Use of wax emulsions for upgrading of wood properties
2009 - IRG/WP 09-40451
Waxes are used for treatment of wood surfaces for several decades, predominately as surface treatments, because they did not penetrate into the wood. In order to overcome this issue, water emulsions were applied in present experiment. Five water emulsions of various concentration was used namely; two emulsions of montan wax (LGE, MW1), emulsion of polyethylene (WE1), emulsion of ethylene copolymer...
B Lesar, F Pohleven, M Humar


The invasion channels of damage fungi in bamboo lumber
2010 - IRG/WP 10-10712
The micro-agents on bamboo lumber damage are mould, stain, and decay fungi. This research is about invasion channels of bamboo lumber damage fungi by scanning electron microscope (SEM). The results showed that the conidia of mould were only accumulated on the surface of bamboo and no hyphae detected in bamboo vascular bundle, and hyphae of stain penetrated into bamboo and grew in metaxylem vessel...
Xingxia Ma, Mingliang Jiang, Daochun Qin


Early detection of colonisation by blue stain and mould on modified wood using PCR technique
2010 - IRG/WP 10-10730
The aim of this research was the early detection of fungal attack on the surfaces of modified and unmodified wood after natural weathering. The investigation was carried out by molecular techniques and the development and establishment of genus/species specific PCR for important moulds and sapstain fungi was part of this work. After adaption of the method, a monitoring of the succession of Ascomyc...
A Steitz, B Schmöllerl, N Pfabigan, S Bollmus, G Grüll


Degradation of Carbon-Based Preservatives by Black-stain Fungi
2010 - IRG/WP 10-30533
Some black-stain fungi are known to exhibit resistance to carbon-based preservatives. However, the cause of this resistance is unclear. The fungi may have mechanisms to tolerate these chemicals, or they may be able to degrade and detoxify them. Fungi capable of degrading carbon-based preservatives are of interest for possible bioremediation of carbon-based preservative-treated wood at the end of i...
R Stirling, P I Morris


Comparison of colour change in wood clear-coating systems including inorganic and organic UV absorbers for exterior use
2010 - IRG/WP 10-40499
The aim of this work is to compare the performance of inorganic and organic UV absorbers used in a wood coating application against weathering. Our study has investigated the colour changes of selected UV absorbers; hombitec 402 RM from the Sachtleben Company as an inorganic UV absorber, tinuvin 477 DW from the Ciba Company as an organic UV absorber. The study was carried out on two wood species; ...
Ö Özgenç, B Forsthuber, A Teischinger, C Hansmann


Effects of intumescent formulation of vinyl acetate-based coating on flame-retardancy of thin painted red lauan (Parashorea spp.) plywood
2011 - IRG/WP 10-40537
Using intumescent coatings on wood-based materials is an effective method for fire safety. The intumescent coatings consist of four major components: (1) binder resin (BR), (2) carbonizing substance (CS), (3) foam producing substance (FPS) and (4) dehydrating agent (DA). Previous studies have demonstrated that the formulation of the four components strongly influences the performance of coatings. ...
Chih-Shen Chuang, Kuang-Chung Tsai, Te-Hsin Yang, Ming-Kuang Wang, Chun-Han Ko


Effects of microclimate, wood temperature and surface colour on fungal disfigurement on wooden claddings
2012 - IRG/WP 12-20490
Wooden claddings are common in façades in Norway, and Norway spruce (Picea abies) is the most frequently used species. The cladding is a major part of the facade, and it has visual requirements that may define the aesthetic service life. The visual changes that occur during weathering can be colour changes, abrasion or wear, blistering, flaking, and even cracks in the wood or coating, but more of...
L Ross Gobakken, G I Vestøl


Field-testing of Norway Spruce Claddings with Monitoring of Moisture Content, Material Temperature and Microclimate
2012 - IRG/WP 12-20502
The physical function of a cladding is to protect the interior construction. Under normal circumstances the performance requirements can be met for a very long time, meaning that the technical service life of a wooden cladding can be very long. Since the cladding is a major part of the facade, it also has visual requirements that may define the aesthetic service life, and often it is much shorter ...
G I Vestøl, L Ross Gobakken


Influence of a pulsed electric field on the growth of surface fungi
2013 - IRG/WP 13-10795
The colonization of mold and staining fungi are not only an aesthetical problem. Blue stain fungi are able to penetrate paint films. Maintenance of coatings on wood are time consuming and costly. A new approach uses a pulsed electric field (PLEOT) in order to protect wood against surface fungi. This technology is evaluated in non-sterile laboratory conditions on different coated and uncoated Scots...
M Starck, A Treu


