Optimized composition of alkyd emulsion with nanoparticles of iron oxide for enhancing protection of thermally modified wood
2022 - IRG/WP 22-40940
Thermal treatment is acknowledged as an environmentally friendly method to improve durability of wood and some of its properties, such as biological resistance, dimensional stability, reduced hygroscopy. Despite these improvements, when used outdoors, also thermally treated wood is subjected to the action of environmental factors, like solar radiation, moisture, precipitations, temperature, etc., ...
E Sansonetti, D Cīrule, I Andersone, B Andersons, E Kuka


Influence of weathering on the mechanical properties and performance of exterior wood coatings
2022 - IRG/WP 22-40951
Three commercial coatings were exposed to artificial (EN 927-6) and natural weathering (EN 927-3) on wood samples. Cracking was visually assessed as well as Persoz hardness. Free films of the same coatings were also exposed to the same weathering tests before their tensile properties were measured. Results show that artificial and natural weathering modified the overall mechanical properties of wo...
L Podgorski, J-D Lanvin


Optimisation of accelerated weathering procedure as an alternative to natural weathering
2023 - IRG/WP 23-20693
Comprehensive tests need to be performed to obtain the most accurate data possible on the durability of wood. The most reliable performance tests are field tests. However, since this is very time-consuming, we frequently rely on laboratory tests. To increase the reliability of the laboratory tests, samples are preconditioned with natural or artificially accelerated weathering methods that simulate...
E Keržič, M Humar, V Vek


Influence of weathering of wood surfaces before and after treatment with iron(II) sulphate
2023 - IRG/WP 23-30786
Outdoor wood is exposed to various factors that cause the wood to grey or age. The ageing processes can vary greatly depending on the exposure. Parts of the wood that are not exposed to external factors, e.g. under the eaves, are less exposed and the ageing process is therefore slower. This can be accelerated by solutions based on iron ions. In this way, the wood greys quickly and evenly. However,...
B Lesar, M Humar, F Osvald


Adhesion and performance of exterior wood coatings on chemically and thermally modified wood – Results from 5.5 years outdoor exposure
2023 - IRG/WP 23-40964
Non-durable softwood and hardwood species were treated with the water-soluble cyclic N-methylol compounds 1,3-dimethylol-4,5-dihydroxyethyleneurea (DMDHEU) and methylated DMDHEU. One half of the modified specimens were coated with a waterborne acrylic coating system prior a natural weathering for 5.5 years according to EN 927-3 (2020). By frequent evaluations, the impact of chemical modifications ...
L Emmerich, H Militz


Optimization via artificial intelligence of intumescent coatings for wood substrates
2023 - IRG/WP 23-40987
The development of new materials requires a large amount of experiments representing a major issue to innovate. This is particularly true for complex material formulations such as flame retarded materials that could contain a number of ingredients. Artificial Intelligence based optimization (more precisely Bayesian optimization) techniques appear to be efficient methods to optimize complex systems...
E Verret, S Duquesne, A Collin


X-ray micro-computed tomography of copper distribution in CA, ACQ and MCA treated wood and changes in microstructure of ACQ-treated southern pine following natural weathering
2024 - IRG/WP 24-20707
We hypothesized that X-ray micro-CT would be able to visualize: (a) the distribution of copper in CA-treated southern pine; and (b) microstructural changes in ACQ-treated southern pine exposed to natural weathering. Small blocks were removed from southern pine samples treated with CA and also southern pine treated with ACQ and MCA. Small blocks were also removed from ACQ-treated boards (flat and p...
D Feng, M Turner, P D Evans


Natural weathering of modified pine and Eucalyptus woods by surface charring
2024 - IRG/WP 24-30801
Within various wood modification techniques, surface charring is anticipated to extend the lifespan of wooden components in building facades; however, visual deterioration of charred cladding materials has become a notable concern. This study, conducted through international collaboration, aimed to assess the resistance of bio-based facade materials to weathering in the Turkish climate. The natura...
E E Soyturk, E N Kavakli, S N Kartal, C M Ibanez


Bio-durability and weathering performances of cardanol-treated wood
2024 - IRG/WP 24-30809
Cardanol is an excellent insecticide, fungicide, and termiticide derived from thermally treated cashew nutshell liquid (CNSL) and has been extensively explored in the chemical industry and for medicinal uses. However, its potential for wood protection remains unexplored. This study aims to understand the bio-durability and weathering properties of cardanol-treated wood. The southern pine and yello...
L Liang, McDonald, A G, L Cai


A novel treatment for increasing UV stabuility of wood based on citric acid and urea
2024 - IRG/WP 24-30811
Wood, a fundamental material in the Built Environment, faces challenges related to durability and weathering, notably UV degradation leading to colour changes. This study explored a novel treatment method utilising citric acid and urea to enhance the UV stability of wood. The reaction between these compounds forms fluorescent species and insoluble nanoparticles upon thermal treatment. Two treatmen...
S Jué, A Scharf, C-F Lin, R Moutou Pitti, D Sandberg, D Jones


Shelling of flat and profiled western larch deck-boards exposed to natural weathering
2024 - IRG/WP 24-40997
Shelling is a severe type of raised grain that occurs at the surface of deck-boards made from wood species that have growth rings with pronounced differences in density between earlywood and latewood, for example southern pine (Pinus spp.). Shelling is more severe in deck-boards fixed with their growth rings oriented pith-side-up (concave) rather than bark-side-up (convex). Far less is known about...
L H Leung, P D Evans


Leaching and chemical redistribution of CCA components in refractory heartwood of E. nitens
2024 - IRG/WP 24-41011
Chromated Copper Arsenate (CCA) is a wood preservative widely used to protect against fungal and insect attack. The fixation mechanism of CCA involves complex chemical reactions, including the reduction of chromium (VI) to chromium (III) and the formation of insoluble complexes. Despite fixation efforts, a portion of CCA components tends to leach from treated wood, influenced by factors like wood ...
J R Vargas, L Yermán, K C Wood, T Singh


Previous Page