Your search resulted in 299 documents. Displaying 25 entries per page.


Initial investigations into the spalting potential of Peruvian hardwoods
2014 - IRG/WP 14-10813
This study was performed to determine if several moderately-utilized Peruvian hardwoods had potential for spalting applications. We applied a modified decay jar methodology with six native Peruvian woods and three moulds, with a period of incubation of six weeks. Results showed that Nigrospora sphaerica and Marupa (Simarouba amara) resulted on the highest significant internal pigmentation (black),...
S M Vega Gutiérrez, S C Robinson


Statistical analysis of durability tests - Part 1: Principles of distribution fitting and application on laboratory tests
2013 - IRG/WP 13-20504
Service life prediction is an important topic in wood research, especially with regard to the Construction Products Regulation (CPR). Both laboratory tests as well as in-service performance testing are therefore essential in combination with proper monitoring and analysis tools. A crucial concept is variability in testing and analysis, especially for a biological material such as wood. The larger ...
I De Windt, J Van den Bulcke, C Brischke, C R Welzbacher, A Gellerich, S Bollmus, M Humar,


A critical view on early indicators for above ground field performance of wood
2013 - IRG/WP 13-20509
Above ground field tests are quite often a balancing act between the provision of realistic test conditions, reliable statistics, and acceptable long test durations. Within this study we therefore reviewed 543 data sets from above ground field tests performed at 36 different test sites in 8 countries in Australia and Europe. The main objective was to investigate possible correlations between early...
C Brischke, L Meyer, G Alfredsen, P-O Flæte, L Francis, M Hansson, P Larsson Brelid, J Jermer


Statistical analysis of durability tests - Part 2: Principles of time-to-failure and application on field test data
2013 - IRG/WP 13-20512
Service life prediction is an important topic in wood research, especially with regard to the Construction Products Regulation (CPR). Both laboratory tests as well as in-service performance testing is therefore essential, in combination with proper monitoring and analysis tools. A crucial concept is variability and the incorporation of variability in tests and analysis. In this paper we focus on t...
J Van den Bulcke, I De Windt, C Brischke, C R Welzbacher, A O Rapp, J Van Acker


Image analysis for mould and sapstain detection on wood
2013 - IRG/WP 13-20519
Laboratory tests for mould growth on wood products are time consuming and rely on visual assessments of specimens utilizing subjective rating systems. Accelerated laboratory methods are needed that can provide rapid, quantitative assessment of mould and sapstain growth on solid and composite wood products. Image analysis of scanned spore imprints from southern pine or oriented strandboard (OSB) sp...
C A Clausen, V W Yang


Extraction and analysis of DNA from green and seasoned timber as basic methods for determination of wood species and origin
2013 - IRG/WP 13-20523
Against the background of the European timber trade regulation EUTR, commenced to law by March 2013, the determination of wood species and tracing of its origin is getting a great importance. A promising approach for establishing fast and reliable tracking systems for wood products is DNA analysis. A critical point is the extraction of analysable DNA from the wood and its lignified cell walls. Thu...
K Jacobs, H Mende, W Scheiding


Visualization of Copper in the Voids and Cell Walls of Treated Wood using X-Ray Micro-Computed Tomography
2013 - IRG/WP 13-40640
This study extends our observations of the distribution of copper in treated wood. A small wood block was cut from a southern pine batten that had been treated with a particulate-copper preservative and similar sized block was cut from a batten that had been treated with a copper-amine preservative. Both blocks were imaged using X-ray micro-computed tomography. We obtained tomograms of each treate...
P D Evans, A Limaye, H Averdunk, M Turner, T J Senden


Quantification of copper and chromium in field stakes after different exposure times: Remaining metal content and distribution
2013 - IRG/WP 13-50291
In order to determine the distribution of copper and chromium as well as their remaining concentration EN 252 specimens and thicker pine sapwood stakes (non standard format) were treated with a commercial CC salt in a vacuum pressure process. The stakes were installed in the test field of the Institute of Wood Research, Hamburg, in August 2010. In all cases three stakes were removed after 4, 8, 12...
T Liese, M Bahmani, E Melcher


