IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3421 documents. Displaying 25 entries per page.


Chlorpyrifos as a wood treatment temiticide
1994 - IRG/WP 94-30047
Chlorpyrifos, O,O-diethyl O-(3,5,6-trichloro-2-pyridyl) phosphorothioate, is a broad-spectrum insecticide used worldwide for the control of many insect pests. As a wood preservative, chlorpyrifos is registered with the United States Environmental Protection Agency for protection of seasoned and green lumber and logs from attack by wood destroying insects such as termites, carpenter ants, ambrosia ...
R D Fears


Improvement of wood decay resistance by tannin impregnation
1991 - IRG/WP 2380
The fungical effect of tannins is appraised after exposure of treated woods samples to wood rotting fungi. A screening-test is carried out with several solutions containing extracts of two kinds of tannins; a condensed tannin derived from Quebracho heartwood (Schinopsis sp.) and a hydrolyzable one extracted from chestnut heartwood (Castanea sativa Mill). If a fungicidal action was indeed found it ...
D Dirol, A Scalbert


Using image analysis to rate wood stain trials
1993 - IRG/WP 93-10034
Assessing the extent of fungal discoloration on wood during laboratory trials is a subjective process which provides an opportunity for considerable variation between individual evaluators of specimens. The development of reliable systems for automatically assessing discoloration would minimize evaluator bias and permit comparisons between results from different laboratories. The use of image anal...
C M Sexton, A G Maristany,C C Brunner, J J Morrell


The influence of soil pH on leaching of CCA elements from pressure-treated Eucalyptus saligna sapwood: environmental implication
2003 - IRG/WP 03-50203
Evidence is accumulating as to poor distribution and fixation of CCA in tropical hardwoods, and there is therefore a necessity to investigate the permanency of CCA in tropical hardwoods. The relationship between soil pH and leaching of Cu, Cr and As from CCA pressure-treated sapwood of Kenyan-grown Eucalyptus saligna was tested under laboratory conditions. Small sapwood samples were pressure-tre...
R Venkatasamy, D N Okwara


Effects of surfactants and ultrasonic energy on the treatment of wood with chromated copper arsenate
1977 - IRG/WP 3108
Sugar pine stakes 1'' x 1" x 16" were treated by a hot-water bath followed by soaking in cold CCA solution for 10 to 30 minutes. A similar number of stakes were treated by a cold-cold bath. Half of the stakes were subjected to ultrasonic energy during the CCA bath. The mean absorption for stakes given the hot-cold bath was 18.52 pcf (297 kg/m³) and 4.64 pcf (74 kg/m³) for those...
C S Walters


Decrease in the mechanical resistance of blue stained and "orange stained" Pinus radiata wood
1999 - IRG/WP 99-10313
It is recognised that sapwood attacked by Ceratocystis pilifera increases its permeability to pressure preservative treatments. Since hiphae not only utilise pits, but also the cell wall for crossing from one cell to another, the mechanical resistance of the stained wood might be affected. The orange colour very commonly present in Pinus radiata logs heartwood under water sprinklers, has not recei...
M C Rose, L Reyes, J Alvarez, A Andaur, C Beltran, D Rivera


Soft rot test of copper/chrome/arsenic treated heartwood of three Malaysian timbers
1991 - IRG/WP 2381
Standardized heartwood blocks of kempas (Koompassia malaccensis), keruing (Dipterocarpus sp.) and tualang (Koompassia excelsa) were impregnated with 0 to 6.3% (w/v) CCA and challenged to decay by a mixed inocula of Chaetomium globosum, Glenospora graphii, Humicola grisea, Petriella setifera and Trichurus spiralis in a containerized vermiculite-burial decay system according to draft CEN/TC 38 WG 4....
A H H Wong, R-D Peek


Dimension of lysimeters and the evaluation of the migration of wood preservative components in soil
1996 - IRG/WP 96-50065
In the past, investigations concerning the migration behaviour of wood preservatives were made to a minor extent and no uniform methods of test exist. The migration behaviour of CFB was determined using 5 lysimeters of different dimension. The results of the migration and distribution of the anions in the soil showed considerable differences between both ions. Approximately the whole quantity of c...
E Melcher, R-D Peek


