Comparison of the FRIM and forest research laboratory methods for screening of anti-sapstain formulations
1999 - IRG/WP 99-20170
Two laboratory methods for screening of anti-sapstain formulations were compared. The method adopted by the Forest Research Institute Malaysia (FRIM) involved 3 weeks assessment of rubberwood (Hevea brasiliensis) blocks, dipped in the candidate formulation and inoculated with mycelial/spore suspension of sapstain (Botryodiplodia theobromae) or decay (Schizophyllum commune) fungi, and incubated on ...
A H H Wong, D R Eden, C M Chittenden, M E Hedley, R N Wakeling


Effect of some resin treatments on fungal degradation reactions
1999 - IRG/WP 99-10318
The effect of impregnation of wood with vegetable oil, tall oil and two water soluble on fungal degradation reactions was assessed by hydrolysis and enzyme activity measurements. The experiments were carried out by using isolated enzyme preparations and a living brown-rot fungus Poria placenta. The results indicate that the inhibitory effect of treatments was clearly directec towards the enzymatic...
A-C Ritschkoff, M Rättö, A J Nurmi, H Kokko, A O Rapp, H Militz


Detoxification of methylene bisthiocyanate by bacteria isolated from freshly felled, anti-sapstain treated timber
1993 - IRG/WP 93-10017
The microbial defacement of freshly-felled timber treated with organic biocides continues to be a major problem in stored lumber. As part of a study to investigate the depletion in chemical activity of methylene-bis-thiocyanate (MBT) in green timber, bacteria were isolated from freshly-felled boards of Corsican pine (Pinus nigra var. maritima Arnold) previously treated with different biocides. The...
R J Wallace, R A Eaton, G R Williams


Fungal siderophores and their rôle in wood biodegradation
1990 - IRG/WP 1442
Iron and other metals such as manganese, play an important role in the metabolic functions of fungi that cause wood deterioration. These transition metals are also found in, or associated with, the extracellular fungal enzymes shown to be directly involved in the decay process. Recently our research group was able to show that siderophores (low molecular weight biological chelators) are produced b...
J Jellison, B Goodell, F Fekete, V Chandhoke


Tebuconazole - A new triazole fungicide for wood preservation
1990 - IRG/WP 3629
The main cause of economic damage to timber and millwork worldwide are Basidiomycetes (brown and white rot). After testing a wide range of triazole derivatives for their effectiveness against decay fungi, Tebuconazole, a triazole compound, was selected. The physico-chemical, toxicological and ecotoxicological data of this substance are described. Tebuconazole is unleachable, light-stable, heat-sta...
R Gründlinger, O Exner


Sapstain development on Jack pine logs in Eastern Canada
2000 - IRG/WP 00-10358
During 1998-99, a study was initiated to investigate the influence of seasons, log types and storage time on the sapstain development on jack pine logs at two sites in Eastern Canada. Jack pine trees (Pinus banksiana) were harvested into whole-tree and cut-to-length logs in spring and in autumn. Sapstain development was examined in these logs at 2 to 4 week intervals after felling. The mean stain ...
Dian-Qing Yang, R Beauregard


An observation of seasoning, preservative treatment and storing of CCA treated 30 bangladeshi hardwood species for crossarms
1995 - IRG/WP 95-40058
Observed kiln seasoning, preservative pressure treatment and storing of CCA treated 30 Bangladeshi hardwood species for crossarms. It revealed that it was very difficult to kiln season and preservative pressure treatment of thirty species together in a single charge and found that when species of different specific gravity kiln season together there occur some objectionable seasoning degrades, and...
G N M Ilias, M D Rokib-ul-Hafiz


Regulation of hyphal sheath formation iron-chelator production by the brown rot fungi Gloeophyllum trabeum and Postia placenta
1994 - IRG/WP 94-10074
Hyphal sheath formation and iron-chelator production by liquid cultures of the brown rot fungi Gloeophyllum trabeum and Postia placenta were monitored over time. The effects of incubation at various temperatures, pH's and concentrations of iron, manganese and nitrogen were determined. Hyphal sheath production was observed microscopically and quantified with JAVA video analysis. The hyphal...
Y Chen, J Jellison


Applicability of supercritical carbon dioxide to the preservative treatment of wood-based composites
2001 - IRG/WP 01-40199
Treatability of five structural-use wood-based composites (medium density fiberboard, hardwood plywood, softwood plywood, particleboard and oriented strand board) was evaluated when supercritical (SC) carbon dioxide (CO2) was used as a carrier solvent. Treatments were conducted at three temperature 32 levels (25, 35 and 45°C) and two pressure levels [80 kgf/cm2 (7,845 kPa) and 120 kgf/cm2 (11,768...
M Muin, A Adachi, K Tsunoda


