Serviceability of copper naphthenate-treated poles
2000 - IRG/WP 00-30214
Copper naphthenate-treated poles in service were inspected for deterioration, penetration, retention, and serviceability. The study to date has included poles in all hazard zones in the United States. Poles installed by 12 different utilities and eight different treating companies are included in the survey. Both southern pine and Douglas-fir poles and distribution and transmission poles are inclu...
H M Barnes, M H Freeman, J A Brient, C N Kerr Jr


Fungal Stain Development in Canadian Hardwood Logs
2004 - IRG/WP 04-10505
In most sawmills around the world, trees are harvested into logs and stored in the forest or in a log yard for a period of time before being sawn into lumber. These logs may be attacked by various pigmented fungi, which results in staining of the wood. Since hardwood species are used to a great extent in furniture manufacturing and in the making of other valuable wood products, the reduction of wo...
Dian-Qing Yang, M-C Bisson


Termite and decay resistance of particleboard composed of white cypress pine and radiata pine
1997 - IRG/WP 97-10200
Phenol-formaldehyde bonded particleboard was manufactured from blends of non-durable radiate pine (P. radiate) and heartwood of the naturally durable species, white cypress pine (C. glaucophylla). Board specimens were subjected to bioassays using two termite species, M. darwiniensis and C. acinaciformis, and the basidiomycete fungi, C. puteana and P. ostreatus, and the durability of specimens was ...
P D Evans, J W Creffield, J S G Conroy, S C Barry


Attempt for developing a new method for above ground field testing of wood durability
2000 - IRG/WP 00-20199
Field testing remains the most appropriate way for evaluation of wood preservatives or natural durability of wood species. Above ground tests are designed to answer specific questions concerning the outdoor utilisation of wood. Such methods supply additional information and confirm or reject preliminary laboratory results. The European standard (ENV 12037, "lap-joint") for assessment of the durabi...
N Terziev, M-L Edlund


Presteaming radiata pine heartwood to improve treatability
1983 - IRG/WP 3239
Steaming and holding before preservative treatment by the Bethell process greatly improved the treatment of radiata pine heartwood. Maximum penetration of preservative for the shortest holding period was obtained by the use of steam vacuum but the difference between this and steam venting was small when compared with the standard of treatment of air dried samples. A holding period of one day was s...
A J Bergervoet


The efficacy of Sentry® as a treatment for the control of sapstain in pre-infected radiata pine
2001 - IRG/WP 01-30260
Experiments were conducted to determine the efficacy of Sentry® when used to control sapstain fungi on radiata pine branch billets stored under high fungal hazard conditions. Prior to antisapstain treatment, the billets were pre-infected with a mixed inoculum of staining fungi and held from zero to 10 days at 25°C and 75% relative humidity. This was done to produce billets with different degrees...
C Chittenden, J G van der Waals, B Kreber, R N Wakeling


An evaluation of chemical treatments for the protection of radiata pine logs from fungal degrade
1986 - IRG/WP 3377
Busan 30, Busan 1009, Mitrol PQ375. and sodium pentachlorophenoxide (NaPCP) plus have been evaluated as antisapstain treatments for the long-term protection of debarked radiata pine logs. After 3 months' winter-spring storage, treated debarked logs had less surface and internal sapstain than 'control' logs. After 6 months' storage all logs had internal sapstain ...
J A Drysdale, M E Hedley, J A Butcher


Field tests of preservative-treated radiata pine in Japan
1995 - IRG/WP 95-30083
Test stakes of radiata pine treated with various alkyl ammonium compound (AAC) formulations and with copper-chrome-arsenate (CCA) as reference preservative were installed in 3 test sites in Japan in 1981-82. When inspected in 1995, CCA-treated stakes showed less decay at all three sites than stakes treated with other formulations. Ammoniacal copper quaternary (ACQ)- treatment was only slightly les...
M E Hedley, K Tsunoda, K Suzuki


Wood extractives as carbon sources for staining fungi in the sapwood of lodgepole pine and trembling aspen
1995 - IRG/WP 95-10098
Wood discoloration by sapstaining fungi reduces lumber value. In Canada, the most commonly recorded sapstaining fungi belong to the genera Ophiostoma. This work evaluated the effect that Ophiostoma piceae, Ophiostoma ainoae, and Ophiostoma piliferum used the lipids present in the sapwood of lodgepole pine (Pinus contorta Dougl.) and trembling aspen (Populus tremuloides Michx.). Wood lipids, common...
Yong Gao, C Breuil


