Some data on the activity of alternative fungicides for wood preservation
1985 - IRG/WP 3333
Data from laboratory tests against basidiomycete fungi are presented for 9 alternative fungicides in organic solvent formulations and also in water for one product. Results are compared with data for reference preservatives, tributyltin oxide, copper and zinc naphthenates and pentachlorophenol. Of special interest is the apparently better than additive effect of mixing tributyltin naphthenate and ...
A F Bravery, J K Carey


Investigation on different variation factors in the results of mycological test and means to reduce and avoid them
1986 - IRG/WP 2264
In order to clarify the causes of the dispersion observed in the results obtained with mycological tests made in accordance with standard EN-113, different factors assumed to be sources of the variations were studied. These included the moisture content of the test samples during the test, the influence of certain technological properties of the wood, the virulence of the fungus strains, the metho...
D Dirol


Comparative performance of several ammoniacal copper preservative systems
1997 - IRG/WP 97-30151
The efficacy of several ammoniacal copper-based wood preservative systems was evaluated in this study. The selection of potential co-biocides was based on the results of an agar plate test. Following this, the most promising systems were evaluated in a standard field stake test. Good correlation was found between the agar plate and field stake test results. Of the preservative systems tested, copp...
D D Nicholas, T Schultz


Evaluation of the corrosivity of the treated wood - Laboratory vs field test methodologies
2000 - IRG/WP 00-20211
The corrosivity of treated wood to fasteners has been evaluated using laboratory test procedures, including AWPA Standard E12-94. The standard method was modified in order to allow detailed study of commercial metal fasteners in terms of sample types, installation configuration and exposure conditions. Parallel field tests were also performed. The experimental results generated from these tests su...
L Jin, A F Preston


Effect of mobile fungicides on fungal pre-infection in radiata pine billets.
1999 - IRG/WP 99-30191
In New Zealand, fungal infection of logs begins directly after felling and whilst severe degrade can be prevented if antisapstain-treated within 24 hours, such short turn-around times of logs are not always practicable. However, conventional antisapstain formulations in use only provide an envelope of protection on the log surface but are unable to control pre-infections below the surface. The obj...
D R Eden, T Singh, B Kreber


Acetylated solid wood. Laboratory durability test (part 2) and field trials
1995 - IRG/WP 95-40048
Degradation of acetylated beech, pine and poplar by soft rot fungi was related to strength loss in a laboratory test. No strength loss was noticed for poplar acetylated to a weight percent gain (WPG) of more than 11.2% and beech with a WPG of 12.8%. Several field trials were set up to determine the durability of acetylated products in practice. They included a field test to determine the durabilit...
E P J Beckers, H Militz, M Stevens


Wood-based composites exposed to fungal degradation: Laboratory results
2001 - IRG/WP 01-40215
Oriented strandboard (OSB) and laminated veneer lumber (LVL) are widely used as residential construction materials. The durability of OSB and LVL against biological degradation has not been studied comprehensively. The objective of this research was to investigate the durability of OSB and LVL when exposed to wood decay fungi. Fourteen brown-rot and eight white-rot wood decay fungi were screened f...
V W Yang, B Illman, L A Ferge, R J Ross


Improvement of some technological and biological properties of poplar wood by impregnation with aqueous macromolecular compounds
1992 - IRG/WP 92-3721
Poplars (Populus spp) belong to the most important tree species in afforestation programs of the Netherlands. Due to their rapid growth, the wood quality is usually low. Therefore, studies were performed to elucidate whether some technological properties and the resistance against fungal attack could be improved by impregnation with water-soluble resins. The results showed that swelling and shrink...
R D Peek, H Militz, J J Kettenis


Using image analysis to rate wood stain trials
1993 - IRG/WP 93-10034
Assessing the extent of fungal discoloration on wood during laboratory trials is a subjective process which provides an opportunity for considerable variation between individual evaluators of specimens. The development of reliable systems for automatically assessing discoloration would minimize evaluator bias and permit comparisons between results from different laboratories. The use of image anal...
C M Sexton, A G Maristany,C C Brunner, J J Morrell


