A Case Study of Long-term CCA Preservative Leaching from Treated Hardwood Poles in a Humid Tropical Condition
2016 - IRG/WP 16-50324
Chromated copper arsenate (CCA)-treated Malaysian hardwoods have long been used as utility poles, posts, construction piles and motorway fencing in soil contact exposed to the threats of decay fungi and termites. Despite global concerns citing predominantly temperate conditions of long-term leaching of CCA toxic heavy metals from wood into surrounding soils and groundwater since the 1990’s, the ...
A H H Wong, W S M Chin


10 year Report on COST E37 Round Robin Tests – Comparison of results from laboratory and field tests
2017 - IRG/WP 17-30718
A round robin involving 15 European participants was set up in 2006. The round robin consisted of both a field test according to the double layer test method and a laboratory test with two different preconditioning methods. The laboratory test results were reported in an earlier IRG paper (IRG/WP13-20535) but are included also in this paper in order to facilitate the comparison with the field test...
M Westin, E Conti, J Creemers, P-O Flæte, A Gellerich, I Irbe, M Klamer, E Melcher, R Moeller, L Nunes, S Palanti, L Reinprecht, E Suttie, H Viitanen


Modelling of moisture content in timber bridge details
2017 - IRG/WP 17-20613
The design of details is an important aspect in durability design of timber bridges. Details are often considered the weakest points in bridges due to their tendency to trap and accumulate moisture and thus facilitate decay. When designing maintenance plans and inspection intervals, it is important to know how design choices will come to influence the service life. Moreover, service life and wood ...
J Niklewski, C Brischke, E Frühwald Hansson, L Meyer-Veltrup


COST FP 1303 Cooperative Performance Test – Results after two years outdoor exposure
2017 - IRG/WP 17-20620
COST Action FP 1303 ‘Performance of Bio-Based Building Materials’ started in October 2013 and an ambitious program was set up for four years. Among this a collaborative field test was planned. The idea of the cooperative performance test was to distribute a fairly simple test set up to as many places in Europe as possible in order to collect performance data reflecting the full range of climat...
B Lesar, M Humar, C Brischke, L Meyer-Veltrup, D Jones, N Thaler, J M Abascal, G Alfredsen, B Brunnhuber, E Grodås, M Irle, J Kers, M Klamer, K-C Mahnert, E Melcher, S Palanti, M Noël, E Suttie, N Pfabigan, M Touza


Performance of Norway spruce bridge in North-West Spain after 12 years exposure
2017 - IRG/WP 17-40796
Across Europe is very common to find bridges build in sawn and glue-laminated wood. Most of these bridges used softwood wood species such as: fir, spruce, larch and pine. In Spain wooden bridges, became more and more popular since nineties, when sawn and glue-laminated wood were utilized for building exterior wooden structures in overall Spain. This material, sawn and glue-laminated wood, are ma...
D Lorenzo, J Fernández-Golfín, M Touza, M Guaita, A Lozano, J Benito


The Effects of Pre-Microwave Treatment on Retention Levels And Some Mechanical Properties of Spruce Wood Treated with CCA
2017 - IRG/WP 17-40800
Microwave (MW) treatment of wood has been evaluated in recent years for different purposes by several scientists. Microwave conditioning improves permeability, reduces density and heat conductivity and changes dimensional stability. Furthermore, it could even improve the permeability of refractory wood species such as spruce and Douglas fir. In this study, MW pre-treatment was applied to spruce wo...
E D Gezer, S Kuştaş, S Durmaz


Corrosion of fasteners in furfurylated wood – final report after 9 years exposure outdoors
2017 - IRG/WP 17-40810
The corrosion of some common fastener materials – mild steel, stainless steel, zinc-coated steel, brass and Sanbond Z (nickel, zinc and chromate) coated steel – has been evaluated after nine years exposure outdoors in untreated Scots pine and furfurylated beech and southern yellow pine (SYP). The furfurylation was carried out according to a process that resulted in approximately 40 % WPG (We...
J Jermer, B-L Andersson, J Schalnat


