Soluble nutrient content in wood and its susceptibility to fungal discoloration and decay in above ground and ground tests
2000 - IRG/WP 00-10336
The objective of this comprehensive study was to reveal the impact of soluble nutrients in wood on its susceptibility to fungal discoloration and decay in various tests, which is important for the test methodology and standardisation. Seven tests were carried out including pure culture above and ground contact tests, above ground field test and laboratory ground contact tests. The samples containi...
O M Caballero, N Terziev


MDF manufactured from blends of cypress pine and radiata pine shows enhanced resistance to subterranean termite attack
2001 - IRG/WP 01-40214
Medium density fibreboards consisting of blends of the naturally durable wood species white cypress pine (Callitris glaucophylla) and non-durable wood species were manufactured in a commercial plant and subjected to a bioassay using the subterranean termite species, Coptotermes lacteus. A board composed of 30% cypress pine, 30% slash pine (Pinus elliottii) and 40% of the naturally durable hardwood...
P D Evans, S Dimitriades, C Donnelly, R B Cunningham


A below-ground exposure method for determining the resistance of woody and non-woody materials to attack by subterranean termites
1993 - IRG/WP 93-10012
With existing field test procedures, in which specimens are installed vertically to some of their length into the ground and spaced out from each other ("grave-yard" tests), variations in the rate of contact by termites between replicates can be common. Mechanical damage to specimens during inspection and re-installation may also be difficult to avoid. A new field test method, evaluated in Austral...
M Lenz, J W Creffield


Relative performance of copper/chrome/boron (CCB) and copper/chrome/arsenate (CCA) in ground contact
1992 - IRG/WP 92-3694
The performance of four retentions each of an oxide CCA formulation and a salt formulation of CCB in radiata pine and European beech was compared after 18 years' field exposure. In radiata pine CCA oxide was more effective (4 failures out of 40) than CCB (9 failures out of 40). However, in European beech CCB was substantially more effective (22 failures) than CCA oxide (all failed). Analy...
M E Hedley


L-joint trials: Part 2: The relationship between colonisation by decay fungi and long-term performance
2002 - IRG/WP 02-20251
Many of the L-joint trials conducted at BRE were assessed during the early stages to establish the rate of colonisation by fungi, principally basidiomycetes. At that time, a system of assessment incorporating colonisation studies was proposed for inclusion within the European Standard EN 330 but was rejected for the final version of the standard. The long-term trials associated with the colonisa...
J K Carey


Comparison of three methods for assessing the in-ground termite resistance of treated timber, durable timber and plastics at sites in Australia, USA and Thailand - First results
1998 - IRG/WP 98-20132
The in-ground resistance of materials to attack by subterranean termites is most commonly assessed with one form or another of the conventional graveyard method, despite the significant shortcomings of this method. In Australia, an alternative method, in which all samples of test materials are placed below-ground, has been in use for more than 10 years. The method provides reliable exposure of sam...
M Lenz, A F Preston, J W Creffield, K J Archer, B M Kard, C Vongkaluang, Y Sornnuwat


Determination of the water sorption properties and preliminary results from field tests above ground of thermally modified material from industrial scale processes
2004 - IRG/WP 04-40279
In this study the differences in moisture behavior and durability above ground of heat treated wood originating from different European industrial heat treatment plants by means of the water sorption properties as well as field tests were examined. The manufacturers of heat treated material were: PLATO Hout B.V./Netherlands, Thermo Wood (Premium wood)/ Finland and Menz Holz/ Germany, where Oil-...
C R Welzbacher; A O Rapp


Durability of Bamboos in India against termites and fungi and chemical treatments for its enhancement
2005 - IRG/WP 05-10553
Bamboo is a very important forest resource that benefits the life of people in a myriad ways including meeting the need for structural uses like posts, pole fencing, scaffoldings, house building, etc. Although it is one of the strongest structural material available, often succumbs to fungal decay and biodeterioration by insects (termites and powder post beetles) during storage and usage. Studies...
O K Remadevi, R Muthukrishnan, H C Nagaveni, R Sundararaj, G Vijayalakshmi