Using hyperspectral imaging to detect and quantify mould and blue stain on coated and uncoated wood
2014 - IRG/WP 14-10822
Hyperspectral imaging has been applied on the surface of samples of coated and uncoated Norway spruce (Picea abies) as a new technique to detect and quantify growth of mould and blue stain fungi. Principal Component Analysis of the hyperspectral images resulted in a clear visualization of the fungi and the amount of mould coverage could be estimated. This indicates that NIR hyperspectral imaging c...
L Ross Gobakken, I Burud, A Flø, K Kvaal, T K Thiis


Reducing Extractives Stain in Western Red Cedar Sidewall Shingles
2014 - IRG/WP 14-30654
One of the aesthetic challenges that western red cedar shingles face is extractives redistribution stain, particularly in unpainted sidewall applications. Dip and pressure treatments with a mixture of quaternary ammonium compounds and alkyl amine oxides were investigated for their ability to prevent this stain. After nine months of exposure in Vancouver, extractives stain was present on nearly all...
R Stirling


The role of hydrophobins in surface growth by the Blue Stain fungi Aureobasidium pullulans
2015 - IRG/WP 15-10837
Hydrophobins are small proteins found exclusively in filamentous fungi. These proteins are able to assemble spontaneously into amphiphilic monolayers at hydrophobic–hydrophilic interfaces. Hydrophobins have a diverse role, e.g. allowing the fungi to break through interfaces during aerial hyphae formation, sporulation, fruit body production and cell penetration. In this ongoing study, we are look...
J Stenbæk, L Riber, J Blæsbjerg Nielsen, C Møller Hansen, B Jensen


The whitening cause of Korean wooden heritage by flame retardant treatment
2015 - IRG/WP 15-20560
Korean wooden heritage used to treat by flame retardants in order to protect fire. There are 2 types flame retardant using for wooden heritage. These flame retardants treatment are basic measure that apply to wooden heritage along with other fire protection. The flame retardants cause white stains by reacting with Korean traditional wood painting (Dancheong) and increase wood humidity. The Korean ...
Jin Qyu Kim, Gyu-Seong Han, Yong Jae Chung, Hwa Soo Lee, Dong Won Son


Mould growth on spruce claddings and the effect of selected influencing factors after 4 years of outdoor testing
2015 - IRG/WP 15-30671
Norway spruce (Picea abies) is the most frequently chosen wood species as claddings in façades in Norway, and is used both coated and uncoated. The visual changes that occur during weathering can be colour changes, abrasion or wear, blistering, flaking, and even cracks in the wood or coating, but more often growth of mould and blue stain fungi is the main challenge. A field test with synchronous monitoring of relative humidity, air temperature, material temperature and wood moisture content in Norway spruce claddings has been performed in southern Norway as part of the ClimateLife project. Visual evaluation of blue stain and mould growth according to EN 927-3 was performed, and evaluation data after 46 months exposure is presented. The objectives were to study the effect of 1) environment, 2) cardinal direction and 3) colour of the coated surface on growth of blue stain and mould fungi and to study the variation in relative humidity, air temperature, wood moisture content and material temperature. After 46 months exposure, the red coating system had generally the lowest mould ratings and the uncoated claddings had the highest. Of the white coloured claddings the ones facing south had lower mould ratings than those facing north, but the opposite were found for red coloured claddings. The relative humidity was higher in front of claddings exposed northwards and in a shaded environment compared to an open environment against south. In an open environment red coloured claddings had the lowest wood moisture content and highest material temperature, and red coloured claddings against south had the highest maximum material temperature.
L Ross Gobakken, G I Vestøl


Susceptibility of wood substrates to Aurebasidium pullulans at different temperatures
2016 - IRG/WP 16-10863
There is an increasing awareness of how the aesthetical performance of wood exposed outdoors changes over time and especially in the first few years after installation. Mould and blue stain fungi are biological agents that contribute to the weather grey colour on a wooden façade, and the blue stain fungi Aureobasidium pullulans is commonly identified as colonizer on coated and uncoated wood expos...
L Ross Gobakken, G Alfredsen


Identification of the key factors influencing development of the blue stain fungi
2016 - IRG/WP 16-10872
Service life of wood is more and more frequently affected by aesthetic requirements than functional ones. In order to elucidate various aspects of service life, model house with façade elements made of 22 materials was built on the field test site at Department of Wood Science and Technology in Ljubljana. Colour and fungal disfigurement is among other parameters monitored on this house. In parall...
D Kržišnik, B Lesar, N Thaler, M Humar


