IRG/WP 10-40490
The aim of this work is to demonstrate the performances of cornstarch-quebracho tannin-based resins designed as adhesive in the plywood production. In this way, the cornstarch and quebracho tannin was introduced in the classic adhesive formulation in order to supply a part of phenol-formaldehyde (PF). In order to evaluate the mechanical performances of optimal cornstarch-quebracho tannin-PF, plywo...
F Charrier, A Moubarik, A Allal, A Pizzi, B Charrier


Sorption properties of wood impregnated with aqueous solution of boric acid and montan wax emulsion
2010 - IRG/WP 10-40492
Non-biocidal techniques for wood protection become more and more important, nowadays. One of the possible treatments is use of water repellents. In the present research influence of, one of the possible water repellent, the montan wax emulsion, on the moisturizing and the sorption characteristic of impregnated wood was investigated. To achieve a better protection against wood decay fungi, montan w...
B Lesar, M Humar


Influence addition of boron compounds to adhesives on the bonding quality and fungicidal properties of glued wood
2010 - IRG/WP 10-40497
Wood is one of the most important construction materials. However, users of wood face two issues: limited dimensions and insufficient durability. These issues have been overcome with the development of bonding and wood preservation. The preservation of glued wood is elucidated in this paper. Through the addition of boric acid to adhesives, we tried to improve the fungicidal properties of glued woo...
M Humar, B Lesar, A Ugovsek, M Kariz, P Kralj, M Šernek


Influence of Copper Preservative Type on Earlywood and Latewood Distribution of Copper in Treated Wood
2010 - IRG/WP 10-40507
Some of the new water based copper containing wood preservative systems use particulate “micronized” copper as the primary biocide instead of the more traditional soluble amine copper based systems. Studies were conducted to investigate how this difference in the type of copper system might impact both initial and post drying distribution of the preservatives in wood. Of specific interest wa...
A Zahora


A comparison of the corrosion of alkaline copper and micronized copper treated wood
2010 - IRG/WP 10-40515
With the replacement of chromate copper arsenate (CCA) by alkaline copper wood preservatives, there have been reports of increasing corrosion of metal fasteners and connectors in contact with treated wood. This may be explained by the presence of more mobile copper in the treated wood. One novel industrial response has been to develop a wood preservative based on an aqueous solution containing sus...
M Kofoed, J N R Ruddick


Preservative Treatment of simul (Bombax ceiba) Veneers with Hot and Cold Water Solution of borax-boric acid by Soaking Process
2010 - IRG/WP 10-40528
Veneers of simul (Bombax ceiba) were treated with different concentrations of water- borne preservatives borax-boric acid (BB) by soaking process for different time periods. In the case of hot water treatment, it was found that the average retention of preservative chemicals increased gradually with the increasing treatment period from 20 minutes to 60 minutes. Similar trend was observed in the ca...
K Akhter, Md Abul Hashem, S Akhter


Copper distribution in soil leached from full scale decking boards during one year
2010 - IRG/WP 10-50265
The distribution of copper in the soil under exposed decking boards after one year has been analysed. The decking boards were impregnated with copper HDO, copper quat and copper triazoles. The decking boards were pine sapwood and pressure treated in a full cell process, fixed by heating and then dried. The samples were not surface treated. Each decking sample of five boards (0.25 m2) was placed on...
F G Evans


Combined Effect of Boric Acid and Waste Oil Treatment on Boron Leaching
2010 - IRG/WP 10-50268
In this study it was aimed to investigate the boron leaching amounts in Scots pine wood samples treated with boric acid (BA) and waste oil (WO) alone or by dual treatment. The level of water absorption and water repellent efficiency were determined with cyclical wetting tests, total of 336 hours. Wood samples that have both covered and uncovered transversal section were impregnated with 3% boric a...
Ü C Yildiz, E Dizman


Metal Migration from Douglas-fir Poles Treated with Ammoniacal Copper Zinc Arsenate According to Best Management Practices
2010 - IRG/WP 10-50272
The potential for migration of metal components from ammoniacal copper zinc arsenate treated (ACZA) poles was examined using pole sections treated using Best Management Practices. Copper and zinc levels were highest in runoff collected following the first rainfall events, then declined. Copper and zinc levels in runoff averaged 20 ppm and 5 pm respectively. The metal levels were then used to pr...
J J Morrell, C S Love, C Freitag


