Evaluation of a new anti-sapstain formulation
1994 - IRG/WP 94-30035
A new anti-sapstain mixture, which consists of 2% IPBC (3-iodo-2-propynylbutyl carbamate) and 1.5% DCOI (4,5-dichloro-2-n-octylisothiazolin-3-one), was evaluated by three methods in the laboratory. A standardized test (JWPA standard 2) demonstrated that the new anti-sapstain formulation was highly effective in controlling growth of monocultures of five test fungi on wood substrate. When exposed to...
K Tsunoda, H Kumagai, M Sakurai


A shower test protocol for measuring antisapstain wash-off from small individual log billets
1996 - IRG/WP 96-50069
According to New Zealand Timber Industry Federation statistics New Zealand exported 4,835,000 m³ of logs in 1994 and it is estimated that c. 20% were anti-sapstain treated. Loss of preservative from logs as a result of rain impact after application is of considerable concern both with respect to potential loss of efficacy and environmental contamination. Whilst Environment Canada have a proposed ...
A J Pendlebury, H Pearson


Surface retentions of PCP, TCMTB and MTC obtained during a field trial of antisapstain formulations
1993 - IRG/WP 93-20002
Formulations containing NaPCP or TCMTB and MTC were included as reference products in a recent field trial of antisapstain formulations in Queensland. Retentions of these actives on the surface of treated sawn Pinus elliottii were monitored by ultrasonic solvent extraction of excised samples and analytical determination by high performance liquid chromatography. Distribution of actives with depth ...
D E Ferlazzo, M D Needham, M J Kennedy


Investigation of the suitability of silver fir (Abies alba Mill.) for thermal modification
2004 - IRG/WP 04-40275
In this study the suitability of silver fir (Abies alba Mill.) was examined for thermal modification. Comparative experimental investigations were performed with silver fir and Norway spruce (Picea abies Karst.) after thermal treatments. Besides properties, which characterize the quality of heat treatments, like dimensional stability and resistance against fungal attack, strength properties of the...
C Brischke, A O Rapp


Effectiveness of some microbiocides against the development of molds and sapstain in Pinus elliottii
1981 - IRG/WP 3169
Eleven commercial biocidal formulations were tested in the field to determine their effectiveness in protecting logs and lumber of Pinus elliottii sapwood from sap stain and molds. Among these formulations 2-(thiocyanomethylthio) benzothiazole showed the best performance in controlling both types of fungi. Potassium N-hydroxymethyl-N-methyl dithiocarbamate and the mixture potassium N-methyl dithio...
S Milano


Comparison of the FRIM and forest research laboratory methods for screening of anti-sapstain formulations
1999 - IRG/WP 99-20170
Two laboratory methods for screening of anti-sapstain formulations were compared. The method adopted by the Forest Research Institute Malaysia (FRIM) involved 3 weeks assessment of rubberwood (Hevea brasiliensis) blocks, dipped in the candidate formulation and inoculated with mycelial/spore suspension of sapstain (Botryodiplodia theobromae) or decay (Schizophyllum commune) fungi, and incubated on ...
A H H Wong, D R Eden, C M Chittenden, M E Hedley, R N Wakeling


Some studies on fungal deterioration of rubber wood (Hevea brasiliensis)
1980 - IRG/WP 2140
For the sreening of anti-stain chemicals trials with selected agricultural fungicides and new chemicals were carried out. Botryodiplodia theobromae, Aspergillus sp. and Penicillium sp. were used at test organisms. For testing the durability of rubber wood (Hevea brasiliensis) suitable local rotting fungi (Basidiomycetes), based on high degrading power, which may later be employed in standard tests...
A Sujan, A G Tan, M Stevens


Detoxification of methylene bisthiocyanate by bacteria isolated from freshly felled, anti-sapstain treated timber
1993 - IRG/WP 93-10017
The microbial defacement of freshly-felled timber treated with organic biocides continues to be a major problem in stored lumber. As part of a study to investigate the depletion in chemical activity of methylene-bis-thiocyanate (MBT) in green timber, bacteria were isolated from freshly-felled boards of Corsican pine (Pinus nigra var. maritima Arnold) previously treated with different biocides. The...
R J Wallace, R A Eaton, G R Williams


