IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 2591 documents. Displaying 25 entries per page.


Effects of air-seasoning on fungal colonization and wood strength of Douglas fir poles
1987 - IRG/WP 1315
Air seasoning economically reduces the moisture content of Douglas fir poles before pressure treatment with preservatives. Advanced decay in poles in service has resulted when decay fungi (Basidiomycetes) colonized poles during air-seasoning and survived the treatment process. These problems have led to recommendations to severely limit this practice. To determine the role of these fungi in peeled...
J J Morrell, M E Corden, R D Graham, B L Kropp, P Przybylowicz, S M Smith, C A Sexton


The susceptibility of acetylated Pinus radiata to mould and stain fungi
1992 - IRG/WP 92-1548
The aim of this investigation was to determine the effect of 5, 10, 15 and 20 percent acetylation weight gains on the susceptibility of Pinus radiata sapwood to mould and stain fungi, and to establish if an acrylic paint, an oil-based stain and a water repellant gave superior protection from fungal growth on wood treated to 20% acetylation weight gain, compared to untreated wood. One treatment set...
R N Wakeling, D V Plackett, D R Cronshaw


Effect of substrate type and moisture requirements in relation to colony initiation in two carpenter ant species
1999 - IRG/WP 99-10320
Conditions necessary for optimal colony initiation or the rate of initial colony expansion by early brood in the carpenter ant species Camponotus modoc and C. vicinus on various substrates conditioned to different moisture contents were studied. Camponotus modoc and Camponotus vicinus queens were placed in Douglas-fir, western red cedar and Styrofoam® blocks conditioned in sealed chambers at 70% ...
M E Mankowski, J J Morrell


Antisapstain field trials of NeXgen in New Zealand
1997 - IRG/WP 97-30145
This document covers the results of summer and winter log trials of NeXgen, an antisapstain formulation containing methylene bis thiocyanate plus chlorothalonil. Log billets (20 - 25cm diameter) were stripped of bark using a commercial maul debarker and antisapstain treated within 8 hours of felling by dip application. Billets were stored in a pole barn and assessed for internal sapstain and decay...
R N Wakeling, T L Woods, D R Eden, C M Chittenden, B Carpenter


Decay evaluation of the effectiveness of a LOSP envelope treatment in eucalypt and meranti heartwoods for window joinery
1996 - IRG/WP 96-30099
The effectiveness and penetration in heartwood boards of an LOSP formulation containing TBTN was examined by determining decay resistance to the white-rot fungus Perenniporia tephropora. Boards, one metre long, of Eucalyptus regnans, Eucalyptus delegatensis, Eucalyptus obliqua and Eucalyptus sieberi were treated, along with boards of 'light' and 'dark' meranti. ...
L J Cookson, A Trajstman


Resistance of two commercial cement-bonded rubberwood particle composites to decay and termites
2000 - IRG/WP 00-10338
Two types of cement-bonded rubberwood (Hevea brasiliensis) particle composites (tradenames: Cemboard and Primaflex in Malaysia), were evaluated for termite resistance (prevalent termite: Coptotermes curvignathus) in the field, and decay resistance (test white rot fungi: Schizophyllum commune and Pycnoporus sanguineus; test brown rot fungus: Gloeophyllum trabeum; test soft rot fungi: Phialophora fa...
A A H Wong


The accelerated L-joint test method for determination of the out of ground natural durability
1998 - IRG/WP 98-20146
The accelerated L-joint test incorporates a moistening device and uses a close end water trap in an open joint connection with a laminated tenon member consisting of the perishable reference wood species scots pine sapwood and beech. After one year of exposure it is possible to show a distinct identification of natural durability classes 4 and 5 against the more durable wood species. Both weight ...
J Van Acker, C Brauwers, M Stevens


Chromated copper arsenate preservative treatment of hardwoods. Part 2: leaching performance of seven North American hardwoods
1997 - IRG/WP 97-30132
Seven North American hardwood species were treated with 2% CCA-C solution and fixed at temperatures of 21°C and 50°C and conditions of high relative humidity (95%) as described in Part 1 of this presentation. Red pine (Pinus resinosa) was included as a softwood for comparison. Adequately fixed wood blocks (99.9% chromium fixation) were exposed to leaching tests according to AWPA E11-87 test. Par...
T Stevanovic-Janezic, P A Cooper, Y T Ung


