Tebuconazole - A new triazole fungicide for wood preservation
1990 - IRG/WP 3629
The main cause of economic damage to timber and millwork worldwide are Basidiomycetes (brown and white rot). After testing a wide range of triazole derivatives for their effectiveness against decay fungi, Tebuconazole, a triazole compound, was selected. The physico-chemical, toxicological and ecotoxicological data of this substance are described. Tebuconazole is unleachable, light-stable, heat-sta...
R Gründlinger, O Exner


Microbial decay in an extremely durable Malaysian hardwood Belian (Eusideroxylon zwageri) - an overview
1997 - IRG/WP 97-10216
The heartwood of Belian (Eusideroxylon zwageri) is highly regarded among the naturally durable Malaysian hardwoods, and is therefore a choice timber for soilcontact use in the humid tropics such as untreated telecommunication poles, fence posts and railway sleepers. The high microbial resistance of the wood is evidenced by the mere superficial degradation observed in some pole samples after 20 yea...
A H H Wong, A P Singh


Research on wood protection at the Princes Risborough Laboratory 1975 & 1976
1977 - IRG/WP 3109
This paper is the latest of a 2-yearly series presenting a summarised account of the Laboratory's work in wood preservatives and related fields. The topics dealt with include: environmental studies on the usage of copper-chrome-arsenic and organic solvent preservatives; development of National and International Standards; recent developments in the preservation of external doors and windo...
J M Baker, R A Laidlaw, E R Miller, J G Savory


Movement of water through quaternary ammonium treated wood
1987 - IRG/WP 3440
Radiata pine sapwood stakes were treated with didodecyl methyl 1, 3 dichloropropenyl ammonium chloride and distearyl dimethyl ammonium chloride. Various ratios of these two chemicals were, tested to determine the extent of water movement through the treated wood. Measurements were taken of the amount of water moved through the wood, degree of wetting of various sectors of the stakes, and the distr...
P J Hayward, J Duff


Proposals for further co-operative studies on determining toxic values against wood-destroying Basidiomycetes
1985 - IRG/WP 2237
Document IRC/WP/2194 reported the status of the programme of co-operative experiments up to and including December 1982. During discussions at IRG-13 in Turkey members endorsed the decision to complete the programme of tests and conduct repeat tests. At IRG-14 in Brisbane the report was noted but no further action agreed. At IRG-15 in Sweden a number of interested parties in the European/Scandinav...
A F Bravery


Reduction of preservatives leaching from wood by the application of animal proteins
2005 - IRG/WP 05-30387
The investigations consisted in the estimation of the effectiveness of protein borates and protein propionates in wood preservation against Coniophora puteana. The estimation was made on the basis of mass losses caused by the test fungus action against treated wood which was subjected to leaching with water. The investigations were performed for Scots pine wood (Pinus sylvestris L.) treated with p...
B Mazela, I Ratajczak, M Bartkowiak


The evaluation of the effectiveness of wood preservatives by means of IUFRO's method for field tests with wooden stakes
1985 - IRG/WP 3348
Pinus elliottii and Eucalyptus saligna stakes treated with CCA-A, CCA-C, CCB, Cashew Nut Shell Oil and Benzotar solutions were exposed in seven test sites in Sao Paulo State, Brazil. After five years of exposure, between oil-borne preservatives Benzotar show better performance than CNSL (cashew nut shell liquid), and within waterborne preservatives the performance of CCB is not so good as that of ...
G A C Lopez, A M F Oliveira, E S Lepage


Evaluation of the biocide diffusion from treated wood in indoor air. Bibliographic study
1990 - IRG/WP 3584
Within the frame of the risk assessment of the wood preservation products for the Health, the treated wood risk particularly when it is installed in dwellings becomes most important. The European directive "Building materials" (89/106/CEE) mentions the basic requirements with the buildings must comply. Annexe l states in particular that "the building must be conceived and built in order not to bec...
A Pichard