Changes in pore structure and cell wall volume in wood decayed by brown- and white-rot fungi
1991 - IRG/WP 1501
Sweetgum (Liquidambar styraciflua L.) wood blocks were decayed by Postia (=Poria) placenta or Phanerochaete chrysosporium in soil-block cultures. Decay was terminated at various weight losses, and the pore volumes available to probes of various molecular weight and diameter were determined by the solute exclusion technique (Stone, J.E. and A.M. Scallan. 1968. Cellulose Chem. Technol. 2, 343-358.)....
D S Flournoy


Natural Durability of Tropical Species – Variations and Prospects
2005 - IRG/WP 05-10568
The tropical timber resources of the world play an unequivocal role in economic development of both the tropical timber producing and importing regions. This paper describes natural durability as an important and preferred wood quality of tropical species of the world with emphasis on Malaysian hardwoods, the link between various aspects of tropical hardwood durability, hardwood utilization and bi...
A H H Wong, Yoon Soo Kim, A P Singh, Wang Choon Ling


The fungal degradation of quaternary ammonium compounds in wood
1998 - IRG/WP 98-10263
This work focuses on the biodegradation of didecyldimethylammonium chloride (DDAC) by the mould fungus Gliocladium roseum within a woody matrix. Three sawdust types, distinguished by their treatment and amount of DDAC retained, were inoculated with the fungus and their DDAC loss was measured over 11 weeks. The rates of degradation varied depending on the sawdust; however, a significant loss of DDA...
J W Dubois, J N R Ruddick


Accelerated decay tests to investigate postulated effects of tannins on CCA efficacy in wood
1988 - IRG/WP 3497
Five groups of blocks (10 x 10 x 5 mm³) viz., Pinus patula, Pinus patula impregnated to 4% (w/w) tannin; Eucalyptus grandis, Eucalyptus grandis with natural tannins extracted; and extracted Eucalyptus grandis with tannins returned as above; were prepared. Blocks from each group were then treated to 0, 5, 10 and 15 kg/m³ CCA and challenged in four 15-week decay tests, viz., soil burial, and expos...
U L Scherer, A A W Baecker


The implementation of restrictions on the use of arsenic and chromium based wood preservatives in Sweden
1995 - IRG/WP 95-50062
In 1992 the Swedish National Chemicals Inspectorate introduced restrictions on the use of wood treated with arsenic and/or chromium based wood preservatives. Such wood is now in principle only allowed for use in ground contact or in water. These restrictions have had considerable influence on the use of wood preservatives for sawn timber for the Swedish domestic market. Thus only 35% of the preser...
J Jermer, M-L Edlund, K Nilsson


Generic code of good practices for wood preservation facilities
1994 - IRG/WP 94-50037
Wood preservation chemicals are designed to be toxic to wood destroying organisms. This toxicity, however, may not be limited to target organisms but the use of these chemicals can potentially harm various biota and humans as well. This fact dictates that adequate precautionary measures be employed to prevent any harmful effects to humans and the environment. The extensive experience with wood tre...
V N P Mathur, G Das


Industrial wood preservation in Kenya. Present status – future prospects
2005 - IRG/WP 05-30385
Although some 50 years old, industrial wood preservation in Kenya does not appear to have technically, scientifically, and commercially evolved and contributed to significantly extend service lives of timbers, protect health and the environment, and curb unnecessary over-exploitation of forests. The population of the country has increased by 530% over the past 50 years; regular excisions have red...
R Venkatasamy


Laboratory evaluation of metallic naphthenates as wood preservatives
1991 - IRG/WP 3654
Fungicidal and termiticidal efficacy of copper and zinc naphthenates was appraised according to Japanese standardized laboratory testing methods. Copper and zinc naphthenates succeeded in protecting wood from decay fungi at retentions of 0.5 and 1.0 kg/m³ as metal, respectively. [JIS A 9302 (1976)] when they were applied to vacuum/soak impregnation [JIS A 9301 (1976)]. With respect to the fungici...
K Tsunoda, M Sakurai


Protection of rubberwood with modified creosote
1998 - IRG/WP 98-30165
Creosote is a renowned wood preservative but has certain disadvantages like obnoxius odour and colour, with its unpaintability and bleeding from wood surface may create environmental hazards. An effort has been made to isolate chemical fractions from creosote to obtain clean odourless preservative formulations by subjecting to steam distillation (SVC). Rubberwood treated with SVC and tested for it...
H C Nagaveni, H S Ananthapadmanabha, G Vijayalakshmi, M N Sharma, K H Shankaranarayana


