Testing biological durability of wood-plastic composites
2006 - IRG/WP 06-20347
Testing biological durability is inherently different for wood-plastic composites (WPC) compared to solid timber. However there is clearly a need for more information on the durability of WPC’s, on the effect of decay on the material properties of WPC’s and on methods for assessing decay of WPC’s. For the emerging European WPC market there has been some discussions on how to work on these to...
J Van Acker


Wood plastic composites from modified wood. Part 3. Durability of WPCs with bioderived matrix
2008 - IRG/WP 08-40423
The decay resistance of fully bio-derived wood plastic composites, WPCs, was tested in both laboratory and field tests. The laboratory tests were performed according to modified versions of AWPA E10 (soil-block test) and ENV 807 (tests in three un-sterile soils) and the field tests according to EN 252 (stakes in ground) and EN 275 (resistance to marine borers). The WPC materials for laboratory tes...
M Westin, P Larsson Brelid, B K Segerholm, M Van den Oever


Moisture dynamics of WPC as basis for biological durability
2010 - IRG/WP 10-40520
The largest market for wood-polymer composites (WPCs) is currently decking. Although many products are commercially available, a proper standard for the assessment of the biological durability of WPC does not exist. Recommended standards for testing resistance against basidiomycetes should be completed with a method to bring the specimens in a worst case situation, obtaining a moisture level high ...
N Defoirdt, J Van Acker, J Van den Bulcke


Resistance of WPC against wood destroying fungi
2013 - IRG/WP 13-40627
The investigation of biological durability is a fundamental topic to assess the performance of Wood Plastic Composites (WPC) particularly for outdoor applications. In the last years, different test setups based on existing standards on the field of wood as well as the field of plastics were used for WPC. But the test methodologies give different information about the durability of the tested mater...
A Gellerich, S Bollmus, A Krause


Some comments on durability testing of WPC according to EN 15534-1
2015 - IRG/WP 15-40695
The standard EN 15534-1 (2014) gives advice for broad characterization of WPC materials and products. It contains instructions for test procedures concerning different properties e.g. mechanical properties, thermal properties, as well as durability. In this paper some WPC materials from the market were tested for their resistance against brown rot. Furthermore, the water uptake and bending prope...
S Bollmus, A Gellerich, H Militz


The use of new, aqueous chemical wood modifications to improve the durability of wood-plastic composites
2017 - IRG/WP 17-40787
The wood flour used in wood-plastic composites (WPCs) can biologically deteriorate and thus the overall mechanical performance of WPCs decrease when exposed to moisture and fungal decay. Protecting the wood flour by chemical modification can improve the durability of the wood in a nontoxic way so it is not harmful to the environment. WPCs were made with modified wood flour and then evaluated for m...
R E Ibach, C M Clemons, G C Chen


Long-term field exposure of wood-plastic composites processed on a commercial-size extruder
2020 - IRG/WP 20-40894
Wood-plastic composites (WPC) contain wood fiber (or flour), thermoplastics and additives and are exposed to UV light, moisture, and biological deterioration in outdoor installations. Accelerated laboratory tests can help to predict the durability of WPCs, but long term evaluations are needed to validate these results. Field exposed above-ground WPC deck boards (30.5 x 139.7 x 609.6 mm) and in-gro...
R E Ibach, C M Clemmons, N M Stark


Effects of acetylation on the dimensional stability and decay resistance of kenaf (Hibiscus cannabinus L.) fiberboard
1996 - IRG/WP 96-40059
The objective of this study was to investigate the influence of the acetylation treated kenaf fiber, Phenol formaldehyde resin content level, and three fungi species on the dimensional stability and decay resistance of high density non wood composition boards. A standard ASTM method was used to evaluate weight loss and thickness change. The linear shrinkage and expansion of each species were also ...
P Chow, T Harp, R Meimban, J A Youngquist, R M Rowell


Wood preservation in Lithuania
2004 - IRG/WP 04-30363
This article is intended to give basic information on wood preservation activities in Lithuania and the main actors in wood preservations practice and research. Currently the main actors in practical Lithuanian wood preservation activity are enterprises of wood preservation industry united by the Lithuanian Wood Preservation Association. The most intensive activity in wood preservation practice an...
J Saladis


Natural durability transfer from sawmill residues of white cypress (Callitris glaucophylla). - Part 3: Full penetration of the refractory sapwood of white cypress
2000 - IRG/WP 00-40167
The heartwood of white cypress, Callitris glaucophylla, is renowned for its termite resistance and durability against decay. The sapwood, which can represent up to 30% of log volume, is non-durable and refractory to conventional preservative treatment. Previous work ascribes the lack of permeability to oily deposits within tracheids and ray cells. Environmental scanning electron microscopy was use...
M J Kennedy, L M Stephens, M A Powell


