IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1687 documents. Displaying 25 entries per page.


Decay potential of various New Zealand Phlebiopsis gigantea strains using a soil block method
1999 - IRG/WP 99-10309
The objective of the current study was to determine the decay potential of different strains of Phlebiopsis gigantea using Pinus radiata and European Fagus sylvatica, respectively. A soil block method was used to determine mass weight loss of P. radiata and F. sylvatica following 10 weeks incubation with different strains of P. gigantea. For comparison, Trametes versicolor, Postia placenta, Gloeop...
B Kreber, J G Van der Waals


Limitations of the Pilodyn when assessing decay in graveyard test stakes
1982 - IRG/WP 2168
The following examination was designed to evaluate more precisely the usefulness of the Pilodyn for routine, objective assessments of the condition of field test stakes and to examine its limitations, particularly in respect to: 1.) The importance of variables other than extent of decay which may affect Pilodyn readings; 2.) Practicality of obtaining multiple readings in decayed and non-decayed re...
M E Hedley


Benzalkonium chloride (an AAC preservative): Criteria for approval, performance in service, and implications for the future
1985 - IRG/WP 3328
The data base generated for benzalkonium chloride was considered adequate for commercial approvals, particularly after revision in late 1982. Field trials, although not part of the approval criteria, generally supported commercial use; decay observed in one test (post and rails) after 6 years' exposure would have resulted in some caution in setting retentions. No laboratory trial, nor fie...
J A Butcher


Dominant genera of fungi isolated from the surfaces of Sugi (Cryptomeria japonica D. Don) heartwood lumbers exposed at six test sites from northern to southern regions of Japanese islands
1999 - IRG/WP 99-10304
The surfaces of wood materials are disintegrated not only by sunlight and rainwater but also by microbes when exposed above ground condition. This paper deals with the investigation of fungi isolated from the surfaces of Sugi heartwood lumbers (W100 by T10 by L300 mm) exposed at an angle of 45° without ground contact for 16 months at the six test sites from northern to southern regions of Japan. ...
S Doi, M Mori, M Kiguchi, Y Imamura, M Hasegawa, S Morita, S Nakamra, Y Kadegaru


The movement of iron into field test stakes
1987 - IRG/WP 2284
Failed and sacrificial stakes recovered from the Westham Island field test site were examined for their iron content. Varying amounts were recorded, which were greatest in the failed stakes. The possible role of the iron taken up by the below ground portion of the stakes, in accelerating the decay process and/or the preservative leaching is under investigation. The reaction of the iron with the ch...
J N R Ruddick, P I Morris


Termite resistance of treated wood in an above-ground field test
1985 - IRG/WP 2241
A field test method has been developed for evaluating the susceptibility of wood products to termites in protected situations above ground. In this method fungal attack on the wood products is minimal, though decay has been observed in conjunction with termite attack in some specimens. Preliminary results from exposure of replicate wood samples treated with preservatives in Florida to Reticuliterm...
A F Preston, P A McKaig, P J Walcheski


Termite resistance of treated wood in an above-ground field test
1986 - IRG/WP 1300
This paper provides an update on the results from an above ground field test evaluating the effectiveness of wood preservatives against subterranean termites. Results for the one and two year inspections of treated southern pine sapwood exposed in Hawaii to Coptotermes formosanus are presented. Chromated copper arsenate is providing excellent protection as is the pyrethroid deltamethrin. Borate an...
A F Preston, P A McKaig, P J Walcheski


A field study on the suitability of the European lap-joint test
2001 - IRG/WP 01-20239
Within the framework of the European SM&T Research Project "Co-normative research on field tests for wood preservatives out of ground contact in conjunction with methods for preconditioning test specimens prior to test" (FACT) one aim was to establish the suitability of the European lap-joint test (as it is described in ENV 12037:1996) to assess wood preservatives in the field in EHC 3. Scots ...
M Grinda, Ö Bergman, H-V Borck, D Dickinson, P Esser, R Gründlinger, H Leithoff, S Molnar, L Paajanen, N Pfabigan, E D Suttie, F Thomassin, T Nilsson, J Van Acker, M Van Der Zee, A Voss


Performance of borate-treated lumber in a protected, above-ground field test in Japan
2004 - IRG/WP 04-30344
This document is supplemental to the previous IRG document (Tsunoda et al., 2002). An experiment to simulate the sill plate (dodai) of the Japanese houses was conducted at the termite field test site of the Wood Research Institute in Kagoshima, Japan where two economically important subterranean termite species [Coptotermes formosanus Shiraki and Reticulitermes speratus (Kolbe)] are established. ...
K Tsunoda, A Byrne, P I Morris, J K Grace


