IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3065 documents. Displaying 25 entries per page.


An investigation on some physical properties of oil heat treated poplar wood
2010 - IRG/WP 10-40509
In this study some physical properties of small samples (20×20×20 cm) of poplar wood (Populus nigra var.pyramidalis) after oil heat treatment with linseed oil was investigated. Two time levels (4.5 & 6 hours) and three temperature stages (180,200 & 220°C) were selected. The results of this study showed significant differences in effects of treatment temperature on physical properties of wood....
B Bazyar, D Parsapajouh, H Khademiesalam


Performance of selected types of coated and uncoated modified wood in artificial and natural weathering
2010 - IRG/WP 10-40510
The objective of the present work was to investigate the influence of commercial wood modification methods on weathering behaviour and coating performance. It was aimed to compare modification methods and to set up maps of weathering behaviour for these methods with and without a semi-transparent wood stain. Artificial and natural weathering trials were carried out with a selection of different ty...
G Grüll, L Podgorski, M Truskaller, I Spitaler, V Georges, S Bollmus, A Steitz


A comparison of the corrosion of alkaline copper and micronized copper treated wood
2010 - IRG/WP 10-40515
With the replacement of chromate copper arsenate (CCA) by alkaline copper wood preservatives, there have been reports of increasing corrosion of metal fasteners and connectors in contact with treated wood. This may be explained by the presence of more mobile copper in the treated wood. One novel industrial response has been to develop a wood preservative based on an aqueous solution containing sus...
M Kofoed, J N R Ruddick


Study of Microscopy Properties of Modified Wood During Weathering Process
2010 - IRG/WP 10-40517
In this study spruce (Picea excelsa) and Beech (Fagus orientalis) wood acetylated and has been subjected of artificial weathering in difference times (0, 50,150&300 h), then wood surface analyzed using Scanning Electron Microscopy (SEM). The SEM results shown that the surface of wood exposed to weathering undergoes distinct physical changes and the surface degradation appears to be directly propor...
M Akhtari


Acquisition of sorption isotherms for modified woods by the use of dynamic vapour sorption instrumentation: Principles and Practice
2010 - IRG/WP 10-40518
The complex wood-water relationship has been the topic of numerous studies. Sorption isotherms – in particular – have been derived for hundreds of wood species, their sap- and heartwood sections as well as for decayed, engineered and modified wood materials. However, the traditional methods for obtaining sorption isotherms are very time consuming. With new dynamic vapour sorption (DVS) instrum...
E T Engelund, M Klamer, T Mark Venås


Impact of wood species on the performance of exterior wood coatings
2010 - IRG/WP 10-40519
To prolong the service life of a wooden construction the protective function of a coating is of utmost importance. The chemical composition as well as the wood-coating interface affects the performance of this protective layer and obviously wood species have an impact too. This paper discusses the influence of wood species on the overall coating performance. Therefore, a range of opaque waterborne...
I De Windt, J Van den Bulcke, J Van Acker


Moisture dynamics of WPC as basis for biological durability
2010 - IRG/WP 10-40520
The largest market for wood-polymer composites (WPCs) is currently decking. Although many products are commercially available, a proper standard for the assessment of the biological durability of WPC does not exist. Recommended standards for testing resistance against basidiomycetes should be completed with a method to bring the specimens in a worst case situation, obtaining a moisture level high ...
N Defoirdt, J Van Acker, J Van den Bulcke


Biological degradation of acetylated wood after 18 years in ground contact and 10 years in marine water
2010 - IRG/WP 10-40522
This paper addresses the resistance to biological degradation of acetylated wood. Firstly, it presents results from an EN 252 test after 18 years’ exposure. The test is still running in Nordic NWPC test fields, Simlångsdalen in Sweden and Viikki in Finland. Results from this test were presented after 5 years’ exposure ( IRG/WP 97-30139), and showed that the resistance of acetylated wood wit...
P Larsson Brelid, M Westin


Testing of decay resistance of sapwood and heartwood of thermally modified Scots pine and Norway spruce
2010 - IRG/WP 10-40523
Thermal modification at elevated temperatures changes the chemical, biological and physical properties of wood. One of the main targets of thermal modification is to increase the biological durability and decay resistance of wood. Although the effects of thermal modification on wood have been widely studied, the significance of sapwood and heartwood on the resistance of thermally modified wood has...
H Viitanen, S Metsä-Kortelainen


