The effective control of moulds on freshly impregnated wood
2004 - IRG/WP 04-30352
Beside natural timber it is known, that moulds can also groth at the surface of impregnated wood. This material shows “defects” like resistant dark spots or color changes and causes complaints. During the last years, the problem by moulds seems to increase. Laboratory studies were carried out to show the effect of impregnations against moulds. Wood samples (Pinus sylvestris L.) were impregn...
G Cofta, K Lutomski, P Jüngel


The Pilodyn instrument as a non-destructive tester of the shock resistance of wood
1978 - IRG/WP 2107
A new non-destructive shock resistance tester, the PILODYN, has been developed. The instrument measures the fracture surface area created by a constant amount of energy. It operates by shooting a blunt pin into wood by an exact amount of energy. The penetration depth is read on a scale. A wide field of application is open to a non-destructive shock resistance tester such as: 1) assessment of the r...
P Hoffmeyer


The First Annual Report of the International Research Group on Wood Preservation 1969-1970
1970 - IRG/WP A 7
IRG Secretariat


Cleaner prodiction and the wood preserving industry
1995 - IRG/WP 95-50040-29
H Carr-Harris, C R Coggins


Work program of CEN/TC 38 (January 1994). Durability of wood and derived materials
1994 - IRG/WP 94-20019
R Hüe


The most important wood-destroying insects in various countries (Results of questionnaire)
1981 - IRG/WP 1136
M-M Serment


Wood preservation in China
1989 - IRG/WP 3546
Huiming Zhou, Zhongwei Jin


New conception for shortering the duration of fungitoxic test on wood preservatives. Part 1: State-of-art
1994 - IRG/WP 94-20044
The review of agar-block and soil-block methods published during 90 years focused of shortening the duration of fungitoxic test of wood preservatives is presented. Special attention was given to miniaturisation of wood specimens....
J Wazny, P Witomski


Factors affecting the sorption of preservative during diffusion treatment of wood
1988 - IRG/WP 3500
The sorption of preservative into wood during soaking in aqueous solution was found to comprise absorption as well as diffusion of solute. Absorption was increased by partially seasoning the wood prior to soaking and was characterised by (a) a very rapid initial rate of uptake and (b) an extended period of slow uptake, the rate of which varied with prior conditioning. It was concluded that some pa...
P Vinden


Environmental risk assessment of preservative treated wood
1998 - IRG/WP 98-50101-19
This paper reviews the status of the environmental risk assessment of preservative treated wood and confirms the distinction between the risks presented by wood preservatives and preservative treated wood. The paper proposes a tiered approach to risk assessment and discusses the rationale. Flowcharts are presented which summarise the tiered approach to risk assessment, show the tests required, and...
E F Baines, S J Davis


Detection of trace organics by ion mobility spectrometry
1990 - IRG/WP 3635
Ion Mobility Spectrometry (IMS) is a time of flight analytical technique that is suited to detect chemicals in the low parts per billion range. Some of the advantages of IMS are: operation at atmospheric pressure, fast response time (0.1-10 sec), and the ability to characterize individual chemical species in complex matrices without any prior sample preparation. In this paper, the utility of IMS i...
A H Lawrence


Differential behaviour of wood rotters at water repellent Rubberwood
2000 - IRG/WP 00-10386
Rubberwood samples treated with different concentration of aqueous solution of chromic acid has induced significant increase in water repellency and attains dimensional stability. Though water repellency and dimensional stability was achieved by treatment, the fungal invasion could not be completely controlled. Differential level of decay of brown and white rot in wood treated with water repellent...
H C Nagaveni, S S Chauhan, K S Rao


Bacterial wood degradation by a pure culture
1995 - IRG/WP 95-10093
A single-celled bacterium isolated from lake water yielded cell wall degradation in Scots pine sapwood samples. The bacterium attacked all cell wall layers in one month of laboratory culture. It was identified as Aureobacterium luteolum....
O Schmidt


List of Members of IRG and contributing workers proposed for membership in IRG/WP/ - I - Sub-group 5
1976 - IRG/WP 154
S Cymorek


Wood-destroying Rhinotermitidae (Isoptera) in the oriental region
1984 - IRG/WP 1236
Species of the family Rhinotermitidae are important wood-destroying termites. From the Oriental zoogeographical region, 85 species of the family are reported of which some are wide spread and cause extensive damage to wood, wooden articles and other cellulosic products. The distribution, biology, ecology and pest status of the important wood-destroying species, in the Oriental region, are given in...
O B Chhotani


