IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 512 documents. Displaying 25 entries per page.


A laboratory technique to measure the performance of preservative treated hardwoods in ground contact
1982 - IRG/WP 2172
A laboratory technique to measure the performance of preservative treated timber in ground contact is described. It uses partially sealed blocks of timber which are treated, leached and sawn into small stakelets for soil exposure in a fungal cellar. Performance is monitored by the loss of static bending strength with time, and a simple apparatus for measuring the deflection of a stakelet under a l...
E F Baines


The field performance of CCA-C treated sawn refractory softwoods from North America
1997 - IRG/WP 97-40085
Approximately 15% of the total volume of wood treated in the United States consists of difficult to treat softwoods known as "refractory softwoods". The long term positive performance record of CCA treated sawn material is based upon the testing of yellow pine sapwood stakes with only limited field data available for sawn refractory softwoods. As a result, the existing North American wood preserva...
M J Richards, W S McNamara


Biostatic film as a primary treatment against pole failure in soil
1995 - IRG/WP 95-40053
Field liners of low density polyethylene (LDPE) film applied as primary treatment of soil-contact surfaces of creosote-treated poles prevented their detoxification and premature failure by establishing hurdles against microbiological colonisation. These hurdles include low water activity, low oxygen tension and nutrient limitations. Moreover, under conditions of high soil moisture, field trials sh...
A A W Baecker, M Behr


Environmental risk assessment of treated wood - A mesocosm study
2005 - IRG/WP 05-50224-8
In order to evaluate the environmental impact of treated poles, we have developed physical models (mesocosms) containing around 250 kg of natural soil and a treated pole. On the top of each mesocosm, a spraying mechanism, which can distribute ultrapure water through several nozzles, was built. On the lower part of each mesocosm, a small tank, which can contain some litres of leachate, was placed...
P Marchal, F Poly


The Efficacy of Wood Preservative Treatments in Laboratory Soil-Bed Test
2004 - IRG/WP 04-20289
The efficacy of wood preservatives were determined in laboratory soil-bed test. Pine and alder wood samples (10 x 10 x 10 mm) were treated with CCA (1, 2%), ACQ-1900 (2, 3%), ACQ-2200 (1, 2%), Tanalith E 3491 (2, 2,8%), Wolmanit CX-8 (1, 2%). The leached and unleached samples were exposed 76 days at Simlångsdalen soil and determined mass loss. The results of this study showed that mass losses o...
A Temiz, T Nilsson, Ü C Yildiz, E D Gezer, S Yildiz


IUFRO rating system compares favourably to weight loss for soil-bed testing
1990 - IRG/WP 2343
The soil-bed/small stake test is commonly used for rapidly evaluating the performance of new, more environmentally acceptable, preservatives. In a 1.5 year experiment with three copper-based waterborne preservatives, visual evaluation and probing using the IUFRO performance rating scale (0-4) gave very similar toxic thresholds to those derived from measurement of weight loss at the end of the expe...
P I Morris


Field Liners™ prevent creosote migration from transmission poles to soil during service
1996 - IRG/WP 96-40067
A full scale trial utilised 150 12m Eucalyptus grandis transmission poles treated with standard retentions of creosote according to SABS Method 457. One hundred poles had Field Liners™ applied while 50 did not. The 150 poles were used to complete an electricity transmission line in Southern KwaZulu-Natal. After 18 months service, incremental cores were taken from 15 cm below the ground lines of ...
M R Behr, G D Shelver, A A W Baecker


Growth of selected wood decay fungi on various agar-supplemented media
2003 - IRG/WP 03-10456
The growth rates of a selection of wood decay fungi (brown and white rots) on various agar-supplemented media have been determined and compared. The agar media investigated were Malt extract agar (MEA), Potato dextrose agar (PDA), YMPG agar (yeast extract, malt extract, bacto-peptone, glucose, asparagine and thiamine), YMPG agar (without amino acids) and Beech wood powder agar (BWA). The tested wo...
S A Amartey, M Humar, F Pohleven


