Severe decay damages of bridges made of ekki (Lophira alata) wood known as a durable species
2000 - IRG/WP 00-10383
Bridges made of ekki (azobe, bongossi, Lophira alata Banks et Gaertn.) timbers were severely decayed only 10 years after the construction possibly caused from no maintenance for the periods. The reason of no maintenance is due to the misunderstandings on wood durability against wood-decaying fungi. Some civil-engineers and architectures understand "durable species" means "absolutely decay-durable ...
S Doi, T Sasaki, Y Iijima


NIR spectroscopy for rapid estimation of decay resistance
2004 - IRG/WP 04-20294
In Scandinavia Scots pine (Pinus sylvestris L.) is an important commercial tree species. Its heartwood has traditionally been used in constructions exposed to risk of decay. In a laboratory experiment Scots pine wood specimens sampled from inner heartwood, outer heartwood and sapwood were exposed to the brown rot fungus Poria placenta. In general outer heartwood was more resistant than inner heart...
P O Flæte, E Ystrøm Haartveit


The WOODCARE project: Development of detection methods for Death watch beetle larvae and fungal decay
1999 - IRG/WP 99-20172
Woodcare was a European project coordinated by English Heritage. The aim of the research was to develop more targeted and more environmentally friendly treatment methods for Death watch beetle infections in Oak constructions of historical buildings. TNO has developed two new methods for fast and reliable detection of Death watch beetle larvae and related fungal decay in Oak. The problem with Death...
P Esser, P Van Staalduinen, A C Tas


Durability of surface coating systems. Mycologg - an accelerated mycological test.
2004 - IRG/WP 04-20301
Field testing and natural aging/degradation of test sample, e.g. coated wooden surfaces is a slow process. Accelerated tests focus on mechanical properties, water uptake or sometimes stain fungi. Artificially weathered coated panels are not easily compared with naturally aged panels, and show the importance of involving the biological component among the degrading facors. It is a need for acce...
L Ross Gobakken, J Mattsson, B Jacobsen, F G Evans


Biological resistance of wood treated with waterbased resins and drying oils in a mini-block test
1998 - IRG/WP 98-40107
In recent years it was found that the resistance of wood against fungal degradation could be increased by impregnation with an etherificated melamine formaldehyde resin. Using this resin as a reference, a waterbased fatty acid modificated alkyd-resin and two drying-oils were assessed for their biological performance in a mini-block laboratory test. Although drying-oils, like linseed-oil, are often...
M Sailer, A O Rapp, R-D Peek


Treatment of poplar plywood with solvent and water-borne preservatives
1989 - IRG/WP 3538
Poplar as a light hardwood is appropriate for plywood production. Owing to its low natural durability it is generally recommended to preserve it in all conditions where risks of fungal attack may be present. A research project has been carried out on preservative treatments of plywood commodities. Parameters studied were various treatment cycles, three types of plywood, and a number of solvent and...
J Van Acker, M Stevens


Disodium octaborate tetrahydrate, alone and in conjunction with a selected isolate of Trichoderma viride, reduces decay of fresh felled pine independent of the effect of weathering
1994 - IRG/WP 94-10054
Unpeeled billets of Corsican pine were treated with the following: 5% aqueous disodium octaborate tetrahydrate (DOT) solution; 5% DOT solution with an isolate of Trichoderma viride with a low susceptibility to borate; the Trichoderma viride isolate alone. Half of the billets in each treatment group were also placed in large-diameter plastic pipes to protect the billets from the weather. All three ...
M W Schoeman, D J Dickinson, J F Webber


Comparison of methods for monitoring CCA fixation
1994 - IRG/WP 94-40023
The CCA fixation status in the outer 12.5 mm of pole sections of southern pine (Pinus sp.), red pine (Pinus resinosa) and lodgepole pine (Pinus contorta var. latifolia) were followed during fixation at 21°C under non-drying conditions by the following procedures: - Qualitative CrVI indication by the chromotropic acid spot test. - Quantitative CrVI in the expressate by the diphenylcarbazide method...
P A Cooper, Y T Ung, G Zanjani


