Protection of pine sawtimber and sawn timber against blue stain in Poland
1983 - IRG/WP 3193
The purpose of this paper is the synthesis of more important results of basic and applied research that have been grouped in the following problems: 1.: Fungi causing blue stain in the pine wood, occurring in Poland. 2.: Moisture content changes of pine sawtimber and sawn timber as the factor of blue stain producing fungi development. 3.: Effect of sapwood moisture content on the degree of wood st...
E Tarocinski, M H Zielinski


Effects of boron formulation on specific timber types used in ships of historical importance
1991 - IRG/WP 3676
This paper reports results of preservative treatment and leaching experiments, using borax, polybor and boracol 20, on small wood blocks of English oak and American pitch pine heartwood. Earlier experiments on the performance of various biocides as possible additives to bilgewater to prevent fungal decay of shipping timbers had suggested that some formulations of boron might be associated with phy...
B King, G M Smith, J W Palfreyman, S McCutcheon


Some textile auxiliaries as wood protective agents
2007 - IRG/WP 07-30417
This study evaluated some textile auxiliaries applicable for wood protection. Commercial alkoxysilane quarternary ammonium formulation and fluorocarbon based water-oil repellent were tested for their ability to provide hydrophobicity and antifungal effect to solid wood samples. Scots pine (Pinus sylvestris L.) sapwood samples were impregnated with 25, 50 and 100 % concentrations of the above menti...
E Dizman, A Temiz, N Terziev, Ü C Yildiz


Protection of wood for above ground application through modification with a fatty acid modified N-methylol/paraffin formulation
2007 - IRG/WP 07-40378
Hydrophobic chemical modification can be regarded as an alternative approach to conventional wood preservation using biocides in order to protect wood in hazard class 3 according the European Standard EN 335-1. A formulation containing fatty acid modified N-methylol/paraffin and an aluminium salt catalyst was used to change the material properties of wood in order to protect wood from fungal dec...
Nguyen Hong Minh, H Militz, C Mai


Amine Oxides for Use in Wood Protection: I. A Formulation Adjuvant and Performance Enhancer for Wood
2007 - IRG/WP 07-30425
Amine oxides have great potential for use in the area of wood protection. This paper highlights the advantages of using amine oxides as a formulation adjuvant and performance enhancer for different azoles. It was found that azoles are readily soluble in aqueous amine oxide solutions and form soluble concentrates. These azole/amine oxide concentrates have excellent storage stability and can be dilu...
Xiao Jiang, L Walker


Detection of Anti-Fungal Sapwood Extractives in Non-Durable Scots Pine (Pinus sylvestris), Rubberwood (Hevea brasiliensis) and Jelutong (Dyera costulata)
2007 - IRG/WP 07-10634
A general laboratory bioassay method of Woodward and Pearce (1985) was adopted to detect anti-fungal activity of sapwood or heartwood extractives of 5 Malaysian hardwoods [dark red meranti heartwood (Shorea spp.), red balau heartwood (Shorea spp.), kulim heartwood (Scorodocarpus borneensis), jelutong sapwood (Dyera costulata) and rubberwood sapwood (Hevea brasiliensis), including the temperate Pin...
A H H Wong, R B Pearce


Effect of amphiphilic antioxidant alkyl ammonium ascorbate on inhibition of fungal growth: Application to wood preservatives formulation
2008 - IRG/WP 08-30466
Amphiphilic surfactants were synthesized from ascorbic acid and different fatty amines and evaluated for formulation of wood preservation products. Characterization of physicochemical properties of the new compounds indicated classical behavior of cationic surfactants. Antioxidant properties, estimated using methyl linoleate oxidation inhibition method, were similar to that of ascorbic acid teste...
C Gérardin , T Koumbi Mounanga, P Gérardin


The role of chromium in wood preservatives under BPD - a review and the current situation in Europe
2008 - IRG/WP 08-30468
Already during the IRG-meeting in Trømso a paper was presented to give an overview regarding the situation on chromium (JÜNGEL et al. 2006). Already in that year there was an increased attempt to achieve a science-based correct and harmonised solution in Europe regarding the chromium-question by the European Commission. Nevertheless the competent authorities (CAs) and the industry were similarly...
P Jüngel, S Hellkamp


