Influence of soil moisture, Sarawak soil types and decay types on decay susceptibility of rubberwood and kelempayan
2012 - IRG/WP 12-10780
Wood and soils are important natural resources of the land, the former widely used as structural supports in contact with the latter. Many low durability wood species exposed to soil contact has reportedly high incidence of decay failures in poorly treated and untreated materials depending on soil types, properties and soil microbial virulence. This paper probes the relationship of the main soil t...
A H.H. Wong, P K.F. Chong, J Sabang


Determination of Izod Impact Strength on Wood: A Suitable Method to Detect Fungal Decay in Protective Effectiveness-Screenings of Wood Preservatives
2012 - IRG/WP 12-20484
For testing a large number of different substances regarding fungicide properties, the reduction of the decay test duration is advantageous. In the present paper the suitability of a method for testing plastics using an impact testing machine was examined. The results clearly show that the fungal attack of European beech by the white-rot fungus Trametes versicolor leads to a decrease of izod imp...
H Delenk, M Zauer, A Wagenführ


Evaluation of fungal infestation and decay in a simulated use class 3 situation (block test) after some years of exposure
2012 - IRG/WP 12-20487
The so named “block test” was designed as part of the assessment methodology for testing the behaviour of natural and modified wood used under use class 3 (EN 335-2) conditions. The test was developed to expose the wood close to the ground to an environment with high humidity and high biological activity, but not in soil contact. The present study describes the evaluation of fungal infestatio...
A Gellerich, K Röhl, S Adamopoulos, H Militz


Effects of microclimate, wood temperature and surface colour on fungal disfigurement on wooden claddings
2012 - IRG/WP 12-20490
Wooden claddings are common in façades in Norway, and Norway spruce (Picea abies) is the most frequently used species. The cladding is a major part of the facade, and it has visual requirements that may define the aesthetic service life. The visual changes that occur during weathering can be colour changes, abrasion or wear, blistering, flaking, and even cracks in the wood or coating, but more of...
L Ross Gobakken, G I Vestøl


Effects of oil types and treatment temperature on the properties of wood subjected to thermal modification in oil medium
2012 - IRG/WP 12-40574
The effect of the use of oil as a medium of heat transfer during thermal modification of different species of wood has been widely investigated with different results accruing with regards to the various end-use properties of the materials. However very little have been done on the effect of oil types as well as its interaction with treatment temperature on the resultant properties of the material...
L Awoyemi, M M Apetogbor, A A Oteng-Amoako


Effects of Nano-Wollastonite on Ignition Time Reduction in MDF
2012 - IRG/WP 12-40576
Effects of wollastonite nano-fibers on ignition time reduction in medium density fiberboard were studied. Nanowollastonite was applied at 5, 10, 15, and 20 g/kg dry weight basis of wood fibers and compared with control specimens. Two application methods of nanowollastonite were used: surface application, and internal application. Specimens of 150×130×9 mm were prepared and the ignition times wer...
H Reza Taghiyari, H Rangavar, P Noori, A Karimi


Biological performance of wood- and bamboo-polypropylene composites: Effects of particle content, particle size and Zn borate
2012 - IRG/WP 12-40577
Particle content and size of wood material in wood plastic composites (WPCs) can affect efficacy of WPCs against fungi and termites. This study evaluated fungal and termite resistance of WPCs manufactured by using two different levels of particle content (50 and 70%) and three different particle sizes (30, 60, and 100 mesh). In fungal resistance tests, Tyromyces palustris, a standardized test fung...
S N Kartal, S Aysal, E Terzi, T Yoshimura, K Tsunoda


Study on the Effect of Combined Nanosilver-Hygrothermal Treatment on Wood Properties
2012 - IRG/WP 12-40581
In this study, the impregnation process with nanosilver solution, before hygrothermal treatment was carried out to investigate its effect on some physical and mechanical properties of Iranian beech (Fagus orientalis Lipsky) and Russian imported spruce (Picea abies). Wood specimens were impregnated with nanosilver solution (400ppm) in an impregnation tank under pressure of 0.25 Mpa, for 20 minutes....
G Rassam, H Reza Taghiyari, A Karimi, B Jamnani, M Ebrahimi