Current status of AAC preservatives in New Zealand
1980 - IRG/WP 3141
Two types of alkylammonium compounds (AAC) have been approved as commercially acceptable wood preservatives by the NZ Timber Preservation Authority (TPA). They are alkyldimethylbenzyl ammonium chloride and alkyldimethylamine acetate, both of which must contain either (a) 70% alkyl chains of C12 + C14 and less than 10% of any other individual chain length, or (b) 85% alkyl chains of C12 + C14 with ...
J A Butcher


A comment on problem orientated research for the preservation industry
1984 - IRG/WP 3303
Wood preservation is a technological discipline, based upon a number of fundamental sciences, including biology and chemistry. The International Research Group on Wood Preservation (IRG) is presently structured to support the preservation industry, since IRG working groups attempt to strike a balance between fundamental aspects and technological needs. Over the years there has been an increasing r...
H Greaves


European standardization for wood preservation
1991 - IRG/WP 2365
Since the last IRG 21 conference in New-Zealand, there one meeting of the plenary committee and several meetings of working groups. The interprative documents prepared by CCE for expliciting the essential requirements of the CCE Directive on the construction products and specially: mechanical resistance and stability / hygiene, health and environment / safety in use are waited to valid the progra...
Anonymous


Synergistic combination of an antioxidant and wood preservative: a preliminary study
1998 - IRG/WP 98-30172
We previously proposed that extractives in highly durable angiosperm heartwood may protect wood against white-rot fungal colonization and subsequent degradation by a dual mechanism: extractives have some fungicidal activity and are also free radical scavengers (antioxidants) and thus interfere with the fungal free radical degradative mechanisms. We tested this hypothesis using the commercial bioci...
T Schultz, D D Nicholas, J Minn, K D McMurtrey, T H Fisher


An observation of seasoning, preservative treatment and storing of CCA treated 30 bangladeshi hardwood species for crossarms
1995 - IRG/WP 95-40058
Observed kiln seasoning, preservative pressure treatment and storing of CCA treated 30 Bangladeshi hardwood species for crossarms. It revealed that it was very difficult to kiln season and preservative pressure treatment of thirty species together in a single charge and found that when species of different specific gravity kiln season together there occur some objectionable seasoning degrades, and...
G N M Ilias, M D Rokib-ul-Hafiz


The high decay resistance in the sapwood of the naturally durable Malaysian hardwood Belian (Eusideroxylon zwageri)
2001 - IRG/WP 01-10410
It has long been assumed that the observed natural durability of the heartwood in certain timbers is perhaps associated with a relatively lower decay susceptibility also of the sapwood of these species. While the heartwood of Belian is reputedly highly decay resistant among the tropical hardwoods of Southeast Asia, laboratory decay tests reported in this paper have also confirmed the high decay re...
A A H Wong, A P Singh


Ponding of radiata pine (Pinus radiata) - 2. The effect of ponding on coating penetration into wood
1998 - IRG/WP 98-10249
Radiata pine (Pinus radiata) wood panels which had been ponded for periods ranging from 2 to 12 weeks, dried and subsequently coated with a primer and examined by light microscopy after staining sections with Sudan IV to enhance the contrast of the primer material. A correlation between the extent of ponding and the extent of coating penetration into wood was observed. The coating penetration var...
A P Singh, S S Gallagher, U Schmitt, B S Dawson, Yoon Soo Kim


Time limits for holding logs to achieve successful antisapstain treatment
1997 - IRG/WP 97-30126
The purpose of these trials was to determine the maximum time that logs can be left in winter and summer before treatment if sapstain, caused by pre-treatment infection, was to be prevented. Pre-treatment storage conditions representative of average temperature and humidity for the winter months of June, July and August, and of moderately severe summer conditions, for the Bay of Plenty, New Zealan...
D R Eden, R N Wakeling, C M Chittenden, J G Van der Waals, B Carpenter


A comparison between high and conventional incision densities for improving preservative treatment of Douglas-fir heartwood lumber
1993 - IRG/WP 93-40009
Incising is required for the preservative treatment of most wood species from the western United States; however, there is considerable debate about the density of incisions required to achieve adequate treatment. Previous studies have shown that the incision effect on treatment is relatively narrow, suggesting that incision densities should be significantly increased over current practices and st...
S T Lebow, J J Morrell


