A soil-less test of treated wood
1978 - IRG/WP 2105
The objective of this work is to devise an accelerated test for preservatives to be used in places away from soil contact. There may be compounds or mixtures which will protect wood or wood derived materials from decay in such articles as sash and doors, boardwalks, steps, laminated arches and the like, and possess properties that make them preferable to the heavy-duty preservatives used for poles...
E A Behr


Lab and field test results for wood treated with polymeric alkylphenol polysulfide
2001 - IRG/WP 01-30268
A new wood preservative based on polymeric alkyphenol polysulfide (PXTS-A) is being evaluated in a series of laboratory and field tests and the results continue to show promise. A modified formulation (PXTS-B), which contains additives to reduce the viscosity, is being evaluated along with the original formulation. Soil block decay tests comparing PXTS-B with CCA-C indicate that PXTS-B is equally ...
J Goswami, A Abramson, R Buff, D D Nicholas, T Schultz


Performance of Two Imidacloprid-Treated Malaysian Hardwoods in an Accelerated Aboveground Termite Test
2005 - IRG/WP 05-30389
The performance of the chloronicotinyl insecticide imidacloprid as a wood protecting termiticide, under a simulated Malaysian biological hazard class H2 (exposure aboveground indoors against termites and wood borers), was evaluated by a novel termite field test protocol. Replicate end-grain sealed air dried test blocks (20 x 20 x 20 mm) of two Malaysian hardwoods, Kembang Semangkok (Scaphium spp.)...
A H H Wong


The remaining concentration of inorganic wood preservative components in EN 252 stakes after ground contact
2000 - IRG/WP 00-50159
In order to determine the biological efficiency and the remaining concentration of different inorganic and organic active ingredients during service, EN 252 specimens were impregnated with 3 copper based wood preservatives. The stakes were installed in the test field of the DESOWAG GmbH, Rheinberg, for at least 7 years. At the end of the field test some of these stakes were divided into 10 uniform...
E Melcher, H-W Wegen


Resistance of borate-treated lumber to subterranean termites in the field
1998 - IRG/WP 98-10255
Borate-treated wood samples were tested for their resistance against subterranean termites in the field. Wood samples (10.5x10.5x40cm3) of western hemlock were pressure impregnated with disodium octaborate tetrahydrate (DOT) and didecyldimethylammonium chloride (DDAC), and assigned into two groups on the basis of boron contents:high retention (1.5-2.2%BAE) and low retention(O.7~1.3%BAE). Eight rep...
K Tsunoda, A Adachi, T Yoshimura, A Byrne, P I Morris, J K Grace


Relative merits of laboratory and field tests for assessing wood decay resistance
1993 - IRG/WP 93-20009
Laboratory and field trials have long been employed for assessing natural durability of a variety of wood species, but there is a continuing debate concerning the relative merits of approach. While laboratory tests provide carefully controlled conditions for decay, they are often criticized for being too artificial to produce meaningful results. Conversely, field trials often vary widely between t...
T C Scheffer, J J Morrell


Resistance of acetylated wood to biological degradation. Evaluation of field test
1997 - IRG/WP 97-30139
Acetylated wood samples were tested in ground contact (stake test) at two test fields, one in Simlångsdalen, Sweden, and one in Viikki, Finland, according to European standard EN 252. The test samples were inspected annually and their condition was compared with that of untreated controls and of samples treated with two reference CCA preservatives. The use of untreated controls and preservative t...
P Larsson Brelid, R Simonson, Ö Bergman


Growth of sapstain fungi in scots pine and the effect of timber ageing
1998 - IRG/WP 98-10269
A trial was initiated to study the growth of known isolates of sapstain fungi in scots pine (Pinus sylvestris) which had been naturally aged or sterilised by autoclaving or irradiation. Sawlogs cut from commercial thinnings were reduced to billet size and the exposed ends were painted with a bituminous sealant to reduce moisture loss. Some billets were inoculated after autoclaving or gamma-irradia...
N J Strong, J F Webber, R A Eaton