The assessment of biological and mechanical properties of wood treated with ionic liquids – N,N-dimethylamine and 1-decylimidazole derivatives
2012 - IRG/WP 12-40582
This paper presents the results of tests of the effectiveness of action of new imidazolium and bis-ammonium ionic liquids against Basidiomycotina and Ascomycotina wood-destroying fungi. All the investigated ionic liquids showed high fungicidal action against Coniophora puteana. In order to characterize the influence of ionic liquids on mechanical wood properties, the compression strength along the...
W Przybylska


Effects Of Wood Preservative On Mechanical Properties Of Glulam Manufactured From Lower Density Malaysian Tropical Timber
2012 - IRG/WP 12-40590
This study is to investigate the effect of wood preservative on the mechanical properties of glulam timbers made from low density Malaysian hardwood timbers. Utilization of lower density Malaysian tropical timber for structural applications have not exploited extensively due to their inferior strength. By converting into treated glued laminated (glulam) timbers it could offer the possibility of th...
L Francis, Z Ahmad


Mechanical Properties of Hydrothermally Treated Beech Wood in Buffered Mediums
2012 - IRG/WP 12-40597
Hydrothermal treatment of beech wood in buffered mediums was carried out by aim of controlling the destructive effect of acids formed by degradation of carbohydrates on strength properties. Different mediums (water, buffer5, 7 and 8) and temperatures (160 and 180 °C) were used. Mechanical properties of specimens including modulus of rupture (MOR), modulus of elasticity (MOE) and toughness were de...
A Talaei A Karimi, K Yaghoobi, A Talaei


Improvement of the biological performance and dimensional stability of two tropical woods by thermal modification
2012 - IRG/WP 12-40605
Pink cedar wood and rubberwood were thermally modified at 230°C in air for 4 h or for 8 h, and then subjected to bending, compression and hardness tests to evaluate the effect of the treatment on these mechanical properties. The biological performance of the modified wood was also determined, according to EN113, and the dimensional stability measured by means of the anti-swelling efficiency. The ...
M M González-Peña


Nano structural properties of La2O3-Beech Wood Flour With XRD technique
2012 - IRG/WP 12-40607
This research was considered to study various properties of the Lanthana mixed with beech wood flour (BWF), as a new structure. For this purpose, La2O3 powders in the BWF have been obtained by sol-gel method using simultaneous gelation of all cations. La2O3 - BW samples are analysed by X-ray diffraction .The obtained results showed the formation of nano crystalline La2O3 phases. The average crys...
M Ghorbani Kokandeh, I Bahamni, A Bahari


Biodegration of treated wood waste by native fungal communities of tropical soil in French Guiana
2012 - IRG/WP 12-50285
Woods have been protected with fungicides for a long time, and the effects of these fungicides on soil after being leached into the ground have turned out to be a true environmental issue. It is in this perspective that we are proposing to study fungal communities of these contaminated woods in a purpose of bioremediation. Most of precedent studies have focused on ability of some Basidiomycetes an...
A Zaremski, L Gastonguay, C Zaremski, F Chaffannel, J Beauchêne, G LeFloch


Study on the Effect of Combined Nanosilver-Hygrothermal Treatment on Wood Properties
2012 - IRG/WP 12-40581
In this study, the impregnation process with nanosilver solution, before hygrothermal treatment was carried out to investigate its effect on some physical and mechanical properties of Iranian beech (Fagus orientalis Lipsky) and imported Russian spruce (Picea abies). Wood specimens were impregnated with nanosilver solution (400ppm) in an impregnation tank under pressure of 0.25 Mpa, for 20 minutes....
G Rassam, H Reza Taghiyari, A Karimi, B Jamnani, M Ebrahimi


Succession after Fire of Fungal Fruiting Bodies in Mediterranean Pinus pinaster Stands in Spain
2012 - IRG/WP 12-10789
In this study we present the results of a 4-year survey aimed at describing the succession of fungal communities following fire in a Mediterranean ecosystem in Northwest Spain, dominated by Pinus pinaster Ait. After a large wildfire in 2002, six 2 x 50 m study plots were established in burned and unburned areas corresponding to early and late succession stages. During the autumn seasons from 2003 ...
P Vásquez Gassibe, M Hernández-Rodriguez, R Fraile Fabero, J A Oria-De-Rueda, P Martín-Pinto


