IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1022 documents. Displaying 25 entries per page.


Comparison of colour change in wood clear-coating systems including inorganic and organic UV absorbers for exterior use
2010 - IRG/WP 10-40499
The aim of this work is to compare the performance of inorganic and organic UV absorbers used in a wood coating application against weathering. Our study has investigated the colour changes of selected UV absorbers; hombitec 402 RM from the Sachtleben Company as an inorganic UV absorber, tinuvin 477 DW from the Ciba Company as an organic UV absorber. The study was carried out on two wood species; ...
Ö Özgenç, B Forsthuber, A Teischinger, C Hansmann


TMT–Interlab–Test to establish suitable quality control techniques - Structure and first results
2010 - IRG/WP 10-40503
As a result of growing quality demands from manufacturers and end-consumers of thermally modified timber (TMT) recent scientific research activities are increasingly focussed on modification mechanisms and by this on the development of suitable quality control methods. To deepen the knowledge in modification mechanisms and to obtain a larger variety of scientific data for TMT depending on the trea...
C R Welzbacher


Wood protection by means of electro osmotic pulsing technology (PLEOT)
2010 - IRG/WP 10-40505
Wood protection is mainly based on chemical protection of wood. The disposal of wood preservative treated material causes restrictions in its later use or recirculation into the eco-cycle. A new protective system, electro-osmotic pulsing technology on wood, called PLEOT, is tested in a fungi test and in soil contact. Mass loss and moisture content of Scots pine sapwood samples was calculated after...
A Treu, E Larnøy


Moisture dynamics of WPC as basis for biological durability
2010 - IRG/WP 10-40520
The largest market for wood-polymer composites (WPCs) is currently decking. Although many products are commercially available, a proper standard for the assessment of the biological durability of WPC does not exist. Recommended standards for testing resistance against basidiomycetes should be completed with a method to bring the specimens in a worst case situation, obtaining a moisture level high ...
N Defoirdt, J Van Acker, J Van den Bulcke


Wet and dry adhesion of coatings on modified and unmodified wood: comparison of the pull-off test and the cross-cut test
2010 - IRG/WP 10-40524
The objective of this paper is to study the influence of several types of modification (acetylation, furfurylation, thermal modification) on coatings adhesion and to compare two methods of assessing the adhesion: the cross-cut test and the pull-off test both tested in dry and wet conditions. The study also investigates the effect of other parameters of the wood substrates on adhesion like the ring...
L Podgorski, G Grüll, M Truskaller, J D Lanvin, V Georges, S Bollmus


Comparison of laboratory and semi-field tests for the estimation of leaching rates from treated wood
2010 - IRG/WP 10-50274
The authorization of wood preservative formulations in the European Union according to the Biocidal Products Directive (BPD) includes the assessment of environmental risks by the emission of active ingredients. This risk assessment includes scenarios for preserved wood (e.g. house scenario, noise barrier), in which the predicted environmental concentration (PEC) for soil and water is calculated, u...
N Morsing, M Klamer, B Seidel, J Wittenzellner, M Maier, J Habicht


Chapter 14 - Accelerated fixation of CCA-treated bamboo
2007 - IRG/WP 07-10635-14
Chromated copper arsenate type C (CCA-C) fixation study on impregnated (with adequate w/v 6% CCA solution) then boiled, oven-dried, normal, air-dried and steamed bamboo slices of airdried borakbamboo (Bambusa balcooa Roxb.) of Bangladesh, revealed almost complete fixation in steamed (accelerated fixation) and air-dried (3 weeks, slow fixation) bamboo slices compared to moderate to low fixati...
A K Lahiry


Fungal biodegradation of CCA-treated wood wastes
2011 - IRG/WP 10-50276
Fungal biodegradation could be employed as a pretreatment method to alleviate problems caused by landfill disposal of CCA-treated wood wastes (e.g. a shortage of landfill space and a release of leacheate). It could be used to decrease the volume of waste and to remove metals from waste simultaneously. We have screened hundreds of decay fungi, including fungi isolated from CCA-treated wood in servi...
Gyu-Hyeok Kim, Yong-Seok Choi, Jae-Jin Kim