Influencia de la impregnación con soluciones tánicas en la estabilidad dimensional de la madera de Pinus pinaster Ait. procedente de España
1992 - IRG/WP 92-3686
En virtud de la importancia que presenta la madera de Pinus pinaster Ait. en el sector constructivo español, se ha sometido a esta a tratamientos en autoclave con distintas soluciones tánicas naturales y artificiales a fin de estudiar su incidencia en la estabilidad dimensional frente a exposiciones exteriores. En el estudio se pone de manifiesto el efecto creado por el tratamiento protector en ...
J A Rodríguez Barreal, J Cubillo Jordan de Urries, L Garcia Esteban


Observations on the effect of two preservatives on settlement and development of the marine wood-borer Martesia striata L
1983 - IRG/WP 498
Small heartwood specimens of three tropical hardwoods namely kusia or opepe (Nauclea diderrichii (De Wild) Merrill), emire or idigbo (Terminalia ivorensis A. Chev.) and subaha or abura (Mitragyna stipulose (D.C.) O. Kuntze) were treated with either creosote (BSS 144 type) or a copper-chrome-arsenic preservative and submerged in the sea at Tema, Ghana. They were regularly cleaned of fouling and obs...
J E Barnacle, F F K Ampong


Longterm monitoring of termite activity on multiple feeding sites: a laboratory method intended for the determination of attractant/repellent properties of wood preservatives and baits
2001 - IRG/WP 01-20225
A method is introduced allowing the continuous monitoring of the activity of a small laboratory termite- colony at 8 different feeding sites simultaneously. The test assembly consists of a small central polycarbonate-tube containing a colonie of Reticulitermes santonensis (de Feytaud) beeing connected with 8 external feeding sites by small glass-capillaries. The termites passing through the glass ...
M Pallaske, E Graf, H Takiuchi


The degradation of wood surfaces by water
1984 - IRG/WP 3289
Thin radial/longitudinal sections (~100 µ) of Scots Pine (Pinus sylvestris) and lime (Tilia vulgaris), were exposed to deionised water over the temperature range 25-65°C. Losses in wet tensile strength and toughness occurred rapidly at temperatures from about 50°C upwards. After about 2 months' exposure pine lost some 10-30% of its tensile strength and 20-60% of its toughness. For lime...
W B Banks, P D Evans


Comparative study on leaching of CCA from treated timber: Modelling of emission data
1994 - IRG/WP 94-50027
Results of a comparative study on leaching of CCA from treated timber are reported. The study aims at investigating the applicability of prestandard leaching test methods for modelling purposes. Prestandards used are the European standard proposed by CEN/TC38/WG11 and NEN 7345 (Dutch prestandard for building materials). Parameters of study are type of fixation, wood species (pine - spruce), specim...
G M F Van Eetvelde, M Stevens, L Van der Mijnsbrugge


Application of roller-pressing method to the novel liquid impregnation treatment of green timber
2001 - IRG/WP 01-40198
A transverse compression technique enabled us to impregnate liquid into green timber through replacement of the free water in the timber with a treatment liquid without any critical physical damage to the timber by the roller-pressing method. The roller-pressing is supposed to remove free water the cell cavities and to concurrently introduce the treatment solution into green timber in the treatmen...
M Inoue, K Adachi, K Tsunoda, Y Imamura, S Kawai


An attempt to develop a direct and reliable method for testing the preventive action of preservation treatments of wood against fungal decay
1980 - IRG/WP 2139
In wood preservation there are two classical ways for assessing the reliability of preventive treatments against wood decay: the laboratory tests in which the various parameters are evaluated independently and the field tests or service tests in which those parameters are acting together in the natural environment. One has always tried to build bridges between the two types of experiments and to e...
M Fougerousse


Soft rot decay of Belian (Eusideroxylon zwageri) wood
1995 - IRG/WP 95-10119
The heartwood of Belian (Eusideroxylon zwageri), an East Malaysian timber species, is naturally durable due to its certain unique anatomical features and high content of extractives. The timber can tolerate years of exposure to hazardous conditions in ground contact and other situations without any significant loss in its strength. A few Belian transmission poles sampled from one locality in Saraw...
A H H Wong, A P Singh


Previous Page | Next Page