Behaviour of some selective Indian species towards treatment with solvent based water repellent preservative
1984 - IRG/WP 3309
This paper discusses a solvent based preservative using PCP and a water repellent for preserving three species of timber commonly used in India for the manufacture of doors and windows. It examines the method of treatment to achieve desired levels of penetration and retention of the preservative-cum-water repellent, and tests made on these timbers to examine the success of the processing methods a...
V R Sonti, B Chatterjee


Environmental fate of copper-based wood preservatives in different soil substrates - Part 2: Study of the metal sorption and migration potential under simulated rainfall
1998 - IRG/WP 98-50101-21 b
In order to examine the potential environmental impact of spillages of the saltborne wood preservative CCA in treatment plants, four large scale experiments are set-up so as to follow the water transport and ion mobility in various field soils. A plastic container is filled with a sand, silt, clay and potting soil, made up at their respective bulk density and wetted to a given moisture content. U...
G M F Van Eetvelde, R Hartmann, J M Mwangi, H S Öztürk, M Stevens


Composting of waste building up in sawmill dipping basins
1990 - IRG/WP 3570
We have studied composting of waste building up in dipping basins at sawmills although this waste can also be disposed of by incineration. Controlled composting within the sawmill area seems to be a feasible method. Another possibility is to accomplish composting directly at the local dumping site. Waste containing antistain chemicals is generally classed as hazardous. It cannot therefore be place...
I A Linderborg, U Ek


Field performance of novel antisapstain formulations
1997 - IRG/WP 97-30125
The effectiveness as antisapstain formulations of combinations of oxine copper (Cu-8), carbendazim, hexaconazole, cyproconazole, flusilazole, didecyldimethyl ammonium chloride (DDAC), an alkanolamine borate (SB), benzalkonium chloride (BAC), 2-n-octylisothiazolin -3-one (isothiazoline) and p-chlorophenyl-3-iodopropagilformal (CPIPF) was determined for freshly sawn, block-stacked radiata pine in th...
D R Eden, R N Wakeling, C M Chittenden, J G Van der Waals


Effectiveness of the new chemical wood preservative Borosol 9? against a house longhorn beetle Hylotrupes bajulus
2004 - IRG/WP 04-30355
Chemical wood preservative Borosol 9, consisting of boric acid - alkanolamine complex, is a new wood preservative with proven efficacy against wood decay fungi. However, we were interested in its efficacy against larvae of house longhorn beetle (Hylotrupes bajulus). Thus, experiment according to the EN 46 procedure was performed. Specimens made of Norway spruce wood (Picea abies) were ...
G Babuder, M Petric, F Cadež, M Humar, F Pohleven


Qualifying ecotoxicity research on tropical hardwood leachates
1997 - IRG/WP 97-50096
Almost as a rule, quantification and identification of various types of environmental contamination is grounded on chemical evaluation principles. Yet for monitoring surface water pollution, aquatic bio-assays may provide a more direct way to assess the potential hazard of environmental samples. A battery of such tests is experienced onto leachates of tropical hardwoods used in ground and water co...
G M F Van Eetvelde, P Marchal, M Stevens


New approaches to practical evaluation method of bio-degradation of wooden construction - Non-destructive detection of defects using radar technique
2000 - IRG/WP 00-20214
There have been a number of researches and developments on the techniques and apparatus for the nondestructive evaluation of the biological deterioration in wood and wooden constructions, such as decay or insect attack in house, public buildings or in historically important architectures. As for the detection of the decay in wood, techniques using sound in audible or in ultrasonic frequency ranges...
Y Fujii, Y Komatsu, Y Yanase, S Okumura, Y Imamura, M Tarumi, H Takiuchi, A Inai


Laboratory and Pilot Evaluation of Chlorothalonil Formulations for Mold and Stain Control on some Wood Species
2003 - IRG/WP 03-30317
Laboratory and pilot test of the efficacy of several fungicides such as chlorothalonil and carbendazim for control of mold and sap- stain on bamboo and slash pine and rubberwood were conducted in this paper. The result indicates that: -- Clorothalonil/carbendazim are more effective for controlling mold and stain than that of carbendazim alone in laboratory test. --Higher concentration at 0.1-0.2...
Mingliang Jiang, Zhaobang Li