NHA Choice test: Feeding dilemma for Reticulitermes flavipes (Kollar)
2011 - IRG/WP 11-10746
An AWPA laboratory choice test was performed with Reticulitermes flavipes (Kollar) to determine the role of feeding stimulation or aggregation by N’N napthaloylhydroxylamine (NHA). Pine blocks were vacuum treated with aqueous concentrations of NHA ranging from 250-10,000ppm and exposed to one gram R. flavipes workers in the dual block choice test which included one treated and one untreated ...
F Green III, S N Kartal, P K Lebow, R A Arango


Basidiomycete colonization of Scots pine sapwood quantified by qPCR and TGA
2011 - IRG/WP 11-10750
Scots pine (Pinus sylvestris L.) is an important softwood species in Northern Europe and is frequently used as material for various wood protection systems. In Europe, EN 113 is the standard basidiomycete laboratory durability test method, using mass loss as evaluation criteria. In this paper quantitative real-time PCR (qPCR) and thermogravimetric analysis (TGA) was used to characterize coloniza...
G Alfredsen, S Bollmus, T K Bader, K Hofstetter


Measuring fungal cellulolytic enzyme activity in degrading wood
2011 - IRG/WP 11-10753
An enzyme assay which measures enzyme activity directly from wood will assist in the fundamental understanding of the enzyme components of the decay mechanism of rot fungi and any changes in the presence of wood protectants. At present, to measure fungal carbohydrate degrading enzyme activity in the presence of wood, two methods are used: either 1) the enzyme is measured in the growth media contai...
S M Duncan, J S Schilling


Molecular investigation of Postia placenta growing in modified wood
2011 - IRG/WP 11-10756
Brown rot is the most common and destructive type of fungal decay for wood in service. These fungi depolymerize preferentially the structural carbohydrates, cellulose and hemicellulose in the cell wall leaving oxidized lignin behind. Modified wood can provide protection against a variety of wood deteriorating organisms, including decay fungi. However, there is still little known about the mode of ...
B Schmöllerl, G Alfredsen, C G Fossdal, M Westin, A Steitz


Growth conditions for fungal decay in wooden constructions – practical experience versus literature
2011 - IRG/WP 11-10758
Data regarding moisture and temperature requirements of decay fungi found in literature have been compared to experience from observations in a large number of Norwegian buildings. A number of selected situations are discussed, among those exposure to high relative humidity, exposure to free water and decay in the supposedly adverse conditions on Svalbard. The moisture content in wood has to be at...
M Sand Sivertsen, J Mattsson


The influence of moisture content and wood pH variation on fungal melanin formation in wood substrates
2011 - IRG/WP 11-10759
Wood decay patterns are strongly influenced by the conditions of the wood substrate, including moisture content and pH. In an antagonistic environment some fungi respond with pigment formation that helps to isolate and protect their mycelium. This is often associated with slower fungal growth and delay of wood mass loss. Dark colored melanin is the most common pigment formed by wood decay fungi, a...
D Tudor, S C Robinson, P A Cooper


Durability testing of coconut shell according to ENV 807
2011 - IRG/WP 11-10761
Coconut shell was tested in the laboratory according to the European standard ENV 807 with three different soil types: compost soil, brown rot/soft rot rich soil and white rot/soft rot rich soil. Mass losses between 14 and 16 % were achieved with all three soils, indicating that the decay type is of little importance in the degradation process. Somewhat higher mass losses, 19-22 % were obtained fo...
J Jermer, A H H Wong, K Segerholm, T Nilsson


Decay hazard mapping for Europe
2011 - IRG/WP 11-20463
In this study, two different dose-response models for above-ground decay as well as a model transferring macro climate data to wood climate data are presented. The models base on data from field trials, which had been conducted at 28 European test sites, and were used to calculate the relative risk for decay caused by climate variability in Europe. The two dose-response models give coherent result...
C Brischke, E Frühwald Hansson, D Kavurmaci, S Thelandersson


Service life prediction of wooden components - Part 3: Approaching a comprehensive test methodology
2011 - IRG/WP 11-20464
This paper is the third in a series on 'service life prediction' of wooden components and should be considered as a discussion paper. The authors tried to analyze the topic with a look from a distance and comment sometimes with a smile on the current controversial discussion about SLP issues. Nevertheless, the viewpoints of different groups, such as natural scientists, engineers, approva...
C Brischke, C R Welzbacher, L Meyer, T Bornemann, P Larsson Brelid, A Pilgård, E Frühwald-Hansson, M Westin, A O Rapp, S Thelandersson, J Jermer