Resistance of painted wood to mould fungi. Part 3. The effect of weathering, wood substrate and fungicides on mould growth
1998 - IRG/WP 98-10284
The effect of 6 month outdoor weathering on the resistance of acrylate paint systems on different types of pine and spruce sapwood to mould fungi was studied. Dipping into the preservative prior to painting, a primer with and without a fungicide (propiconazole + IPBC 0.50 + 0.2%) and a topcoat with and without a fungicide (propiconazole + IPBC 0.25 + 0.12%) were combinations of the treatments stud...
H Viitanen, P Ahola


Biocidal screening method of wood extractives by a direct use of cellulose TLC plate
2001 - IRG/WP 01-20226
Most of the methods to evaluate the biological durability of woods have focused on decay fungi and termite as deteriorating organisms and it is well known that one of the most important factors affecting the biological characteristics of wood is extractives. Bioassays for evaluating the biological activities of wood extractives have been mainly conducted with treated filter papers for termites or ...
R Yusiasih, T Yoshimura, T Umezawa, Y Imamura


Decay and termite durabilities of heat-treated wood
2004 - IRG/WP 04-40272
Decay and termite resistances of Plato-treated timbers were evaluated using a modified JIS decay test method, feeding test in a laboratory scale and a field exposure against Reticulitermes speratus (Kolbe) or Coptotermes formosanus Shiraki. The results showed that no significant decay durability of the treated timbers although mass loss from decay slightly decreased in case of treated timbers. ...
S Doi, K Hanataa, E Kamonji, Yuuji Miyazaki


L-joint trials: Part 3: Relative performance of a range of preservative products
2002 - IRG/WP 02-30292
Long-term trials using the L-joints described in BS EN 330 and AWPA Standard E9-97 have been in progress at BRE since 1982. This paper records the current assessments of decay of L-joints in trials started between 1982 and 1994 with treatments applied to both Scots pine sapwood (Pinus sylvestris) and spruce (Picea sp.). Data are provided on a range of active ingredients including TnBTO, PCP, a...
J K Carey


Assessment of wood decay in small-scale unsterile soil-bed tests
1997 - IRG/WP 97-20111
This study is concerned with the investigation of wood decay in small-scale unsterile soil-bed tests. Tests were performed with untreated heartwood samples from five hardwood species of different natural durability classes ranging from highly perishable to very resistant. Our results confirmed the critical role of soil moisture content on wood decay. The highest decay rates were observed at moistu...
L Machek, A M Derksen, R Sierra-Alvarez


The natural durability story
1997 - IRG/WP 97-20119
Wood species with superior natural durability were in use since the beginning of timber utilisation. Their importance decreased with increasing industrial timber impregnation. In recent time, however, they gained worldwide new interest due to environmental problems involved with treated timber. In Europe a special Standard (EN 350) has been published and a multinational research project on testing...
H Willeitner, R-D Peek


Remedial ground-line treatment of CCA poles in service. Results of chemical and microbiological analyses 6 months after treatment
1986 - IRG/WP 3388
CCA-treated poles in service with incipient internal soft rot were remedially treated by inserting borate rods, brushing with a boron/glycol solution and injecting boric acid paste, copper/creosote paste or a commercial product (DFCK paste). The spread of active chemicals in the treated zone as well as the change in microflora have been studied with time. After six months chemicals had spread to m...
B Henningsson, H Friis-Hansen, A Käärik, M-L Edlund


Quality of timber impregnated with preservatives of class AB after three years in service
2002 - IRG/WP 02-20241
Quality of impregnated timber is most often expressed by penetration and retention of the preservative used. Relatively less information is available about the performance of the final product, e.g. decks, panels etc. regarding product’s surface checks, deformations and overall appearance. Together with the timber durability, the above mention features are of esthetical importance in the above g...
N Terziev


Durability of five wood species against Coriolus versicolor
1992 - IRG/WP 92-1578
The durability of following five wood species Zelkova carpinifolia, Ulmus glabra, Carpinus betulus, Acer trauvetteri and Pterocarya fraxinifolia were studied against Coriolus versicolor under laboratory conditions according to DIN 52176 standards. Zelkova caprinifolia shows a reduction in weight of 2.19%, Ulmus glabra 41.69%, Carpinus betulus 45.64%, Acer trauvetteri 53.05%, and Pterocarya fraxini...
S M Kazemi


