IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 2591 documents. Displaying 25 entries per page.


Investigations into the use of Maleic Anhydride/Sodium Hypophosphite as a Wood Modification Process
2020 - IRG/WP 20-40891
The formation of crosslinked bonds between wood constituents is believed to be an effective way to stabilize wood against wet conditions. The possibility to use maleic anhydride (MA) combined with sodium hypophosphite (SHP) as crosslinking agents was studied, using Scots pine sapwood and a model compound. The modified wood showed weight gain and bulking effect after treatment and subsequent Soxhle...
I Kim, D Jones, O Karlsson, D Sandberg, O N Antzutkin, F Ullah Shah


Biological durability of sapling wood
2020 - IRG/WP 20-10967
Sapling-wood products from different wood species such as willow (Salix spp.) and Common hazel (Corylus avellana) are frequently used for gardening and outdoor decoration purposes. Remaining bark is suggested to provide additional biological durability. Even for temporary outdoor use it seemed questionable that durability of juvenile sapwood can provide acceptably long service lives of horticultur...
C Brischke, L Emmerich, D G B Nienaber, S Bollmus


Longterm Performance of Treated Timbers in Marine Exposures
2020 - IRG/WP 20-10969
The performance of preservative-treated or modified woods in marine exposures was evaluated at test sites in Newport, Oregon, USA and Brisbane, Queensland, Australia. All samples have exhibited excellent performance at the Newport, Oregon site, while attack was more aggressive at the sub-tropical Brisbane site. Acetylated wood as well as samples treated with 7.3% chromated copper arsenate (CCA-T...
M Konkler, A R Zahora, J Norton, J J Morrell


Modelling decay rates of timber exposed above ground on four different continents
2020 - IRG/WP 20-20670
Durability performance data from an international decking trial were analysed to explore relationships with climate variables, particularly those related to temperature and rainfall. Matched decking samples of slash pine (Pinus elliottii) sapwood and heartwood, spotted gum (Corymbia citriodora), Norway spruce (Picea abies) and Scots pine sapwood (Pinus sylvestris) were exposed to the weather above...
L P Francis, J J Morrell, C Brischke, P B Van Niekerk, J Norton


The role of specimen format in wood durability testing
2020 - IRG/WP 20-20672
The experimental basis for testing the biological durability of wood are often incubation experiments with wood-destroying basidiomycetes. Numerous parameters can affect the mass loss by fungal decay (MLF) in laboratory durability tests and therefore being decisive for the resulting durability classification. Among others, the dimension of the wood specimen and the time of incubation impact on fun...
C Brischke, L K Grünwald, S Bollmus


Monitoring uptake and penetration of pesticides during impregnation of pine (Pinus sylvestris) and spruce (Picea abies) wood with bio-based microemulsion gel formulations
2020 - IRG/WP 20-30756
Even in dry state wood is susceptible to biological degradation. Preservation against biological decay in exposed conditions is conventionally achieved by impregnating the wood with pesticides applied at professional and industrial levels. Impregnation of wood with preservatives is a complex process that involves wood macro- and microstructure, and the physical characteristics of woods. Here we fo...
D Messaoudi, K Ruel, J-P Joseleau


A summary of decay performance with citric acid and sorbitol modification
2020 - IRG/WP 20-40898
Application of wood-based products as construction materials is one piece of the big puzzle to mitigate climate change. Wood is susceptible to biological deterioration. Environmentally motivated legislation is making the use of biocides less attractive from a commercial perspective. Ideally, a wood modification technology should be of low cost, water based and make use of thermal curing. This rese...
G Alfredsen, E Larnøy, G Beck, J Biørnstad, L R Gobakken, C A S Hill, A Treu


Durability of acetylated Radiata pine: Laboratory tests and performance in practice
2020 - IRG/WP 20-40899
Wood acetylation is an established process to enhance biological durability and dimensional stability of lower valuable wood species without the use of biocides. Acetylated Radiata pine (ACCOYA® wood) has been on the market for more than 10 years now, starting in 2007. Numerous lab tests have confirmed the high durability of acetylated Radiata pine. Here, additional data with four Radiata pine ...
K Jacobs, W Scheiding, B Weiß


Assessing the risk of marine borer attack of the timber trestles and decay of timber above the intertidal zone of the Barmouth Viaduct
2021 - IRG/WP 21-10974
The Barmouth Viaduct is a Grade II* listed structure which carries the single track of the Dovey Junction to Pwllheli line and footway over the Mawddach estuary. It is in a marine environment where timber below the high tide mark is at most risk in Use Class 5 and all timber above in Use Class 3.2, permanently exposed to the risk of wetting. The structure consists of a timber trestle viaduct of ...
J R Williams


