Chapter 11 - Preservation of talla bamboo
2007 - IRG/WP 07-10635-11
Researches revealed that the talla bamboo (Bambusa tulda Roxb.)) in Bangladesh could be full-cell pressure treated with CCA in green and dry conditions. The dry bamboo gives higher loading absorptions than green one when impregnated at same treating conditions. Also higher absorptions are obtained at nodes rather than internodes. Adequate penetration and retention results for ground and wate...
A K Lahiry


Chapter 12 - Treatment Groups of Bamboo
2007 - IRG/WP 07-10635-12
Study on distribution of CCA in three major bamboo species in Bangladesh, full-cell pressure treated at green and dry conditions revealed two treatment groups and some treating principles. Higher adequate treatment for ground and water contact use is only possible by treating problematic bamboo species pre-kiln dried up to half of its FSP and non-problematic species pre-dried up to FSP (20% ...
A K Lahiry


Preservative treatment of round bamboos by a new technique - Some further studies. Part 1
1990 - IRG/WP 3607
In general, the easy susceptibility of bamboos to wood destroying agencies is a major constraint in its rational utilisation. This is more so in tropical countries like India where wood destroying agencies are quite active. In an earlier publication, it was reported that round bamboo specimens of Bambusa balcooa, having three nodes, could be satisfactorily treated by CCA by a new technique develop...
V R Sonti, B Chatterjee


Effects of acetylation on the dimensional stability and decay resistance of kenaf (Hibiscus cannabinus L.) fiberboard
1996 - IRG/WP 96-40059
The objective of this study was to investigate the influence of the acetylation treated kenaf fiber, Phenol formaldehyde resin content level, and three fungi species on the dimensional stability and decay resistance of high density non wood composition boards. A standard ASTM method was used to evaluate weight loss and thickness change. The linear shrinkage and expansion of each species were also ...
P Chow, T Harp, R Meimban, J A Youngquist, R M Rowell


The dry rot fungus Serpula lacrymans. Examples of attack and remedial treatment
1988 - IRG/WP 1347
The film deals with several aspects of dry rot attack and eradication in buildings. The detailed biology and morphological charasteristics of the fungus are portrayed. The various forms of mycelial growth, the role of the strands in the nourishment and spread of the fungus, as well as the many types of fruitbody formation are outlined. Environmental and nutritional requirements of the fungus as we...
G Buchwald, B M Hegarty, W Metzner, R Pospischil, H Siegmund, P Grabow


Ultra-structural observations on the degradation of wood surfaces during weathering
1987 - IRG/WP 2280
Radiata pine (Pinus radiata D. Don) sapwood was converted into blocks with a transverse face about 5 mm square and measuring 8 mm longitudinally. Transverse (T.S.), Radial (R.L.S.) and Tangential (T.L.S.) surfaces were prepared and specimens exposed to the weather inclined at 45° facing equatorially for periods of between 20-60 days. After 30 days exposure erosion of the middle lamella was observ...
P D Evans, S Thein


Resistance of Alstonia scholaris vestures to degradation by tunnelling bacteria
1992 - IRG/WP 92-1547
Electron microscopic examination of vessels and fibre-tracheids in the wood of Alstonia scholaris exposed to tunnelling bacteria (TB) in a liquid culture showed degradation of all areas of the secondary wall. The highly lignified middle lamella was also degraded in advanced stages of TB attack. However, vestured pit membranes and vestures appeared to be resistant to degradation by TB even when oth...
A P Singh, T Nilsson, G F Daniel


Information from COIPM Wood Group
1985 - IRG/WP 4120
During the last COIPM Meeting (which took place in Athens, Greece in September 1984) the Wood Group met and discussed the co-operative work 'Durability in sea-water of wood with plastic wraps and wood treated with polymere'....
A Gambetta


Ultrastructural observations on wood-degrading erosion bacteria
1986 - IRG/WP 1283
G F Daniel, T Nilsson


