The efficacy of remedial treatments for controlling fungal decay in window millwork used in the United States
1987 - IRG/WP 3432
Conventional window millwork was subjected to basidiomycete decay by inoculation and sampled for active growth of the decay fungus before and eight months after remedial preservative treatment with fused disodium octaborate rods (IMPEL) at boric acid levels of 1.5 and 4.0 kg/m³ or liquid bifluoride injections (IMPROSOL) at 1 kg/m³. The elimination of decay fungus after remedial treatment was nea...
M G Dietz, E L Schmidt


An electron spin resonance study of manganese changes in wood decayed by the brown-rot fungus, Postia placenta
1988 - IRG/WP 1359
Electron spin resonance (ESR) spectrometry was used to examine wood decay by the brown-rot fungus, Postia placenta. Wood slivers of Douglas-fir, white fir, redwood, sweetgum and yellow poplar were incubated for 4 weeks in custom-made quartz ESR tubes with or without Postia placenta. In all wood species without fungus, a weak partially resolved signal (about g=2, presumably due to manganese) was de...
B Illman, D C Meinholtz, T L Highley


Assessment of the toxicity of some copper-, zinc- and boron-based wood preservatives to the cellar fungus Coniophora cerebella Schröet
1974 - IRG/WP 242
This article reports the use of a method based on the determination of the probability of the protection of timber against destruction by fungi. By converting the probability values to probit values and plotting them as a function of the amount of preservative retained in the timber, curves of the toxic effect are obtained, enabling any timber protection probability to be assessed....
V N Sozonova, D A Belenkov


Preservative treatments of window components with a water-based borate formulation
2000 - IRG/WP 00-40171
Factory finished window joinery components were treated with an aqueous borate preservative in order to investigate penetration and retention levels, associated drying times; and the potential impact of using a water-based treatment on finished items. It was found that by using borates applied by light double vacuum schedules, it was possible to meet standards for penetration and retention, to air...
J Jermer, J D Lloyd


Standardisation of sapstain tests - A challenge
1992 - IRG/WP 92-2403
In the last decade many new anti-sapstain products have been tested world-wide under laboratory and field conditions. Several extensive test programmes have been executed with different non-standardized test methods and procedures, with the result that the biological findings cannot be compared with each other. In this paper, gathered recommendations will be given in order to standardize test meth...
G Rustenburg, C J Klaver


Incorporation of phenyl boronic acid treatment with vapor phase formalization
1997 - IRG/WP 97-40083
Phenylboronic acid (PBA) treatment was incorporated with vapor phase formalization (VPF) in order to increase dimensional stability and boron fixation as well as enhancement of biological resistance. Five and ten hours VPF were applied after PBA treatment as 0.34, 0.50, 1.00 and 2.00% concs. aqueous solutions. Anti swelling efficiency (ASE) attended to 71% in specimens impregnated with 0.50% PBA s...
M K Yalinkilic, S Yusuf, T Yoshimura, W-Y Su, K Tsunoda, M Takahashi


Effect of soil parameters on biocide depletion: laboratory and field studies of water- and emulsion-borne preservatives
2000 - IRG/WP 00-30234
Two field test sites with different soils were selected. Soil analysis showed that the soil at the two sites had considerable texture, base saturation, acidity, and cation exchange capacity differences. Five sets of field stakes were treated as follows: three with water-borne CCA to about 0.4 pcf (6.4 kgm-3) retention, one with 0.75% DDAC, and one with 0.75% DDAC:0.25% chlorothalonil. The last two...
T Schultz, D D Nicholas, D E Pettry, M G Kim


Effectiveness of copper/chromium salts as wood preservatives against Limnoria tripunctata Menzies in laboratory tests
1977 - IRG/WP 431
During the last joint meeting of IRG and COIPM a co-operative programme of tests with copper/chromium salts as wood preservatives against marine borers was discussed and agreed. In this connection the results of a laboratory test in the BAM with Limnoria tripunctata Menzies will be of interest. But as the respective paper is written in German (H. Kühne; G. Becker: Laboratoriumsversuche über die ...
H Kühne