Comparison of AE-apparatus for detection of activity of Old house borer larvae, including reality check
2021 - IRG/WP 21-10981
As part of the German funded project ‘InsectDetect’ comparative measurements were done with three different Acoustic-Emission-(AE)-apparatus on 14 pine beams in order to assess presence of active attack by the Old house borer (Hylotrupes bajulus (L.)). In all beams active attack was measured, though in varying intensity. This was corroborated by completely dissecting 10 of the beams. All thre...
J Creemers, B Plinke, U Noldt


Studies on the material resistance and moisture dynamics of Douglas fir and Sitka spruce from Slovenia
2021 - IRG/WP 21-20677
Wood in outdoor applications is subject to various decomposition factors. Wood degradation can be prevented by construction details, biocide protection of wood, wood modification, or selection of naturally durable wood species. Unfortunately, the majority of timber species in Europe do not have naturally durable wood. Imported tree species represent a new pool from which we can draw wood species w...
M Humar, B Lesar, D Krzisnik, E Kerzic, R Brus


Estimation of residual compressive strength on cross laminated timber with biodeterioration damage
2021 - IRG/WP 21-40918
CLT is susceptible to biodeterioration such as fungal decay and termite attack during long-term use for buildings. It is necessary to know the residual strength performance of biodegraded CLT for estimating future performance and aging of CLT. In this study, compression tests of CLT damaged by brown rot fungi and termites were conducted to clarify the relationship between residual strength and mas...
R Inoue, T Mori, K Kambara, W Ohmura


Effect of a Water Repellent Treatment on Moisture Behavior of Three Australian Hardwoods: A Preliminary Report
2021 - IRG/WP 21-40921
Wood is inherently hygroscopic and will sorb moisture either directly from the atmosphere or via capillary action. Moisture can have marked effects on wood properties and repeated wetting and drying creates dimensional changes that lead to physical damage. Exposure to elevated moisture levels also increases the risk of fungal attack. Wood preservatives have long been used to minimize the risk of ...
B Hassan, J J Morrell, K Wood


Evaluation of decay and energy properties from thermally modified biomasses during fungal deterioration by NIR-spectrometry
2021 - IRG/WP 21-40922
This study is focused on the prediction of fungal weight loss (WL) and high heating value (HHV) from raw and torrefied waste lignocellulosic feedstocks, according to their exposure duration to wood-destroying fungi, using near infrared spectroscopy (NIR) and chemometrics models. Sugarcane bagasse, coffee husk, eucalyptus and pine shavings were torrefied at 290 °C in a screw reactor, during 5, 7...
B de Freitas Homem de Faria, P Santana Barbosa, J Valente Roque, A de Cassia Oliveira Carneiro, P Rousset, K Candelier, R F Teofilo


Application of suberin fatty acids extracted from birch bark for wood coating
2021 - IRG/WP 21-40914
It is well known that chemical modifications to improve decay resistance also reduce the equilibrium moisture content (EMC) of wood. The mechanism of this action, however, has been the subject of much debate. Several groups have suggested that decay resistance is a result of lower diffusion rates of fungal degradation agents through the wood cell wall. A recent paper explained the fundamental prin...
A Kumar, Risto Korpinen, Veikko Möttönen


Dynamics of fungi colonization on the surface of Scots pine wood during natural weathering in different European climate zones
2022 - IRG/WP 22-10984
Wood The presence of fungi leads to biomaterial decay and/or changes in aesthetical appeal. The start of fungi colonization as well as the following growth on wood are primarily influenced by four factors: ambient temperature, moisture history of the object, access to oxygen, and intrinsic properties of the exposed wood, considered here as a source of nutrients for microorganisms. A prevalence of ...
F Poohphajai, O Myronycheva, O Karlsson, L Rautkari, J Sandak, A Sandak


Decay capacity and degradation patterns of Xylaria hypoxylon on different wood species
2022 - IRG/WP 22-10985
A host of physical and environmental factors may influence fungal decay including the wood substrate, temperature, moisture, oxygen, light, pH, and nitrogen. Understanding the effects of these factors on fungal decay is important for the effective utilization of wood decay fungi in biotechnological processes and for understanding the role of these organisms in global carbon cycling. The ascomycete...
E Bari, G Daniel, A Singh, J J Morrell