Aureobasidium or Hormonema? A Genetic Approach.
2004 - IRG/WP 04-10529
Aureobasidium pullulans is the main organism causing disfigurement of coatings on wood and the surface of exposed timber. This disfigurement of timber in-service is referred to as “bluestain in-service”. A. pullulans is also associated with the sapstaining of dead wood in the forest and in-service. A. pullulans is noted for its highly variable growth forms (polymorphisms). This variability pre...
M J Ray, D J Dickinson, M Buck


Development process of a new anti-sapstain formulation and its present status with the relevant problems
2001 - IRG/WP 01-30257
An anti-sapstain formulation, which contains 2-(thiocyanomethylthio)benzothiazol (TCMTB) and methylene-bis-thiocyanate (MBT) as active ingredients, was developed by a technical agreement with Buckman Laboratories (Memphis, TN, USA) as an alternative to chlorinated phenols for the Japanese market. The formulation was commercialized as BAM 12 years ago. As anti-sapstain treatment is commonly conduct...
K Nobashi, Y Nomura, K Tsunoda


Effect of species composition of preservative-treated Douglas fir plywood on its decay resistance
1978 - IRG/WP 2114
Plywood is now commonly used for constructional purposes in environmental situations where decay by wood-destroying fungi can be a considerable risk. However there seems to be a lack of understanding of the relative durability of plywood, both untreated and when treated with wood preservatives. Part of the reason for this situation has been the difficulty of carrying out laboratory decay tests on ...
R S Smith, P Balcaen


Isolation and identification of non-decay fungi affecting the performance of alkylammonium compounds
1993 - IRG/WP 93-10020
The isolation of DDAC tolerant fungi was carried out on lumber treated with a range of antisapstain chemicals containing DDAC as one of their active ingredients. The tolerant fungi were selected by using malt media spiked with DDAC (100 and 2500 ppm). Isolations were tentatively identified into a range of fungi commonly found associated with wood deterioration (i.e. Penicillium sp. and Trichoderma...
A K Doyle, J N R Ruddick


Estimation of the impregnation degree of pine wood by the distribution analysis of active ions concentration in the cross-section
1999 - IRG/WP 99-20174
Samples in the form of pine wood rollers of diversified moisture content of ca. 50, 28 and 12% were impregnated with a water solution of the mixture type CCB with the use of the full-cell process. Moisture content was determined in individual layers from the girth to the pith. In the same way the concentrations of copper and chromium ions with the use of the spectrophotometric method and recalcula...
K Lutomski, B Mazela


The performance of chlorothalonil after 4.5 years in the accelerated field simulator
1994 - IRG/WP 94-30041
The decay resistance of chlorothalonil in oil was examined in an accelerated field simulator (AFS). Pinus radiata D. Don and Eucalyptus regnans F. Muell. sapwood stakes were treated, placed in soil in the AFS, and monitored over 4.5 years. CCA type C treated stakes were included for comparison. Water and toluene treated control stakes were heavily decayed after 1-2.5 years. Oil treated controls, t...
L J Cookson


Extracellular mucilage (ECM) in wood decay basidiomycetes
2002 - IRG/WP 02-10439
The ability of wood decay basidiomycetes to produce extracellular mucilage (ECM) and its relationship with total biomass production is being investigated. Growth and ECM production by the brown-rot fungus Gloeophyllum trabeum (FPRL 108 N) and the white-rot fungus Coriolus versicolor (CTB 863 A) was assessed in liquid culture under different conditions and in the presence of the fungicide cyprocona...
D Vesentini, D J Dickinson, R J Murphy


Evidence for actinomycete degradation of wood cell walls
1990 - IRG/WP 1444
Several unique patterns of degradation occurring in wood cell walls have been observed in wooden stakes inserted in unsterile soil in the laboratory. Some of the patterns have also been observed in coniferous wood taken from forest floors. All the observed attack types occur within wood cell walls, mainly within the S2 layer. Attack is characterised by channels of varying diameter or small fusifor...
T Nilsson, G F Daniel, S L Bardage


