Performance of wood exterior structures above ground in Spain built with softwood species. The situation case of a shelter bridge
2018 - IRG/WP 18-40844
Across Europe is very common to find wood exterior structures build in sawn and glue-laminated wood. Most of these exterior wood structures use softwood wood species such as: fir, spruce, larch and pine. In Spain exterior wood structures, became more and more popular since nineties, when sawn and glue-laminated wood were utilized for building exterior wood structures in overall Spain. This paper s...
D Lorenzo, M Touza, J Fernández-Golfín, A Lozano, J Benito


Preserved Wood in the Story of Sustainable Forestry
2018 - IRG/WP 18-50344
Sustainable forestry, at its simplest, is about growing trees. The full story, though, is much more complex. An important chapter of that story is the role that preserved wood plays in ensuring sustainability. Too often, this part of the sustainability story is rarely mentioned. It is time for the preserved wood industry to deliver a unified message of our critical role in sustainability. By res...
D Brookes


Performance of untreated timbers in above ground decking tests: Preliminary results from an international collaborative trial
2019 - IRG/WP 19-10940
The ability to accurately predict wood decay risks under varying environmental conditions has long been of interest to timber users. Accurate predictions are difficult owing to the myriad of variables associated with the decay process including wood species, wood inhabiting organisms, timber building element design and environmental conditions. Despite these difficulties, decay predictions have be...
L P Francis, J Norton, E Melcher, A H H Wong, J Kok Lai, M Klamer, M J Konkler, J J. Morrell


Determining the natural durability on xylarium samples: mini-block test, wood powder and chemical profiling
2019 - IRG/WP 19-10944
Xylaria, or wood collections, can be considered sleeping beauties in terms of wood technological and biological output. In this study we focus on determining the natural durability of xylarium specimens from the Federal Xylarium in the Royal Museum for Central Africa. The Federal Xylarium contains over 80,000 specimens, covering more than 13,000 species, mainly from Central Africa. These specimens...
V Deklerck, L De Ligne, J Van den Bulcke, E Espinoza, H Beeckman, J Van Acker


Diversity of wood decay fungi isolated from ground-contact wood stakes in Korea
2019 - IRG/WP 19-10952
This study was conducted to investigate wood decay fungi from 5 different ground-contact wood stakes in Korea. A total of 73 basidiomycetes were isolated and identified into 20 genera and 22 species by using molecular method. Among all fungi, only 6 species were brown-rot fungi and the others were white-rot fungi. Pinus densiflora and Quercus variabilis showed high fungal diversity and isolation f...
S-M Yoon, M-J Kim, W-J Hwang, Y-S Choi, D-W Son


Improvement of analytical methods of wood preservatives and its validation with collaborative testing
2019 - IRG/WP 19-20655
This discussion paper presents on-going collaborative test of analytical methods of wood preservatives according to the standardization process of Japan Agricultural Standard (JAS) by the Ministry of Agriculture, Forestry and Fisheries (MAFF). Food and Agricultural Materials Inspection Center (FAMIC) in close cooperated organization with the MAFF, has wide range of tasks about inspections and anal...
T Miyauchi, K Yamamoto, N Shota, Y Akabori, M Ikeda, J Eisawa, K Kambara, T Osawa, C Igarashi, Y Baba, W Ohmura, M Shimizu, M Samejima


Durability classification of preservative treated and modified wood
2019 - IRG/WP 19-20659
EN 350 (2016) allows formally to determine durability classes (DC) for wood products and wood-based materials, which was previously only possible for untreated wood in the form of natural durability. In a first study, the University of Goettingen carried out the durability classification of chemically modified (modified with 1,3-dimethylol-4,5-dihydroxyethyleneurea, DMDHEU) and preservative-treate...
S Bollmus, L Bachle, C Brischke, H Militz


Impact of water holding capacity and moisture content of soil substrates on the moisture content of wood in terrestrial microcosms
2019 - IRG/WP 19-20662
Terrestrial microcosms (TMC) are frequently used for testing the durability of wood and wood-based materials as well as the protective effectiveness of wood preservatives. In contrary to experiments in soil ecology sciences, the experimental set-up is usually rather simple. However, for service life prediction of wood exposed in ground, it is of immanent interest to better understand the different...
C Brischke, F L Wegener