Tolerance of Wood Decay Fungi to Commercial Copper Based Wood Preservatives
2002 - IRG/WP 02-30291
Due to the use of copper based preservatives like CCB or CCA for more than a century, copper tolerant fungi have appeared in some European countries in recent times. It is therefore important to find out whether this phenomenon is specific for only classical copper ingredients, or generally for all copper based formulation. Thus, we tested the tolerance of three commercial copper based pres...
F Pohleven, M Humar, S A Amartey, J Benedik


Effect of vapour boron treatment on mechanical properties of wood based board materials
1992 - IRG/WP 92-3727
The mechanical properties of Medium density fibre board, Chipboard and Oriented strand board were investigated after treatment to two retention levels of boric acid applied as a vapour phase system. A range of mechanical properties were investigated. The vapour boron treatment does not have any significant effect on most of the mechanical properties of the boards. The exception is a reduction in i...
R Hashim, D J Dickinson, R J Murphy, J Dinwoodie


Fumigation of New Zealand grown western red cedar for export markets
2001 - IRG/WP 01-30262
The objective of this study was to demonstrate that methyl bromide fumigant penetrates into the centre of western red cedar (Thuja plicata L.) timber to meet the standard for export markets. Kiln dried western red cedar was used and a cavity (50x 30 x 13mm3) was prepared into the centre of each sample board (500 x 200 x 26 mm3 thick). An absorbent sachet used in industry for cross checking that th...
B Kreber, G Durbin, D Wilson


New boron-based biocides for the protection of wood
2002 - IRG/WP 02-30283
Boric acid and other simple inorganic oxides of boron are amongst the oldest wood preservatives currently in use. Their relatively low toxicity and broad-spectrum activity are just some of their desirable characteristics. The primary disadvantage associated with conventional boron-based preservatives is their lack of permanence in exposed applications. A collaborative project between CSIRO and the...
D G Humphrey, P J Duggan, E M Tyndall, J M Carr, L J Cookson


The performance of metal-chromium-arsenic formulations after 32 to 38 years' in-ground exposure in Australia
2000 - IRG/WP 00-30240
Two trials of metal-chromium-arsenic preservatives were exposed in-ground in Australia. In Trial 1, Pinus radiata stakes treated with Boliden K.33, Boliden S.25, Celcure A, Tanalith C and Tanalith CA were installed at Sydney and Narrandera in 1961/1962. In Trial 2, P. radiata and Eucalyptus regnans sapwood were treated with Celcure A, Celcure A21-N, Celcure A 21-O and Tanalith CA (new) and install...
G C Johnson, J D Thornton, J Beesley


Scandinavian experience – 25 years’ experience in transforming used creosoted wood into bio-fuel
2005 - IRG/WP 05-50224-18
Swedish experiences show that the best and most efficient way to handle the creosoted wood waste is through combustion. The preparation of creosoted waste wood to fuel chips at IQR AB’s plant in Trollhättan is done by splinting the wood according to a special method. Mainly railroad sleepers, but also other wooden commodities, from all over Europe are delivered to the plant. The wood material i...
T Karlström


A non-pressure method of protection based on hurdle theory to control the spectrum of internal environmental factors which affect the decay of poles in soil contact
1993 - IRG/WP 93-20005
A field trial was conducted to establish whether superficial barrier linings on poles in soil contact could function as environmental hurdles against the growth of biological agents and thus provide preventative methodology to preclude premature failure of vineyard poles under flood-irrigation. Assessment after 52 weeks exposure to the prevailing conditions and sub-tropical environment showed that...
A A W Baecker


Laboratory and field trials of novel antisapstain formulations
1997 - IRG/WP 97-30146
This document covers the results of laboratory and field trials of combinations of fungicides formulated using a patented technology (PCT NZ 96/00143). A 3 week laboratory trial that uses radiata pine (Pinus radiata D. Don) branch discs as a substrate was used to determine which combinations possessed a suitable spectrum of fungitoxicity against key sapstain, mould and decay fungi. In particular f...
R N Wakeling, P N Maynard, D R Eden, C M Chittenden, B Carpenter