Influences of the hydro-thermal treatment on physical properties of beech wood (Fagus orientalis)
2005 - IRG/WP 05-40303
Influences of the hydro-thermal treatment on physical properties of beech wood were studied. Wood specimens (2×2×2cm) were treated in two steps. At first step, samples were treated at 160,180 & 200ºC for 4, 5 & 6 hours. At second step, treated samples were cured based on their first step treatment temperatures (160,180 & 200ºC) for 16 hours. The treated samples were soaked in water...
B Mohebby, I Sanaei


Time limits for holding logs to achieve successful antisapstain treatment
1997 - IRG/WP 97-30126
The purpose of these trials was to determine the maximum time that logs can be left in winter and summer before treatment if sapstain, caused by pre-treatment infection, was to be prevented. Pre-treatment storage conditions representative of average temperature and humidity for the winter months of June, July and August, and of moderately severe summer conditions, for the Bay of Plenty, New Zealan...
D R Eden, R N Wakeling, C M Chittenden, J G Van der Waals, B Carpenter


Performance of Tuff Brite C™ and other formulations against blue-stain, mold and brown-stain in freshly-sawn rubberwood (Hevea brasiliensis) in the humid tropics of Peninsular Malaysia
1997 - IRG/WP 97-30163
The relative anti-sapstain and anti-mold efficacies, including brown-stain development in freshly-sawn rubberwood (Hevea brasiliensis) in the Malaysian tropics, between selected water-based product concentrations of formulations Tuff Brite CTM without/with added Borax (at 1.5/0, 1/1.5, 1.5/1.5 and 2%/1.5%), PQ8TM without/with added Borax (at 2.5/0, 1.5/1.5, 2/1.5 and 2.5%/1.5%) and NeXgenTM/NeX-Br...
A H H Wong, T L Woods


A field test with anti-stain chemicals on sawn pine timber in Brazil
1989 - IRG/WP 3513
Field tests were carried out in São Paulo State - Brazil, to evaluate pre-treatment formulations of O-Phenyl-Phenol (OPP) based products. The Sodium Pentachlorophenate solution was used as a reference formulation. The treated test blocks were stacked in a covered shed, and in an uncovered place for air drying. The evaluation was done by measuring the percentage of stained surface on each test blo...
M B B Monteiro, S Brazolin


Evaluation of the effectiveness of defence anti-stain in the control of sapstain in laboratory and field tests
1990 - IRG/WP 3593
The anti-sapstain product Defence Anti-stain (DAS) has been evaluated internationally in laboratory and field tests during the years 1988 and 1989. Results of tests carried out by institutes and by own companies in countries like Indonesia, Ivory Coast, Japan, Portugal, Belgium, The Netherlands and Spain will be presented. In the several tests Defence Anti-stain showed a high fungicidal activity t...
G Rustenburg, C J Klaver


Comparison of two laboratory methods for screening potential anti-sapstain chemicals
1993 - IRG/WP 93-10036
Two methods were used to screen a number of potential anti-sapstain chemicals in the laboratory. In one method miniature boards of freshly felled Scots pine sapwood were dip treated with the candidate chemical, sprayed with a suspension of stainers or moulds and incubated for five weeks. In the other method antibiotic assay discs were treated with precise quantities of chemical, plated out on malt...
S M Gray, D J Dickinson


Commercial antisapstain chemicals in New Zealand
1980 - IRG/WP 3142
Almost all sawn timber of exotic softwoods (principally Pinus radiata) and a large proportion of indigenous sawn timber receives an antisapstain chemical treatment to prevent fungal degrade during subsequent seasoning, storage, or transportation (if exported). Antisapstain chemicals are also widely used to protect freshly peeled round produce during drying. A further, specialised, use is as the fu...
J A Butcher


Anti-bluestain treatment developed for log cargoes stacked in subtropical conditions for export on logging ships
1995 - IRG/WP 95-30081
Subtropical environments impose conditions of temperature, humidity and rainfall which are optimal for growth of bluestain fungi. Unprotected softwoods under such conditions become bluestained three days after felling. Furthermore, intervals between harvesting and delivery to export marketplaces exceed the 30-day protection periods attributed to anti-bluestain formulations in such conditions. Thes...
A A W Baecker, M Behr, G D Shelver


Development process of a new anti-sapstain formulation and its present status with the relevant problems
2001 - IRG/WP 01-30257
An anti-sapstain formulation, which contains 2-(thiocyanomethylthio)benzothiazol (TCMTB) and methylene-bis-thiocyanate (MBT) as active ingredients, was developed by a technical agreement with Buckman Laboratories (Memphis, TN, USA) as an alternative to chlorinated phenols for the Japanese market. The formulation was commercialized as BAM 12 years ago. As anti-sapstain treatment is commonly conduct...
K Nobashi, Y Nomura, K Tsunoda