Termite physical barriers: Update on retrofitting Granitgard around 'mock up' buildings after four years
1996 - IRG/WP 96-10140
This field experiment was installed four years ago (March 1992) to evaluate the effectiveness of graded crushed granite stone, commercially marketed under the name, Granitgard, as a physical termite barrier when retrofitted around 'mock-up' buildings. The field site is located at Walpeup in the semi-arid mallee region of north-west Victoria (360 km from Melbourne), and there are ...
B M Ahmed, J R J French


Comparative field performance of CCA and CCA-water repellent treated Southern pine lumber
1995 - IRG/WP 95-30089
This paper describes the field performance of end-matched southern pine boards treated with either CCA type C or CCA type C containing an emulsion water repellent (WR) additive. Boards were either kiln or air-dried after treatment, constructed into decks, and exposed for over 3 years at Harrisburg, NC. During this exposure, matched boards were monitored for internal moisture content, cupping at mi...
A R Zahora


Pentachlorophenol and tributyltin oxide - the performance of treated Pinus radiata after 12 years' exposure
1986 - IRG/WP 3361
Pinus radiata samples were impregnated with a range of light organic solvent preservatives and copper/chrome/arsenic salt and exposed with no surface coating both in and above ground for 12 years. Inspection of the test samples revealed that some formulations of light organic solvent preservatives will give good fungal protection and reduce splitting in Pinus radiata exposed externally without a s...
R S Johnstone


Five years leaching of Boron
1999 - IRG/WP 99-30195
The diffusibility of Boron in wood and thus its leaching behaviour in water contact is known since long. Nevertheless quantitative data on the long-term leaching behaviour are rare. Consequently, field exposure tests were started with beam-segments treated with pure boric acid and with poles treated with CCB. Detailed data of more than five years of field exposure are now available. Pure boron tre...
A Peylo, H Willeitner


Influences of the hydro-thermal treatment on physical properties of beech wood (Fagus orientalis)
2005 - IRG/WP 05-40303
Influences of the hydro-thermal treatment on physical properties of beech wood were studied. Wood specimens (2×2×2cm) were treated in two steps. At first step, samples were treated at 160,180 & 200ºC for 4, 5 & 6 hours. At second step, treated samples were cured based on their first step treatment temperatures (160,180 & 200ºC) for 16 hours. The treated samples were soaked in water...
B Mohebby, I Sanaei


The need for realism in wood preservation research. A key address
1983 - IRG/WP 3254
The approval of a chemical for use as a timber preservative and the design of in service retention requirements represents an act linking fundamental research and commercial timber preservation. How difficult is it to translate figures generated through controlled experimentation into working specifications and how confident can we be in the methods used to provide such figures? The chairman of Wo...
L E Leightley


Evaluation of teak sawdayst Tectona grandis L Fil as a potential source to obtain a natural wood preservative in Colombia
2004 - IRG/WP 04-30356
Plantation Teak (Tectona grandis L. Fil) has been tested as a possible source of natural wood preservatives due to the known excellent durability of old-growth teak wood. Field tests (ground proximity termite and above ground simulated decking exposures) were established in Colombia in April 2003 at two different test sites with different climates (Tropical Dry and Rain forest). Teak heartwood ex...
A Castillo, Y Cabrera, A F Preston, R Morris


Sapstain development on Jack pine logs in Eastern Canada
2000 - IRG/WP 00-10358
During 1998-99, a study was initiated to investigate the influence of seasons, log types and storage time on the sapstain development on jack pine logs at two sites in Eastern Canada. Jack pine trees (Pinus banksiana) were harvested into whole-tree and cut-to-length logs in spring and in autumn. Sapstain development was examined in these logs at 2 to 4 week intervals after felling. The mean stain ...
Dian-Qing Yang, R Beauregard


The evaluation of the effectiveness of wood preservatives by means of IUFRO's method for field tests with wooden stakes
1985 - IRG/WP 3348
Pinus elliottii and Eucalyptus saligna stakes treated with CCA-A, CCA-C, CCB, Cashew Nut Shell Oil and Benzotar solutions were exposed in seven test sites in Sao Paulo State, Brazil. After five years of exposure, between oil-borne preservatives Benzotar show better performance than CNSL (cashew nut shell liquid), and within waterborne preservatives the performance of CCB is not so good as that of ...
G A C Lopez, A M F Oliveira, E S Lepage