Test of N-tritylmorpholine in combination with synthetic pyrethroids against marine borers in tropical Australia and Panama
1991 - IRG/WP 4168
Test blocks ol Pinus sylvestris sapwood were pressure impregnated with white spirit solutions of N-tritylmorpholine, either alone or in combination with permethrin, deltamethrin or cypermethrin. They were exposed in the intertidal zone at Mourilyan Harbour, North Queensland, Australia and subtidally at either end of the Panama Canal. After 5 months' exposure at Naos Island at the Pacific ...
S M Cragg, J D Bultman


Field test results for the elimination of subterranean termite (Coptotermes formosanus) colonies by a bait system containing the IGR hexaflumuron
1997 - IRG/WP 97-10222
Field studies were conducted at Chichijima (Ogasawara Islands, Tokyo) to determine the effectiveness of a termite bait system (commercial name: Sentricon* system) containing hexaflumuron (Insect Growth Regulator: IGR) in the elimination of subterranean termite (Coptotermes formosanus) colonies. The level of subterranean termite activity on Ogasawara Islands is high resulting in extensive damage to...
K Suzuki, Y Morita, K Yamauchi


Experiences from a Danish large scale test by means of a new method of treatment by attack of true dry rot fungus (Serpula lacrymans) in buildings
1994 - IRG/WP 94-10064
Experiences from a new and epoch-making method of treatment in connection with the repair of attack of the true dry rot fungus, Serpula lacrymans (Fr.) S.F. Gray, are described. The paper presents the background of a large scale test comprising repair of more than 150 Danish buildings over a period of approximate 5 years. The method being both gentle to the building and presenting savings of at le...
O Munck, H Sundberg


Fungal-termite associations in the natural resistance of selected eucalypt timbers
1978 - IRG/WP 173
Butt billets of Eucalyptus regnans F. Muell., Eucalyptus grandis W. Hill ex Maiden, and Eucalyptus camaldulensis Dehnh., showing no visible signs of decay, were examined for the presence of fungi in outer, middle and inner heartwood. Fungi obtained in pure culture were characterized. Eucalyptus regnans yielded Cytospora eucalypticola van der Westhuizen, Trichoderma harzianum Rifai and Penicillium ...
D B A Ruyooka


Soft rot test of copper/chrome/arsenic treated heartwood of three Malaysian timbers
1991 - IRG/WP 2381
Standardized heartwood blocks of kempas (Koompassia malaccensis), keruing (Dipterocarpus sp.) and tualang (Koompassia excelsa) were impregnated with 0 to 6.3% (w/v) CCA and challenged to decay by a mixed inocula of Chaetomium globosum, Glenospora graphii, Humicola grisea, Petriella setifera and Trichurus spiralis in a containerized vermiculite-burial decay system according to draft CEN/TC 38 WG 4....
A H H Wong, R-D Peek


Contradiction between uptake of preservative in practical situation and laboratory testing
1992 - IRG/WP 92-2392
By brush treatment water- and solvent-based products were applied on boards of Scots pine and Norway spruce to achieve an uptake of 100 and 200 g/ml. In addition the scope of work to achieve the required uptake of preservative was determined under practical conditions for both product groups. EN 113 (RAL-GZ 830) tests were carried out to test the biological efficacy of products. After 18 months ex...
R Gründlinger, O Janotta, M Melzer


The fungal degradation of quaternary ammonium compounds in wood
1998 - IRG/WP 98-10263
This work focuses on the biodegradation of didecyldimethylammonium chloride (DDAC) by the mould fungus Gliocladium roseum within a woody matrix. Three sawdust types, distinguished by their treatment and amount of DDAC retained, were inoculated with the fungus and their DDAC loss was measured over 11 weeks. The rates of degradation varied depending on the sawdust; however, a significant loss of DDA...
J W Dubois, J N R Ruddick


