Soft rot test of copper/chrome/arsenic treated heartwood of three Malaysian timbers by the vermiculite-burial method. (+ correction document of 25 July 1990)
1990 - IRG/WP 2354
Heartwood of copper-chrome-arsenic (CCA) treated kempas (Koompassia malaccensis), tualang (Koompassia excelsa) and keruing (Dipterocarpus spec.) was found to be susceptible to soft rot in recent pole surveys. Standardized heartwood blocks were impregnated with 0 to 6.3% (w/v) CCA and challenged to decay for twelve weeks by a mixed inocula of Chaetomium globosum, Glenospora graphii, Humicula grisea...
R-D Peek, A H H Wong


Oral toxicity of a slow-acting insecticide Amdro® to the Formosan subterranean termite
1982 - IRG/WP 1162
The use of toxic baits to control the Formosan subterranean termite Coptotermes formosanus Shiraki requires an insecticide that is non-repellent and sufficiently slow acting that poisoned termites leave treated areas before dying. Of the many insecticides screened, only Amdro® exhibited these characteristics. The oral toxicity (LD 50) of Amdro® to Coptotermes formosanus was estimated at 12.33 µ...
N-Y Su, M Tamashiro, J R Yates III


Performance of proprietary formulations of anti-sapstain preservatives on Hevea brasiliensis timbers in laboratory tests
1989 - IRG/WP 3532
A total of 10 proprietary and two experimental formulations were assessed for their effectiveness against sap-stain caused by Botryodiplodia theobromae on Rubberwood (Hevea brasiliensis). Sterilized wood samples 5x20x40 mm³ were dipped in the test chemicals for 60 seconds and then inoculated with 0.5 ml of culture filtrate of Botryodiplodia theobromae for incubation in sterile, damp petri dishes....
L T Hong


Objectives of future collaborative soft rot tests
1972 - IRG/WP 209
Progress has been made towards acceptance of a defined laboratory test method for determining the toxicity of preservatives against soft rot fungi (Documents IRG/WP/201 and IRG/WP/208) and, at the 1971 meeting in Brussels, the framework of collaboration for the next phase of testing was discussed. Time available at Brussels did not permit restatement of objectives, consideration of the stages by w...
J G Savory


Multiple-Phase Pressure (MPP) Process: One-stage CCA treatment and accelerated fixation process. 4. MPP compared with other processes for achieving acceptable treatment of radiata pine heartwood
1998 - IRG/WP 98-40115
Although radiata pine sapwood is very amenable to preservative treatment, it is often difficult to achieve the required standard for heartwood treatment. A preliminary investigation showed that to achieve the NZ Timber Preservation Council minimum penetration requirements for radiata pine heartwood using the Multiple-Phase Pressure (MPP) Process, a hydraulic pressure of at least 1250 kPa for 20 m...
K Nasheri, J A Drysdale, G Durbin, M E Hedley


Exposure of preservative treated wood to terrestrial microcosms, pure cultures of fungi and in the field
1997 - IRG/WP 97-20114
Small stakes (5x10x100 mm3) of treated and untreated Pinus sylvestris sapwood were exposed in terrestrial microcosms with different soils, two taken from test fields in Sweden, one soil from a conifer forest and one garden compost soil. Stakes of the same size were also exposed to pure cultures of the brown and white rot fungi, Postia placenta and Phanerochaete chrysosporium. After exposure, weigh...
M-L Edlund


On the possibilities of the use of juvenile hormone in wood protection
1976 - IRG/WP 363
The annual world-wide extent of losses caused by wood-destroying insects in timber in buildings and timberyards is very difficult to estimate. In general exact values are only known in cases of claims for damages from insurance companies or in litigation. At present the best known wood destroying insects in Switzerland are the house longhorn beetle (Hylotrupes bajulus) and the common furniture bee...
P Tscholl


Co-operative research project on L-joint testing. Sampling after 4 years exposure
1987 - IRG/WP 2274
In September 1983, Document No: IRG/WP/2208 was distributed giving guidance on sampling after 8 months exposure and including tables on which to record the test results. Similarly in September 1984, Document No: IRG/WP/2233 was distributed concerning sampling after 18 months exposure. No major problems have been notified to Princes Risborough Laboratory concerning the sampling method. It is theref...
J K Carey, A F Bravery


Field test of wood preservatives with Nasutitermes rippertii RAMBUR in Cuba
1996 - IRG/WP 96-10181
A field test of wood preservatives was carried out with Nasutitermes rippertii RAMBUR in the vicinity of the Material Testing Centre „Alexander von Humboldt" in Santiago de las Vegas/ Havana (Cuba) for 12 and 24 months. Test specimens of Pinus sylvestris L., Picea abies (L.) Karst. and Fagus sylvatica L. with dimensions of 25 x 25 x 490 mm³ were arranged vertically or horizontally in a circle o...
W Unger


