Corrosion of fasteners in heat-treated wood – progress report after nine years’ exposure outdoors
2012 - IRG/WP 12-40601
The corrosion of common fastener materials now in use - mild steel, zinc-coated steel, aluminium and Sanbond Z-coated steel – has been evaluated after nine years’ exposure outdoors in untreated and heat-treated (thermally modified) spruce (Picea abies). Spruce from south-western Sweden was used. The heat-treatment was carried out in Finland by Stora-Enso Oy according to the ThermoWood process ...
J Jermer, B-L Andersson


Field-testing of Norway Spruce Claddings with Monitoring of Moisture Content, Material Temperature and Microclimate
2012 - IRG/WP 12-20502
The physical function of a cladding is to protect the interior construction. Under normal circumstances the performance requirements can be met for a very long time, meaning that the technical service life of a wooden cladding can be very long. Since the cladding is a major part of the facade, it also has visual requirements that may define the aesthetic service life, and often it is much shorter ...
G I Vestøl, L Ross Gobakken


Mould growth on wood-based materials – a simulated in-service study
2012 - IRG/WP 12-20503
Ten different wood-based materials including preservative-treated wood, fire retardant-treated wood, modified wood, WPCs and untreated references of pine sapwood and spruce were placed in three different environments (an attic and two crawl spaces) for a period of 26 months. Mould growth was analysed at five to seven month intervals in an effort to map the growth development. The relative humidit...
G Bok, P Johansson, J Jermer


Effectiveness of CCA-C and CCB preservatives after a 30 years stake test
2012 - IRG/WP 12-30606
The objective of this experiment was to assess the durability of four pine species treated with waterborne preservatives. In order to determinate this, a stake field test, following the IUFRO (International Union of Forestry Research Organizations) recommendations, was installed at Experimental Station of Luiz Antonio (21º 32’ S and 47º 42’ W), State of São Paulo, Brazil. Species under t...
I PJankowsky, E S Lepage, C Salvela, J M Vidal, S Takeshita


The effect on moisture content of water trapped in wood joints
2012 - IRG/WP 12-40613
To predict the service life of a structure, a model where the exposure of a structure is compared to its resistance can be used. Which exposure and resistance parameters that are relevant depend on which materials the structure consist of. This approach, with an exposure and a resistance parameter, is similar to the one used in structural engineering where a load (exposure) is compared to the bear...
M Fredriksson, L Wadsö, P Johansson


An assessment of soft rot in preservative-treated poles in two test sites and two network areas in New South Wales
2013 - IRG/WP 13-10801
This document presents an extended summary of recent investigations into soft rot attack of preservative treated power poles from the re-inspection of samples selected from two field sites and two in-service trials located in New South Wales, Australia. The in-ground sapwood of selected poles was assessed by probing and, after core sampling, by microscopy to determine the severity and extent of s...
W D Gardner, M A Powell, C Kirton


Resistance of Consolidated Deteriorated Wood to Wood Decay Fungi
2013 - IRG 13-10812
The main purpose of the experiment was to establish which consolidating products in impregnated wood are the most effective against wood decay fungi. Five different consolidators were tested: Paraloid B-72, Consolidating restaurateur, SG 715 BLANC (epoxy resin), R.712 polyester and the wood consolidant agent containing nano particles, which is still in development. From the already damaged wood ...
F Pohleven, A Valantič, M Petrič


Characterization of test fields
2013 - IRG/WP 13-20508
Test field characteristics and impact of test fields on wood degradation is important when testing wood protection. The current EN 252 standard has no requirement for knowledge of decay hazards, but most commonly a test field is known as a “brown”,- “white”,- or “soft rot” field. To understand which decay hazard wood preservatives are tested against, each test field should be character...
U Råberg, N Terziev, G Daniel


Quasi-in-situ durability tests on oak timber bridges
2013 - IRG/WP 13-20510
This study aims on developing a method for determination of wood durability on samples taken from real structures in service. Therefore quasi-in-situ durability tests have been conducted exemplarily on timber bridges made from English oak (Quercus robur L.). Drilling cores were found to be a feasible alternative to standard specimens for laboratory durability tests against pure cultures of Basidio...
C Brischke, C J Behnen, M-T Lenz, K Brandt, E Melcher