Accelerated decay tests to investigate postulated effects of tannins on CCA efficacy in wood
1988 - IRG/WP 3497
Five groups of blocks (10 x 10 x 5 mm³) viz., Pinus patula, Pinus patula impregnated to 4% (w/w) tannin; Eucalyptus grandis, Eucalyptus grandis with natural tannins extracted; and extracted Eucalyptus grandis with tannins returned as above; were prepared. Blocks from each group were then treated to 0, 5, 10 and 15 kg/m³ CCA and challenged in four 15-week decay tests, viz., soil burial, and expos...
U L Scherer, A A W Baecker


Effect of angle of exposure on degradation of radiata pine during weathering trials
1988 - IRG/WP 2301
The importance of angle of exposure on the degree of weathering of materials has not been adequately resolved. In conventional tests, specimens are exposed at an angle of 45° facing the equator, but more recently experiments on polymeric materials have suggested that an angle of 0° may be preferable since this angle maximises levels of received ultra-violet radiation. In this paper the degradati...
P D Evans


Glulaminated poles - Progress report after 7 years' testing
1987 - IRG/WP 3444
In 1979 a number of glulaminated poles with various preservative treatments were placed in a greenhouse at Uppsala, at the Simlångsdalen test field in southern Sweden and under a power line just south of the Arctic circle in order to study their resistance against biological degradation. The tests have shown that the comparatively best performance will be obtained if each lamination is treated wi...
J Jermer, Ö Bergman


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 1: Treatment of reference samples
1977 - IRG/WP 426
It was agreed in Wildhaus on 15 May 1976 that preparations for the test detailed in Document No: IRG/WP/414 should commence immediately, but that initially only two water-borne preservatives should be used - a copper/chrome/arsenic (CCA) and a copper/chrome/boron (CCB) formulation respectively. PRL, England (R Cockcroft) would be responsible for supplying samples of the reference timbers treated w...
R Cockcroft, T B Dearling, W O Schulz, H V Borck


Fungal associates of Buprestis langi Mannerheim colonizing stored douglas-fir logs
1997 - IRG/WP 97-10220
Buprestid beetles are important colonizers of dead and dying conifers. The larvae of these beetles initially mine a gallery beneath the bark, then tunnel deep within the log. These beetles can cause extensive damage to wood, but it is their frequent association with internal fungal decay that causes the greatest concern. Many insects are capable of vectoring fungi that enhance their prospects for ...
C M Garcia, M Y Giron, J J Morrell


Comparison of the effects of borate, germanate and tellurate on fungal growth and wood decay
1992 - IRG/WP 92-1533
The tetra-hydroxy borate ion is known to undergo complexation with polyols and has been shown to inhibit dehydrogenase enzymes in this way. It has been previously suggested that this complexation is responsible for the inhibition of fungal growth and the protection of boron treated timber. Other ions that have the ability to complex with polyols have also been shown to inhibit dehydrogenase activi...
J D Lloyd, D J Dickinson


Soluble nutrient content in wood and its susceptibility to fungal discoloration and decay in above ground and ground tests
2000 - IRG/WP 00-10336
The objective of this comprehensive study was to reveal the impact of soluble nutrients in wood on its susceptibility to fungal discoloration and decay in various tests, which is important for the test methodology and standardisation. Seven tests were carried out including pure culture above and ground contact tests, above ground field test and laboratory ground contact tests. The samples containi...
O M Caballero, N Terziev


A below-ground exposure method for determining the resistance of woody and non-woody materials to attack by subterranean termites
1993 - IRG/WP 93-10012
With existing field test procedures, in which specimens are installed vertically to some of their length into the ground and spaced out from each other ("grave-yard" tests), variations in the rate of contact by termites between replicates can be common. Mechanical damage to specimens during inspection and re-installation may also be difficult to avoid. A new field test method, evaluated in Austral...
M Lenz, J W Creffield


Field testing of alkylammonium wood preservatives
1983 - IRG/WP 3248
The field test performance of five alkylammonium wood preservatives is described. The relative effectiveness of three unmodified formulations was determined by calculation of a Performance Index. Of the three, didecyldimethylammonium chloride was found to be superior to octyldecyldimethylammonium chloride, and both were more effective than alkyltrimethylammonium chloride. However, none were consid...
J N R Ruddick