Development of accelerated decay test for CLT using a fungus grown on agar medium
2019 - IRG/WP 19-20664
CLT is a large-scale wooden board which consists of several layers of sawn lumber stacked in altering directions. Therefore, a lot of large cross sections appear on all narrow faces of CLT. As water penetrates easily into timber from cross section, wooden material whose cross section is exposed to water in in a usage environment is susceptible to deterioration by organisms. Wood deterioration orga...
T Miyauchi, K Kambara, W Ohmura, T Mori, H Matsunaga, N Hattori


Exemplary aboveground hardwood protection from Coptotermes curvignathus under weathered conditions conferred by proprietary microemulsion-based cypermethrin (SARPECO®) and permethrin (AXIL®) biocides
2019 - IRG/WP 19-30749
SARPECO® (with cypermethrin) and AXIL® (with permethrin) solutions are water-based wood preservatives approved for dipping treatment providing 25 years of termite protection for solid wood and wood-based products in Europe and for more than 10 years in Indonesia. SARPECO® and AXIL® solutions are patented formulations based on concentrated microemulsions (ME) diluted with water as a dipping tre...
D Messaoudi, A H H Wong, C A D Tawi, N Bourguiba, O Fahy


Chemical Analysis of Southern Pine Pole Stubs Sixty Months Following Treatment with a Methylisothiocyanate-Based Solid Fumigant Stick
2019 - IRG/WP 19-30740
Methylisothiocyanate-based fumigants have been commercially used in the United States for over 35 years to control internal decay in utility poles and other wooden structures with little technological advancement. The most recently commercialized methylisothiocyanate-based fumigant is chemically known as dazomet. Dazomet is a free-flowing powder or granule that decomposes in the presence of mois...
D J Herdman, T Pope, R R Browning


Color change of timber exposed outdoors - Influence of season exposure test starts
2019 - IRG/WP 19-40865
For the client the material and color of the exterior wall are important, because they affect the impression of the building [1]. However, discoloration of the exterior wall begins as soon as the building is completed, by various factors such as rainfall. We tried to quantitatively evaluate the changes of the exterior wood, and to organize the influences of climate conditions, in order to use the ...
K Usami, H Ishiyama


Protecting wood exterior infrastructures above ground in Spain. The importance of protection by design in the performance
2019 - IRG/WP 19-40874
Across Spain is very common to find wood exterior infrastructures build mainly in sawn and glue-laminated wood. Most of these exterior wood infrastructures use softwood wood species such as: fir, spruce, larch and pine. In Spain exterior wood infrastructures, became more and more popular since nineties, when sawn and glue-laminated wood were utilized for building exterior wood infrastructures in o...
D Lorenzo, M Touza, J Fernandez-Golfín, A Lozano, J Benito, M T Troya, L Robertson


Performance of naturally durable decks after 15 years of field exposure
2020 - IRG/WP 20-10963
A decking test of Canadian species considered to be naturally durable was inspected after 15 years of exposure at test sites in Ontario and British Columbia. Based on the materials used in this experiment, Douglas-fir and yellow cypress had the greatest decay resistance, followed by eastern white cedar and western redcedar, and then by western larch and tamarack. All materials tested were more dur...
R Stirling, D Wong


Performance of bio-based building materials – durability and moisture dynamics
2020 - IRG/WP 20-20666
When exposed to conditions favourable for decay, bio-based building materials can be susceptible to degradation. Their ability to withstand deterioration over time (performance) depends on the intrinsic or enhanced durability of the material as well as its wetting and drying behaviour. The effect of fungicidal components in wood is known since long. Other material characteristics, such as the mate...
L De Ligne, J Caes, S Omar, J Van den Bulcke, J M Baetens, B De Baets, J Van Acker


Water interactions in wood polyesterified with sorbitol and citric acid
2020 - IRG/WP 20-40888
Polyesterifcation of wood with sorbitol and citric acid seems to be a promising chemical wood modification technique that is both low-cost and produced from bio-based chemicals. An interesting aspect of the modification is the interaction of water with the polyesterified wood since the relationship with moisture appears to be unique compared to other wood modification systems. This communication p...
G Beck, A Treu, E Larnøy


Modelling decay rates of timber exposed above ground on four different continents
2020 - IRG/WP 20-20670
Durability performance data from an international decking trial were analysed to explore relationships with climate variables, particularly those related to temperature and rainfall. Matched decking samples of slash pine (Pinus elliottii) sapwood and heartwood, spotted gum (Corymbia citriodora), Norway spruce (Picea abies) and Scots pine sapwood (Pinus sylvestris) were exposed to the weather above...
L P Francis, J J Morrell, C Brischke, P B Van Niekerk, J Norton