Vacuum drying of European oakwood: Color, chemistry and anti-oxidant potency of wood. Improving appearance in forest value added products
2008 - IRG/WP 08-40432
In hardwoods used for decorative and appearance purposes, wood colour is one of the most important factors of wood quality; in addition colour is related with durability and biological decay of wood. Wood discolouration during drying is mainly affected by heat, light, physiological reactions, combinations of reactions, biochemical and chemical reactions, and micro-organisms attack. In freshly fell...
S Sandoval, W Jomaa, F Marc, J-R Puiggali


Discovering anti-fungal agents in New Zealand native plants for use in wood protection
2009 - IRG/WP 09-10692
Extracts from Hinau (Elaeocarpus dentatus) leaves were tested in the laboratory for antifungal activity. In addition, the anatomical structure of the leaf was also examined by a combination of light and scanning electron microscopy. Chemical characterisation of the extracts and investigation into potential use of its components for wood protection is underway. A combination of light microscopy (...
C Rickard, T Singh, A Singh, R Newman


Evaluation of Water Repellency of Treated Wood Using Several Alternative Methods
2009 - IRG/WP 09-20419
In this study, the results of water repellency testing using a digital swellometer method for water-borne organic-preservative systems with water repellent additives are reported. The findings suggest that the traditional method of using matched untreated controls as a reference developed from historic solvent-based treatments for determination anti-swelling efficacy (ASE) may underestimate the a...
L Jin, A F Preston


Synthesis of a rosin amide and its resistance to wood decay fungi
2009 - IRG/WP 09-30517
Rosin was reacted with diethyltriamine (DETA) after being modified by acryl acid with the weight ratio of 4.5:1 and a rosin amide (RA) derivative was produced at the conditions as follows: modified rosin and DETA mole ratio of 1:3.5, dimethylbenzene as water carrying agent, reaction temperature of 160-180°C, and reaction time of 8h. The chemical structure of the product as RA was identified by F...
Shuangyue Li, Shujun Li, Jing Wang


Evaluation of formulation type on the efficacy of bifenthrin as a glueline termiticide for veneer based wood products
2010 - IRG/WP 10-40486
Field trials were carried out in Australia on Coptotermes acinaciformis to evaluate the efficacy of various bifenthrin formulations. One trial tested plywood made by Zelam at their research facility in New Zealand and compared three emulsifiable concentrate formulations (EC), a suspension concentrate (SC) and an encapsulated formulation (CS). A second trial compared laminated veneer lumber (LVL)...
P Lobb, A Siraa


Effects of intumescent formulation of vinyl acetate-based coating on flame-retardancy of thin painted red lauan (Parashorea spp.) plywood
2011 - IRG/WP 10-40537
Using intumescent coatings on wood-based materials is an effective method for fire safety. The intumescent coatings consist of four major components: (1) binder resin (BR), (2) carbonizing substance (CS), (3) foam producing substance (FPS) and (4) dehydrating agent (DA). Previous studies have demonstrated that the formulation of the four components strongly influences the performance of coatings. ...
Chih-Shen Chuang, Kuang-Chung Tsai, Te-Hsin Yang, Ming-Kuang Wang, Chun-Han Ko


Novel Approaches to the Development and Testing of Anti After-glow Additives for CCA-based Treatments of Poles
2011 - IRG/WP 11-30561
In this paper, a field fire stake testing screen method is described. This method uses stake samples from matched wood sources allowing replicates from different boards to be included. The method is easy to control and can provide quick comparative fire resistance test results. The parameters measured from the tests are percentage weight loss, minimum residual circumference and residual thicknes...
L Jin, P Walcheski, A Preston


Relationships between heat treatment intensity and some conferred properties of different European softwood and hardwood species
2012 - IRG/WP 12-40593
Effect of treatment intensity on conferred properties like elemental composition, durability, anti swelling efficiency (ASE) and equilibrium moisture content (EMC) of different European softwood and hardwood species subjected to mild pyrolysis at 230°C under nitrogen for different durations has been investigated. Independently of the wood species studied, elemental composition is strongly correl...
M Chaouch, S Dumarçay, A Pétrissans, M Pétrissans, P Gérardin