Evaluating the resistance of wood-based panel products to fungal attack
1995 - IRG/WP 95-20071
At present there is considerable disagreement among national research institutes within Europe and panel product manufacturers on the most appropriate method of testing and indeed the need for specific biological durability testing. This paper seeks to place before a broader international audience, the issues related to development of a European standard for evaluating the resistance to fungal dec...
R G Lea, R W Berry


Detection of wood decay fungi in wood using a PCR-based analysis
1998 - IRG/WP 98-10279
We have developed a DNA-based assay to reliably detect brown rot and white rot fungi in wood at different stages of decay. DNA, isolated by a series of CTAB and organic extractions, was amplified by the polymerase chain reaction using published universal primers and basidiomycete-specific primers derived from ribosomal DNA sequences. We have surveyed 7 species of brown rot fungi, 7 species of whit...
C Jasalavich, A Ostrofsky, J Jellison


Evaluation of chlorothalonil for stain and mould control on lumber
1992 - IRG/WP 92-3713
Chlorothalonil is a commercially important fungicide with many industrial and agricultural applications. It has a very low mammalian toxicity and is considered to be an environmentally benign material. This paper describes the laboratory evaluation of chlorothalonil as a wood antisapstain treatment. Chlorothalonil was tested as three formulation types - an emulsifiable concentrate (EC), a water-ba...
P E Laks, T L Woods, D L Richter


The biological effectiveness of wood modified with heptadecenylsuccinic anhydride against two brown rot fungi: Coniophora puteana and Gloeophyllum trabeum
1992 - IRG/WP 92-3705
A modified soil block test was carried out using wood samples reacted with heptadecenylsuccinic anhydride (ASA). This modification gave good resistance to decay brought about by the brown rot fungi Coniophora puteana and Gloeophyllum trabeum during the twelve week exposure period. Results indicated that there was a good correlation between increased loading of modifying reagent and an increase in ...
C Codd, W B Banks, J A Cornfield, G R Williams


Surface retentions of PCP, TCMTB and MTC obtained during a field trial of antisapstain formulations
1993 - IRG/WP 93-20002
Formulations containing NaPCP or TCMTB and MTC were included as reference products in a recent field trial of antisapstain formulations in Queensland. Retentions of these actives on the surface of treated sawn Pinus elliottii were monitored by ultrasonic solvent extraction of excised samples and analytical determination by high performance liquid chromatography. Distribution of actives with depth ...
D E Ferlazzo, M D Needham, M J Kennedy


Water-based silicones on wood
1997 - IRG/WP 97-30144
Five waterbased silicones commonly used on masonry where tested as water repellents for wood. The Water Repellent Effectiveness was determined by swellometer-tests and by measuring the water uptake of samples after 24 hours complete immersion and by immersion in a water level of 4 mm for 24 hours. The different methods are compared and discussed. Artificial and natural weathering was performed to ...
D Lukowsky, R D Peek, A O Rapp


Influence of carboxylic acids on LEACHING of copper amine based preservatives
2005 - IRG/WP 05-30365
The importance of chromium free preservatives is increasing. Leaching of copper from wood preserved with such solutions is still higher compared to leaching from wood impregnated with copper chromium ones. In order to decrease leaching, different carboxylic acids (octanoic, 2-etilheksanoic, decanoic) were added to copper/amine/boron aqueous solutions. Experiment of leaching of copper from Norway s...
M Humar, P Kalan, F Pohleven


Computer-assisted ranking of potential biocontrol fungi based on data from laboratory screening trials
1993 - IRG/WP 93-10023
Forty two fungal isolates were screened for antibiotic activity. In these sceering tests inhibition of target wood decay fungi was expressed as a series of numerical scores for each isolate. These scores, along with values for 5 other charactetistics, were used to assess the isolates. Using selection indices, isolates were judged on the basis of all the characteristics combined and, ranked in orde...
M W Schoeman, D J Dickinson


The effect of alternative pre-conditioning procedures on the durability of wood based board materials to decay fungi
1997 - IRG/WP 97-20105
In the biological testing of wood based board materials it has been shown that exposure of boards in a closed vessel system may lead to inaccurate results due to the build up of volatile substances that inhibit the test fungi. It is thought that this is a transitory effect of freshly manufactured boards. In the European standard for testing fungal durability of board materials which is currently u...
S F Curling, R J Murphy, J K Carey