Accelerated diffusion treatment of sawn Sitka spruce grown in the UK
1986 - IRG/WP 3395
The treatment of 'green' sapwood and heartwood of Sitka spruce by diffusion methods was investigated. Steam/dip treatment processes gave increased solution uptakes and depths of penetration of copper in comparison with a simple dip treatment. Further investigation is required to reduce diffusion gradients with copper based formulations and to improve the penetration of '...
R J Murphy, D J Dickinson


Clean creosote - its development, and comparison with conventional high temperature creosote
1983 - IRG/WP 3235
Pigment emulsified creosote (PEC) is presently being tested and shows considerable stability in terms of water content, pigment level, pH, viscosity, rheological behaviour and microscopy. Timber samples from several eucalypt species have been treated with PEC and side matched samples treated with conventional high temperature creosote (HTC). The PEC treated specimens showed higher weight retention...
C W Chin, J B Watkins, H Greaves


Intraspecific variability of durability of Wapa courbaril (Eperua grandiflora) against Antrodia sp. and Coriolus versicolor: effect of radial and height position in the stem
2004 - IRG/WP 04-10531
The variation of a lesser-used species, Eperua grandiflora attacked by brown and white rot has been examined. Trees of this specie showed differences in their behaviour against the type of rot used and also showed evidence of intra and inter tree variation. The “tree” effect is very significant concerning natural resistance. In the same way, there is variation of durability observed according ...
N Amusant, J Beauchêne, M Fournier


Results on field stake tests against termite – Maximum for 8 years examination at Kumamoto in Japan
2003 - IRG/WP 03-10463
Various preservative treated or modified wood and charcoal painting stakes were tested in field, maximum for eight years in Kumamoto, distributed two main termite species, Coptotermes formosanus and Reticulitermes speratus. After two years in field, untreated sapwood of sugi (Cryptomeria japonica) were observed severe attacks by termites, but the preservative treated stakes were observed no signif...
K Suzuki


Assessing the importance of degradation mechanisms on the loss of effectiveness of wood preservatives
2000 - IRG/WP 00-20193
Accelerated ageing systems developed for application to samples in the laboratory prior to biological tests, should reflect those natural deterioration processes that are likely to occur in the hazard classes defined in EN 335-1. Losses through evaporation or the effects of leaching have been recognised, however their importance, relative to other mechanisms has not been quantified. Degradation me...
E D Suttie, R J Orsler, T Dearling


The Effect on Biological and Moisture Resistance of Epichlorohydrin Chemically Modified Wood
2002 - IRG/WP 02-40224
Southern pine solid wood and fiber were chemically modified with epichlorohydrin to help in understanding the role of moisture in the mechanism of biological effectiveness of chemically modified wood. The solid wood had weight gains from 11% to 34%, while the fiber had weight gains from 9% to 75%. After modification, part of the specimens were water leached for 2 weeks or extracted for 2 hours ...
R E Ibach, B-G Lee


Microwave digestion of preserved wood for the determination of Cu, Cr, As, B and P in quality control
1991 - IRG/WP 2364
A microwave digestion method for the determination of copper, chromium, arsenic, boron and phosphorus in preserved woods is described. Samples were digested with nitric acid in pressure-relief type teflon PFA vessels by microwave heating in a commercial laboratory microwave oven. Fast, efficient and complete digestion was achieved within 29 min for 12 samples. The digestion time compared favourabl...
N Bernth, L B Sheard


Bacterial degradation of Pinus radiata compression wood
1996 - IRG/WP 96-10153
An inspection of twelve year old, CCA-treated Pinus radiata wood from an industrial cooling tower showed extensive surface decay of wood. Electron microscopic examination of decaying compression wood indicated that compression wood cells were attacked exclusively by bacteria, which were of erosion and tunnelling types. As compared to the normal wood, compression wood appeared to be more resistance...