Termites in Uruguay; control, prevention and environment
1991 - IRG/WP 1474
When Prof. La Fage's questionaire on termites was received by 1987, few were aware of termite damage in Uruguay and infestations were not much reported. Further contacts between scientists, operators and homeowners, are now shaping the real threat of termite attack. Before letting the problem faIl in the hands of the layman, with all ist environmental risks, it seemed reasonable to: 1) re...
A Aber, G Baillod


Treatment application method and CCA efficacy in Corsican pine - Assessment by serial exposure and soil burial tests
1993 - IRG/WP 93-40006
A previous report on this research (Newman and Murphy, 1992) identified possible variation in the efficacy of a CCA preservative applied to Corsican pine (Pinus nigra var. maritima) dependant upon the treatment application method (Bethel, Lowry or Steam/Bethel). This paper presents further data from biological testing of CCA treated Corsican pine using serial exposure and unsterile soil techniques...
P R Newman, R J Murphy


The WOODCARE project: Development of detection methods for Death watch beetle larvae and fungal decay
1999 - IRG/WP 99-20172
Woodcare was a European project coordinated by English Heritage. The aim of the research was to develop more targeted and more environmentally friendly treatment methods for Death watch beetle infections in Oak constructions of historical buildings. TNO has developed two new methods for fast and reliable detection of Death watch beetle larvae and related fungal decay in Oak. The problem with Death...
P Esser, P Van Staalduinen, A C Tas


Losses of CCA components and creosote from treated timber to soil
1997 - IRG/WP 97-50098
Components of creosote and CCA preservatives can migrate within the wood and move into surrounding soil. However, at present, the ecological significance of such losses is uncertain. This paper examines the distribution of four target polyaromatic hydrocarbons (PAHs ) and of copper, chromium and arsenic in treated stakes and surrounding soil after long term exposure in field trials. Concentrations...
N J Hudson, R J Murphy


Comparison of methods for monitoring CCA fixation
1994 - IRG/WP 94-40023
The CCA fixation status in the outer 12.5 mm of pole sections of southern pine (Pinus sp.), red pine (Pinus resinosa) and lodgepole pine (Pinus contorta var. latifolia) were followed during fixation at 21°C under non-drying conditions by the following procedures: - Qualitative CrVI indication by the chromotropic acid spot test. - Quantitative CrVI in the expressate by the diphenylcarbazide method...
P A Cooper, Y T Ung, G Zanjani


Remediation of a large CCA-impregnation plant
1998 - IRG/WP 98-50101-13
During 1949-85 the Swedish Telecom ran a plant for pressure impregnation of poles in Hjältevad, 80 km east of Jönköping in the southern part of Sweden. About one million poles were treated with CCA-preservaties. Leaks and accidential spills have contaminated soil and groundwater within the 5 ha large site. The total amount of released arsenic, the main pollutant, is estimated to 6-7 metric tons...
P Englöv


Laboratory testing of wood natural durability - In soil-bed assays
1998 - IRG/WP 98-20141
Laboratory methods for assessing wood decay resistance are being investigated in the framework of an ongoing European research project. This paper summarizes the main results obtained for soil-bed tests based on the European prestandard ENV 807-Test 2. The data suggest that this testing methodology is suitable for evaluating the natural durability of timber species in soil-contact under conditions...
R Sierra-Alvarez, I Le Bayon, J K Carey, I Stephan, J Van Acker, M Grinda, G Kleist, H Militz, R-D Peek


A comparison of the migration behaviour in soil of different waterborne wood preservatives and their leachates
1997 - IRG/WP 97-50091
Lysimeter tests were carried out on water-soluble wood preservatives and on wood preservative components leached out of impregnated wood. The purpose of these tests was to determine the extent to which the migration behaviour of environmentally relevant ions in the soil is influenced under comparable conditions. The results clearly show that the groundwater is especially at risk when wood preserva...
E Melcher, R-D Peek


Screening techniques for potential wood preservative chemicals. Proceedings of a special seminar held in association with the 10th Annual Meeting of the IRG, Peebles 1978. Report No 136, 1979
1980 - IRG/WP 2138
This paper continues following issues: I. SCREENING INSECTICIDES 1) R W Berry (BRE/PRL, UK): Screen testing of insecticides for use in remedial wood preservatives. 2) D J Cross (FRI, New Zealand): Rapid screening of contact insecticides for use on forest products. 3) C R Coggins; A Forsyth; A E Glaser (Rentokil, UK): Experience in the use of indicative screening techniques for termiticides. ...
Anonymous


