Your search resulted in 318 documents. Displaying 25 entries per page.
New approaches to practical evaluation method of bio-degradation of wooden construction - Non-destructive detection of defects using radar technique
2000 - IRG/WP 00-20214
There have been a number of researches and developments on the techniques and apparatus for the nondestructive evaluation of the biological deterioration in wood and wooden constructions, such as decay or insect attack in house, public buildings or in historically important architectures. As for the detection of the decay in wood, techniques using sound in audible or in ultrasonic frequency ranges...
Y Fujii, Y Komatsu, Y Yanase, S Okumura, Y Imamura, M Tarumi, H Takiuchi, A Inai
Biological resistance of wood treated with waterbased resins and drying oils in a mini-block test
1998 - IRG/WP 98-40107
In recent years it was found that the resistance of wood against fungal degradation could be increased by impregnation with an etherificated melamine formaldehyde resin. Using this resin as a reference, a waterbased fatty acid modificated alkyd-resin and two drying-oils were assessed for their biological performance in a mini-block laboratory test. Although drying-oils, like linseed-oil, are often...
M Sailer, A O Rapp, R-D Peek
Tolerance of Wood Decay Fungi to Commercial Copper Based Wood Preservatives
2002 - IRG/WP 02-30291
Due to the use of copper based preservatives like CCB or CCA for more than a century, copper tolerant fungi have appeared in some European countries in recent times. It is therefore important to find out whether this phenomenon is specific for only classical copper ingredients, or generally for all copper based formulation. Thus, we tested the tolerance of three commercial copper based
pres...
F Pohleven, M Humar, S A Amartey, J Benedik
Effect of vapour boron treatment on mechanical properties of wood based board materials
1992 - IRG/WP 92-3727
The mechanical properties of Medium density fibre board, Chipboard and Oriented strand board were investigated after treatment to two retention levels of boric acid applied as a vapour phase system. A range of mechanical properties were investigated. The vapour boron treatment does not have any significant effect on most of the mechanical properties of the boards. The exception is a reduction in i...
R Hashim, D J Dickinson, R J Murphy, J Dinwoodie
Fumigation of New Zealand grown western red cedar for export markets
2001 - IRG/WP 01-30262
The objective of this study was to demonstrate that methyl bromide fumigant penetrates into the centre of western red cedar (Thuja plicata L.) timber to meet the standard for export markets. Kiln dried western red cedar was used and a cavity (50x 30 x 13mm3) was prepared into the centre of each sample board (500 x 200 x 26 mm3 thick). An absorbent sachet used in industry for cross checking that th...
B Kreber, G Durbin, D Wilson
New boron-based biocides for the protection of wood
2002 - IRG/WP 02-30283
Boric acid and other simple inorganic oxides of boron are amongst the oldest wood preservatives currently in use. Their relatively low toxicity and broad-spectrum activity are just some of their desirable characteristics. The primary disadvantage associated with conventional boron-based preservatives is their lack of permanence in exposed applications. A collaborative project between CSIRO and the...
D G Humphrey, P J Duggan, E M Tyndall, J M Carr, L J Cookson
Influence of different resin treatments on the dimension stability of wood
1997 - IRG/WP 97-40090
The dimension stability of wood is considered to be an important contribution to its durability and its performance in practice. A number of different treatments have been developed to improve the dimension stability of wood. One applied method is the treatment of wood with monomers or resins. The application of appropriate impregnation conditions seemed to be essential to enhance the efficiency o...
M Sailer, A O Rapp
Scandinavian experience – 25 years’ experience in transforming used creosoted wood into bio-fuel
2005 - IRG/WP 05-50224-18
Swedish experiences show that the best and most efficient way to handle the creosoted wood waste is through combustion. The preparation of creosoted waste wood to fuel chips at IQR AB’s plant in Trollhättan is done by splinting the wood according to a special method. Mainly railroad sleepers, but also other wooden commodities, from all over Europe are delivered to the plant. The wood material i...