A comparative study of some anti-splitting devices, using Eucalyptus saligna and hybrids of Eucalyptus saligna X Eucalyptus spp poles
1983 - IRG/WP 3251
It is commom for some Brazilian wood pole users to require devices such as banding steel, to avoid or reduce splits at the end of Eucalyptus treated poles. On other hand users and manufacturers do not have data to confirm the effectiveness of the banding steel types normally used such as galvanized "Steel-Belt" and galvanized "Wire-Belt". For this reason a comparative study was carried out includi...
F C Geraldo, J A C Sodré


Thermal modification of non-durable wood species 2. Improved wood properties of thermal treated wood
1998 - IRG/WP 98-40124
Properties of wood treated in a new heat-treatment process called the PLATO-process have been studied. Several wood species have been treated using this new thermal modification process using a range of process conditions (mainly time and temperature). In this study the characteristics of the treated wood were determined using samples from whole planks treated on pilot plant scale. The modified ch...
B F Tjeerdsma, M J Boonstra, H Militz


Performance of Tuff Brite C™ and other formulations against blue-stain, mold and brown-stain in freshly-sawn rubberwood (Hevea brasiliensis) in the humid tropics of Peninsular Malaysia
1997 - IRG/WP 97-30163
The relative anti-sapstain and anti-mold efficacies, including brown-stain development in freshly-sawn rubberwood (Hevea brasiliensis) in the Malaysian tropics, between selected water-based product concentrations of formulations Tuff Brite CTM without/with added Borax (at 1.5/0, 1/1.5, 1.5/1.5 and 2%/1.5%), PQ8TM without/with added Borax (at 2.5/0, 1.5/1.5, 2/1.5 and 2.5%/1.5%) and NeXgenTM/NeX-Br...
A H H Wong, T L Woods


New applications of silafluofen to termite control
2001 - IRG/WP 01-30274
Silafluofen-based termiticides are widely used for soil and timber treatments in Japan, as silafluofen possesses advantageous properties of low fish toxicity and high chemical stability (to light, in soil, in alkaline environments, etc) in addition to high termiticidal activity and low mammalian toxicity. As new applications of silafluofen to termite control, we have developed another type of prod...
K Nakayama, Y Minamite, S Koike, Y Katsuda, K Nishimoto


A field test with anti-stain chemicals on sawn pine timber in Brazil
1989 - IRG/WP 3513
Field tests were carried out in São Paulo State - Brazil, to evaluate pre-treatment formulations of O-Phenyl-Phenol (OPP) based products. The Sodium Pentachlorophenate solution was used as a reference formulation. The treated test blocks were stacked in a covered shed, and in an uncovered place for air drying. The evaluation was done by measuring the percentage of stained surface on each test blo...
M B B Monteiro, S Brazolin


Effect of point of preservative addition on the mechanical and physical properties of strandboard treated with Tanalith 3485
2000 - IRG/WP 00-40152
Preservative has been added to a PF bonded strandboard at various different stages in the manufacturing cycle and the physical and mechanical properties of the boards have been evaluated (modulus of elasticity, modulus of rupture, thickness swelling, water absorption, internal bond strength, and shear strength). Preservative addition has been examined at five different stages namely green strand d...
G J Goroyias, M D C Hale


Properties of cellulose degraded by the brown rot fungus, Postia placenta
1988 - IRG/WP 1350
To gain further understanding of the nature of the cellulose depolymerizing agent or agents of brown-rot fungi, brown-rotted cellulose was chemically and physically characterized. Various culture conditions, such as low nitrogen and elevated oxygen levels, did not induce degradation of cellulose by Postia placenta in liquid cultures. Therefore, brown-rotted cellulose for analysis was prepared by a...
T L Highley, R E Ibach, T K Kirk


Breakdown of cellulose derivatives by cellulolytic enzymes. I. Action of fungal ß-glucosidases toward substituted PNP ß-D-glucopyranosides
1998 - IRG/WP 98-10281
The action of fungal ß-glucosidases on the methyl derivatives of p-nitrophenyl (PNP) ß-D-glucopyranoside, which were regioselectively substituted at 0-2, 0-3, 0-4 and 0-6 positions was studied. Several ß-glucosidases from brown-rot, white-rot, and soft-rot fungi and almond were used for the study. These ß-glucosidases did not act on the 2, 3, and 4-0-methyl derivatives, while the 6-0-methyl on...
T Nishimura, I Momohara, M Ishihara