Above ground testing at tropical test sites, what have we learned?
2011 - IRG/WP 11-20473
Three different above ground test methods have been utilized at a selection of five tropical and sub-tropical test sites with a variety of treated and untreated material. The results show that a multi-site approach to above ground field tests presents the opportunity for exposure to un-predicted biodeterioration hazards, which may be important for developmental products of poorly characterized fu...
A Preston, A Zahora, Y Cabrera, L Jin, C Schauwecker, P Walcheski


A comparative study and evaluation of methodologies used for determining wood preservative penetration
2011 - IRG/WP 11-20475
A series of methods for determining penetration of wood preservatives into the wood structure have been developed for either quality control (QC) or research and development purposes. QC methods range from monitoring the solution uptake, applying colour indicators or sampling specific wood samples followed by wood acid digestion/atomic absorption spectroscopy (AAS) or solvent extraction/chromatogr...
R Craciun, R Moeller, J Wittenzellner, T Jakob, J Habicht


Ten Year Field Tests of Borate-Treated Wood Against Subterranean Termites
2011 - IRG/WP 11-30557
In the mid 1990s, Forintek Canada Corp. initiated a study of the termite resistance of borate-treated lumber above ground, protected from rain in Canada, Japan and Hawaii. Predominant termite species at three test were Reticulitermes flavipes in Canada, and Coptotermes formosanus in both Japan and Hawaii. The material included hemlock and amabilis fir lumber treated with disodium octaborate tetrah...
P I Morris, J K Grace, K Tsunoda


Novel Approaches to the Development and Testing of Anti After-glow Additives for CCA-based Treatments of Poles
2011 - IRG/WP 11-30561
In this paper, a field fire stake testing screen method is described. This method uses stake samples from matched wood sources allowing replicates from different boards to be included. The method is easy to control and can provide quick comparative fire resistance test results. The parameters measured from the tests are percentage weight loss, minimum residual circumference and residual thicknes...
L Jin, P Walcheski, A Preston


Comparison of rates of wood decay from four different field test protocols following 4-5 years exposure at a site in New Zealand
2011 - IRG/WP 11-30565
The rate of decay of Pinus radiata was evaluated using four different field test protocols at a site near New Plymouth, New Zealand. The average Scheffer index was 86 over the five year period of testing. The field tests were an in-ground stake test (AWPA Std E7-01) and three above ground tests – lap-joint (AWPA Std E16-98), decking (AWPC protocol) and ground proximity tests (AWPA Std E18-06) T...
P Lobb, K Day, A Siraa


The case for using borates in termite control in tropical Australia
2011 - IRG/WP 11-30573
A brief historical overview of boron based wood preservatives efficacy against subterranean termite management worldwide, and in Australia, is presented. The boron based compounds to be used in H2 hazard conditions, may be applied as a surface treatment by dip, flood coat or spray, and rapidly penetrates to the centre of timber substrates, whether containing sapwood or heartwood. However, section ...
B M Ahmed (Shiday), J R J French


Challenges and new developments in testing electro osmotic pulsing technology (PLEOT) by means of conventional laboratory methods
2011 - IRG/WP 11-40555
A new wood protection system, electro-osmotic pulsing technology, called PLEOT, is tested in lab trials using different test setup. The technology is tested on Scots pine sapwood and beech wood samples exposed to brown- and white rot fungi. Mass loss and moisture content is calculated after testing and a chitin analysis are performed on the sample powder. Two different electrodes are used in ord...
A Treu, E Larnøy


Wet and dry adhesion of coatings on modified and unmodified wood: influence of 18 months of natural weathering on the pull-off test and cross-cut test results
2011 - IRG/WP 11-40569
The objective of this paper is to study the influence of several types of modification (acetylation, furfurylation, heat treatment) on coatings adhesion after 18 months of natural weathering according to EN 927-3 in Vienna (Austria). The paper compares two methods for assessing the adhesion: the cross-cut test (EN ISO 2409) which is the conventional method used and recommended in EN 927-3 and th...
L Podgorski, G Grüll, M Truskaller, J D Lanvin, S Bollmus


Previous Page | Next Page