T Karlström
A non-pressure method of protection based on hurdle theory to control the spectrum of internal environmental factors which affect the decay of poles in soil contact
1993 - IRG/WP 93-20005
A field trial was conducted to establish whether superficial barrier linings on poles in soil contact could function as environmental hurdles against the growth of biological agents and thus provide preventative methodology to preclude premature failure of vineyard poles under flood-irrigation. Assessment after 52 weeks exposure to the prevailing conditions and sub-tropical environment showed that...
A A W Baecker
Evaluating the resistance of wood-based panel products to fungal attack
1995 - IRG/WP 95-20071
At present there is considerable disagreement among national research institutes within Europe and panel product manufacturers on the most appropriate method of testing and indeed the need for specific biological durability testing. This paper seeks to place before a broader international audience, the issues related to development of a European standard for evaluating the resistance to fungal dec...
R G Lea, R W Berry
Detection of wood decay fungi in wood using a PCR-based analysis
1998 - IRG/WP 98-10279
We have developed a DNA-based assay to reliably detect brown rot and white rot fungi in wood at different stages of decay. DNA, isolated by a series of CTAB and organic extractions, was amplified by the polymerase chain reaction using published universal primers and basidiomycete-specific primers derived from ribosomal DNA sequences. We have surveyed 7 species of brown rot fungi, 7 species of whit...
C Jasalavich, A Ostrofsky, J Jellison
The biological effectiveness of wood modified with heptadecenylsuccinic anhydride against two brown rot fungi: Coniophora puteana and Gloeophyllum trabeum
1992 - IRG/WP 92-3705
A modified soil block test was carried out using wood samples reacted with heptadecenylsuccinic anhydride (ASA). This modification gave good resistance to decay brought about by the brown rot fungi Coniophora puteana and Gloeophyllum trabeum during the twelve week exposure period. Results indicated that there was a good correlation between increased loading of modifying reagent and an increase in ...
C Codd, W B Banks, J A Cornfield, G R Williams
Water-based silicones on wood
1997 - IRG/WP 97-30144
Five waterbased silicones commonly used on masonry where tested as water repellents for wood. The Water Repellent Effectiveness was determined by swellometer-tests and by measuring the water uptake of samples after 24 hours complete immersion and by immersion in a water level of 4 mm for 24 hours. The different methods are compared and discussed. Artificial and natural weathering was performed to ...
D Lukowsky, R D Peek, A O Rapp
Influence of carboxylic acids on LEACHING of copper amine based preservatives
2005 - IRG/WP 05-30365
The importance of chromium free preservatives is increasing. Leaching of copper from wood preserved with such solutions is still higher compared to leaching from wood impregnated with copper chromium ones. In order to decrease leaching, different carboxylic acids (octanoic, 2-etilheksanoic, decanoic) were added to copper/amine/boron aqueous solutions. Experiment of leaching of copper from Norway s...
M Humar, P Kalan, F Pohleven
Computer-assisted ranking of potential biocontrol fungi based on data from laboratory screening trials
1993 - IRG/WP 93-10023
Forty two fungal isolates were screened for antibiotic activity. In these sceering tests inhibition of target wood decay fungi was expressed as a series of numerical scores for each isolate. These scores, along with values for 5 other charactetistics, were used to assess the isolates. Using selection indices, isolates were judged on the basis of all the characteristics combined and, ranked in orde...
M W Schoeman, D J Dickinson
The effect of alternative pre-conditioning procedures on the durability of wood based board materials to decay fungi
1997 - IRG/WP 97-20105
In the biological testing of wood based board materials it has been shown that exposure of boards in a closed vessel system may lead to inaccurate results due to the build up of volatile substances that inhibit the test fungi. It is thought that this is a transitory effect of freshly manufactured boards. In the European standard for testing fungal durability of board materials which is currently u...
S F Curling, R J Murphy, J K Carey
Improvement of intrinsic properties of wood by chemical wood densification - Hydrophobic aspects and durability aspects
1999 - IRG/WP 99-40149
To improve the intrinsic properties of Scot pine wood ((1) hydrophobic surface and (2) durability), two ways of chemical modification have been tested. The first one is the chemical modification of hydroxyl groups by active substances like diisocyanate compounds with a copolymerization step. The second way is a densification by an impregnation of resins and a gamma polymerisation. This second way ...
