A field trial to assess the potential of antisapstain chemicals for long-term protection of sawn radiata pine
1986 - IRG/WP 3375
Seven chemical formulations were tested as antisapstain treatments for freshly sawn radiata pine sapwood (90x50 mm²). Each formulation was used with and without a water-repellent additive and was sprayed on to 1 m long boards. The boards were then stacked into "mini" packets and stored unprotected from the weather for 6 months. Haipen 50w (at 0.2 or 0.4% active) and NaPCP (1% active) plus 1.5% bo...
J A Drysdale


Moisture Adsorption Behaviour of Rubber Wood Decayed by Brown and White rot Fungi
2005 - IRG/WP 05-40306
Moisture adsorption behaviour of rubber wood blocks decayed by each brown rot and white rot fungi was studied. The adsorption isotherms of decayed wood were compared with the isotherm of undecayed wood. The wood decayed by brown rot adsorbed less moisture as compared to sound or undecayed wood at all humidity levels. No significant difference was observed in adsorption behaviour of white rot dec...
S S Chauhan, H C Nagaveni


Movement of chloropicrin, Vapam, and methylisothiocyanate in southern pine and Douglas fir timbers
1987 - IRG/WP 3410
Douglas fir and southern pine timbers, 15.2 x 15.2 x 426 cm³ (6-in x 6-in x 14-ft), were "inoculated" with brown-rot and white-rot fungi as vapor-sensing agents to evaluate the movement and distribution of fungitoxic concentrations of chloropicrin, Vapam, and methylisothiocyanate (MIT) over a 20-week period. Residual fumigant in timbers was determined by a bioassay with Gloeophyllum trabeum. The ...
T L Highley


Prevention of sapstain in logs using water barriers
1997 - IRG/WP 97-30147
Placing logs in ponds or under water sprinklers to keep moisture levels high enough to prevent oxygen tensions rising above inhibitory levels, is a proven method of preventing sapstain. The objective of this experiment was to determine if water barriers significantly reduce the rate of sapstain penetration into logs by maintaining moisture contents, and consequently oxygen tensions, at inhibitory ...
R N Wakeling, D R Eden, C M Chittenden, B Carpenter, I Dorset, J Wakeman, R Kuluz


Mycoparasitism by some white rot fungi on blue stain fungi in culture
1986 - IRG/WP 1304
When studying biological control of blue stain an interesting phenomenon of parasitism by some white rot fungi on blue stain fungi has been encountered. The majority of the 22 tested white rot fungi act parasitically upon blue stain fungi. The most interesting species among them is Bjerkandera adusta (Willd. ex Fr.) Karst., causing almost complete or complete decoloration of the hyphae of the blue...
R Benko, B Henningsson


The effect of kerfing on check formation in treated white spruce (Picea glauca) poles
1981 - IRG/WP 3167
62 white spruce poles, 6 m in length, were cut from full size utility poles commercially pressure treated with preservative. 21 of the poles were treated with pentachlorophenol, while of the remainder, all of which were treated with ammoniacal copper arsenate, 22 were kerfed and 19 were unkerfed. The poles were installed in the Westham Island field test site, near Vancouver, and inspected annually...
J N R Ruddick


Pretreatment decay in poles of Pinus sylvestris
1987 - IRG/WP 1329
Storage damage by blue stain and decay in poles before impregnation has been increasingly observed during recent years and there have been reports that salt-impregnated poles today are of lower quality because of incipient decay being increasingly common. The attacks may have started at the time of cutting and then continued during the period of seasoning at the plant, which could be as long as tw...
H Lundström, M-L Edlund


Antagonism of Gliocladium virens against wood decay fungi
1995 - IRG/WP 95-10102
Antagonistic abilities of a commercial biofungicide, Gliocladium virens (GL-21, Grace) were evaluated against three white-rot fungi, Trametes versicolor, Phlebia brevispora, Irpex lacteus, and three brown-rot fungi, Postia placenta, Neolentinus lepideus, Gloeophyllum trabeum. In dual culture of Gliocladium virens and wood decay fungi, Gliocladium virens rapidly overgrow the decay fungi and killed ...
T L Highley, L Ferge