Effect of the Storage Time of Logs in Anti-Stain Treatment Effectiveness
2016 - IRG/WP 16-30683
Storage of green lumber, for 7 months, operationally treated with anti-stain products, depending on the storage time of the logs (10, 20 and 30 days) post harvesting allows to affirm that with increasing storage time of the logs, occurs a progressive increase in intensity, severity and types of fungi present in the logs. It is further noted, a significant increase in the percentage of sawn lumber ...
M A Peredo, C Barria


Assessment of the biological durability of wood treated with organosilicon compounds
2016 - IRG/WP 16-30685
The European wood construction market is in need of environmentally friendly wood-based products whose service life meets the expectations of end users. Non-biocidal silicon-based water repellents, which can be applied to different materials, help minimize their vulnerability/susceptibility to liquid water. Consequently, they have the potential of increasing wood’s resistance against decay fungi...
M Kutnik, M Montibus, S Derocker, S Salivati, J-P Lecomte


Colorant Treatments to Enhance the Weathering Resistance of Western Red cedar
2016 - IRG/WP 16-40737
Western redcedar is renowned for its decay resistance, but, like most wood products, it requires frequent maintenance in many exterior applications to maintain its appearance. To provide adequate long-term performance in exterior applications, it must be protected against light, water, and disfiguring fungal growth. Colorant treatments, with and without preservatives, were investigated for their a...
R Stirling, V Landry


Development of methodologies to evaluate tanning blocking coatings
2016 - IRG/WP 16-40760
In Europe an increased interest in using home-grown hardwoods as sustainable and renewable construction materials started a few years ago. Amongst these species oak and chestnut are two interesting candidates as their heartwood contain a significant amount of tannins which contribute to their natural durability. To avoid wood greying and dimensional variations, oak and chestnut must be protected b...
C Reynaud, L Podgorski


Effects of climatic factors and material properties on mould growth on untreated wooden claddings
2017 - IRG/WP 17-10884
Mould growth is an important contributor to colour change of untreated wood exposed outdoors. Predicting the development of mould growth is therefore important to ensure successful use of untreated wood as a façade material. More knowledge about the factors affecting mould growth on outdoor exposed wood is required to give better predictions. In this study, climatic factors and material propertie...
S Karlsen Lie, G I Vestøl, O Høibø, L Ross Gobakken


Fungal growth on coated wood exposed outdoors: influence of coating pigmentation, cardinal direction and inclination of wood surfaces
2017 - IRG/WP 17-10896
The objective of the SERVOWOOD project was to develop and establish European Standards that will facilitate the prediction of service life for exterior wood coatings. One of the objective of this project was to study fungal growth of the field exposed panels. Two coatings applied in 2 and 3 coats were exposed for one year outdoors at 45° south: one solventborne (alkyd based) and one waterborne (a...
L Podgorski, C Reynaud, M Montibus


Bio-friendly wood protection systems - resistance to mould and blue-stain fungi
2017 - IRG/WP 17-30713
With stricter restrictions on the use of biocides and increasing environmental awareness there is a pronounced need for effective bio-friendly protection systems in the wood preservative and wood coating industry. One of the possible pathways is to exploit and utilize natural substances with active biological effects. Silanes, caffeine, natural oils and potassium carbonate were chosen as compounds...
L Ross Gobakken, W Perdoch, B Mazela, P Kwaśniewska-Sip, G Cofta


Susceptibility to filamentous fungi of plywood for furniture coated with waterborne acrylic lacquers
2017 - IRG/WP 17-40778
Filamentous fungi (mould), thanks to their little trophic requirements belong to organisms which grow exceptionally easy and fast in favorable hygrothermal conditions and attack both organic and inorganic materials even with only trace amounts of organic substances on the surface. The fungi often cause spoilage of foodstuffs, worsen the aesthetic of wood-based elements, and pose a threat to the en...
A Fojutowski, M Nowaczyk-Organista, P Hochmańska


The Comparison of Weathering Resistance of New Generation Wood-Coating Systems
2017 - IRG/WP 17-40789
In this study, the performance of wood-coating systems containing different UV absorbers was evaluated in artificial weathering conditions. Acrylic-based resin containing three different UV absorbers was applied on oriental beech and scots pine surfaces. Weathering conditions were sustained for 84 days. After the weathering test, the change of color and roughness on the wood surface was measured t...
Ö Özgenç, S Durmaz


Previous Page | Next Page