Leaching of active components from preservative-treated timber. Stages 2 & 3: Laboratory testing and comparison with semi-field testing
2004 - IRG/WP 04-20303
This part of the project is focussed on leaching from preservative-treated wood obtained by the laboratory test method CEN/OECD draft guideline, February 2003 ”OECD guideline for the testing of chemicals proposal for new guideline XXX. Estimation of Emissions from Preservative-treated Wood to the Environment: Laboratory Method for wood held in the storage yard after treatment and for wooden comm...
N Morsing, B Lindegaard


Time limits for holding logs to achieve successful antisapstain treatment
1997 - IRG/WP 97-30126
The purpose of these trials was to determine the maximum time that logs can be left in winter and summer before treatment if sapstain, caused by pre-treatment infection, was to be prevented. Pre-treatment storage conditions representative of average temperature and humidity for the winter months of June, July and August, and of moderately severe summer conditions, for the Bay of Plenty, New Zealan...
D R Eden, R N Wakeling, C M Chittenden, J G Van der Waals, B Carpenter


Co-operative research project on L-joint testing. Progress report to March 1986
1986 - IRG/WP 2272
Further sets of data received from CTFT (France) after 18 months exposure, BAM (Germany) after 18 months exposure, STU (Sweden) after 9.5 months exposure and TI (Denmark) after 12 and 17.5 months exposure are presented and discussed in conjunction with data previously reported. The new data are generally in agreement with those presented previously and indicate the major difference between the co-...
J K Carey, A F Bravery


A comparative study of some anti-splitting devices, using Eucalyptus saligna and hybrids of Eucalyptus saligna X Eucalyptus spp poles
1983 - IRG/WP 3251
It is commom for some Brazilian wood pole users to require devices such as banding steel, to avoid or reduce splits at the end of Eucalyptus treated poles. On other hand users and manufacturers do not have data to confirm the effectiveness of the banding steel types normally used such as galvanized "Steel-Belt" and galvanized "Wire-Belt". For this reason a comparative study was carried out includi...
F C Geraldo, J A C Sodré


Results on field stake tests against termite – Maximum for 8 years examination at Kumamoto in Japan
2003 - IRG/WP 03-10463
Various preservative treated or modified wood and charcoal painting stakes were tested in field, maximum for eight years in Kumamoto, distributed two main termite species, Coptotermes formosanus and Reticulitermes speratus. After two years in field, untreated sapwood of sugi (Cryptomeria japonica) were observed severe attacks by termites, but the preservative treated stakes were observed no signif...
K Suzuki


New applications of silafluofen to termite control
2001 - IRG/WP 01-30274
Silafluofen-based termiticides are widely used for soil and timber treatments in Japan, as silafluofen possesses advantageous properties of low fish toxicity and high chemical stability (to light, in soil, in alkaline environments, etc) in addition to high termiticidal activity and low mammalian toxicity. As new applications of silafluofen to termite control, we have developed another type of prod...
K Nakayama, Y Minamite, S Koike, Y Katsuda, K Nishimoto


Colonisation and detection of New Zealand sapstain fungi
2000 - IRG/WP 00-10329
Sapstain is the bluish black discolouration in logs and timber caused in New Zealand by Sphaeropsis sapinea (Diploida pinea) and more than twenty different species of the Ophiostomataceae Family. Laboratory and field trials were conducted by inoculating radiata pine to establish staining colour and extent of colonisation with various New Zealand sapstaining fungal species. Colonisation patterns, c...
J M Thwaites, R L Farrell


Suitability of cotton strip testing as a screening method for the development of wood preservative formulations
2003 - IRG/WP 03-20270
This paper outlines a simple and rapid test method for screening the efficacy of wood preservative formulations against microbiological attack using cotton strips. The method was evaluated against soft rot and was found to provide reliable information on the protection of lignocellulosic material against microbiological attack. The assessment is based on visual interpretation of decay and on a sim...