Migration of chlorothalonil and carbendazim in fruits stored in wood treated with the anti-sapstain formulation Tuff Brite C
1997 - IRG/WP 97-50097
Fruits and vegetables stored in treated wood boxes are in contact with the products used for the treatment. In order to obtain regulatory approval for incidental food contact it is necessary to determine the quantity of residues on these fruits or vegetables. When the active materials are used in agriculture it is required that residues found are below to the MRL fixed for these substances. In the...
J F Cooper, D Riboul, M De Vleeschauwer, T L Woods


A new type of biocide suitable for use in different fields of wood preservation
1993 - IRG/WP 93-30014
A new type of polymeric biocides was developed containing quaternary ammonium and boron ester groups as active structure elements, to overcome the disadvantages of AAC's in wood preservation use and to utilise their good performance due to a broad efficacy against fungi on the other hand. The new biocides called polymeric betains have been tested in laboratory and field tests and especial...
V Barth, H Härtner


An appraisal of anti-sapstain chemicals in Queensland, Australia
1985 - IRG/WP 3331
Eleven formulations were tested in the field for effectiveness against sapstain, mould and fungi on Pinus elliottii in Queensland. The commercially used sodium pentachlorophenoxide (0.5% a.i.) and Captafol (0.2% a.i.) performed well. Busan 1009 (0.3% a.i.), Protek T (5.0% a.i.), Woodgard E.S. and E.C. (0.8% a.i.), together with sodium tetrachlorophenoxide (0.5% a.i.) offer potential as anti-sapsta...
L E Leightley


An anti-termite formulation for soil treatment with natural products and its efficacy against Coptotermes formosanus Shiraki
2003 - IRG/WP 03-30319
An anti-termite formulation of an environmental conservation type for soil treatment was developed. The formulation was composed of decanoic acid (n-capric acid, an fatty acid derived from coconut oil with ten carbons) as an active ingredient and other natural products. Experiments to examine the efficacy of the formulation against Coptotermes formosanus Shiraki were conducted at the termite field...
S Yoshida, T Nakagaki, A Igarashi, A Enoki


Japanese standardized method for evaluating effectiveness of anti-sapstain and anti-mould chemicals
1988 - IRG/WP 2299
Japan Wood Preserving Association established a method for testing effectiveness of chemicals against sapstain and mold fungi on wood in 1979. The method is concerned with a laboratory technique using small timber specimens (20 x 50 x 3 mm³), petri dish and 5 test fungi. Effectiveness of each candidate chemical is evaluated on the basis of the relative resistance to sapstain and mold fungi which ...
K Tsunoda, K Nishimoto


Field evaluation of anti-sapstain products
1987 - IRG/WP 3402
Product A based on methylenebisthiocyanate, product B based on methylenebisthiocyanate plus 2-thiocyanomethylthio-benzothiazole, product C based on 2-thiocyanomethilthio-benzothiazole and product D based on didecyl dimethil ammonium chloride plus 3-iodo-2 propynil butyl carbarnate were evaluated on Pinus radiata sawn timber as fungicides for sapstain and mould in the Sawmill Division of the Univer...
M C Rose, A Bedoya


Evaluation of the effectiveness of Tuff Brite C in the control of sapstain in laboratory and field tests
1992 - IRG/WP 92-3718
Since 1990, the anti-sapstain product Tuff Brite C (ASC 66898) has been evaluated internationally in laboratory and field tests, and has been commercially introduced in New Zealand. The product is an aqueous flowable formulation of chlorothalonil and carbendazim. Efficacy tests which have been carried out in New Zealand, Australia, USA, South Africa and Europe are described and summarized. Tuff Br...
T L Woods, C J Klaver


Performance of proprietary formulations of anti-sapstain preservatives on Hevea brasiliensis timbers in laboratory tests
1989 - IRG/WP 3532
A total of 10 proprietary and two experimental formulations were assessed for their effectiveness against sap-stain caused by Botryodiplodia theobromae on Rubberwood (Hevea brasiliensis). Sterilized wood samples 5x20x40 mm³ were dipped in the test chemicals for 60 seconds and then inoculated with 0.5 ml of culture filtrate of Botryodiplodia theobromae for incubation in sterile, damp petri dishes....