Observation of Boring Process of Larvae of the Bamboo Powder-post Beetle (Dinoderus minutus)
2014 - IRG/WP 14-10821
The bamboo powder-post beetle Dinoderus minutus is a major pest of felled bamboo in Japan. X-ray computer tomography (CT) was applied to non-destructively trace the movement of the larvae of this beetle inside the infested bamboo samples. The bamboo samples were prepared from pieces of the Japanese timber bamboo Phyllostachys bambusoides culms that were enclosed with adult D. minutus beetles for a...
H Watanabe, Y Yanase, Y Fujii


Identification of soft-rot fungi existed in the samples from the galley excavated at Yenikapi
2014 - IRG/WP 14-10833
The shipwrecks of the Middle Byzantine period were excavated during the construction of the Marmaray railway and metro station in Yenikapı between 2004 and 2012. This has become the largest investigations because of the size and the number of the shipwrecks and its associated artifacts. In the previous report, the electron micrographs of the samples revealed that a wide range in the degree of...
T Wada, C Köse, K Igarashi


Microbial Community Analysis of Naturally Durable Wood in an Above Ground Field Test
2014 - IRG/WP 14-10826
This paper presents preliminary results of an above ground field test wherein eight naturally durable wood species were exposed concurrently at two sites in North America. Surface samples were taken at regular intervals from non-durable controls and compared to their more durable counterparts. Terminal Restriction Fragment Length Polymorphism was performed to characterize the microbial (bacteria, ...
G T Kirker, S V Diehl, P K Lebow


Statistical analysis of 40 years of preservative in-ground stake testing in Australia
2014 - IRG/WP 14-20552
Wood is widely recognized as a valuable material, yet the natural durability of some wood species limits its use for certain outdoor purposes. For decades, a wide range of methods and chemicals have been developed to increase the resistance of wood against degrading microorganisms and termites. Preservative treatment has a long and widespread tradition in wood protection. Proper testing of the eff...
J Van den Bulcke, L J Cookson, I De Windt, W Li, J Van Acker


Scanning Transmission X-ray Microscopy as a tool for examining chemical changes in wood cell walls due to enzymatic activity
2014 - IRG/WP 14-20556
As development of techniques for examining enzymatic activity on solid, complex biological materials, is considered to be an important factor in further development of enzyme applications and for understanding the decay of plant materials, this study explores applicability of Scanning Transmission X-ray Microscope (STXM) for determining chemical changes in enzymatically treated samples at the cell...
D Jeremic, R Goacher, R Yan, C Karunakaran, E R Master


VOC-free remedial treatment agent on organic solvent basis with surface cleaning by photocatalysis using titanium dioxide
2014 - IRG/WP 14-40651
Due to the EU Regulations according to the harmonisation of the European market of biocidal products and the EU Regulations regarding emissions of volatile organic compounds in residential properties a new VOC free yet organic solvent based remedial treatment agent is introduced including a potential method to clean up the wooden surface of remaining biocides after a remedial treatment using photo...
H Ahl, J Fromm, P Jüngel, E Melcher, M Pallaske


Dynamic mechanical analysis (DMA) of nano cupric oxide (CuO) modified aqueous phenol formaldehyde (PF) resin
2014 - IRG/WP 14-40654
Phenol formaldehyde (PF) resins, modified by nano CuO incorporating alkane surfactant and polyvinyl alcohol (PVA) 17-99, were analyzed by dynamic mechanical analysis (DMA). The mechanical properties of its bonded plywood including tensile strength, modulus of rupture (MOR), modulus of elasticity (MOE) and shear strength under five test conditions were evaluated. Results indicated that the incorpor...
Wei Gao, Guanben Du


Modern Instrumental Methods to Investigate the Mechanism of Biological Decay in Wood Plastic Composites
2014 - IRG/WP 14-40674
Various instrumental techniques were used to study the fungal decay process in wood plastic composite (WPC) boards. Commercial boards exposed near Hilo, Hawaii (HI) for eight years in both sun and shadow locations were inspected and tested periodically. After eight years of exposure, both boards were evaluated using magnetic resonance imaging (MRI), while a selected area of the board exposed in sh...
G Sun, R Ibach, M Gnatowski, J Glaeser, M Leung, J Haight


Compatibility of Acetylated Wood and Wet Concrete
2014 - IRG/WP 14-40673
One of the newer commercial technologies to provide stability and durability to wood and wood composites is the process of acetylation (the reaction of acetic anhydride with wood). Wood is often used in contact with concrete, although only a very limited amount of species are suitable for this type of application because of durability issues. From this perspective durability class 1 timber such ...
R Rowell, C Lankveld, J Alexander