The effect of sapwood and heartwood differences on durability of short rotation teak wood
2022 - IRG/WP 22-10991
Short rotation teak has been developed to overcome the limited supply of long rotation teak. The aim of this study was to investigate the effect of sapwood and heartwood differences on durability of short rotation teak. The following basic properties were studied: extractive content, dimensional stability (volumetric swelling and water uptake), decay resistance, and termite resistance. The result...
R Martha, M Mubarok, F O Akong, B George, C Gérardin, S Dumarçay, I S Rahayu, I Batubara, W Darmawan, P Gérardin


Evaluation of weathering and termite resistance of the Myoung-oil as a Korean traditional coating agent
2022 - IRG/WP 22-10996
This study investigated the applicability of Myoung-oil (MO) as an eco-friendly preservative of Korean wooden cultural properties and buildings. Wood test specimens painted with various concentrations of MO were exposed in the external environment. Then color change and wettability of the wood surface were evaluated and compared depending on the exposure time. As a result of exposure for 12 months...
S-M Yoon, Y Park, W-S Jeon, H-M Lee, J-G Park, K Dal Nam, W-J Hwang


Introduction to the project ‘Deterioration and decay of wooden cultural heritage in Arctic and Alpine environments’ (ArcticAlpineDecay)
2022 - IRG/WP 22-10997
The Arctic is already affected by climate change, and this is expected to accelerate over the coming decades. Alpine regions in Norway are projected to face similar challenges. Current knowledge on Norwegian wooden cultural heritage in Arctic and Alpine regions is scattered and contains significant knowledge gaps. Historically, - scientists, sectorial governance, tourist trade and commerce have ma...
G Alfredsen, L Ross, A W Hegnes, M S Austigard, J Mattsson, N B Pedersen, A Sinitsyn, V V Martens, A-C Flyen


Studies into the effect of soil type and soil layer on the in-ground decay of European beech
2022 - IRG/WP 22-20681
In this study, European beech (Fagus sylvatica L.) specimens were exposed to three different soil types; Podsol (Podzol), Braunerde (Cambisol), and Pararendzina (Regosol), in adapted terrestrial microcosm (TMC) tests according to CEN/TS 15083-2 (2005). Soils were sampled (250 mm deep) from field sites and separated into their constituent layers to deliver three TMC setups; mineral soil layer only ...
B N Marais, S Kovacs, M Jansen, C Brischke


Measurement of copper concentration in Cu-HDO treating solutions by handheld XRF
2022 - IRG/WP 22-20685
Copper based preservatives diluted in water dominate the wood preservative industry around the world. Periodically measurements and adjustments of the concentration of treating solutions must be performed as a part of the quality control at the treatment plant to achieve desired quality of the preservative treated wood. Many analytical methods are time consuming and must be performed under laborat...
P O Flaete


Using satellite-retrieved soil moisture data to model the decay risk of in-ground timber
2022 - IRG/WP 22-20689
Satellite-derived soil moisture data from the Soil Moisture Active Passive (SMAP) was extracted for a 9 x 9 km point grid over Europe. The data was then used as input to a dose-response wood decay model based on terrestrial microcosm (TMC) tests. The resulting hazard map plotted dose as an indicator of in-ground wood decay based on differences in annual temperature and soil moisture characteristic...
P B van Niekerk, M Schönauer, B N Marais, C Brischke


Analysis of wooden shingles after seven years of exposure
2022 - IRG/WP 22-20690
Wood is a traditional roofing material in the Alpine regions. In the 17th century, wooden roofing was typically used on more important buildings. Still, today it is predominately used on huts and houses in the hilly regions of northern and north-western Slovenia. Because wooden roofing is expensive, we investigated the possibility of extending the service life of the roofing through impregnation a...
M Humar, B Lesar, D Kržišnik, E Keržič, B Jemec


Brief introduction to a research project on preparations of various paste formulations from boron, fluoride and copper for supplemental treatments
2022 - IRG/WP 22-30759
Wood preservatives to be used for supplemental purposes are present in various forms such as powders, liquids, rods, pastes, or gels. Boron compounds have been receiving a lot of attention in supplemental treatments since they have good mobility in wood. Application of boron compounds via internal treatments is vital to stop decay to be occurred inside the wood since large wood elements are too th...
E E Soytürk, D Bakır, E Terzi, C Köse, S N Kartal


Previous Page | Next Page