Triazole – based ionic liquids to protect of lignocellulosic materials against fungi
2012 - IRG/WP 12-30601
In presented paper we examined on biotic properties of novel structure of tebuconazole derivatieves: tebuconazole hydrochloride, allyltebuconazole chloride, methyltebuconazole iodide, tebuconazole dihydrocitrate. Our investigation against wood-degrading fungi were contained also the didecyldimethylammonium 3-aminotriazolate as well as didecyldime-thylammonium nitrate(V) with tebuconazole or wit...
J Zabielska-Matejuk, J Pernak, I Frąckowiak, A Stangierska, W Przybylska, M Kot


Wood Aging. Characteristics of aged Hinoki wood from Japanese historical buildings
2012 - IRG/WP 12-40610
Wood has always played a major role in Japanese traditional culture. More than 90% of buildings listed as a National property or a nationally important cultural property of Japan are constructed with wood. In the ancient capitals Kyoto and Nara, many traditional wooden buildings were inscribed as World Cultural Heritage of the UNESCO. The most famous and the world’s oldest wooden construction st...
M Yokohama, S Kawai


Development of a quality control assessment method to predict properties of heat treated wood
2012 - IRG/WP 12-40611
Heat treatment has been used to improve properties of non durable European species. Chemical modification of some of the wood components provides improved dimensional stability and biological performance against decay fungi while mechanical properties such as modulus of rupture are reduced. Quality control of commercially made thermally treated wood is one of the major challenges to allow its indu...
M Chaouch, K Candelier, S Dumarcay, A Pétrissans, M Pétrissans, P Gérardin


Differences between heat treated Pinus pinaster heartwood and sapwood
2012 - IRG/WP 12-40617
Heat treatment is a well known process to improve the durability and dimensional stability of less noble woods. The treatment can be applied for heartwood unlike the traditional treatments based on impregnation due to the difficulty of impregnating heartwood. Pure sapwood and pure heartwood samples were treated in an oven at 190ºC and 200ºC for 2h, 4h and 6h. Dimensional stability, measured a...
B Esteves, L Nunes, I Domingos, H Pereira


Activities of moulds on wood as a function of relative humidity during desorption and absorption processes
2013 - IRG/WP 13-10794
Three different types of indoor moulds: Penicillium brevicompactum, primary colonizer; Alternaria tenuissima, secondary colonizer and Trichoderma harzianum, tertiary colonizer, grown on wood were measured for their activities under different relative humidity levels. The activities were measured by isothermal calorimetry. The activities of the moulds changed with the change of the relative humidit...
Yujing Li, L Wadsö


High-throughput sequencing highlighted contrasted pioneer fungal communities associated to coniferous and deciduous wood preservation assays
2013 - IRG/WP 13-10800
Studying the fungal communities in the wood, in particular during the first events of the colonization, and the factors that underlie the dynamics of fungal species assemblages remain a challenge in ecology, because of the absence of fructification during the pioneer steps of wood degradation. The use of Next-generation DNA sequencing methods, which produce massive volumes of data, provided new pe...
Y Mathieu, A Dassé, I Le Bayon, M Kutnik, L Harvengt, E Gelhaye, M Buée


The chemistry of wood degradation by Basidiomycetes studied in a van Krevelen diagram
2013 - IRG/WP 13-10805
The atomic composition ratios of decayed wood by Basidiomycetes are mapped in a van Krevelen diagram. It is shown that the wood residue after decay is chemically reduced, rather than oxidized. A previously developed and verified theoretical model for thermal wood modification, relating atomic composition ratios to moisture sorption and fungal resistance properties has tentatively been applied to w...
W Willems, H Militz


Resistance of Consolidated Deteriorated Wood to Wood Decay Fungi
2013 - IRG 13-10812
The main purpose of the experiment was to establish which consolidating products in impregnated wood are the most effective against wood decay fungi. Five different consolidators were tested: Paraloid B-72, Consolidating restaurateur, SG 715 BLANC (epoxy resin), R.712 polyester and the wood consolidant agent containing nano particles, which is still in development. From the already damaged wood ...
F Pohleven, A Valantič, M Petrič


Characterization of test fields
2013 - IRG/WP 13-20508
Test field characteristics and impact of test fields on wood degradation is important when testing wood protection. The current EN 252 standard has no requirement for knowledge of decay hazards, but most commonly a test field is known as a “brown”,- “white”,- or “soft rot” field. To understand which decay hazard wood preservatives are tested against, each test field should be character...