Effects of exposure time on detection of the behavior of white-rot fungi on Oriental beech wood properties
2017 - IRG/WP 17-10902
The comparison of fungal degradation of Orientalis beechwood by two white-rot fungi was evaluated in this study. Biological, mechanical, and chemical assessments of beech wood were carried out at 30 day interval for 120 days. The results demonstrated that both fungi have greater effects on beech wood during each exposure time. However, Trametes versicolor degraded beech wood more effectively than ...
E Bari, D D Nicholas, K M Ohno


Natural resistance of Bambusa vulgaris to termite and powder-post beetle attack in laboratory and graveyard tests
2018 - IRG/WP 18-10925
Deterioration is the major setback to the utilisation of bamboo products. To enhance bamboo utilization, an understanding of the level of resistance to degradation is important. In this study, level at which Bambusa vulgaris will naturally resistant attack by subterranean termites and powder-post beetles were evaluated. B. vulgaris aged 2, 3 and 4 years were subjected to attack by subterranean ter...
N A Sadiku, S O Bada


Visual appearance of unpainted wooden claddings during the first year of outdoor exposure: Evaluation of surface mould growth, lightness (L*) and wasp attack
2018 - IRG/WP 18-40841
This study addresses changes in visual appearance of unpainted wood materials exposed outdoors. Specimens of Norway spruce (Picea abies) Scots pine (Pinus sylvestris), aspen (Populus tremula), acetylated Radiata pine (Pinus radiata) and DMDHEU-modified Scots pine sapwood were exposed facing south in Ås, Norway for 60 weeks. During this period, surface mould growth development and wasp attack were...
S Karlsen Lie, L Ross Gobakken, G I Vestøl, O Høibø


Performance of wood decking after 5 years of exposure: verification of the combined effect of wetting ability and durability
2019 - IRG/WP 19-20647
Wood is one of the most important construction materials and its use in building applications has further expanded in recent decades. In order to enable even more extensive and reliable use of wood, factors affecting wood’s service life need to be understood. More recently, a new concept to characterize the durability of wood-based materials and to predict the service lives of wood was proposed,...
M Humar, D Krzisnik, B Lesar, C Brischke


CCA wood preservative: Trust with destiny
2019 - IRG/WP 19-30731
This paper traces the history of Copper-Chrome-Arsenic (CCA) and its current status in India and worldwide. CCA was invented as ASCU at the Forest Research Institute, Dehra Dun in 1933 by Dr. Sonti Kamesam. Although its efficacy was doubted by the British colonial rulers resulting in several hiccups at home, the patent rights were purchased by US Bell Telephone Co. and it was adopted by the US woo...
S Kumar


Color change of timber exposed outdoors - Influence of season exposure test starts
2019 - IRG/WP 19-40865
For the client the material and color of the exterior wall are important, because they affect the impression of the building [1]. However, discoloration of the exterior wall begins as soon as the building is completed, by various factors such as rainfall. We tried to quantitatively evaluate the changes of the exterior wood, and to organize the influences of climate conditions, in order to use the ...
K Usami, H Ishiyama


Natural durability and performance of Eucalyptus globulus single family house in Spain after 17 years exposure
2019 - IRG/WP 19-40873
From last century, in the country side in Spain is common to find wooden houses. The reason is mainly due the improvements in glues, materials, design by computer and processing in factories. All these technological advances have facilitated the development industrialized systems cheaper. However, the variety of row materials, designs and construction systems, combined with some hard climates, cou...
D Lorenzo, M Touza, J Fernandez-Golfín, A Lozano, J Benito


Performance of naturally durable decks after 15 years of field exposure
2020 - IRG/WP 20-10963
A decking test of Canadian species considered to be naturally durable was inspected after 15 years of exposure at test sites in Ontario and British Columbia. Based on the materials used in this experiment, Douglas-fir and yellow cypress had the greatest decay resistance, followed by eastern white cedar and western redcedar, and then by western larch and tamarack. All materials tested were more dur...
R Stirling, D Wong


Potenzy of Azadirachta indica heart wood extracts as wood bio-preservative against termite attack
2020 - IRG/WP 20-10972
Extractives in wood are one of the main reasons for wood resistance against bio-degradation. The chemical compositions of extractives from matured Azadirachta indica that are known to be very resistant against bio-degradation were studied to assess their role as wood preservative. Ethanol and toluene were used in the extraction of these compounds from the heartwood of Azadirahcta indica. Chemical ...
L O Aguda, O B Olajide, O Y Aguda