Redistribution of boric acid in radiata pine during drying after preservative treatment
1993 - IRG/WP 93-40010
Samples of 100 x 50 mm² radiata pine were processed with a variety of options to produce dry, boron-treated wood. Concentrations of boric acid in the central one-ninth and in the whole of the wood cross-sections were determined by chemical analysis and compared. Diffusion treated material was dried by air, conventional kiln (70/60°C), or high temperature kiln (120/70°C). Four different predryin...
A J Bergervoet, D R Page, J A Drysdale


Analysis of the boron content of preservative treated oak and pitch pine heartwood before and after leaching
1992 - IRG/WP 92-3697
Studies to determine the effects, if any, of a variety of boron formulations on heartwood of English oak and American Pitch pine have been previously reported (King et al (1991)). Small wood blocks were treated, at 10°C or 45°C, with borax, polybor or Boracol 20 for periods of 1 month or 4 months then analysed or continuously leached with tap water for a period of 1 month. Reported results showe...
S McCutcheon, G M Smith, J W Palfreyman, B King


Safe handling of solvents in relation to classification and labelling
1990 - IRG/WP 3569
The classification and labelling of chemical products, safety data sheets and personal protective equipment are topics which at present are given a very high priority in Denmark. The area is very large and may seem extremely difficult to comprehend. The frequent publication of acts and announcements from the authorities does not make the work any easier. In the following I will try explain how we ...
J Haugaard


Effect of soil chemistry and physical properties on wood preservative leaching
1998 - IRG/WP 98-50111
When treated wood is placed in contact with soil, complicated mass transfer and chemical reactions occur which causes the preservative components to leach from the wood. There are several factors that are known to affect the amount of chemical leached from wood. These are properties of the preservative and carrier, preservative retention, degree of fixation, exposure time, grain orientation, surfa...
Joan-Hao Wang, D D Nicholas, L S Sites, D E Pettry


The control and pretreatment decay in air seasoning Scots and Corsican pine poles in England
1990 - IRG/WP 1451
Previous work clearly showed that air-seasoned, British grown Scots and Corsican pine poles are subject to serious pretreatment decay. In order to control these infections a range of pretreatments are currently being investigated. One series of treatments is designed not only to control decay but also allow the development of mould and stain fungi in order to achieve the desired increases in poros...
D J Dickinson, A R Zahora, A P Dodson


CCA type C depletion of Southern yellow pine utility poles
1995 - IRG/WP 95-50049
Depletion and redistribution of preservative components were evaluated on five CCA-C treated poles in service for over six years in Conley, Georgia. A statistical approach was taken in which retentions below ground were compared to retentions above ground due to a lack of initial data on individual poles. It was hypothesized that the below ground retentions should be lower than the corresponding a...
P D Osborne, R F Fox


Preliminary indications of the natural durability of Spruce bark board
1999 - IRG/WP 99-10312
A board material made from pressed bark, with no added adhesive, has been developed by Forintek's composites group and tested for durability by Forintek's treated-wood group and the University of Hawaii. This material was also manufactured with veneers in a one-step process. Since one role of bark on the tree is protection against pests and diseases, barkboard was expected to hav...
P I Morris, J K Grace, G E Troughton


Upgrading the fungal resistance of OSB
1999 - IRG/WP 99-40138
There is a perception that oriented strand board (OSB) is less resistant to fungl than plywood under conditions of moderate exposure to moisture. Douglas fir-faced plywood (DFP) has been suggested as a benchmark for acceptable durability under such conditions. This project was initiated to determine the minimum level of low-toxicity chemical treatment needed to upgrade the fungal resistance of OSB...
P I Morris, J E Clark, D Minchin, R Wellwood


Evaluation of hydroxamates as wood preservatives
2004 - IRG/WP 04-30330
Fungicidal activity of different hydroxamates was investigated by laboratory malt-agar block tests to evaluate their potential as wood preservatives. Results obtained indicate that benzohydroxamic acids substituted or not on the aromatic nuclei were unable to protect wood blocks against the white rot fungus Coriolus versicolor while 2-hydroxypyridine-N-oxide (2-HPNO) possesses an interesting activ...
P Gérardin, S Dumarçay, E Gelhaye, A Mbamba, V Mussavu