Improved preservative penetration of spruce after pre-treatment with selected fungi. I. Fungal pre-treatment of pole sections
1998 - IRG/WP 98-40117
European spruce logs were pre-treated with either Phanaerochete chrysosporium, Dichomitus squalens, Trichoderma viride and Trichoderma aureoviride for incubation periods of between 1-4 weeks prior to pressure treatment with creosote in a commercial treatment plant and analysed for strength and creosote uptake (see part II Tucker et al.). A method to pre-treat logs was optimised. The pole sections ...
B Rosner, K Messner, E J B Tucker, A Bruce


Artificial weathering exposure as an alternative for standard ageing according to EN 84 (leaching) and EN 73 (evaporation)
2002 - IRG/WP 02-20254
In order to verify potential weaknesses of wood preservatives fungal tests are carried out after ageing of wood preservative treated test blocks. The European standard EN 599 as a framework for efficacy assessment of wood preservatives includes the use of two ageing methods prior to fungal testing, namely a leaching method (EN 84) and an evaporation method (EN 73). The European research project "F...
J Van Acker, M Grinda, D J Dickinson


Microwave modification of wood properties - Improvements in wood permeability
2000 - IRG/WP 00-40181
A new method of microwave (MW) wood modification is described. Microwave irradiation of timber provides an improvement in wood permeability mainly in the radial and longitudinal directions. This is achieved by physically modifying ray cells and forming a large number of cavities in the radial - longitudinal planes. More extensive MW irradiation of different species transforms the wood into a new m...
G Torgovnikov, P Vinden


IPBC - A new fungicide for wood protection
1984 - IRG/WP 3295
3-iodo-2-propynyl butyl carbamate (IPBC) is presented as a potential low toxic alternative to pentachlorophenol and the sodium chlorophenoxides. Data on its effect against basidiomycetes is shown. Tests according to both the European standard method, EN-113, and American, ASTM D-413, have shown its potential. The chemical gives protection against both the wood destroying fungi, blue stain, mould and algae. It is possible to have it formulated in both water-based and organic solvent-based products. Treatment of wood out of ground contact (vac-vac products, pretreatment products, primers, stains, etc.) and sapstain control are some of the most potential end use areas within wood protection. Besides wood protection, the IPBC is used as a fungicide in paint, adhesives, caulks and sealants, cement, leather, paper, cutting oil, ink and in different roofing materials.
J Hansen


A report on the development of "Technical Recommendations Document for the Canadian wood preservation and protection facilities"
1987 - IRG/WP 3447
The wood preservation and wood protection industry uses chemicals which are similar. However, because the methods of applications of preservatives are different in wood preservation (pressure treatment) and wood protection (surface treatment) plants, their problems need to be resolved separately. As a part of a federal strategy to protect the environment and human health from potentially toxic com...
G Das, V N P Mathur


Fungicidal properties of wood tar being a side product of pyrolysis of previously treated wood with preservatives
2004 - IRG/WP 04-30340
The objective of the paper was to estimate the limit of the fungicidal value of wood tar being a product of pyrolysis of wood previously treated with creosote oil or salt preservative of the CCB type. The effectiveness of wood tar in wood protection against fungi causing brown rot and soft rot was compared to the effectiveness of creosote oil (type WEI-B). Wood was impregnated with alcohol solutio...
B Mazela, M Kielczewski, W Grzeskowiak


Effect of origin and orientation of Radiata pine substrates on the development of fungal degrade
2000 - IRG/WP 00-30221
The objective of this study was to determine the influence of different radiata pine substrates on colonisation by sapstain fungi. Freshly-cut branch wood, stem wood and sawn lumber were used to prepare test samples with the largest wood surface area showing a transverse, radial or tangential face. Test samples were evaluated against sapstain fungi using a rapid laboratory antisapstain screening m...
B Kreber, D R Eden, C M Chittenden, B Carpenter, J G Van der Waals


Comparison of two laboratory methods for screening potential anti-sapstain chemicals
1993 - IRG/WP 93-10036
Two methods were used to screen a number of potential anti-sapstain chemicals in the laboratory. In one method miniature boards of freshly felled Scots pine sapwood were dip treated with the candidate chemical, sprayed with a suspension of stainers or moulds and incubated for five weeks. In the other method antibiotic assay discs were treated with precise quantities of chemical, plated out on malt...
S M Gray, D J Dickinson