Surface checking of CCA-treated radiata pine decking timber exposed to natural weathering
2000 - IRG/WP 00-40165
A field trial was established at four locations in Australia to assess the effect of CCA and CCA-wax treatment on the checking (cracking) of radiata pine decking timber exposed to natural weathering. Untreated decking timber and timber that had been pressure treated with water acted as controls. After 1 year's exposure the number and sizes of checks occurring in treated timber and control...
P D Evans, P J Beutel, C F Donnelly, R B Cunningham


Potential toxicants for controlling soft rot in preservative treated hardwoods. Part 2: Laboratory screening tests using sawdust
1977 - IRG/WP 2101
A technique is described for the rapid screening of toxicants against microorganisms, represented by the brown rot, Gloeophyllum trabeum, and a natural inoculum from soft rotted wood. Sawdust, in this case from sapwood of Eucalyptus maculata, is pretreated with the candidate formulation and moistened before inoculation. Visual scoring of growth can be used to discriminate suitable candidates as ea...
J D Thornton


Surface Barriers for Protection of Culture and Heritage Wooden Objects from Insect Attack
2004 - IRG/WP 04-40286
Anoxic treatment is an environment friendly procedure for eradication of wood boring insects in wooden objects of cultural and historical heritage. However, after the anoxic treatment, wooden antiques remain susceptible to further insect attacks. Possible protection against insects could be provided by the so-called post-repression protective barriers. Potential coating materials for such barriers...
M Petric, M Pavlic, B Kricej, M Humar, F Pohleven


Screening of the technical performance and aquatic toxicity of N-methylolacrylamide treated wood
2000 - IRG/WP 00-40166
In the course of the last decades chemical modification of wood species, with a limited natural durability, has been subjected to intensive research. As a possible alternative and supplementary treatment of non-durable wood in a range of applications it remains one of the major topics in the wood preservation world. Different modification systems have been scaled-up and are now in an industrialisi...
V Rijckaert, S De Geyter, J Van Acker, M Stevens


Surface protection of wood with titanium, zirconium and manganese compounds
2005 - IRG/WP 05-30376
Thin radiata pine veneers were treated with a range of titanium, zirconium and manganese compounds and exposed to natural weathering. Veneer weight and tensile strength losses were used to assess the protective efficacy of the compounds. The oxidative manganese compounds potassium permanganate and manganic acetate restricted both weight and tensile strength loss of treated wood veneers during weat...
K J Schmalzl, P D Evans


A technique for measuring preservative loss or redistribution during leaching
1983 - IRG/WP 2199
Radiata pine sapwood stakes were treated with benzalkonium chloride (AAC) or copper-chrome-arsenate (CCA). After fixation and drying the outer 2 mm and 2-4 mm layers were removed from one radial longitudinal face. The planed face was coated with a waterproof coating and AAC-treated stakes were leached for 6, 12 or 18 weeks; 12 weeks for the CCA-treated stakes. After airdrying three 2 mm layers (0-...
J A Drysdale


The movement of iron into field test stakes
1987 - IRG/WP 2284
Failed and sacrificial stakes recovered from the Westham Island field test site were examined for their iron content. Varying amounts were recorded, which were greatest in the failed stakes. The possible role of the iron taken up by the below ground portion of the stakes, in accelerating the decay process and/or the preservative leaching is under investigation. The reaction of the iron with the ch...
J N R Ruddick, P I Morris


Testing blue stain fungicides for joinery timber in combination with natural weathering
1976 - IRG/WP 268
Joinery timber in outside use becomes affected by blue-stain after a short time of exposure. This is especially the case with pine sapwood treated with unpigmented lacquer, but also with other timber species as well as different types of surface treatment. According to the basic investigations of BUTIN this is due to special types of blue-stain fungi, called "Lack-bläue" (lacquer blue-stain), in ...
H Willeitner


Studies in an accelerated soil bed facility on the decay susceptibility of U.K. grown spruce and pine poles treated with copper/chrome/arsenic (CCA) by pressurised sap-displacement. Part 1: Setting up of soil beds and initial soft rot results
1990 - IRG/WP 2344
The paper describes the methodology used in the construction and early operation of an accelerated soil bed facility used to examine the decay susceptibility of U.K. grown Scots and Corsican pine and Sitka and Norway spruce treated with C.C.A. by high pressure sap-displacememt. The design and control of the facility as well as the preparation, soil exposure and soft rot decay analysis of quarter p...
A Bruce, S D Hainey, G M Smith, B King, P D Evans


