Preliminary observations of the effect of growth ring orientation on the surface checking of flat sawn Southern pine decking
2005 - IRG/WP 05-20313
Checking in decking timber is a serious defect and methods of reducing its severity are required to ensure that wood can compete with alternative decking materials. The first aim of this research was to test the hypothesis that flat sawn Southern pine decking boards with growth rings oriented concave to the exposed surface will develop less severe checking when exposed outdoors than similarly expo...
K Urban, P D Evans


Resistance of twenty-five species of timbers to marine borer attack at Visakhapatnam, east coast of India
1994 - IRG/WP 94-30036
Observations on the natural resistance of 25 species of timbers to marine borer attack for a twelve month period at the fishing harbour, Visakhapatnam, East Coast of India, indicate that none of the species was free from borer attack. The damage was mainly by teredinids - Teredo furcifera and Lyrodus pedicellatus. Martesia striata, Teredo parski, Bankia campanellata and Lyrodus bipartitus were als...
K S Rao, M Balaji, V V Srinivasan


Test methods for modifies wood: The EU-Thematic network approach
2002 - IRG/WP 02-20255
The last decade wood modification systems have become new wood treatment methods in Europe. Alongside several industrial initiatives for heat treatments also scaling up and pilot plant projects for chemical wood modification have recently been carried out. In 2000 an initiative to create a network related to these new developments was supported by the European Commission. Within the work proposed ...
J Van Acker, D Jones


Impregnation of timber with tannin as a mean of improving its dimensional stability
1992 - IRG/WP 92-3695
The results of a joint project carried out at the Timber Division of LNEC under the 2nd research programme of the CEC DGXII - "Wood as a renewable raw material" entitled "Stabilization of wood by impregnation processes" is presented. Pieces Maritime pine timber was impregnated with tannin under pressure to see if the treatment with tannin improved the behavior of wood regarding its dimensional sta...
J S Machado


IRG/COIPM INTERNATIONAL MARINE TEST - To determine the effect of timber substrate on the efectiveness of different preservatives in sea-water: Coding scheme
1976 - IRG/WP 420
It was agreed in Wildhaus on 15 May 1976 that preparations for the test detailed in Document No: IRG/WP/414 should commence immediately, but that initially only two water-borne preservatives should be used - a copper/chrome/arsenic (CCA) and a copper/chrome/boron (CCB) formulation respectively. PRL, England (R Cockcroft) would be responsible for supplying only the reference species treated with th...
Anonymous


A Novel Type of Multiple Cavity Attack in Wood Cell Walls of Heat-treated Timber Exposed in Seawater – Preliminary Observations
2004 - IRG/WP 04-10523
Samples of untreated and heat-treated Norway spruce and Douglas fir were submerged in Langstone Harbour, Portsmouth for 4 years at a depth of ca. 0.3 metres. The heat-treated samples had been prepared using the Plato process. Samples were initially assessed for the severity of marine borer damage and were then examined microscopically for evidence of microbial decay. Longitudinal and transverse wo...
R A Eaton, C Björdal, T Nilsson


Biocidal Products Directive 98/8/EC and PT 08
2005 - IRG/WP 05-50224-1
The ECB Biocides Work Area is responsible for the scientific and technical issues concerning the approval of active substances in biocidal products as laid down in Directive 98/8/EC concerning the placing of biocidal products on the market. The first part of the presentation will deal with the Review Programme, especially it's legal context, the status of submitted dossiers and the p...
K van der Jagt


Whitewood - An external joinery timber?
1975 - IRG/WP 253
The timber used traditionally for softwood joinery in the UK is redwood (Pinus sylvestris). In the past its ready availability in the desired sizes and quality and its durability in service encouraged little competition. However, the past decade has seen some erosion of this position, particularly through the increased proportion of sapwood in redwood supplies. Since the sapwood is less durable th...
J W W Morgan


The use of lap-joints in natural durability testing: moisture content development during 36 months outside exposure trials
2000 - IRG/WP 00-20217
Lap-joint trials (following European Standard ENV 12037) were set up with 11 different softwood and hardwood species. The main aim was to evaluate the suitability of this test standard (developed for testing wood preservative effectiveness) for natural durability testing. The moisture development has been followed during a 36 months period. In this paper, the outcomes of different moisture content...
H Militz, C J Bloom