Impact of fungal decay on the bending properties of wood
2020 - IRG/WP 20-20671
Wood used outdoors is generally prone to fungal degradation, and its impact on the structural integrity of wood is an immanent factor for service life planning with timber. Wood decayed to very small mass losses can suffer from a significant reduction in mechanical strength and elastic properties. Hence, the latter are preferred indicators to detect decay in wood durability studies. Numerous previ...
S Bollmus, P B van Niekerk, C Brischke


Evaluation of weathering and termite resistance of the Myoung-oil as a Korean traditional coating agent
2022 - IRG/WP 22-10996
This study investigated the applicability of Myoung-oil (MO) as an eco-friendly preservative of Korean wooden cultural properties and buildings. Wood test specimens painted with various concentrations of MO were exposed in the external environment. Then color change and wettability of the wood surface were evaluated and compared depending on the exposure time. As a result of exposure for 12 months...
S-M Yoon, Y Park, W-S Jeon, H-M Lee, J-G Park, K Dal Nam, W-J Hwang


Performance of wood exterior structures above ground in Spain. Performance and durability of a shelter of spruce in a shopping centre after 20 years
2022 - IRG/WP 22-20680
Across Europe is very common to find wood exterior structures mainly build in sawn and glue-laminated wood. Most of these exterior wood structures use softwood wood species such as: fir, spruce, pine or douglas. In Spain exterior wood structures, became more and more popular since nineties, when sawn and glue-laminated wood were utilized for building exterior wood structures in overall Spain. In m...
D Lorenzo, A Lozano, M Alonso, J Fernández-Golfín, M Touza, J Benito


Studies into the effect of soil type and soil layer on the in-ground decay of European beech
2022 - IRG/WP 22-20681
In this study, European beech (Fagus sylvatica L.) specimens were exposed to three different soil types; Podsol (Podzol), Braunerde (Cambisol), and Pararendzina (Regosol), in adapted terrestrial microcosm (TMC) tests according to CEN/TS 15083-2 (2005). Soils were sampled (250 mm deep) from field sites and separated into their constituent layers to deliver three TMC setups; mineral soil layer only ...
B N Marais, S Kovacs, M Jansen, C Brischke


Combining MRI and X-ray CT to monitor fungal decay of plywood and OSB in a lab test
2022 - IRG/WP 22-20683
Bio-based building materials, such as wood and wood-engineered products, are susceptible to degradation by decay fungi. In-depth knowledge on the intricate material-fungus relationship as well as performance data for many bio-based building materials are still lacking, and especially knowledge on how a material’s structure and moisture properties affect the degradation process is missing. Althou...
L De Ligne, T Núñez Guitar, C Vanhove, J Van Acker, J Van den Bulcke


Using satellite-retrieved soil moisture data to model the decay risk of in-ground timber
2022 - IRG/WP 22-20689
Satellite-derived soil moisture data from the Soil Moisture Active Passive (SMAP) was extracted for a 9 x 9 km point grid over Europe. The data was then used as input to a dose-response wood decay model based on terrestrial microcosm (TMC) tests. The resulting hazard map plotted dose as an indicator of in-ground wood decay based on differences in annual temperature and soil moisture characteristic...
P B van Niekerk, M Schönauer, B N Marais, C Brischke


Durability against fungal decay of sorbitol and citric acid (SorCA) modified wood
2022 - IRG/WP 22-40928
Most European-grown wood species are susceptible to biological degradation, specifically, they suffer from a poor resistance against wood-destroying fungi. Therefore, prior to outdoor exposure, wood has to be treated either by applying a protective coating on its surface or by full-volume impregnation with antifungal chemicals. However, due to environmental and health concerns, the most frequently...
K Kurkowiak, L Emmerich, H Militz


Biological assessment of bio-based phase change materials in wood for construction applications
2022 - IRG/WP 22-40935
Solid wood can serve multi-functionality for energy savings in buildings. The study reveals the results of bio-deterioration and degradation of solid Scots pine wood used to incorporate single or multicomponent fatty acid mixtures as bio-based phase change materials (BPCMs). The sapwood samples were impregnated with capric acid (CA), methyl palmitate (MP), lauryl alcohol (LA) and a mixture of coco...
S Palanti, A Temiz, G Köse Demirel, G Hekimoğlu, A Sari, M Nazari, J Gao, M Jebrane, T Schnabel, N Terziev