Influence of coatings on water uptake of wood surfaces before and after natural and artificial weathering
2013 - IRG/WP 13-40641
Liquid water absorption of wood surfaces with and without coating, before and after exposure to artificial and natural weathering has been studied. Spruce, oak and sapele samples have been exposed to the cycle of EN 927-6, to the cycle of the Gardner wheel and to natural weathering. Five coatings were tested including solventborne and waterborne, semi-transparent and opaque products. Exposure to w...
L Podgorski, S Collignan, J-D Lanvin


Effect of electron beam irradiation on the fire retardant penetration into wood
2013 - IRG/WP 13-40642
Electron beam processing which can fast and easy change the nature of the material has received considerable attention recently. Studies using electron beam has been conducted in various fields and it has been applied in many industrial sectors. Electron beam has higher energy than other electromagnetic waves. It has excellent object permeability. It affects degradation of intermolecular cross-lin...
Dong won Son, Jong Sin Lee, Mee Ran Kang, Sang Bum Park


Influence of Heat Treatment Medium on Fungal Resistance of Beech Wood
2013 - IRG/WP 13-40643
Hydrothermal treatment of beech wood (Fagus orientalis) performed in acidic, neutral and alkaline buffered mediums in 160 and 180°C. White rot fungi (Coriolus versicolor) and brown rot fungi (Coniophora puteana) were used to determine the influence of heat treatment mediums on the behaviour of fungal resistance. White rot of wood digest lignin rather than cellulose; while brown rot digests the ce...
A Talaei, A Karimi, M-F Thévenon


Investigation of Nanocopper-Hygrothermally Treated Wood Properties
2013 - IRG/WP 13-40644
Nanometals with high thermal conductivity can be considered as modifiers, especially in thermal modification of wood. This study was aimed to investigate some physical and mechanical properties of nanocopper impregnated Iranian beach (Fagus orientalis Lipsky), which was hygrothermally treated. For this purpose, nanocopper solution (400 ppm) was used for impregnation process. Hygrothermal treatment...
G Rassam, B Jamnani, A Faraji Heris


COST Action FP0904 – Increasing the Understanding of Thermo-Hydro-Mechanical Wood Behaviour and Processing
2013 - IRG/WP 13-40646
The polymeric components of wood and its porous structure allow its properties to be modified under the combined effects of temperature, moisture and mechanical action – so-called Thermo-Hydro-Mechanical (THM) treatments. Various types of processing techniques, including high temperature steam with or without an applied mechanical force, can be utilised to enhance wood properties, to produce eco...
D Jones, P Navi


Moisture and Fungal Durability of Wood-Plastic Composites Made With Chemically Modified and Treated Wood Flour
2013 - IRG/WP 13-40648
Evaluating the fungal durability of wood-plastic composites (WPCs) is complicated by the influence of slow moisture sorption. Recently, the American Wood Protection Association (AWPA) Standard Method E10, Testing Wood Preservatives by Laboratory Soil-Block Cultures, was modified to incorporate not only solid wood, but also wood-based composites and WPCs. To simulate long term WPC performance, cond...
B K Segerholm, R E Ibach


Effect of bio-resin from cashew nut shell liquid (CNSL) on decay resistance properties of wood
2013 - IRG/WP 13-40649
This study assesses the decay resistance properties of bio-resin modified wood against decay fungi of the Basidiomycota according to the EN 113 protocol. A bio-resin system was developed by ozonolysis process from cashew nut shell liquid (CNSL), a naturally occurring mixture of phenolics. Small wood blocks from sapwood of Scots pine (Pinus sylvestris), Obeche (Triplochiton scleroxylon) and Gmelina...
M Ashaduzzaman, M D Hale, V Tverezovskiy, G A Ormondroyd


Bio-based thermoset resins for bonding and eco-friendly preservation in the wood industry
2013 - IRG/WP 13-40650
Yellow dextrins and tannins were used in wood adhesives formulation to substitute resins based on formaldehyde. Several formulations were carried out in alkaline aqueous media by varying the weight fraction of two compounds from 10% to 30%. The cross-linking was performed using epichlorohydrin as a reticulant agent. Rheological behaviours and initial adhesion of three liquid formulations, before r...
C Motillon, A Allal, A Visse, F Charrier, B Charrier, A Baldé