Macro biological degradation of wood treated with sorbitol and citric acid – first results from marine environment and termite exposure
2020 - IRG/WP 20-40901
Most European wood species are rapidly and severely degraded in termite-infested areas and the marine environment. There is a need for new solutions, especially in the marine environment, since we lack wood preservatives approved for marine applications in Europe. Several wood modification systems show high resistance against both marine borers and subterranean termites. However, the existing comm...
A Treu, L Nunes, E Larnøy


Effect of MVOC exposure on mycelial growth of wood rotting fungi
2021 - IRG/WP 21-10977
It is well known that wood rotting fungi produce microbial volatile organic compounds (MVOCs) as metabolites. In our previous studies, we have found that some MVOCs produced by wood rotting fungi are common to fungal species tested in the studies, while others are specific to each species. Furthermore, it has been also shown that each wood rotting fungi do not always produce the same type of MVOCs...
S Horikawa, R Konuma, M Yoshida


Evaluation of Decay Resistance of Copper-based Preservatives Treated-Wood exposed to different field test sites in Korea
2022 - IRG/WP 22-20679
In Korea, preservative treated wood is required to have a stamp on the surface which contains information such as wood species, use categories, and the company that treated the wood. Such stamping is necessary to safely and appropriately use the treated wood. Since majority of treated wood is being used outdoor environment, the treated wood must have efficacy against wood decay fungi or termite. I...
W-J Hwang, S-M Yoon, Y Park, Y-S Choi, H-M Lee, J-W Kim


Copper-octanoate - a potential reference preservative replacement for CCA in field test standards?
2022 - IRG/WP 22-20688
Finding a CCA reference replacement for use in standardised test methods is of high priority since this chemical is being phased out and may in the near future be banned also for experimental and approval purposes. In this paper we assess the possibility to replace CCA reference preservative with an historical copper octanoate product. There is a huge amount of lab and field test data available fo...
R Ringman, M Westin, M Klamer, A Christof, F Friese


Analysis of wooden shingles after seven years of exposure
2022 - IRG/WP 22-20690
Wood is a traditional roofing material in the Alpine regions. In the 17th century, wooden roofing was typically used on more important buildings. Still, today it is predominately used on huts and houses in the hilly regions of northern and north-western Slovenia. Because wooden roofing is expensive, we investigated the possibility of extending the service life of the roofing through impregnation a...
M Humar, B Lesar, D Kržišnik, E Keržič, B Jemec


Service trial of different materials exposed in jetties at Öresund. Progress report No. 5
2022 - IRG/WP 22-30764
This report contains results of the fifth inspection on the performance of different decking materials – preservative-treated wood, modified wood, natural durable wood, re-cycled plastics and wood-plastic composites (WPCs) - available on the market and exposed since 2013 (some since 2014 and 2016) by the City of Malmö in two jetties near the Øresund Bridge, south of central Malmö in Sweden. T...
J Jermer


Effect of nano-particle characteristics and concentration on UV protection of timber: A field exposure test
2022 - IRG/WP 22-40941
Wood has a well-known susceptibility to ultra-violet light degradation, leading to premature replacement. A variety of products have been developed to protect against this damage, but most provide less than 12 months of protection and must be regularly reapplied. Developing improved coatings would help reduce wood losses and reduce maintenance costs. Nano-particles have a variety of attractive pro...
T Yi, J J Morrell


The influence of thermal modification and surface charring to different levels on wettability of Norway spruce wood
2022 - IRG/WP 22-40942
The wood can alternatively be protected from water absorption by thermal modification and charring. Both techniques cause certain chemical and physical changes in the wood, the extent of which depends on the level of temperature applied. The objective of this study was to determine how the combination of charring to different levels and thermal modification affects the chemical, morphological, and...
J Žigon, C Gerardin, M E P Wålinder, P Gerardin


Mechanical Properties of Thermally Modified Wood after twelve Months of Field Exposure
2022 - IRG/WP 22-40945
This study aimed to evaluate the durability and mechanical properties of two different woood species, namely beech (Fagus sp.) and silver fir (Abies alba), from Bosnia and Herzegovina thermally modified at three different temperatures and duration at maximum temperature. Samples of the mentioned wood species wood (Abies alba) were prepared according to EN 408+A1 standard. The maximum 4-point bendi...