Wet and dry adhesion of coatings on modified and unmodified wood: comparison of the pull-off test and the cross-cut test
2010 - IRG/WP 10-40524
The objective of this paper is to study the influence of several types of modification (acetylation, furfurylation, thermal modification) on coatings adhesion and to compare two methods of assessing the adhesion: the cross-cut test and the pull-off test both tested in dry and wet conditions. The study also investigates the effect of other parameters of the wood substrates on adhesion like the ring...
L Podgorski, G Grüll, M Truskaller, J D Lanvin, V Georges, S Bollmus


Lignin blocking effects on weathering process of wood plastic composites
2010 - IRG/WP 10-40529
The weathering of wood–plastic composites (WPC) causes discoloration which affects their aesthetic aspects. It has been proved that these discolorations are due to lignin degradation. Effects of blocking the susceptible structure of lignin assessed by chemical treatment such as acetylation and methylation are reported in this study. Surface chemical change of wood plastic composite (WPC) formula...
P Darabi, A Naghi karimi, S Ahmade Mirshokraie, M-F Thévenon


Silicon compounds as additives improving alkyd-based wood coatings performance
2010 - IRG/WP 10-40531
The reactivity of cellulose with solvent-born alkyd-based wood coatings supplemented with organosilanes was analyzed. Structural analysis of cellulose subjected to the reaction with organosilanes and following extraction with water was performed using Fourier-transform infrared spectroscopy (FTIR). The analyzed IR spectra comprise bands 1250 cm-1 typical for the SiC group and 800 cm-1 typical for ...
B Mazela, I Ratajczak, K Wichłacz-Szentner, P Hochmańska


Bioresistance of Poplar Wood Compressed by Combined-Hydro-Thermo-Mechanical Wood Modification (CHTM) Process
2010 - IRG/WP 10-40532
Bioresistance of treated Poplar wood by CHTM process (Combined-Hydro-Thermo-Mechanical Wood Modification) was studied in the current research work. Resistance against brown rot fungus Gloeophyllum trabeum as well as the soft rot decay was the main concern of this work. Poplar wood blocks were hydrothermally treated at temperatures of 120,150 and 180°C for holding time of 0, 30 and 90 min. afterwa...
L Khademi-Bami, B Mohebby


Effect of Nano-Silver Treatment on Densified Wood Properties. Part One: Swelling, Recovery Set, Bending Strength
2010 - IRG/WP 10-40533
In this research the effect of Nano-Silver treatment on compressed wood properties, was studied. Wood specimens were cut from Popolus alba (poplar) and impregnated with Nano-Silver and water. Then the saturated samples were compressed through radial direction in a hot press under pressure of 6 MPa, for 1 and 4 hours. The temperatures of press were 150°C and 175°C. Swelling (24h), recovery set ...
G Rassam, H Reza Taghiyari, B Jamnani, M Ali Khaje


Comparative Study of Heat Treatment of Beech Wood in Hot Water and Steam Medium
2010 - IRG/WP 10-40536
Heat treatment of wood is an effective method to improve the dimensional stability and durability against biodegradation. Heat treatments of beech wood in 2 different mediums (hot water and steam) in 180ºC were compared in physical, mechanical and anatomical properties. Mass loss in hydrothermally treated wood was higher than hygrothermally treated samples. Mechanical properties (MOR, MOE and CS)...
A Talaei, K Yaghoobi, A N Karimi


Optimization of oxalic acid production for bioleaching of metal components from CCA-treated wood by an unknown Polyporales sp. KUC8959
2010 - IRG/WP 10-50266
A brown-rot fungus, an unknown Polyporales sp. KUC8959, has recently been identified and proven as a prominent fungal species for bioremediation of CCA-treated wood wastes in our Lab. The fungus produced a larger amount of oxalic acid than other fungi tested, and removed 90 % or more of chromium, copper and arsenic from CCA-treated wood sawdust through bioleaching process. The bioleaching process ...
Yong-Seok Choi, Min-Ji Kim, Jae-Jin Kim, Gyu-Hyeok Kim