Effect of mobile fungicides on fungal pre-infection in radiata pine billets.
1999 - IRG/WP 99-30191
In New Zealand, fungal infection of logs begins directly after felling and whilst severe degrade can be prevented if antisapstain-treated within 24 hours, such short turn-around times of logs are not always practicable. However, conventional antisapstain formulations in use only provide an envelope of protection on the log surface but are unable to control pre-infections below the surface. The obj...
D R Eden, T Singh, B Kreber


Moisture requirements and wood degradation of pine and spruce wood by some Basidiomycetes-fungi
1989 - IRG/WP 1406
The minimum moisture requirements for the growth of the brown rot fungi, Coniophora puteana, Gloeophyllum trabeum and Serpula lacrymans were near or above the fibre saturation point of pine and spruce, sap and heartwood, during 160 days incubation according to the standard method EN 113. The moisture of wood for the optimum growth of Coniophora puteana and Serpula lacrymans was about 35-80% and fo...
H Viitanen, A-C Ritschkoff


Effect of angle of exposure on degradation of radiata pine during weathering trials
1988 - IRG/WP 2301
The importance of angle of exposure on the degree of weathering of materials has not been adequately resolved. In conventional tests, specimens are exposed at an angle of 45° facing the equator, but more recently experiments on polymeric materials have suggested that an angle of 0° may be preferable since this angle maximises levels of received ultra-violet radiation. In this paper the degradati...
P D Evans


Effect of Scytalidium lignicola on decay resistance and strength of wood
1994 - IRG/WP 94-10061
We reported previously that in laboratory tests, pretreatment of Douglas-fir and Southern Pine blocks with Scytalidium lignicola prevented decay. In the present work, we determined 1) the ability of Scytalidium lignicola to colonize and survive in wood exposed in the field, 2) the decay resistance of blocks removed from previously treated Scytalidium lignicola wood and 3) the effect of Scytalidium...
T L Highley


Soluble nutrient content in wood and its susceptibility to fungal discoloration and decay in above ground and ground tests
2000 - IRG/WP 00-10336
The objective of this comprehensive study was to reveal the impact of soluble nutrients in wood on its susceptibility to fungal discoloration and decay in various tests, which is important for the test methodology and standardisation. Seven tests were carried out including pure culture above and ground contact tests, above ground field test and laboratory ground contact tests. The samples containi...
O M Caballero, N Terziev


MDF manufactured from blends of cypress pine and radiata pine shows enhanced resistance to subterranean termite attack
2001 - IRG/WP 01-40214
Medium density fibreboards consisting of blends of the naturally durable wood species white cypress pine (Callitris glaucophylla) and non-durable wood species were manufactured in a commercial plant and subjected to a bioassay using the subterranean termite species, Coptotermes lacteus. A board composed of 30% cypress pine, 30% slash pine (Pinus elliottii) and 40% of the naturally durable hardwood...
P D Evans, S Dimitriades, C Donnelly, R B Cunningham


Chemical evaluation of borate treated pine sapwood attacked by the subterranean termite Coptotermes acinaciformis
1993 - IRG/WP 93-20003
Sapwood of hoop (Araucaria cunninghamii Ait. ex D. Don) and slash (Pinus elliottii Englem.) pines were treated by Vacuum Pressure Impregnation (VPI) to provide test specimens. The concentration of boron was defined by chemical analyses of the timber, in the zone of primary attack by the termite being bioassayed. A common method of definition of preservative retention, weight uptake of preservative...
A R Moffat, B C Peters


Influence of concentration, catalyst, and temperature on dimensional stability of DMDHEU modified scots pine
1998 - IRG/WP 98-40119
Dimethyloldihydroxyethyleneurea (DMDHEU) is being used in textile industry to improve wrinkle recovery. Trials on solid wood have been performed to minimise swelling of the wood. This paper focuses on the effect of various types and concentrations of catalyst and reaction temperature on the dimensional stability of Scots pine. Three different catalysts, NKS (based on magnesium chloride), 3282 (bas...
M Van der Zee, E P J Beckers, H Militz