The potential of high pressure pulsation processes to treat white spruce lumber with water-borne preservatives
1988 - IRG/WP 3471
Laboratory work using end sealed 4x8x46 cm³ white spruce samples has been done to explore the suitability of three variants of a 2.1 MPa pulsation process for the impregnation of white spruce with CCA. The results showed that the process improved significantly the penetration of the preservatives and reduced significantly cell collapse, when compared with the results of treatment using a 2.1 MPa ...
J P Hösli, J N R Ruddick


Preservation of basidiomycete hyphae in ancient waterlogged wood materials
1992 - IRG/WP 92-1536
Studies on waterlogged archaeological wood show that basidiomycete hyphae may persist as long as 800 years. In two pine wood samples with Phellinus pini heartrot, one from the foremast of the ship Vasa and the other from a bulwark constructed in the first part of the 12th century, numerous resin covered hyphae were observed. Hyphae with clamp connections that were associated with brown and white r...
T Nilsson, G F Daniel


Protection of pine sawtimber and sawn timber against blue stain in Poland
1983 - IRG/WP 3193
The purpose of this paper is the synthesis of more important results of basic and applied research that have been grouped in the following problems: 1.: Fungi causing blue stain in the pine wood, occurring in Poland. 2.: Moisture content changes of pine sawtimber and sawn timber as the factor of blue stain producing fungi development. 3.: Effect of sapwood moisture content on the degree of wood st...
E Tarocinski, M H Zielinski


Antagonism of Scytalidium lignicola against wood decay fungi
1989 - IRG/WP 1392
Antagonistic abilities of Scytalidium lignicola against white- and brown-rot wood decay fungi were evaluated. Scytalidium lignicola did not produce inhibition zones but overgrew the decay fungi on a malt-agar medium and in most cases killed them. Pretreatment of Douglas-fir and Southern pine blocks with Scytalidium lignicola prevented decay. Blocks that were heated or treated with propylene oxide ...
T L Highley


Biological Control of Bluestain - Log Field Trials in Canada
2002 - IRG/WP 02-10423
In the summer of 2000 we ran two field experiments (in Alberta and British Columbia) to test the feasibility of using an albino bluestain isolate (Cartapip97TM) to protect lodgepole pine logs from being stained by wild-type bluestain fungi. Results showed that Cartapip applied at the recommended concentration significantly reduced the amount of stain found in the Alberta trials. Cartapip applie...
A Uzunovic, D Minchin, A Byrne


Immunolabelling studies on the detection of enzymes during the degradation of wood by Phanerochaete chrysosporium
1988 - IRG/WP 1364
The degradation of lignin in native lignocellulosic substrates by white rot fungi is poorly understood. Biochemical studies have shown the involvement of a number extracellular ligninolytic enzymes released by white rot fungi which are capable of the oxidative conversion of DHP's (lignin model compounds) in vitro, but to date conclusive evidence for occurrence of these enzymes in wood und...
G F Daniel, T Nilsson, B Pettersson


Evaporation and redistribution of creosote in pine poles during storage
1996 - IRG/WP 96-50064
During the work with European standards for pressure treated wood, it has been questioned if the lapse of time between impregnation and chemical analysis of the retention is critical, especially for creosote. "The Norwegian Control Scheme for Preservative Treated Wood" has not discovered any retention problems analysing CCA preservatives in wood. If the lapse of time between impregnation with creo...
F G Evans, B Nossen


Multiple-Phase Pressure (MPP) Process: One-stage CCA treatment and accelerated fixation process. 3. Effect of process variables on sapwood treatment and CCA fixation.
1998 - IRG/WP 98-40114
The Multiple-Phase Pressure (MPP) Process achieves treatment and fixation as combined process using hot CCA, within a 2-3 hour time-frame. Timber is treated to saturation with hot CCA using an empty cell process. During the pneumatic pressure phase, hot solution is held in the wood in an otherwise liquid-free treatment vessel until fixation is >95% complete. This report details a factorial des...
H Pearson, K Nasheri, J A Drysdale, G Durbin, M E Hedley