Climate change and wood protection, increasing demand of long life wood products and decreasing production of treated wood
2010 - IRG/WP 10-50269
Several new topics related to wood protection sector has appeared in Japan, as the awareness of climate change becomes bigger and bigger. The “Basic act for housing (2006)” and the “Long-life housing promotion act (2009)” were enforced to form a safe and high quality housing stock and to form a long-service-life housing respectively. Despite of the favorable background for wood protection ...
K Yamamoto, H Kato


Effects of global climate change on mould growth - Interactions of concern
2010 - IRG/WP 10-50270
An evident change in climate the last decades has been recorded, and combined effects of increased CO2, elevated temperature and altered precipitation regimes have been observed to represent a change to the fundamental drivers within ecosystems. Growth of moulds, both in nature and on man-made constructions and objects, will most likely increase due to changes in the climate. The survival, the rep...
L Ross Gobakken


Riverbed Construction Technology using Thinned Timbers for Carbon Dioxide Sink in Korea
2010 - IRG/WP 10-50271
The Climatic Change Convention is a big burden in limiting the energy usage like the blood of economy. The certification standard about the carbon storage of timbers after harvesting them is expected to be an important role in setting the goal for future reduction of the green house gas(CO2). The extension of a timber's life span through its preservation is one of technologies for carbon sink...
Dong-heub Lee, Won-Joung Hwang


Towards designing eco-friendly buildings with in-built termite protection
2010 - IRG/WP 10-50273
The increase in greenhouse gases, leading to global warming, is considered by a consistent scientific worldview not due to natural variation, but due to the growing concentration of carbon dioxide (CO2), methane (CH4) and other atmospheric pollutants. Global emissions of carbon dioxide from fossil fuel combustion and cement production rose from 22.6 billion tons in 1990 to an estimated 31.2 billio...
J R J French, B M Ahmed Shiday, B Maggiolo, D Maggiolo


Comparison of laboratory and semi-field tests for the estimation of leaching rates from treated wood
2010 - IRG/WP 10-50274
The authorization of wood preservative formulations in the European Union according to the Biocidal Products Directive (BPD) includes the assessment of environmental risks by the emission of active ingredients. This risk assessment includes scenarios for preserved wood (e.g. house scenario, noise barrier), in which the predicted environmental concentration (PEC) for soil and water is calculated, u...
N Morsing, M Klamer, B Seidel, J Wittenzellner, M Maier, J Habicht


Theoretic discussion on the way and driving forces of moisture migration in wood during vacuum drying
2011 - IRG/WP 10-40538
Most of parameters in conventional drying cannot explain a lot of phenomena appeared in vacuum condition, so it is necessary to further explore the moisture migration way and driving forces in wood under vacuum condition. For the water movement channel in wood is very narrow, the characteristic of heat and mass transfer in wood is similar to that in microscale. This article applies theory of liqui...
Zhengbin He, Xueli Yao, Liqiong Chen, Songlin Yi


Multilayer hot-press drying and chemical modifying of poplar wood with urea-formaldehyde prepolymer
2011 - IRG/WP 10-40539
The objective of this study was to determine the technology of chemical modifying and multilayer hot-press drying on poplar wood. The chemicals were impregnated into cell lumen space by pulse-dipping machine to improve the dimension stability and mechanical property of timber. The timbers were compressed and dried by the multilayer hot-press drying to increase the density of timber. Results indica...
Guofeng Wu, Yifei Jiang, Sheng Yao, Junwen


Determination of Equilibrium Moisture Content (EMC) of wood in the neighboring Countries of Iran
2011 - IRG/WP 10-40540
The mean value of annual temperature and relative humidity of 33 cities in Azerbaijan, Armenia, Turkmenistan, Afghanistan, Pakistan, Oman, United Arab Emirates, Bahrain, Qatar, Kuwait, Iraq and Turkey were determined using climatic data of the past 11 years. The EMC values were calculated using the Hailwood-Horrobin sorption model and its annual fluctuation, together with Temperature and relati...
A A Enayati, H Z Hosseinabadi


Increased sustainability for wood construction by recycling
2011 - IRG/WP 10-50275
Wood is the only renewable and certified industrially available construction material that has also unique opportunities as carbon storing, energy-independent and generally approved resource. However, if burning into energy is not counted, there are only few viable and competitive solutions for re-use or recycling of various wood products. The biggest challenge related to recycling of wood product...
H Heräjärvi, I Pirhonen, T Räty, P Saukkola


Previous Page | Next Page