Alternatives to CCA for ground contact protection of timber: a perspective from UK on performance and service life expectations
2002 - IRG/WP 02-30289
The proposed amendment to the European Union's Marketing and Use Directive (1976/769/EEC) in respect of arsenic in CCA wood preservatives seeks to restrict the use of CCA across the European Union. CCA is an extremely important wood preservative in the UK from the manufacturing of the product to the extent of use of CCA-treated timber. Based on our experience and judgement on the use of ...
E D Suttie, A F Bravery, T B Dearling


Work programme of CEN/TC 38 (May 1995) - Durability of wood and derived materials
1995 - IRG/WP 95-20069
Standardization of the characteristics of natural or conferred durability of wood and its derived materials against biological agents, including the characteristics of protection products and associated processes to obtain this durability. This applies in particular to: - the identification of hazard classes; - the test methods (wood preservatives as treated wood and wood based materials) and inte...
R Hüe


Chlorothalonil: A new ground contact wood preservative
1992 - IRG/WP 92-3712
Extensive investigations have been conducted in recent years on the performance of chlorothalonil (tetrachloroisophthalonitrile) as a ground contact wood preservative. Efficacy information is presented on a soil block test with 11 Basidiomycetes, a fungus cellar evaluation, above-ground field testing against termites in Australia and Hawaii, and ground-contact field stakes installed in Florida (9 ...
P E Laks, T L Woods


Some Experiences with Stake Tests at BAM Test Fields and in the BAM Fungus Cellar Part 2: Comparison of Static and Dynamic Moduli of Elasticity (MOE)
2005 - IRG/WP 05-20320
In routine in-ground stake tests of wood preservatives at the BAM test field Horstwalde and in the BAM fungus cellar periodical determinations of both static moduli of elasticity (MOE) on the basis of bending tests and dynamic MOE on the basis of the vibration method were performed as a possible method for the assessment of fungal attack. As expected from other publications, the absolute values of...
M Grinda, S Göller


Natural resistance of Bamboo (Bambusa sp.) to marine wood-borers in Goa waters (India)
1993 - IRG/WP 93-10032
The paper deals with the natural durability of Bambusa sp. against the attack of marine wood-borers in Goa waters. Test specimens of this species were completely destroyed within a short period of nine months due to severe attack of borers indicating its very low natural resistance. Wood-borers involved were Martesia striata (Linnaeus), Nausitora hedleyi Schepman and Lyrodus pedicellatus (Quatrefa...
L N Santhakumaran, S G Sawant


Comparing the resistance of a number of lesser known species of tropical hardwoods to the marine borer Limnoria using a short term laboratory assay
2003 - IRG/WP 03-10500
Naturally durable species of timber are used as an alternative to preservative treated timber for marine structures, but many species have not been evaluated for their potential for use in this environment. EN 275 specifies a 5-year test period - too long a period for screening tests to be economically viable. In this study, durability was assessed by measuring the production of faecal pellets by ...
L M S Borges, S M Cragg, J R Williams


Relationship of wood durability and extractives
2003 - IRG/WP 03-10493
The durability of the following five wood species, Zelkova carpinifolia, Ulmus glabra, Pterocarya fraxinifolia, Carpinius betulus and Acer laetum, were studied. Wood blocks were exposed to Coriolus versicolor under laboratory conditions according to DIN 52176 standard. After 16 weeks incubation the heart wood of Z carpinifolia showed 2,19 % weight loss, U glabra 41,69 %, C betulus 45,64 %, A laetu...
S M Kazemi


Natural durability of 4 different Larix species tested in soil contact
2002 - IRG/WP 02-10434
Importers of Siberian Larch claimed to have a material which can replace pressure treated wood in soil contact. This gave reason to investigate the durability of 4 different Larix species (L. decidua, L. sibirica, L. decidua x sibirica, L. gmelini var ologenis) coming from 7 different origins in comparison with sapwood of Pinus sylvestris untreated as well as pressure impregnated with retentions o...
A O Rapp, H Viitanen, T Nilsson