The risk assessment process. Point of view of a biocide manufacturer [Évaluation du risque. Point de vue d'un fabricant de biocide]
1990 - IRG/WP 3568
Risk assessment is an inherent part of our everyday lives. The risk assessment equation combines Hazards and Exposure. For the Wood Preservation Industry, the hazards may be characterised by the toxicity a the ecotoxicity of chemicals and the exposure by the identification of exposed people, of the exposure routes and exposure frequency. To quantify the exposure, good co-operation is required betw...
D Baur


Bethoguard; A new wood protecting fungicide for use in metal free ground contact wood preservatives
2002 - IRG/WP 02-30301
Research has identified the limitations in both the spectrum of activity and permanence of organic biocides placed in wood in high hazard environments, particularly in the absence of heavy metals such as copper. More specifically, the control of soft rot decay in wood in soil contact has proven to be most problematic. The new organic biocide, Bethoguard; an oxathiazine, has demonstrated excellen...
S C Forster, G R Williams, M Van Der Flaas, M Bacon, J Gors


Aggressiveness of Reticulitermes species in laboratory test
1993 - IRG/WP 93-10026
In European Standards concerned with the preventive action of wood preservatives against termites, i.e. EN 117, EN 118 the obligatory test species is Reticulitermes santonensis. It is argued that this species is more aggressive than the second European Reticulitermtes species, Reticulitermes lucifugus. Since Reticulitermes santonensis is confined to certain smaller areas in France and thus not rea...
H Hertel, S Pantos, D Rudolph


Relating CCA fixation to leaching of CCA components from treated products
1995 - IRG/WP 95-50045
The relationship between chromium fixation in CCA-C treated wood, as determined by CrVI analysis of solution expressed from treated wood and the leaching of Cu, Cr, As and CrVI in a simulated rain test are evaluated for dimension lumber (2"x6") and pole sections. Leachate concentrations after 2 hour exposure to a misting spray (about 300 mm cumulative rainfall) decrease rapidly with increased degr...
P A Cooper, R MacVicar, Y T Ung


Methods of testing anti-stain chemicals for protecting sawn timber during storage and transport
1976 - IRG/WP 273
No international standard method for testing anti-stain chemicals for protecting fresh sawn timber exists. The methods used can be divided into three types: a) Rapid screening tests for finding chemicals effective against blue-stain and mould fungi. The chemicals are tested in agar medium, in pieces of filter paper or on small pieces of wood using pure cultures. b) Laboratory tests for evaluating ...
T Vihavainen


Influence of fungal exposure on the redistribution of copper in treated spruce wood
2002 - IRG/WP 02-10450
The redistribution of copper in treated wood after exposure to basidiomycete decay fungi is described. The micro-distribution of copper in copper(II) sulphate or copper(II) octanoate/ethanolamine treated Norway spruce wood before and after exposure to 3 different wood decay fungi was studied using transmission electron microscopy with X-ray microanalysis. The copper content of the mycelium and the...
M Humar, F Pohleven, R J Murphy, D J Dickinson, I Moris, M Zupancic, P Kalan, M Petric


What is OECD doing to promote harmonization of biocide regulations
1999 - IRG/WP 99-20182
OECD began work on biocides in 1997 to help Member countries co-operate in the assessment and registration of these products. The work is a part of OECD's Pesticide Programme, and is co-ordinated by the Biocides Steering Group. The goal is to harmonize regulatory approaches to allow countries to conduct evaluations of biocides more efficiently. More efficient evaluations can advance the p...
M Paneli, N Grandy


Resistance of board materials against fungal decay: A comparative experiment on Kolle flask tests method and direct test method
1985 - IRG/WP 2243
Two sets of plywood (Aucoumea klaineana Pierre) 7 and 11 ply, treated by two preservatives, and untreated, were tested by two methods: 1. Kolle flask test method on malt-agar substrate according to the French standard NF B 51.295; 2. A direct test method in non sterile conditions according to DocNo: IRG/WP/2214. The exposure time far both methods was 12 weeks. After exposure, the degree of attack ...
G R Y Déon, L N Trong