Analysing the characteristic role of moisture content for drying and fluid flow in Sitka spruce. - Part 1: The drying process of sapwood and heartwood of two different thickness of Sitka spruce using a kiln. - Part 2: Effects of moisture content on longitudinal permeability of Sitka spruce in vertical variation of the tree
2000 - IRG/WP 00-40173
The characteristic role of the moisture content in Sitka spruce (Picea sitchensis (Bong.) Carr.) that grown in the United Kingdom was examined by this study on the basis of (1) the reduction of moisture content in two different thickness of sapwood and heartwood by kiln drying process, and (2) the effects of moisture content to the longitudinal void volume filled of tanalith-C by the full-cell pro...
I Usta


Water-based water repellents for treatment of wood
1987 - IRG/WP 3446
The water uptake by wood can be reduced by treatment with a water repellent. The water repellents most commonly used are solvent based. In the present work a new type of water repellent that is water-based has been investigated. Two different treatments have shown an effect of the same order as a commercial solvent based product. The cellular distribution of the water repellents has been investiga...
I G Svensson, G Hägglund, I Johansson, W B Banks


Treatment of particleboard with isocyanate resin to impart improved dimensional stability and water repellency
2000 - IRG/WP 00-40178
Standard particleboard panels (for interior use) of 16 mm nominal thickness were cut into samples measuring 6.4 mm x 78 mm2. The samples were divided into 4 end matched batches. Two batches were treated with isocyanate resin and cured. The other 2 batches were left untreated. One of the treated batched and 1 of the untreated batches were edge sealed with epoxy resin prior to isocyanate resin appli...
K M Filcock, P Vinden


Laboratory and field evaluation of Plasmite Reticulation System using bifenthrin as a chemical barrier within wall cavities against subterranean termites.
2005 - IRG/WP 05-20307
Laboratory and field bioassays undertaken to demonstrate Plasmite Reticulation system effectively delivers the termiticide (bifenthrin) within a simulated wall cavity at the required concentration. The chemical assay indicated that the amount of bifenthrin sampled at 5, 10, 15, 20, and 25m along the simulated reticulation system tested (30m) exceeded the manufacturer’s minimum recommendation of ...
J R J French, B M Ahmed, J Thorpe, A Anderson


Degradation of the normal fibre walls of rubberwood (Hevea brasiliensis) by the tropical blue-stain fungus Botryodiplodia theobromae
1998 - IRG/WP 98-10286
Rubberwood was examined by light microscopy and transmission electron microscopy (TEM) after exposure to the common tropical sapstain fungus Botryodiplodia theobromae for four weeks to study hyphal colonisation of wood cells and to determine if this fungus also degraded lignified normal fibre cell walls in addition to the walls of non-lignified elements. Light microscopy revealed relatively large ...
A A H Wong, A P Singh


Ancillary properties of vapor boron-treated composites
2001 - IRG/WP 01-40210
This paper discusses the water absorption, thickness swelling, and internal bond strength of North American composites treated using a vapor boron treatment process. For oriented strandboard, high boron loadings led to lower internal bond strength and lower thickness swelling. Water absorption results were variable but no deleterious effect of treatment was noted. For medium density fiberboard, th...
W A Jones, H M Barnes, R J Murphy


Ultrastructural aspects of bacterial attacks on an archaeological wood
1993 - IRG/WP 93-10007
Transmission electron microscopy of wood from a Chinese ship submerged in the mud for over 900 years showed bacteria to be the main factor for its deterioration. The micromorphology of degraded wood cell walls was similar to that observed during the attacks of wood by erosion bacteria. Other bacterial forms, previously considered lo be scavenging bacteria, were also abundant in degraded areas of t...
Yoon Soo Kim, A P Singh


The Relationship of Fiber Cell Wall Ultrastructure to Soft Rot Decay in Kempas (Koompassia malaccensis) Heartwoo
2004 - IRG/WP 04-10541
The ultrastructure of fiber walls in kempas (koompassia malaccensis) heartwood was examined in relation to soft rot cavity formation. The fibers consisted of middle lamella and thick secondary wall. The secondary wall was differentiated in to a S1 layer, and a unique multi-lamellar S2 layer. Two distinct forms of lamellae were recognisable, one type being considerably thicker than the other. They ...
A P Singh, A H H Wong, Yoon Soo Kim, Seung-Gon Wi