Kiln drying of poles as a means of solving the problems of pre-treatment decay in poles
1985 - IRG/WP 1263
The concept that pre-treatment decay can cause wide variation in the treatability of wood and especially wood poles has caused much discussion and debate in wood preservation circles. Yet it seem only logical that if decay has effected the strength characteristics of the wood and caused a differential moisture content in the wood the treatment of the end product will be highly variable and the lon...
J A Taylor


Occurrence of termite species on decaying heartwood specimens exposed 18 to 23 years at an Australian site
1998 - IRG/WP 98-10270
The occurrence of species of subterranean termites on hardwood and softwood specimens (including preservative-treated), exposed in-ground at a semi-arid site at Walpeup (north-western Victoria), 18 to 23 years after installation, is reported. This paper presents maps of the cumulative occurrence on specimens, after six annual inspections, of the following species: Coptotermes acinaciformis, Hetero...
J W Creffield, J-D Thornton, G C Johnson


Above-Ground Durability Estimation in Australia. Results after 16 years exposure
2005 - IRG/WP 05-20314
A program of research was established in 1987 to examine the above-ground durability of a selection of timbers that are commercially significant in Australia. Test samples were assembled in an L-Joint design and placed on exposure racks in a format to replicate joinery that is exposed to the weather above ground. Both painted and unpainted material has been exposed. Test samples have been evaluat...
L P Francis, J Norton


Decay resistance of Platanus acerifolia wood against White Rot Fungi (Coriolus versicolor)
2002 - IRG/WP 02-10431
Degradation of the lignocellulose complex in wood varies on the microorganism causing decay and chemical composition of wood. The weight loss of Platanus acerifolia wood after decay by white rot fungus (Coriolus versicolor) for period 16 weeks were evaluated according to European standard EN 113 and beech wood as a control. The samples were collected in October 2000 from Nantes, France. The aim of...
M Irmouli, O Duchelier, N Ayadi, B Charrier


On the laboratory use of X-rays in timber decay evaluations
1981 - IRG/WP 2144
The paper reports the results of laboratory experiments on the X-raying of some Pinus radiata sapwood blocks infected with Serpula lacrymans to determine the effect of density and moisture content on the absorption of X-rays by wood. It is concluded that with increasing moisture content there is a very marked increase in time required to pass a constant quantity of X-rays through a test block and ...
J D Thornton, J W Creffield, O Collett


The wood-attacking insects in wooden houses of an old open air museum in southern Finland
1989 - IRG/WP 1409
Harmful insects of wood in a open-air museum were investigated in 1985-1988 by order of the National Board of Antiquities and Historical Monuments of Finland in nine old log houses. Many thousands of insects and altogether 1073 anobiids (Coleoptera, Anobidae) were obtained by window and light traps. The most common Anobiidae-species were Hadrobregmus confusus (Kraatz) 60.3%, Hadrobregmus pertinax ...
H Viitanen, M Pulkkinen


The long road to understanding brown-rot decay. A view from the ditch
1995 - IRG/WP 95-10101
Interest in understanding how brown-rot fungi decay wood has received increasing interest in recent years because of a need to identify novel targets that can be inhibited for the next generation of antifungal wood preservatives. Brown-rot fungi are unique in that they can degrade holocellulose (cellulose and hemicellulose) in wood without first removing the lignin. Furthermore, they degrade holoc...
F Green III, T L Highley


Assessment of the Inhibition of wood decay fungi by volatile organic compounds identified from Trichoderma spp.
1999 - IRG/WP 99-10302
Previous research identified five volatile organic compounds produced by Trichoderma spp. that may be inhibitory to wood decay fungi. The effects of four of these volatile organic compounds, 2-propanone, 2-methyl-1-butanol, heptanal and octanal were tested over a range of concentrations against four selected wood decay fungi. The fungi were incubated in malt extract broth under appropriate conditi...
S N Humphris, R E Wheatley, A Bruce, C Payne


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 18. Report of seventh inspection (72 months) in Australia
1984 - IRG/WP 4108
This report includes the results for the 72 month inspection of the IRG/COIPM International Marine Test installed in Sydney Harbour. Although, overall, attack by teredinid and limnorid borers have been most commonly encountered in test specimens at this site, slight attack, mainly by sphaeromatids, has recently been initiated on some hitherto unattacked treated Alstonia scholaris and Pinus sylvest...
L J Cookson, J E Barnacle