A non-pressure method of protection based on hurdle theory to control the spectrum of internal environmental factors which affect the decay of poles in soil contact
1993 - IRG/WP 93-20005
A field trial was conducted to establish whether superficial barrier linings on poles in soil contact could function as environmental hurdles against the growth of biological agents and thus provide preventative methodology to preclude premature failure of vineyard poles under flood-irrigation. Assessment after 52 weeks exposure to the prevailing conditions and sub-tropical environment showed that...
A A W Baecker


Comparison between two laboratory test methods for determining the effectiveness on wood preservatives against blue stain in fresh wood
1987 - IRG/WP 2289
Most of the work done on determination of the effectiveness of new formulae for treating fresh wood against blue stain have been focussed on their use in the manufacture of saw timber. This work explains two laboratory methods, one which simulates the working and climatological conditions of factories making packages for fruit and vegetables in the Spanish Levante, showing that contamination of wo...
A M Navarrete, M T De Troya


Soil-bed decay resistance evaluation of strandboards treated with preservative at different points of the manufacture process after 18 months exposure
2002 - IRG/WP 02-40230
Strandboards were treated with a copper-boron water-based preservative at different points of manufacture process namely, green strand diffusion, vacuum, spray application in the resin blender and post manufacture heat and cold quench. Preservative was applied to achieve five different retentions (0, 1.5, 3, 6, 12 kg m-3). The modulus of rupture and modulus of elasticity were assessed before expo...
G J Goroyias, M D C Hale


The effect of preservative distribution in small blocks of Pinus sylvestris on the toxicity of tributyltin oxide to Reticulitermes santonensis Feytaud
1971 - IRG/WP 206
Small blocks of Pinus sylvestris (50x25x15 mm³) were treated by a full-cell method with various concentrations of tributyltin oxide in benzene. Replicate blocks were then freeze dried, rapidly air dried or slowly air dried and exposed to surface attack by the subterranean moistwood termite Reticulitermes santonensis Feytaud. At all concentrations it was found that the freeze-dried blocks were mor...
M P Levi, D N R Smith


Subterranean termite attack potential in field test sites: assessment methods and field characterization
2003 - IRG/WP 03-10472
To assess subterranean termite attack potential in the field and seasonal variations, trials were set up in each of two managed silvicultural plantations, of Eucalyptus globulus and Pinus pinaster, respectively. Termite occupancy in lying dead wood was evaluated by an adaptation of the line-intersection method, and attack potential in soil was assessed by a system of stakes inserted into the groun...
T Nobre, L Nunes, L Brinca, D E Bignell


Effect of soil type and moisture content on soft rot testin
1986 - IRG/WP 2270
Several soils of different types were tested at a range of moisture contents for their suitability for use in a soil burial soft rot test. Their effectiveness was assessed by weight loss in CCA treated and untreated beech and birch outerwood. A horticultural loam (John Innes No. 2) was the most appropriare soil in terms of amount of weight loss caused, tolerance to changes in soil moisture content...
S M Gray


Test methods for wood preservatives against Lyctus: (1) Testing of treated veneer. (2) Testing of glue-line treated plywood. (Laboratory methods)
1977 - IRG/WP 293
Powder-post beetles destroy large quantities of veneer and plywood. Two test procedures are described which can be used to support application-oriented research into veneer and plywood preservatives. These procedures simulate practical conditions on a laboratory scale. Their characteristic feature is that wood species of special susceptibility are used for the tests; the susceptibility of the spec...
S Cymorek


Methods of culturing Lyctidae
1980 - IRG/WP 1126
Members of the tropical countries in the IRG Sub-Group "Insects in dry wood" requested a paper on the breeding of lyctids. Compared with other wood boring insects, such as cerambycids and anobiids, the breeding of lyctids is not as difficult and time consuming. Nevertheless some basic principles have to be observed in the laboratory to obtain successful cu·ltures. It is the intention of this repo...
H Kühne


Previous Page | Next Page