Comparison of laboratory and semi-field tests for the estimation of leaching rates from treated wood
2010 - IRG/WP 10-50274
The authorization of wood preservative formulations in the European Union according to the Biocidal Products Directive (BPD) includes the assessment of environmental risks by the emission of active ingredients. This risk assessment includes scenarios for preserved wood (e.g. house scenario, noise barrier), in which the predicted environmental concentration (PEC) for soil and water is calculated, u...
N Morsing, M Klamer, B Seidel, J Wittenzellner, M Maier, J Habicht


Chapter 8 - Episode of bamboo
2007 - IRG/WP 07-10635-08
In this chapter 7 (seven) poems entitled “The Bamboo’s Preface”, “The Bamboo’s Interim”, “The Fast Growing Grass”, “The Wild Grasses”, “The Bamboo’s Episode”, “The Bamboo’s Outlook”, “The Commitment” have been composed based on the habit, nature, introduction, properties, values, outlooks, importance, uses and melodies of bamboos in Asia. The conservation a...
A K Lahiry


Isolation and evaluation of Lactobacillus brevis from chilli waste for potential use as a wood preservative
2011 - IRG/WP 11-10749
Lactic acid bacteria were isolated from chilli waste and evaluated for their ability to arrest wood rotting basidiomycetes. In previous work a quick screening method using 96 well plates and measuring absorbance to determine fungal growth was developed specifically to investigate the efficacy of isolated bacteria against wood decay fungi. Using this method, one bacterium (isolate C11) was identif...
D O’Callahan, T Singh, I R McDonald


The decontamination of a historical xylotheque with liquid carbon dioxide
2011 - IRG/WP 11-10757
The pharmacist Johann Heinrich Linck senior (1674-1734) created the xylotheque (collection of wood species) in Leipzig, Saxony (Germany). His son, Johann Heinrich Linck junior (1734-1807), continued the valuable and unique collection, which now belongs to the Museum Waldenburg near Dresden, Germany. In the past the cupboard, including the wood specimens, was impregnated with a wood preservative co...
S Zoppke, A Unger, J Mankiewicz, M Eisbein


Comparative investigations between thermal and microwave assisted digestion as a novel tool for the chemical analysis of inorganic wood preservative components
2011 - IRG/WP 11-20461
The correct chemical impregnation of wood requires an internal as well as external quality control of the treated wood. The active is located in a solid matrix, therefore it is often difficult to analyse such material since most analytical procedures are based on liquid systems. Because of this quite a number of methods – like extraction or thermal digestion - were developed in order to transfer...
H Ahl, J Fromm, E Melcher


Methods of field data evaluation - time versus reliability
2011 - IRG/WP 11-20466
Field testing of wood and wood-based products is so far the most reliable way to get information on performance with respect to durability and expected service life. However, field trials are extremely time and cost consuming. The main objective of the present study was to investigate possible correlations between early stages of decay, preferably during the first 5 years, and the actual service l...
P Larsson Brelid, C Brischke, A O Rapp, M Hansson, M Westin, J Jermer, A Pilgård


A comparative study and evaluation of methodologies used for determining wood preservative penetration
2011 - IRG/WP 11-20475
A series of methods for determining penetration of wood preservatives into the wood structure have been developed for either quality control (QC) or research and development purposes. QC methods range from monitoring the solution uptake, applying colour indicators or sampling specific wood samples followed by wood acid digestion/atomic absorption spectroscopy (AAS) or solvent extraction/chromatogr...
R Craciun, R Moeller, J Wittenzellner, T Jakob, J Habicht


A Method for Studying Boron Redistribution and Leaching in Timber Framing
2011 - IRG/WP 11-20476
In typical New Zealand timber framed house construction, the timber framing has a vapour permeable building wrap applied to the exterior and a cladding applied over 20 mm battens. An interior lining usually of gypsum plasterboard is then fixed once the timber framing has a moisture content of < 20%. Timber framing within the building envelope is not expected to be wet in-service or exposed to a le...
J A Drysdale, N Marston, M E Hedley


Previous Page | Next Page