Biodegradation of acetylated southern pine and aspen composition boards
1994 - IRG/WP 94-40020
This objective of this study was to investigate the influence of the acetylation treated wood fiber, Phenol-formaldehyde resin content level, two wood fiber species, three fungi species on the dimensional stability and decay resistence of high density composition boards. A standard ASTM method was used to evaluate weight loss and thickness change. The linear shrinkage and expansion of each species...
P Chow, T Harp, R Meimban, J A Youngquist, R M Powell


Estimation of effective diffusion path lengths in wood by swelling studies
1989 - IRG/WP 3524
The effective average distance that a solute must diffuse to penetrate the cell wall matrix following pressure treatment is estimated from the rate of swelling of wood, vacuum treated with water. It is assumed that the diffusion paths are similar for water and a solute such as a wood preservative component. Since bound water diffusion coefficients for water in wood have been estimated by others, t...
P A Cooper, R Churma


The attack of naturally durable and creosote treated timbers by Limnoria tripunctata Menzies
1995 - IRG/WP 95-10132
Limnoria tripunctata was found tunnelling in creosote treated Douglas fir (Pseudotsuga menziesii) pilings and naturally durable greenheart (Ocotea rodiaei) gate seals at two sites on the south coast of the United Kingdom. Examination of thc creosote-treated wood showed that Limnoria tunnels were concentrated at a depth of 2-3 cm from the timber surface, where creosote loading was lower. Fewer tunn...
A J Pitman, G S Sawyer, G F Daniel


Role of cell wall structure in soft rot decay of bamboo
1995 - IRG/WP 95-10133
Models of soft rot hyphal penetration of bamboo cell walls are proposed. Soft rot hyphae show an interesting capability of penetrating the bamboo cell wall in different forms; typical longitudinal penetrating hyphae and tangentially orientated penetrating hyphae. The second form of penetration was found to be different from that normally associated with wood cell walls. The differences can be attr...
O Sulaiman, R J Murphy


Ultrastructure of degraded, CCA-treated Pinus radiata wood from a marine pile
1990 - IRG/WP 1461
During an inspection of marine piles, 12 years after installation, severe degradation was noted on one of them in the vicinity of a corroded eye-bolt. The wood was dark brown in colour and tended to crumble easily. Wood fragments were examined by light microscopy and scanning and transmission electron microscopy and were also analysed for carbohydrates and lignin. Light microscopy showed numerous ...
A P Singh, M E Hedley


A Preliminary Report on the Properties of Engineered Wood Composite Panels Treated with Copper Naphthenate
2005 - IRG/WP 05-40294
This paper reports on our preliminary investigation of the properties of randomly oriented strandboard which had waterborne or powdered copper naphthenate (CuN) incorporated into the board during manufacture. When compared to zinc borate-treated controls (ZnB), the mechanical properties of strandboard (MOR, MOE, work-to-maximum load, internal bond strength) were not adversely affected by treatmen...
J W Kirkpatrick, H M Barnes


Degradation of the gelatinous-layer in aspen and rubber wood by the blue stain fungus Lasiodiplodia theobromae
1996 - IRG/WP 96-10168
Studies on the degradative ability of the blue stain fungus Lasiodiplodia theobromae Pat. have shown several strains to cause significant weight losses (i.e. ca 20%) in the temperate and tropical wood species, aspen (Populus tremula) and rubber wood (Hevea brasiliensis). In addition to the consumption of soluble carbohydrates and extractives, major changes in the ultrastructure of fibre cell walls...
O Encinas, G F Daniel


Decay Resistance and Bonding Properties of Structural Flakeboard
2002 - IRG/WP 02-40233
Experimental structural flakeboard panels consisting of differing furnishes and resins were produced and tested for internal bond, linear expansion, thickness swell, and decay resistance. One group of panels was produced with recycled CCA-treated wood as the furnish and commercial phenol formaldehyde (PF) resin as the binder. Other groups of panels were produced with either mixed hardwoods or so...
T F Shupe, Chung-Yun Hse