Basilit CCFZ. Further studies on ecotoxicological behaviour
1992 - IRG/WP 92-3722
Basilit CCFZ is a new developed water based preservative for the protection of timber in hazard class 4 and 5 (ground-, fresh- and salt-water contact). The active components of this salt are copper, chromium, zinc and fluorine. In addition to primarily studies on the acute toxicity against organisms of the aquatic food chain a long term ecotoxicological study was performed. In a prolonged toxicity...
H W Wegen


Arbeitsverfahren zum Herstellen und mikroskopischen Auswerten von Dünnschnitten aus Holz-Bohrkernen. [Working method for producing and evaluating microscopically thin cuts of bore samples]
1980 - IRG/WP 2133
Bore samples are important specimens; e.g. they are in use to investigate poles in service. On the basis of known methods of microtomy a technique is described which permits the production of longitudinal cuts from bore samples. For this purpose, the bore sample is glued onto a mounting; the surface of cut is coated with a polystyrene solution. The cut thus consolidated can be stained, drained, an...
S Cymorek


The ecotoxicology assessment of wood preservatives and their active ingredients by means of germination tests using cress - A critical consideration
1999 - IRG/WP 99-50125
With putting the Biocidal Products Directive 98/08/EC (BPD) in place an environmental risk assessment for wood preservatives and impregnated timber is requested. To assess possible risks, suitable test methods are required, which reveal the ecotoxicological profile including environmental fate and behaviour of treated commodities. Germination and growth tests could contribute to the determination ...
P Jüngel, A O Rapp, E Melcher


Investigations into the biology of Meruliporia incrassata
2004 - IRG/WP 04-10508
The dry rot fungus Meruliporia incrassata (Berk. and Curt.) Murr. is a highly destructive brown rot wood decay fungus and is a significant pest of wooden structures. The fungus, know commonly as ‘Poria’, is characterized in culture by strand mycelium and skin-like surface mycelium. In structural environments it is found to produce prominent water conducting rhizomorphs, is a copious spore prod...
J Jellison, C Howell, B Goodell, S L Quarles


Further studies on soft rot decay in CCA treated Eucalyptus power transmission poles in Queensland, Australia
1980 - IRG/WP 1115
Preliminary results on the examination of fungi isolated from CCA treated Eucalyptus power transmission poles were presented at the 10th Annual IRG Meeting. Since then further examination and identification of fungal isolates has been completed together with screening tests for wood decay ability and tolerance to creosote and CCA and its components. Chemical analyses for CCA retention have also be...
L E Leightley


Eradication of wood decay fungi by means of radio frequency
1998 - IRG/WP 98-10292
High frequency electromagnetic fields i.e. radio frequency (RF) are used in wood industry for heating, gluing and bending of wood and are also appropriate for eradicating of wood decay fungi and insects. We investigated the effects of RF exposure on wood samples which were in vitro infected by Coniophora puteana, Gloeophyllum trabeum and Lentinus lepideus. For each fungus, the lethal temperature a...
F Pohleven, J Resnik, A Kobe


Silicic acid-Boric acid complexes as wood preservatives
2001 - IRG/WP 01-30273
A silicic acid monomer aqueous solution (SAMS) or colloidal silicic acid solution (CSAS) was combined with various metal compounds or boric acid. Agents where SAMS or CSAS was combined with boric acid gave good protection against decay caused by the brown-rot fungus Fomitopsis palustris, the treated wood (Cryptomera japonica D. Don) specimens after the leaching test maintained a high resistance to...
H Yamaguchi


Report on the efficacy and performance of the insecticide candidate termiticide in H2 field trials
2004 - IRG/WP 04-10516
This paper explains the field results of phenol pyrazole treated timber against in an above ground mound colonies of Coptotermes acinaciformis (Froggatt). C. acinaciformis (‘termites’) are the major pest of human structures throughout tropical and sub tropical regions, causing billions of dollars in damage to timber-in-service worldwide. The result of this field test have shown that candidate ...
B M Ahmed, P Vinden, J Hann, J R J French


The influence of staining fungi on the decay resistance of wood treated with alkylammonium compounds
1984 - IRG/WP 3308
Although found to be very effective in laboratory tests, alkylammonium compounds (AAC's) have failed to perform as well in field stake tests. Examination of leachability showed that this was not the cause. The present study investigated the possibility that staining fungi, (which have been observed to rapidly infect the field stakes), degrade the AAC wood preservative. Soil-blocks were tr...
J N R Ruddick


Previous Page | Next Page