Effects of nano-wollastonite impregnation on fire resistance and dimensional stability of Poplar wood
2012 - IRG/WP 12-40595
The fire-retardant properties of Nano-Wollastonite (NW) in poplar wood (Populus nigra) were determined in this study. Some physical properties such as water absorption, volumetric swelling and Anti-Swelling Efficiency (ASE) were also measured. Specimens were prepared according to the ISO 11925 standard for the fire-retarding properties, and ASTM D4446-2002 standard for the physical properties. Imp...
A Karimi, A Haghighi Poshtir, H Reza Taghiyari, Y Hamzeh, A Akbar Enayati


The Effect of Water Repellent on Semi-Field Leaching of Active Substances from Metal Free Wood Preservative Formulation
2013 - IRG/WP 13-30615
The risk assessments for the use of wood preservatives proposed by the OECD and used under the Biocidal Products Directive (BPD) (98/8/EC) require the derivation of leaching rates for active substances. These rates are to be used as input data in to agreed exposure scenarios. A comparison of the leaching of active substances from wood treated with a metal free preservative formulation with and wit...
D G Cantrell


Coconut shell pyrolytic oil as wood protectant against biodeterioration
2014 - IRG/WP 14-30648
Extensive research on various plant and microbial extracts has been conducted as an alternative to using synthetic or inorganic chemicals for wood protection. Development of effective and low environmental impact products and technologies for wood protection is imperative. In the present study, the efficacy of coconut shell pyrolytic oil as a wood protectant is analysed in terms of its antifungal,...
K S Shiny, O K Remadevi


Improving dimensional stability of thermally treated wood by secondary modification – potential and limitations
2014 - IRG/WP 14-40664
The potential of treating thermally modified wood with melamine resin to improve the dimensional stabilization is tested in this research. Two different boards of poplar (Populus ssp.) were cut into two halves. One half of each board was thermally modified (T1 and T2) in a commercial process, the other half was used as untreated reference material. The material was thermally modified using the vac...
G Behr, K-C Mahnert, S Bollmus, H Militz


Performance of kiln-dried and air-dried anti-sapstain treated pallet timber under use scenarios against wood discolouring fungi
2015 - IRG/WP 30669
During their lifespan there is a high probability that wooden pallets and packaging material will be exposed to rainfall or rewetting conditions, increasing the risk of growth of discolouring fungi. Kiln-drying of wooden pallets and packaging material without anti-sapstain treatment does not give efficient protection against wood discolouring fungi during rewetting periods. However additional temp...
A Steitz, E Stoyanova, N Pfabigan, R Gründlinger


Search for an anti-sapstain treatment for fresh radiata pine wood in compliance with European BPD norms: Field Tests
2015 - IRG/WP 15-30673
In response to the impending restrictions on the use of pesticide active ingredients developed to control the staining of fresh wood, as a result of regulation issued in 2009 by the European Union, a project was proposed to test an alternative anti-sapstain treatment that meets both the European restrictions and the performance required for an export-quality radiata pine fresh wood treatment. A se...
P Montes C, T Hanke W


Effect of the Storage Time of Logs in Anti-Stain Treatment Effectiveness
2016 - IRG/WP 16-30683
Storage of green lumber, for 7 months, operationally treated with anti-stain products, depending on the storage time of the logs (10, 20 and 30 days) post harvesting allows to affirm that with increasing storage time of the logs, occurs a progressive increase in intensity, severity and types of fungi present in the logs. It is further noted, a significant increase in the percentage of sawn lumber ...
M A Peredo, C Barria


Anti-Fungal Activity on Some Wood extracts as a Wood Protectant
2016 - IRG/WP 16-30684
In this study, six different wood barks were used, where obtained bark extracts were blended with potato-agar in order to investigate their antifungal properties. To determine the inhibition effectiveness of extractives, two different fungi; Coniophera puteana and Trametes versicolor were selected. Fungal activity was carefully observed for the duration of seven days. Following biological testing,...
Ö Özgenç, S Durmaz


Superhydrophobic treatment of Norway spruce wood for improvement of its resistance against brown rot and moulds
2016 - IRG/WP 16-40734
Water repellence of wood can be increased and its some other properties influenced by introduction of hydrophobic chemicals into and on cell walls without affecting the wood’s bulk density due to lumen filling. Herein, a simple dipping method to insert octadecyltrichlorosilane (OTS) into cell walls and to deposit the self-assembled hydrophobic monolayers (SAMs) of OTS is reported. It was found o...
A Kumar, P Ryparová, P Hajek, B Kričej, M Pavlič, A S Škapin, M Šernek, J Tywoniak, J Žigon, M Petrič