G Labat, Q K Tran, I Le Bayon
Effect of some resin treatments on fungal degradation reactions
1999 - IRG/WP 99-10318
The effect of impregnation of wood with vegetable oil, tall oil and two water soluble on fungal degradation reactions was assessed by hydrolysis and enzyme activity measurements. The experiments were carried out by using isolated enzyme preparations and a living brown-rot fungus Poria placenta. The results indicate that the inhibitory effect of treatments was clearly directec towards the enzymatic...
A-C Ritschkoff, M Rättö, A J Nurmi, H Kokko, A O Rapp, H Militz
Environmental fate of copper-based wood preservatives in different soil substrates - Part 1: Screening of the metal adsorption potential
1998 - IRG/WP 98-50101-21 a
In treatment plants, spillage of wood preservatives onto soil may be of environmental concern. This potential soil contamination served as an objective for a screening study. Three different mineral soils, a mineral substrate and two horticultural substrates are examined for their sorptive potential of copper through mixing with wood preservative solutions.
Depending on the soil/substrate charact...
G M F Van Eetvelde, J M Mwangi, F Tack, R Hartmann, M Stevens
Preservation of wood-based panels against fungi and insects and and testing its efficiency
1976 - IRG/WP 270
Wood-based panel products which are made of susceptible wood species may be destroyed by fungi under wet conditions and by termites. The glues do not provide sufficient protection unless very high concentrations are applied. Particle boards and fibre boards are not susceptible to beetle infestation, although some species may attack plywood. Various types of preservatives provide sufficient protect...
G Becker, M Gersonde
Applicability of supercritical carbon dioxide to the preservative treatment of wood-based composites
2001 - IRG/WP 01-40199
Treatability of five structural-use wood-based composites (medium density fiberboard, hardwood plywood, softwood plywood, particleboard and oriented strand board) was evaluated when supercritical (SC) carbon dioxide (CO2) was used as a carrier solvent. Treatments were conducted at three temperature 32 levels (25, 35 and 45°C) and two pressure levels [80 kgf/cm2 (7,845 kPa) and 120 kgf/cm2 (11,768...
M Muin, A Adachi, K Tsunoda
Results on field stake tests against termite – Maximum for 8 years examination at Kumamoto in Japan
2003 - IRG/WP 03-10463
Various preservative treated or modified wood and charcoal painting stakes were tested in field, maximum for eight years in Kumamoto, distributed two main termite species, Coptotermes formosanus and Reticulitermes speratus. After two years in field, untreated sapwood of sugi (Cryptomeria japonica) were observed severe attacks by termites, but the preservative treated stakes were observed no signif...
K Suzuki
Effect of point of preservative addition on the mechanical and physical properties of strandboard treated with Tanalith 3485
2000 - IRG/WP 00-40152
Preservative has been added to a PF bonded strandboard at various different stages in the manufacturing cycle and the physical and mechanical properties of the boards have been evaluated (modulus of elasticity, modulus of rupture, thickness swelling, water absorption, internal bond strength, and shear strength). Preservative addition has been examined at five different stages namely green strand d...
G J Goroyias, M D C Hale
Laboratory Evaluation and Field Trial of Chlorothalonil and Copper-based Preservatives and Leaching Performance of Copper in Copper Treated Wood
2002 - IRG/WP 02-30279
Soil block test and field trial of some Chinese plantation wood species pine and poplar treated with chlorothalonil formulations and copper-based preservatives such as ACQ-B and copper citrate (CC) were conducted. The results of soil block test indicated that chlorothalonil formulations and ACQ-B as well as CC are very effective for controlling the 2 fungi species Corious versicolor and Poria plac...
Mingliang Jiang, Ping Wang, Chungen Piao, Zhaobang Li, Quan Lu, Lei Liu
Accelerated termicidal performance data for new water-based copper linoleate formulations
1996 - IRG/WP 96-30104
An organic solvent based copper linoleate (Culin) has proved itself as an effective wood preservative in long term field trials in South Africa over a period of 30 years. Whilst the organic solvent based product offers good wood preservative performance, primary industrial interest has been in an emulsified version of the product. The objective of this study was to evaluate the influence of two di...
D Conradie, P Turner