Preservative absorption response of planks of Anogeissus acuminata for plank-built catamarans
2002 - IRG/WP 02-40245
Due to shortage of timber coupled with other compelling factors, traditional fishermen along the east coast of India, especially of Andhra Pradesh, of late, are departing from conventional log type wooden catamarans. Instead, they are fabricating catamarans out of timber planks of hard woods and utilizing thermocol for buoyancy. Mostly, locally available timber of a Combretaceae species, Anogeis...
V Kuppusamy, M V Rao, M Balaji, K Rao


How to determine what is a realistic emission from treated wood - basic reflections
1998 - IRG/WP 98-50105
Emissions from treated wood occur by evaporation and by leaching. Up to date by far more experience exists on leaching tests than on evaporation test. The methods applied will be of interest to give answers to the questions about the quantity of possible emissions. Standardisation on leaching started very early. One of the first attempts to quantify the effect of leaching on the remaining efficacy...
H Willeitner, R-D Peek


Performance of treated spruce in Canadian field test sites
1989 - IRG/WP 3506
Spruce material under test in Canadian field test sites is performing better than anticipated. From the comparison of the performance of spruce treated with various preservatives, it appears that penetration may be far more important on durability performance than the preservative itself or the retention of preservatives in the wood. However, there is still insufficient data on the influence of pe...
J P Hösli, E E Doyle


36 years of wood preservative tests in Tanzania
1992 - IRG/WP 92-3731
The performanee of major wood presevatives which are used widely commereially are given. These include creosote, CCA's and 5% Pentachlorophenol dissolved in heavy industrial diesel. Tests are conducted at three ecologically different using pine stakes. Results show that the striking performance of creosote and CCA's is noticeable at above 128 kg/m³ and 16 kg/m³ respectively....
K K Murira, P F Nangawe


A method of predicting the average life of field tests on preservative-treated stakes
1977 - IRG/WP 297
The paper presents an analysis of the results of completed field stake tests on untreated and preserved timber, and develops a method of predicting the average life of incomplete stake tests on wood preservatives from the failures that have occurred so far....
D F Purslow


The permanence of permethrin in wood preservation
1984 - IRG/WP 3288
The permanence of the synthetic pyrethroid permethrin in treated wood has been assessed for double vacuum and immersion treated Scots pine sapwood and whitewood using a 0.5% m/m solution of the insecticide in a hydrocarbon solvent. It is concluded that for all but the outermost 0.5 mm of the treated battens the distribution of the permethrin is relatively permanent. The outermost 0.5 mm appears vu...
R J Orsler, M W S Stone


The effects of heat treatment on anatomical changes of beech wood
2004 - IRG/WP 04-40284
The effects of heat treatment on anatomical changes of beech wood (Fagus orientalis) naturally grown and intensively used in forest products industry in Turkey were studied. The wood samples were cut into 2x2x3 cm and than conditioned at 25 °C and 65 % relative humidity for 3 weeks. Heat treatment was than applied to the wood samples at four different temperatures (130 °C, 150 °C, 180 °C and ...
Ü C Yildiz, Z Gerçek, B Serdar, S Yildiz, E D Gezer, E Dizman, A Temiz


Timber Preservation and Sustainable Construction in Australia
2005 - IRG/WP 05-50224-14
Sustainable development has been described as meeting the needs of the present without compromising the ability of future generations to meeting their own needs. (Bruntland 1987) To achieve the sustainable development goal therefore, the maximum performance has to be obtained from existing resources (timber) so that the remaining resource is protected from over-exploitation. Clearly, wood preserva...
J Norton


Metal carboxylates for wood pest control
1996 - IRG/WP 96-30109
Metal carboxylates have been used as wood preservatives for more than fifty years. Predominantly salts of naphtenic acids have been commercially applied so far. They have water repellent as well as fungicidal and insecticidal properties. In the last years, metal carboxylates of saturated fatty acids were introduced. Fatty acids with 7-10 carbon atoms already have fungicidal activity by themselves....
F Pohleven, M Petric


Interaction mechanisms of F/Cr/As/B type preservative and wood
1981 - IRG/WP 3183
The paper reports results of investigations on the fixation of the components of a F/Cr/As/B preservative in wood and its lignin and cellulosic components....
N Ermush, I Andersone