Quantification of copper and chromium in field stakes after different exposure times: Remaining metal content and distribution
2013 - IRG/WP 13-50291
In order to determine the distribution of copper and chromium as well as their remaining concentration EN 252 specimens and thicker pine sapwood stakes (non standard format) were treated with a commercial CC salt in a vacuum pressure process. The stakes were installed in the test field of the Institute of Wood Research, Hamburg, in August 2010. In all cases three stakes were removed after 4, 8, 12...
T Liese, M Bahmani, E Melcher


Bibliographical study: Decontamination of wood and soils polluted by pesticides used in wood preservation: focus on Bioremediation methods using microbes
2013 - IRG/WP 13-50292
The purpose of this bibliographical study was to seek out the existence of projects (past, present, or future) on soil decontamination in wood treatment plants. Indeed, such polluted soils may contain dioxins and various types of furans. The aim was to find out whether there existed one or more methods bringing into play biodegradation techniques using, for example, species of fungi, yeasts, bacte...
Zaremski, L Gastonguay, C Zaremski, S Morel, J Beauchene


Removal of nano- and micronized-copper from treated wood by chelating agents
2013 - IRG/WP 13-50294
Micronized and nano-copper (Cu)-based and arsenic and chromium-free systems have received much attention for wood protection in recent years. Because they have different fixation, and micro-distribution properties, such copper systems may be more or less subject to release using known remediation methods than soluble forms of Cu. This study evaluated Cu recovery from wood treated with micronized- ...
S N Kartal, E Terzi, B Woodward, C A Clausen, S T Lebow


Conclusions and Summary Report on an Environmental Life Cycle Assessment of ACQ-Treated Lumber Decking with Comparisons to Wood Plastic Composite Decking
2013 - IRG/WP 13-50295
The Treated Wood Council has completed a quantitative evaluation of the environmental impacts associated with the national production, use, and disposition of ACQ (alkaline copper quaternary)-treated lumber decking and wood plastic composite decking using life cycle assessment (LCA) methodologies and following ISO 14044 standards. The results for treated wood decking are significant. • Less En...
AquAeTer, Inc.


Durability of alternatives to CCA-treated wood - Results from field tests after 11 years exposure
2013 - IRG/WP 13-30633
The present study was initiated as a consequence of restrictions against the use of CCA-type wood preservatives in Sweden in the 1990s. New copper-based formulations were introduced on the market and to some extent, also alternatives to preservative-treated wood, such as thermally and chemically modified and linseed oil treated wood as well as heartwood of non-tropical naturally durable wood s...
P Larsson Brelid, M-L Edlund


Relevance of natural pre-weathering for laboratory decay tests with native, modified, and preservative-treated wood
2013 - IRG/WP 13-20522
The on-going development of new wood protection systems is hampered by the long term field tests currently in use. New accelerated test methods and novel methods for faster and more accurate evaluation of wood protection methods are requested. For both field decay tests and accelerated laboratory decay tests, limitations are imposed. This study is part of the research program ‘WoodBuild’, whic...
A Pilgård, C Brischke, L Meyer


Estimation of service life of treated wood in ground contact based on early indicators
2013 - IRG/WP 13-20536
A well-known problem with field testing is that it takes a long time before meaningful and reliable results are achieved. Only when a trial has come to an end the so called average life for the samples in a group can be calculated and compared with other samples. The aim of the present study was to investigate if it is possible to get a reasonable and good estimation of the average life long befor...
M Hansson, J Jermer, P Larsson Brelid, N Terziev


Critical moisture levels and mould resistance of five different wood treatments
2013 - IRG/WP 13-30632
Mould resistance of five different treatments were tested using two methods, a recently developed method for the determination of critical moisture levels of building materials (RHcrit), and ASTM D3273-94. The critical moisture level method exposed samples at 22 °C and 98, 92, 86 and 82% relative humidity (RH) for 12 weeks. ASTM D3273-94 was performed at 29 °C and about 95% RH. Treatments c...
G Bok, P Johansson, A Ekstrand Tobin, S Bardage


Effect of Nano and Micronized Particles as Wood Preservatives for Termite Control
2013 - IRG/WP 13-30620
Subterranean termites are a major factor in the biodegradation of wood constructor products. In this study the efficacy of wood treated with micronized copper, zinc oxide and their mixture was compared to that of wood treated with soluble amine copper oxide with subterranean termites in a laboratory test. All of the formulations tested were effective in controlling wood degradation by the term...
M Akhtari, D Nicholas, A Rowlen, M Arefkhani