Determination of the natural durability of solid wood against wood-destroying fungi - a European round-robin test
2013 - IRG/WP 13-20511
In Europe the durability of wood against wood-destroying basidiomycetes is tested according to CEN/TS 15083-1 (2005). Hitherto existing experience with this standard is quite heterogeneous and results from previous round-robin tests have stayed unreported or have been reported incompletely. In particular the need for natural pre-weathering of the test specimens to allow potential detoxification of...
C Brischke, C R Welzbacher, A Gellerich, S Bollmus, M Humar, K Plaschkies, W Scheiding, G Alfredsen, J Van Acker, I De Windt


Climatic impacts on the moisture performance of wooden decking and facades
2013 - IRG/WP 13-20518
In outdoor usage wood is exposed to a variety of influences, which reduce its durability against biological deterioration and wetting. Besides many other factors the service life of wooden facades and cladding is dominated by occurring moisture loads on the one hand and their capability to withstand moisture on the other hand. Hence, climatic factors have a direct impact on the material climate an...
T Bornemann, C Brischke, G Alfredsen


Accelerated H3 above-ground decay testing
2013 - IRG/WP 13-20520
An above-ground H3 fungal field trial was installed at two sites in Australia and one in New Zealand, as well as in two Accelerated Field Simulators. The aim was to find a method that would shorten the time required for evaluating new preservatives and protection systems. One-quarter H3 retentions were installed, as first results suitable for registration occur when these reach 70% soundness. Twel...
L J Cookson, D Page, T Singh


Virulence of two Laboratory Test Strains and one Natural Isolate of Rhodonia (Oligoporus) placenta against Thermally Modified Pine and Beech Wood
2013 - IRG/WP 13-20524
Rhodonia (Oligoporus) placenta is known as a relative aggressive basidiomycete fungus against thermally modified timber. In durability lab tests, this often results in a lower durability class, compared to other test fungi. In the reported work, the virulence of three different strains of Rhodonia placenta for untreated and thermally modified timber was determined and compared. Therefore, two lab ...
K Plaschkies, W Scheiding, K Jacobs, N Rangno


Method for determining the critical moisture level for mould growth on building materials
2013 - IRG/WP 13-20530
The natural conditions of relative humidity (RH) and temperature (T) in different parts of a building is rarely constant over time. Instead, RH and T often vary cyclically and may pose a risk of mould growth as these conditions are the two key environmental parameters that controls mould growth. Consideration to both humidity and temperature conditions and the susceptibility to mould in a material...
A Ekstrand-Tobin, P Johansson, G Bok


Development of a rapid method to assess the rate of fungal colonization of wood
2013 - IRG/WP 13-20531
Testing of wood durability is today done mainly with accelerated exposure tests under rather realistic conditions (in ground, outdoors with moisture traps etc). Although such tests are accelerated with respect to the conditions that outdoor exposed wood structures are exposed to, they tend to take rather long time. The present paper presents the development of a rapid method intended to assess at ...
L Wadsö


Moisture distribution in glulam beams with natural cracks observed with CT Scanning before and after rain
2013 - IRG/WP 13-20534
The way cracks in outdoor wooden constructions affect durability is an interesting topic, since a certain amount of cracks can always be found naturally in wood and glued laminated wood. The question in this was, can cracks lead water into the wood and thereby increase the risk for decay and reduce strength and service life. Moisture balance, i.e., water absorption and water distribution were stud...
K Sandberg


Report on COST E37 Round Robin Tests – Comparison of results from laboratory and field tests
2013 - IRG/WP 13-20535
A round robin involving 15 European participants was set up in 2006. The round robin consists of both a field test according to the double layer test method and a laboratory test with two different preconditioning methods. When comparing EN 84 preconditioning (two weeks water leaching) with natural preconditioning (1 year in field, above ground) according to CEN/TS 15397, no significant difference...
M Westin, E Conti, J Creemers, P-O Flæte, A Gellerich, I Irbe, M Klamer, B Mazela, E Melcher, R Möller, L Nunes, S Palanti, L Reinprecht, E Suttie, H Viitanen