Is laboratory testing of decay resistance questionable as a single criterion for natural durability?
1996 - IRG/WP 96-20096
In a laboratory test set up over 20 hardwood species were evaluated according to the European Standard EN 350-1 including Basidiomycete and soft rot testing. Half of the species used were of a known natural durability. The Basidiomycete testing was carried out using Coriolus versicolor, Gloeophyllum trabeum and Coniophora puteana in a malt agar test similar to EN 113. From this test it was not pos...
J Van Acker, M Stevens, T Van Cauwenberghe, T Seynaeve


A shower test protocol for measuring antisapstain wash-off from small individual log billets
1996 - IRG/WP 96-50069
According to New Zealand Timber Industry Federation statistics New Zealand exported 4,835,000 m³ of logs in 1994 and it is estimated that c. 20% were anti-sapstain treated. Loss of preservative from logs as a result of rain impact after application is of considerable concern both with respect to potential loss of efficacy and environmental contamination. Whilst Environment Canada have a proposed ...
A J Pendlebury, H Pearson


Bestimmung der pilzwidrigen Wirksamkeit von Holzschutzmitteln gegen Moderfäule-Erreger
1977 - IRG/WP 2125
Ziel der vorliegenden Arbeit war der Vergleich der in verschiedenen Ländern zur Bestimmung der pilzwidrigen Wirksamkeit von Holzschutzmitteln gegen Moderfäule-Erreger angewandten Methoden. Als Vergleichsmaterial dienten drei normierte Methoden: die britische (42), skandinavische (45) und die in der DDR angewendete (47) sowie wichtige, von verschiedenen Fachleuten ausgeführte Arbeiten experiment...
J Wazny


Evaluation of a utility pole inspection procedure
1996 - IRG/WP 96-20084
Methods were developed and are currently being utilized to appraise residual strength of utility poles based on visual assessment of increment cores. Strength tests, mycological descriptions and anatomical analyses were performed on eight utility poles taken out of service and one new (never in service) pole. Samples were obtained from increment cores removed from 6 levels in the pole: 2 feet, gro...
S E Anagnost, C J K Wang


Assessment of residual retentions in creosote treated Scots pine (Pinus sylvestris) poles after 45 years ground contact service in the Lemstervaart in the Dutch polder
1994 - IRG/WP 94-50022
In a project funded by the Water State Authorities (RWS) and the Noordoostpolder Water Board, the residual retentions in ten creosote treated Scots pine (Pinus sylvestris) poles were examined after 45 years ground contact service along a canal (Lemstervaart) in the Dutch Noordoostpolder. The Lemstervaart location was selected due to the fact that the poles involved had been originally treated and ...
P Esser, W L D Suitela, A J Pendlebury, H Visscher


The performance of metal-chromium-arsenic formulations after 32 to 38 years' in-ground exposure in Australia
2000 - IRG/WP 00-30240
Two trials of metal-chromium-arsenic preservatives were exposed in-ground in Australia. In Trial 1, Pinus radiata stakes treated with Boliden K.33, Boliden S.25, Celcure A, Tanalith C and Tanalith CA were installed at Sydney and Narrandera in 1961/1962. In Trial 2, P. radiata and Eucalyptus regnans sapwood were treated with Celcure A, Celcure A21-N, Celcure A 21-O and Tanalith CA (new) and install...
G C Johnson, J D Thornton, J Beesley


Field and greenhouse testing of window joinery of pine and spruce treated with LOSP
1991 - IRG/WP 3658
Norwegian window frame components of full size were double vacuum-treated with TBTN and TBTO, and connected as 'L-joints' and subsequently coated with stains. The corner sections were exposed (out of ground contact) both in field (temperated coastal climate, Taastrup, Denmark) and in a greenhouse (Uppsala, Sweden). The window frame L-joints of spruce (Picea abies Karst.) - treate...
F G Evans, B Henningsson, E Borsholt


Micromorphology of Schizophyllum commune attack in pine (Pinus sylvestris) wood
1983 - IRG/WP 1184
The decay pattern caused by Schizophyllum commune in pine latewood tracheids was studied using both light and transmission electron microscopy. The attack began as isolated concentric slits within the S2 layer with extensive lamellation and separation of individual wall layers observed in subsequent stages of decay. The slits resulting from attack appeared to be formed in thin, regular concentric ...
T Nilsson, G F Daniel