Investigating the potential role of creosote oil for the water repellent purposes in fiberboards
2013 - IRG/WP 13-40635
Effect of wood steaming during fiber generation processes and creosote oil on the properties of fiberboard, manufactured from creosote treated solid wood were investigated. Pulp fiber was generated by alkaline pretreatment of waste creosote impregnated wood which being fiberized by laboratory defibrator, atmospherically. These fibers blended with 0, 15, 30, 45 and 100 percent by weight of wood...
M Sheikholeslami


Performance standards for wood in construction – delivering customer service life requirements
2013 - IRG/WP 13-20537
There is increasing need for consideration of performance classification for wood products in construction, as evidenced by the CPR, warranty providers and end user demands for information. This means we need to radically consider how the tests we conduct on wood for durability (especially biological durability) can inform on service life and how they might if possible be translated into a perform...
E Suttie, C Brischke, F Englund, E Heisel, J Jermer, D Lorenzo, M Polášek, S Thelandersson, J Van Acker


Effect of Nano-silver and Nano-copper and Nano-zinc oxide on Paulownia wood exposed to white-rot fungus
2013 - IRG/WP 13-30635
Paulownia is known as a fast growing tree and it can be used in several applications. The present study investigated the effect of Nano-silver and Nano-copper and Nano- zinc oxide on resistance of Paulowina (Paulownia fortunei) wood against the white rot fungus (Coriolus versicolor). Wood specimens with a dry density of 0.37g/cm3 were impregnated with a 400 ppm aqueous suspension of micronized na...
M Akhtari, M Ganjipour


Moisture dynamics of wood – An approach to implement wetting ability of wood into a resistance classification concept
2014 - IRG/WP 14-20557
Within the research programmes WoodBuild and PerformWOOD, wetting ability tests have been conducted with 25 wood-based materials. A first attempt has been made to establish factors for calculating the material resistance of wood materials to be implemented into a design guideline for timber structures. The approach looks promising, but further studies are needed to establish more reliable relation...
C Brischke, C Hesse, L Meyer, S Bardage, J Jermer, T Isaksson


An Overview of Western Red Cedar as a Wood Pole Species
2014 - IRG/WP 14-10815
This paper reviews the characteristics of western red cedar, with particular emphasis on its use in utility poles. Western red cedar naturally grows primarily in British Columbia, Alaska, Washington, Oregon, California, Idaho and Montana. Compared to other commercial softwoods it has low density, increased corrosivity, weaker mechanical properties, high dimensional stability, and high natural dura...
M H Freeman, R Stirling


Performance of recent and old Sweet chestnut (Castanea sativa) wood
2014 - IRG/WP 14-10816
Sweet chestnut (Castanea sativa) hardwood is one of the most durable European wood species. In the present research, various aspects that could potentially influence the durability were elucidated, namely: presence of extractives, ring width, and weathering. Simultaneously, properties of wood, which was in outdoor use for 35 years, were elucidated as well. The results indicate that ring width and ...
M Humar, M Žlahtič, N Thaler


Using hyperspectral imaging to detect and quantify mould and blue stain on coated and uncoated wood
2014 - IRG/WP 14-10822
Hyperspectral imaging has been applied on the surface of samples of coated and uncoated Norway spruce (Picea abies) as a new technique to detect and quantify growth of mould and blue stain fungi. Principal Component Analysis of the hyperspectral images resulted in a clear visualization of the fungi and the amount of mould coverage could be estimated. This indicates that NIR hyperspectral imaging c...
L Ross Gobakken, I Burud, A Flø, K Kvaal, T K Thiis


Emerging function for a glutathione transferase in response to wood extractives toxicity
2014 - IRG/WP 14-10824
The first steps of wood degradation by fungi lead to the release of toxic compounds known as extractives. To better understand how lignolytic fungi cope with these products, a transcriptomic analysis of Phanerochaete chrysosporium genes was performed in presence of oak acetonic extractives. The most up-regulated genes relate to nutrition, nucleic acid modification, gene regulation, signalling and ...
A Thuillier, K Chibani, A Deroy, S Dumarçay, P Gérardin, A Kohler, J-P Jacquot, E Gelhaye, M Morel-Rouhier