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 17: Report of fifth inspection (4 years) in Italy
1983 - IRG/WP 4103
The wood samples of Alstonia scholaris, Fagus sylvatica, Pinus sylvestris were submerged in the sea at Follonica, Italy, in April 1977. Follonica, latitude 42°55' North and longitude 10°45' East, is situated on the Tyrrhenian coast. The recorded temperature varies from 13°C to 25°C, salinity 37-38% and pH about 8. The inspections were carried out after 6 months (10/1977), 12 ...
A Gambetta, E Orlandi


The critical timing of inspections for field testing of natural durability
1994 - IRG/WP 94-20018
An overestimation of performance will almost always result if the condition of a specimen is considered to be attained at the precise time that an inspection is carried out. The time at which the condition is actually attained, referred to in this document as the "Condition time", is best considered to be halfway between two successive inspections. The requirement to obtain data that is relevant t...
J D Thornton


Assessment of untreated Papua New Guinean timbers against subterranean termites. Progress Report 1
1990 - IRG/WP 1436
Eight major commercial timber species (Intsia palembanica, Pometia pinnata, Homalium foetidum, Dracontomelon dao, Calophyllum spp., Eucalyptus deglupta, Nothofagus spp., and Alstonia scholaris) were exposed in ground contact against termites. Five replicates of heartwood stakes of 25x25x250 mm³ of each species were randomly embedded in the soil. Results after 24 months exposure showed that Kwila ...
M Rokova, H C Konabe


Leaching from field test stakes. Results from two different methods of analysis
1993 - IRG/WP 93-50013
Field test stakes treated with Boliden K33 containing copper, chromium and arsenic exposed at three different fields in Sweden and rejected due to decay, have in two studies been analysed regarding leaching and remaining preservatives. The stakes have been exposed during 20 to 43 years. The density of the stakes and content of copper, chromium and arsenic have been determined in the top part of th...
F G Evans, M-L Edlund


The influence of UV and IR radiation on leaching of copper and chromium from preservative-treated pine and spruce
1992 - IRG/WP 92-3687
The influence of artifical UV- and IR-radiation on the leaching of copper and chromium components of a CCB-preservative from freshly treated pine and spruce was evaluated. On small pinewood samples it could be shown, that the leaching of copper and chromium can considerabely be reduced by UV-radiation. A Philips HPA lamp type reduced the leaching most effective. IR-radiation lead to higher leachin...
H Militz


Comparative study on the leaching of wood preservatives between natural exposure and accelerating laboratory conditions
1999 - IRG/WP 99-50134
Impregnated specimens with CCA, ACQ, and BAAC were subjected to leaching tests. Specimens of 2x2x1 cm3 in size were used for the laboratory leaching test for 10 days according to JIS K 1571. Specimens of 25x1 x1 cm3 were used for outdoor leaching test for 6 months. Total leaching amounts of boron per cm3 of specimens treated with BAAC were 325 µg in the laboratory test and 206 µg in the outdoor ...
K Yamamoto, S Motegi, A Inai


Evaluation of extractives from African Padauk (Pterocarpus soyauxii Taub.) for protection of non decay resistant species
2002 - IRG/WP 02-10419
The development of a wood preservative made up of natural extracts is a potentially attractive prospect for the wood preservation industry. In this study, organic solvents were used to remove extractives from African padauk wood samples. The solvent was removed by rotoevaporation, and the total content of the viscous extracts determined to be 54.4mg/ml. The toxicity of various extracts concentrat...
P Nzokou, D P Kamdem


A field evaluation of chromated fluoride as a remedial treatment for creosoted wooden distribution poles
1989 - IRG/WP 3556
A commercial chromated fluoride formulation was applied by injection process to previously inoculated creosoted wooden distribution pole sections at a field site in Scotland and appraisal of the efficacy of the formulation against Lentinus lepideus was undertaken at two month and fifteen month intervals. Preliminary results suggest a rapid elimination of organisms from colonised areas. The usage o...
B King, A Bruce