Soft-rot testing. Memo to CEN
1983 - IRG/WP 2206 A
1. Development of a single test procedure to assess performance of preservatives against soft rot fungi is an ideal that cannot be realised at present, if results are to be both reproducible between laboratories and pertinent to the practical requirements of individual countries. 2. Consensus opinion amongst members of Sub Group I - Soft rot tests, of Working Group II - Fundamentals of Testing, of the IRG, is that the immediate needs of CEN would be best answered by: (a) a code of recommended practice, (b) a multiplicity of test procedures, and (c) a degree of flexibility in test procedures. 3. The code of recommended practice should recognise the need for: (a) a pure culture, synthetic medium (sand or vermiculite + nutrients), single wood species test to be adopted by all laboratories as a common reference point of testing, (b) mixed inoculum and/or unsterile soil laboratory or fungus cellar tests which account for local variations in the fungal flora, (c) incorporation of a range of wood species where applicable (i.e. where mixed hardwoods comprise the main resource), (d) provision of local internal standards of known performance under field conditions, (e) incorporation of leaching procedures other than standard methods with deionized water (e.g. mild acid, milk alkali, ionic solutions of various salts) where applicable to local exposure conditions, (f) precise definition of the criteria used for establishing toxic thresholds (mass loss, strength loss, microscopic examination). 4. Initial screening tests should remain the province of the individual research worker. 5. The code of recommended practice should have the sole purpose of establishing provisional retention levels for subsequent confirmation by field trial. 6. IRG should list and approve test procedures considered adequate to establish toxic thresholds for preservatives against soft rot fungi. 7. It should be clearly understood that when using a series of test techniques, it is inevitable that a range of toxic thresholds will be obtained for the same preservative. 8. Guidelines should be drawn up for interpretation of test data for subsequent transformation to provisional retention levels. 9. Adoption of the broad principles outlines above is recognition of the dynamic nature of toxic thresholds. The additional information obtained by a more flexible, and complex, approach to testing may make interpretation more difficult but should provide data from which response of preservatives to varying biological and environmental hazards can be more realistically assessed. 10. It is recommended that CEN adopt, in principle, the basic philosophy of testing outlined above and move towards formulation of a Working Document in collaboration with IRG
J A Butcher, D J Dickinson


The ground proximity decay test method
2000 - IRG/WP 00-20205
A decay field test method, which has been recently proposed for the standardization by the AWPA, is described for evaluating the relative performance of wood samples in a severe above ground situation exposed to the weather. Data is presented on the relative performance of untreated control samples and standard preservative systems exposed at the same site at different time periods, or at differen...
A F Preston, P J Walcheski, K J Archer, A R Zahora, L Jin


The degradation of wood surfaces by dilute acids
1985 - IRG/WP 3326
Thin radial/longitudinal sections(~100 µ) of Corsican Pine (Pinus nigra) and Lime (Tilia vulgaris), were exposed to Sulphuric, Sulphurous, nitric, acetic, and formic acid at 40°C in the pH range 2-6. After about 3 months exposure to Sulphuric, nitric, acetic and formic acid at pH 2.0 Pine lost some 20-25% of its tensile strength. Losses in tensile strength due to sulphurous acid were greater bei...
P D Evans, W B Banks


Glue-line additives for protecting plywood. A review
1978 - IRG/WP 2102
The conclusions of this review are: 1) Insecticidal glue-line additives can be used satisfactorily to protect plywood against insect attack. 2) It is uncertain, in spite of some claims, wether fungicidal glue-line additives can be similarly used to protect plywood against fungi under damp conditiones. There is a need for further work to validate the mycological tests that may be used to investigat...
R Cockcroft


Durability of some alternatives to preservative treated wood
2004 - IRG/WP 04-30353
The environmental discussion in Sweden has lead to an increasing use of naturally durable domestic wood species and wood treated according to alternative methods for use above ground. A number of these alternatives have been tested according to field- and laboratory tests and compared to wood treated with preservatives for above ground use. Seven untreated wood species, four alternative wood treat...
M-L Edlund


A field study on the suitability of the European lap-joint test
2001 - IRG/WP 01-20239
Within the framework of the European SM&T Research Project "Co-normative research on field tests for wood preservatives out of ground contact in conjunction with methods for preconditioning test specimens prior to test" (FACT) one aim was to establish the suitability of the European lap-joint test (as it is described in ENV 12037:1996) to assess wood preservatives in the field in EHC 3. Scots ...
M Grinda, Ö Bergman, H-V Borck, D Dickinson, P Esser, R Gründlinger, H Leithoff, S Molnar, L Paajanen, N Pfabigan, E D Suttie, F Thomassin, T Nilsson, J Van Acker, M Van Der Zee, A Voss


Quantification of creosote migration down wooden poles and the prevention of its depletion during flood irrigation
1994 - IRG/WP 94-50032
Polyethylene field liners heat-shrunk onto soil-contact surfaces prevented decay of creosote-treated Eucalyptus grandis vineyard poles under flood-irrigation. The present work quantified losses of creosote from these poles after six and 24 months' service. After six months' service the mean creosote retention of unlined poles above the ground line was 12.62% (m/m dry wood), with ...
M Behr, A A W Baecker