Occurrence, prevention and repair of Dry Rot
1990 - IRG/WP 1439
Information about the frequency, detection, identification and repair of Dry Rot attacks (Serpula lacrymans) is summarized from 13 European countries. Based on 28 completed and returned questionnaires it appears that Dry Rot attacks are recognized in all countries participating, and that there is an appreciable similarity in the frequency of attacks and methods of detection and identification. How...
A P Koch


Safe application of copper-chrome-arsenate preservatives
1975 - IRG/WP 377
All wood preservatives contain biologically active substances and must, by design, be in some measure toxic to man. There is nothing fundamentally difficult, however, about using a wood preservative with complete safety. It depends on knowing the risks to health and/or the environment, which the preservative may present, and planning application accordingly. In this paper we examine these and othe...
I N Stalker, P B Cornwell


Experiences with penetration of copper-based wood preservatives
2001 - IRG/WP 01-20233
In the Nordic countries there is a long tradition of result type based specifications for preservative-treated wood. A common Nordic standard for treated pine (Pinus sylvestris) wood was published in 1976. After a revision in 1989 this standard, then named INSTA 140, defined four classes of treated wood: M, A, AB and B. Treaters producing according to this standard had to be affiliated to a qualit...
J Jermer, F G Evans, I Johansson


International comparison of three field methods for assessing the in-ground termite resistance of materials - highlights after two years
1999 - IRG/WP 99-20157
First-year results of a comparative study, evaluating the in-ground termite resistance of a range of materials, including CCA and ACQ-treated timbers, using the below-ground exposure, ground contact and graveyard methods against diverse termite faunas were provided in IRG/WP/98-20132. Further annual inspections have confirmed early trends and identified notable differences between sites and method...
M Lenz, J W Creffield, A F Preston, B M Kard, C Vongkaluang, Y Sornnuwat


Reaction of osmium tetroxide with a diphenolic compound as a model substance for demethylated lignin
1986 - IRG/WP 1303
By using caffeic acid as a model substance for diphenolic moieties of demethylated lignin it was found that electron dense particles called by the authors "osmiophilic particles" in former papers are reaction products of OsO4 with the model substance. By these products it is possible to indicate the enzymatic demethylation of lignin taking place during wood decay. The appearance of the electron de...
K Messner, E Srebotnik


Natural decay resistance of some lesser-used tropical hardwoods from Ghana
2002 - IRG/WP 02-10438
Ghana is a tropical African country that is rich in diverse timber species. In order to reduce over-exploitation of the popular timber species and increase the resource base for the wood industry, lesser-used or lesser-known timber species are being promoted locally and for export. To do this successfully, it is essential to determine the physical, mechanical and biological properties of these tim...
S A Amartey, F R Hanson


The effect of hemicellulose degradation on the mechanical properties of wood during brown rot decay
2001 - IRG/WP 01-20219
Incipient decay of wood by brown rot fungi causes measurable strength losses in wood before measurable weight loss occurs. Previous studies have shown that the high levels of strength loss that occur during incipient brown rot decay may be related to loss in hemicellulose. This paper investigates the effect of decay on hemicellulose composition and the relationship to the mechanical properties of ...
S F Curling, C A Clausen, J E Winandy


Chemical and biological studies of organotin treated and painted wood stakes after outdoor exposure
1987 - IRG/WP 3419
Organotin based wood preservatives containing tributyltin oxide (TBTO) or tributyltin naphthenate (TBTN) are used in Sweden mainly for double-vacuum treatments of window joinery of Pinus sylvestris. After impregnation the joinery is painted or stained in different colours. To evaluate this effect (different colours on the degree of degradation of TBTO and TBTN, effected by different temperatures i...
M-L Edlund, B Henningsson