The use of organic wood preservatives in ground contact and the suitability of laboratory test procedures to determine their efficacy
1999 - IRG/WP 99-20175
Organic fungicides, such as propiconazole, have proven to be highly effective when used as a co-biocide in recently developed wood preservative formulations. They have however been ineffective when used as a stand alone preservative, particularly when used in ground contact (European Hazard class 4). Previous research, using the test methods of ENV 807 (1993), provided conflicting evidence regardi...
I J Herring, D J Dickinson


Leaching of components from CCF treated timber in ground contact
1998 - IRG/WP 98-50108
In order to investigate the depletion of different CCF-salts during service small stakes (10*10*450mm³) were treated with five water-borne wood preservatives and after fixation brought into ground contact for several years. After failing some of the broken down stakes were used to determine the remaining concentration of relevant ions and their distribution in different segments of the stakes. A...
E Melcher


Bethoguard; A new wood protecting fungicide for use in metal free ground contact wood preservatives
2002 - IRG/WP 02-30301
Research has identified the limitations in both the spectrum of activity and permanence of organic biocides placed in wood in high hazard environments, particularly in the absence of heavy metals such as copper. More specifically, the control of soft rot decay in wood in soil contact has proven to be most problematic. The new organic biocide, Bethoguard; an oxathiazine, has demonstrated excellen...
S C Forster, G R Williams, M Van Der Flaas, M Bacon, J Gors


Resistance of board materials against fungal decay: A comparative experiment on Kolle flask tests method and direct test method
1985 - IRG/WP 2243
Two sets of plywood (Aucoumea klaineana Pierre) 7 and 11 ply, treated by two preservatives, and untreated, were tested by two methods: 1. Kolle flask test method on malt-agar substrate according to the French standard NF B 51.295; 2. A direct test method in non sterile conditions according to DocNo: IRG/WP/2214. The exposure time far both methods was 12 weeks. After exposure, the degree of attack ...
G R Y Déon, L N Trong


Evaluation of extractives from African Padauk (Pterocarpus soyauxii Taub.) for protection of non decay resistant species
2002 - IRG/WP 02-10419
The development of a wood preservative made up of natural extracts is a potentially attractive prospect for the wood preservation industry. In this study, organic solvents were used to remove extractives from African padauk wood samples. The solvent was removed by rotoevaporation, and the total content of the viscous extracts determined to be 54.4mg/ml. The toxicity of various extracts concentrat...
P Nzokou, D P Kamdem


Some Experiences with Stake Tests at BAM Test Fields and in the BAM Fungus Cellar Part 1: Comparison of Results of Visual Assessments and Determinations of Static Moduli of Elasticity (MOE)
2005 - IRG/WP 05-20319
With examples of routine in-ground stake tests differences are shown in the performance of wood preservatives at the BAM test fields Lehre and Horstwalde and in the BAM fungus cellar. Signs of attack of micro-organisms were assessed visually according to EN 252. Periodical determinations of static moduli of elasticity (MOE) revealed the influence of the attack on the elastic properties of the wood...
M Grinda, S Göller


Termite resistance of borate-treated lumber in a three-year above-ground field test in Hawaii
2000 - IRG/WP 00-30236
A protected above-ground field test simulating the sill plate (dodai) used in conventional Japanese housing construction was established in both Hawaii and Japan to examine the efficacy of disodium octaborate tetrahydrate (DOT, 2% and 3% shell and through) wood treatments. In Hawaii, chromated copper arsenate (CCA, 4 kg/m3) and ammoniacal copper zinc arsenate (ACZA, 4 kg/m3) were included in the t...
J K Grace, R J Oshiro, A Byrne, P I Morris, K Tsunoda


Laboratory Evaluation of Soft Rot Resistance of Non-Durable Lesser-Known Malaysian Hardwoods
2006 - IRG/WP 06-10582
Resistance of six non-durable lesser-known Malaysian hardwoods, Pulai (Alstonia spp.), Rubberwood (Hevea brasiliensis), Ludai (Sapium spp.), Jelutong (Dyera costulata), Gaham Badak (Blumeodendron tokbrai) and Kayu arang (Diospyros spp.) compared with temperate Scots pine sapwood (Pinus sylvestris), were evaluated using the unsterile soil burial (mixed with Chaetomium globosum) versus vermiculite-b...
A H H Wong