A light and electron microscopic study of decayed CCA-treated radiata pine (Pinus radiata) wood from a cooling tower
1994 - IRG/WP 94-10056
An inspection of an industrial cooling tower in New Zealand showed surface decay of 12 year old Pinus radiata wood panels treated with CCA preservative to a retention of around 15 kg/m³ of salt. Wood decay micromorphology typical of that caused by soft rot fungi, white rot fungi, 'stripy' and 'v-shaped' erosion bacteria and cavitation bacteria were all commonly...
A P Singh, R N Wakeling, D R Page


Termite-tunnels formation on the surface of termite-resistant wood species in field sites
2001 - IRG/WP 01-10400
In this report, termite-tunnels formation by the subterranean termite, Coptotermes formosanus Shiraki on the surface of termite-resistant wood species, namely, Hinoki (Chamaecyparis abtsu), Yoshino Hinoki (Chamaecyparis abtsu), Miyazaki Hinoki (Chamaecyparis abtsu), Hiba (Chamaecyparis abtsu) and Japanese cedar (Cryptomeria japonica) was conducted in field sites. Westernhemlock (Tsuga heterophylla...
Y Kadekaru, K Kinjo, S Yaga


Strength properties of preservative treated pine and spruce wood after super-heated steaming
1984 - IRG/WP 3313
Possible changes of strength properties of CCF pressure impregnated pine and spruce with subsequent steaming at 110°C respective 120°C for 30 min were examined. For spruce analysis of variance indicated that none of the processes had a significant effect on bending strength, compression strength and the corresponding modulus of elasticity as well as on impact bending strength and shear strength ...
R-D Peek


Soft rot decay in acetylated wood. Chemical and anatomical changes in decayed wood
2002 - IRG/WP 02-40231
Acetylated Beech (Fagus sylvatica) and Scots Pine (Pinus sylvestris) wood were studied in soil beds under laboratory conditions for longer periods. High mass losses and dynamic MOE losses were measured in non-acetylated wood and at lower weight percent gains (WPG). Rapid losses of lignin, holocellulose and ?-cellulose occurred in non-acetylated beech wood and no losses were detected at the highest...
B Mohebby, H Militz


Which fungi should be included in the laboratory evaluation of anti-stain chemicals?
2001 - IRG/WP 01-20236
Test fungi for efficacy tests of anti-stain formulations were selected based on the assumptions that test fungi should be fungicide-tolerant antagonists and fungi resistant to both fungicides and fungicide- tolerant antagonists, and such fungi should be re-isolated from treated samples with the highest fungicidal concentration used for laboratory evaluation of fungicides. This paper discusses the ...
Hyung-Jun Kim, Jae-Jin Kim, Gyu-Hyeok Kim


Check development on jack pine logs in Eastern Canada
2001 - IRG/WP 01-10387
Logs in storage are subject to check damage. The severity of the problem may vary with various environmental and storage conditions. In this study, an investigation was conducted on the development of checks in debarked and bark-on jack pine (Pinus banksiana) logs in Eastern Canada. In the summer of 1999, jack pine trees were felled, logs were debarked and stored in a sawmill yard. The logs were i...
Dian-Qing Yang, R Beauregard


Microscopic characteristics of microbial attacks of CCA-treated radiata pine wood
1993 - IRG/WP 93-10011
Light and electron microscopic observations were made of CCA-treated radiata timbers, which had been placed in service in a vineyard soil as supporting poles and as part of a house pile, to determine the cause of their deterioration. The house pile had failed in service after between 9 and 13 years and was of particular interest because decay was more severe in deeper regions than at the surface a...
A P Singh, R N Wakeling


Preservative effect of cellulose insulation material against some mould fungi and brown rot fungus Coniophora puteana in pine sapwood
1991 - IRG/WP 1484
The influence of mineral wool and loose-fill cellulose wool on biodeterioration of pine sapwood was studied. The test fungi were mould fungi Aspergillus versicolor, Cladosporium sphaerospermum, Penicillium sp. and Aureobasidium pullullans and brown rot fungus Coniophora puteana. Cellulose wool inhibited the growth of mould fungi on the face of wood contacted with insulation material at RH of 97 an...
H Viitanen