Variation in infection rates of blue-stain, mould and white rot tropical fungi on mixed light Malaysian woods
2000 - IRG/WP 00-10334
The modified 3-week FRIM laboratory method for screening of anti-sapstain formulations against three representative tropical fungi causing blue-stain (Botryodiplodia theobromae), mould (Paecilomyces variotii) and white rot (Schizophyllum commune) infection of sapwood species was used to examine the relative resistance of the sapwood of eight mixed light Malaysian woods, Scots pine (Pinus sylvestri...
A H H Wong, S Ahmad


Report on the burning of wood treated with wood preservatives containing copper, chromium and arsenic
1976 - IRG/WP 379
Mixtures of copper, chromium and arsenic salts are used extensively in the UK to preserve timber. This report is concerned with the fate of these metals when timber treated with these salts is burned. A large percentage of the arsenic present in the timber is shown to be volatilised during combustion and the potential environmental implications of this are assessed by comparison with the release o...
A J Dobbs, C Grant


A collaborative test to determine the efficacy of polyurethane coatings on wood samples in the marine environment. 2nd Interim Report
1990 - IRG/WP 4161
The results of a collaborative international test to evaluate the performance of elastomeric polyurethane coatings of wooden test samples exposed in seawater at 13 sites around the world are reported. The samples have been exposed at sites with known infestations by molluscan and/or crustacean wood borers. Performance data for up to 4 years exposure at some sites is presented providing information...
R A Eaton


Presteaming radiata pine heartwood to improve treatability
1983 - IRG/WP 3239
Steaming and holding before preservative treatment by the Bethell process greatly improved the treatment of radiata pine heartwood. Maximum penetration of preservative for the shortest holding period was obtained by the use of steam vacuum but the difference between this and steam venting was small when compared with the standard of treatment of air dried samples. A holding period of one day was s...
A J Bergervoet


Co-operative work on the performance of treated timber in ground contact
1975 - IRG/WP 344
At the 6th meeting of The International Research Group on Wood Preservation in Vienna, it was decided to approach all interested parties in order to: collate available information, set up collaborative work and to stimulate research on the performance of treated timber, especially hardwoods, in ground contact. In recent years, considerable concern has been expressed about the performance of preser...
D J Dickinson, J F Levy


The efficacy of Sentry® as a treatment for the control of sapstain in pre-infected radiata pine
2001 - IRG/WP 01-30260
Experiments were conducted to determine the efficacy of Sentry® when used to control sapstain fungi on radiata pine branch billets stored under high fungal hazard conditions. Prior to antisapstain treatment, the billets were pre-infected with a mixed inoculum of staining fungi and held from zero to 10 days at 25°C and 75% relative humidity. This was done to produce billets with different degrees...
C Chittenden, J G van der Waals, B Kreber, R N Wakeling


Investigation on different variation factors in the results of mycological test and means to reduce and avoid them
1986 - IRG/WP 2264
In order to clarify the causes of the dispersion observed in the results obtained with mycological tests made in accordance with standard EN-113, different factors assumed to be sources of the variations were studied. These included the moisture content of the test samples during the test, the influence of certain technological properties of the wood, the virulence of the fungus strains, the metho...
D Dirol


Above-ground field tests undertaken in New Zealand
1995 - IRG/WP 95-20063
In addition to "standard" L-joints, above-ground test material exposed at the NZ FRI test site includes treated and untreated decking units, Y-joints, fence battens and weatherboards either with or without additional protection from surface coatings. The latter tests bridge the gap between "model" test assemblies, such as L-joints, and services tests. Most tests are of preservative-treated radiata...
M E Hedley, D R Page, J B Foster, B E Patterson


Decay and mold resistance of borate modified oriented strandboard
2003 - IRG/WP 03-40260
Decay and mold resistance of zinc borate (ZB) and calcium borate (CB) modified oriented strandboard (OSB) from southern mixed hardwoods and yellow pine was investigated in this study. Tests were done with brown rot, Gloeophyllum trabeum, and white-rot, Trametes versicolar, fungi for 8 and 12 weeks, respectively. Wood species and fungus type had significant influence on the decay resistance. Decay...
Q Wu, S Lee, J P Jones