The natural durability of wood in different use classes - PART II
2006 - IRG/WP 06-10598
The natural durability of important European wood species has been tested on 3970 speci¬mens in field trials. The wood was exposed at five test sites in Germany with different climates, at each site in European use class 4 and 3 (with and without soil contact). Within European use class 3 three different expositions were tested: vertical with sheltered end grain, vertical unsheltered and horizont...
A O Rapp, U Augusta, K Brandt


Is Field Test Data from 20 x 20mm Stakes Reliable? Effects of Decay Hazard, Decay Type and Preservative Depletion Hazard
2006 - IRG/WP 06-20327
Effects of decay hazard, decay type and preservative depletion hazard on the performance of variously preservative treated 20 x 20 x 500 mm Radiata pine and Fagus sylvatica test stakes across 13 field test sites in New Zealand and Queensland Australia were determined. Radiata pine treated with an ammoniacal copper quaternary preservative (ACQ) (1.56% m/m a.i.) and copper chrome arsenate (CCA) (...
R Wakeling


Predicting the decay resistance of timber above-ground: 1. Climate effects
2006 - IRG/WP 06-20330
Despite the benefits of using timber as a building product, it is disadvantaged by current Australian Standard durability classifications which lack the sensitivity desired by engineers and architects. To address the need for more sensitive timber service-life information in Australia, an above-ground durability research program was established in 1987. One focus of research is the relationship be...
L P Francis, J Norton


Effect of wood decay on the proportional limit of thin wood samples stressed in the bending mode
2006 - IRG/WP 06-20334
When using bending stiffness as a measure of wood decay it is advantageous to repeatedly test individual samples after they are exposed to decay fungi for varying periods of time. In order to obtain reliable results, variation in modulus of elasticity (MOE) values of the test samples that are repeatable bent to a given deflection must be considered. In this study it was shown that sound 3mm thick ...
G Li, D Nicholas, T Schultz


The Use of Modulus of Elasticity and Modulus of Rupture to Assess Wood Decay in Laboratory Soil-Bed Test
2006 - IRG/WP 06-20338
The efficacy of wood preservatives were determined in a soil-bed test. Samples of alder wood sapwood (Alnus glutinosa subsp. barbata) (5x10x100 mm) were treated with Solutions of CCA (1 % and 2 %), ACQ-1900 (2 % and 3 %), ACQ-2200 (1 % and 2 %), Tanalith E 3491 (2 % and 2.8 %), Wolmanit CX-8 (% 1 and 2 %). Modulus of Elasticity, modulus of rupture, mass loss and decay rate according to AWPA E7 wer...
A Temiz, Ü C Yildiz


High-energy multiple impact (HEMI)-test – Part 2: A mechanical test for the detection of fungal decay
2006 - IRG/WP 06-20339
The suitability of the high-energy multiple impact (HEMI)-test for detection of early fungal decay was examined. The HEMI – test characterizes the treatment quality of thermally modified wood by stressing the treated material by thousands of impacts of pounding steel balls. This method differentiates between heat treatment intensities, which are expressed by structural changes of the wood. Simil...
C R Welzbacher, C Brischke, A O Rapp


Performance of borate-treated lumber after 8 years in an above-ground termite field test in Hawaii
2006 - IRG/WP 06-30390
We report eight years of field study results from a protected above-ground field test in Hawaii simulating the sill plate (dodai) used in conventional Japanese housing construction. Field tests were established in both Hawaii and Japan to examine the efficacy of disodium octaborate tetrahydrate (DOT, 2% and 3% BAE shell and through) wood treatments. In Hawaii, chromated copper arsenate (CCA, 4 kg...
J K Grace, A Byrne, P I Morris, K Tsunoda


Performance of borate-treated lumber in a protected, above-ground field test in Japan
2006 - IRG/WP 06-30395
This document is supplemental to the previous IRG document (Tsunoda et al. 2004). An experiment to simulate the sill plate (dodai) of the Japanese houses was conducted at the termite field test site of the Research Institute for Sustainable Humanosphere of Kyoto University in Kagoshima Pref., Japan where two economically important subterranean termite species [Coptotermes formosanus Shiraki and R...
K Tsunoda, A Byrne, P I Morris, J K Grace


Previous Page | Next Page