The whitening cause of Korean wooden heritage by flame retardant treatment
2015 - IRG/WP 15-20560
Korean wooden heritage used to treat by flame retardants in order to protect fire. There are 2 types flame retardant using for wooden heritage. These flame retardants treatment are basic measure that apply to wooden heritage along with other fire protection. The flame retardants cause white stains by reacting with Korean traditional wood painting (Dancheong) and increase wood humidity. The Korean ...
Jin Qyu Kim, Gyu-Seong Han, Yong Jae Chung, Hwa Soo Lee, Dong Won Son


Non-destructive monitoring of structure and moisture dynamics of plywood exposed outdoors to improve service life prediction and fit-for-purpose design
2015 - IRG/WP 15-20570
Plywood is an important construction material yet prone to water uptake, which can decrease strength and increase decay risk. To predict service life and improve fit-for-purpose design, it is crucial to understand the moisture behavior and structural changes of plywood. In this research, several plywood specimens were exposed outdoors for approximately one year. During this period, the moisture di...
W Li, J Van den Bulcke, I De Windt, M Dierick, J Van Acker


Impact of early lignification of ray parenchyma cells on the treatability of Scots pine sapwood
2015 - IRG/WP 15-40706
The wood anatomy of Scots pine sapwood can influence its treatability. A microscopic analysis on the wood material from four different stands in Northern Europe was performed using tangential sections from the outer part of Scots pine sapwood. Single correlations of the ray composition and lignification state of the ray parenchyma showed the influence of these factors on radial penetration depth a...
K Zimmer, A Treu


Foundation piles: analysis of beech wood decay in service life conditions
2016 - IRG/WP 16-10858
Wood piles foundation system was largely used over decades. Thus, numerous buildings over the world are based on this constructive system. In the context of reduction of CO2 emissions in the building field of constructions, substitution of concrete by wood as material for foundation piles seems to be a promising alternative. However, fluctuation of the water table level in soil may promote fungal ...
Q Kleindienst, A Besserer, M-L Antoine, C Perrin, J-F Bocquet, L Bléron


Studying fungal growth using automated image analysis and computer simulations
2016 - IRG/WP 16-20590
Wooden materials are prone to fungal attack resulting in damage and economic losses. Therefore many efforts have been made to understand the degradation of wood and to avoid the adverse effect of fungi. Even though the extent of degradation of a material is inversely proportional to the extension of the fungi attacking it, most researchers focus mainly on the former, leaving the study of the latte...
G Vidal-Diez de Ulzurrun, J M Baetens, J Van den Bulcke, B De Baets


How intraspecific radial variability of the European Oak’s may influence mild pyrolysis process and durability of the material
2016 - IRG/WP 16-40725
Last decades wood is promoted as building material. Unprotected wood exposed to outdoor conditions undergoes a variety of degradation induced essentially by fungi attacks. Heat treatment of wood by mild pyrolysis (180°C T 240°C under inert atmosphere) is a preservation process with a weak environmental impact, and therefore, is viewed as an interesting alternative to the chemical impregnation me...
J Hamada, A Pétrissans, F Mothe, M Pétrissans, P Gérardin


Combustion and thermal characteristics of Korean wood species
2016 - IRG/WP 16-40727
This study examined the combustion and thermal characteristics of domestic woods in Korea. Wood was confirmed by a cone calorimeter according to the KS F ISO 5660-1 standard. The combustion properties of the wood were measured in terms of the heat release rate (HRR), total heat released (THR), mass lose rate (MLR), and ignition time (time to ignition; TTI). Also, the thermal properties were measur...
Huyun Jeong Seo, Jung-eun Park, Dong Won Son, Won-Joung Hwang


Dynamic mechanical analysis of viscoelastic properties of heat treated glycerol-impregnation poplar wood
2016 - IRG/WP 16-40732
The viscoelastic properties of glycerol-impregnated poplar wood after heat treatments at various temperatures were examined by dynamic-mechanical analysis. The spectra of storage modulus (E’) and loss tangent (tgδ) in the frequency at 10 Hz were measured at the temperature range from -100 to 300℃. Compared to no peak in E’ spectra and two relaxation processes in tanδ spectra of...
Li Yan