Copper leaching from copper-ethanolamine treated wood during exposure to terrestrial microorganisms
2013 - IRG/WP 13-30621
Copper-ethanolamine based wood preservatives are still the most important solutions for protection of wood in ground applications in Europe. Wood in ground is exposed to variety of organisms, which can act synergistically. In order to simulate these conditions in laboratory, Scots pine (Pinus sylvestris) specimens impregnated with copper-ethanolamine preservative of three different concentrations ...
M Humar, N Thaler, B Lesar


40 year results from the largest preservative in-ground stake trial conducted in Australia
2013 - IRG/WP 13-30624
The final results from Australia’s largest preservative in-ground stake trial are listed. There were eight test sites, six in Australia and two in Papua New Guinea. The preservatives tested include low and high temperature creosotes, PCP and various water-borne preservatives including CCA and copper chromate. The main timbers examined were sawn Pinus radiata sapwood, sawn Eucalyptus regnans hear...
L J Cookson


Potential valorization of wood extractives from waste products of steam distillation of Aniba rosaeodora: antitermitic activity
2013 - IRG/WP 13-30629
Aniba rosaeodora, is a slow growing evergreens of the Lauraceae family which are indigenous over a wide range of the Greater Amazon Region (the Guianas and Venezuela, Brazilian Amazon…). The essential oil obtained from the wood has a characteristic aroma and is a long-established ingredient in the more expensive perfumes. The wood is also composed with alkaloid compounds like anibin. These compo...
N Amusant, A Digeon


Resistance of WPC against wood destroying fungi
2013 - IRG/WP 13-40627
The investigation of biological durability is a fundamental topic to assess the performance of Wood Plastic Composites (WPC) particularly for outdoor applications. In the last years, different test setups based on existing standards on the field of wood as well as the field of plastics were used for WPC. But the test methodologies give different information about the durability of the tested mater...
A Gellerich, S Bollmus, A Krause


Field performance of wood impregnated with siloxanes using supercritical carbon dioxide
2013 - IRG/WP 13-40632
This paper presents preliminary results from a 13-month field test containing pine sapwood samples (Pinus sylvestris) impregnated with a mixture of siloxane and organic biocides using supercritical carbon dioxide as carrier. Samples were exposed above ground at a Danish field test site using matched non-treated sapwood controls for every treated sample. All samples were painted before exposure. Pi...
A Kjellow, F Imsgard, J Fernandes, R Wagner, J Delis


Conclusions and Summary Report on an Environmental Life Cycle Assessment of ACQ-Treated Lumber Decking with Comparisons to Wood Plastic Composite Decking
2013 - IRG/WP 13-50295
The Treated Wood Council has completed a quantitative evaluation of the environmental impacts associated with the national production, use, and disposition of ACQ (alkaline copper quaternary)-treated lumber decking and wood plastic composite decking using life cycle assessment (LCA) methodologies and following ISO 14044 standards. The results for treated wood decking are significant. • Less En...
AquAeTer, Inc.


Durability of alternatives to CCA-treated wood - Results from field tests after 11 years exposure
2013 - IRG/WP 13-30633
The present study was initiated as a consequence of restrictions against the use of CCA-type wood preservatives in Sweden in the 1990s. New copper-based formulations were introduced on the market and to some extent, also alternatives to preservative-treated wood, such as thermally and chemically modified and linseed oil treated wood as well as heartwood of non-tropical naturally durable wood s...
P Larsson Brelid, M-L Edlund


Relevance of natural pre-weathering for laboratory decay tests with native, modified, and preservative-treated wood
2013 - IRG/WP 13-20522
The on-going development of new wood protection systems is hampered by the long term field tests currently in use. New accelerated test methods and novel methods for faster and more accurate evaluation of wood protection methods are requested. For both field decay tests and accelerated laboratory decay tests, limitations are imposed. This study is part of the research program ‘WoodBuild’, whic...
A Pilgård, C Brischke, L Meyer


Previous Page | Next Page