Interspecific variability of European oak durability against white rot fungi (Coriolus versicolor): Comparison between sessile oak and peduncle oak (Quercus petraea and Quercus robur)
2001 - IRG/WP 01-10393
The knowledge of wood natural durability against biologic predators enable its external use. The resistance of European oak wood was reported like durable according to the EN 350-2. However, some individuals may contain high durable wood. Our research was focused to understand this variability in oak population that represent the first french species (4.1 millions of ha). Natural durability of Eur...
N Ayadi, B Charrier, M Irmouli, J P Charpentier, C J Allemand, F Feuillat, R Keller


European standardization for wood preservation
1988 - IRG/WP 2321
G Castan


European standardization for wood preservation
1989 - IRG/WP 2335
G Castan


The susceptibility of 35 Amazon wood species to Cryptotermes brevis (Walker)
1982 - IRG/WP 1160
Laboratory tests were carried to evaluate the susceptibility of 35 Amazon hardwoods to Cryptotermes brevis (Walker). The results were analysed statistically and showed that five wood species were non resistant, nine were resistant and the other twenty-one in between those classes of resistance....
M D Canedo


Possibility of use of wood species per class of biological risks. Attempt to determine criteria based on Pr EN 350-1/2/3
1992 - IRG/WP 92-2409
M Rayzal


Durability of larch (Larix spp.) wood against brown-rot fungi
1997 - IRG/WP 97-10228
Durability of the heartwood of Larix decidua, L. sibirica, L. gmelinii, L. gmelinii var japonica, L. gmelinii var olgensis and L. sibirica x decidua against brown rot fungi Coniophora puteana, Poria placenta and Gloeophyllum trabeum was tested according to EN 113 test method. Parallel samples were used to study the amount and composition of wood extractives. The sample trees originated from the re...
H Viitanen, L Paajanen, P Saranpää, P Viitaniemi


Inspection results of preservative treated stakes, maximum 33 years in field
1992 - IRG/WP 92-3690
Since in 1958, we have undertaken field experiments in Japan. For these field experiments, we used sapwoods of Japanese cedar called Sugi (Cryptomeria japonica) because of majority of plantation forest soft wood species in Japan. For some preservatives, we added sapwood of Japanese beech called Buna (Fagus crenata), a main Japanese hard wood species. Dimensions of these specimens were 30 x 30 x 60...
K Suzuki, K Yamamoto, M Inoue, S Matsuoka


Wood furfurylation process and properties of furfurylated wood
2004 - IRG/WP 04-40289
The first processes for “furfurylation” of wood (wood modification with furfuryl alcohol) were developed several decades ago. Furfuryl alcohol is a renewable chemical since it is derived from furfural, which is produced from hydrolysed biomass waste. Over the last decade modernised processes for furfurylation of wood have been developed. These new processes are based on new catalytic systems a...
M Westin, S Lande, M Schneider


Development of marine borers research in Sao Paulo State, Brazil
1985 - IRG/WP 4117
This paper describes some field tests which have been carried on marine sites in Sao Paulo State mainly to investigate the natural resistance of Brazilian woods and the occurrence of marine borers. Some laboratory breeding tests which are being developed are also describe...
G A C Lopez


Natural Resistance of timbers to marine borer attack. COIPM/IRG CO-OPERATION. Final report concerning panels exposed in the sea at Sekondi, Ghana
1979 - IRG/WP 449
The test was carried out according to Document COIPM/72.044, Revised procedure for the testing of naturally durable timbers against marine borers. The panels of the three species remaining in the test at the end of 1978 were removed and assessed visually. An average rating was given to the panels of each species....
F F K Ampong


Durability of pine modified by 9 different methods
2004 - IRG/WP 04-40288
The decay resistance was studied for pine modified by nine methods of wood modification: 1) Acetylation, 2) Treatment with methylated melamine resin (MMF), 3) Acetylation followed by post-treatment with MMF-resin, 4) Thermal modification, 5) Furfurylation, 6) Maleoylation (using water solution of MG or ethanol solution of maleic anhydride), 7) Succinylation, 8) NMA-modification and 9) modification...
M Westin, A O Rapp, T Nilsson


Chemical compounds from Eperua falcata and Eperua grandiflora heartwood and their biological activities against wood destroying fungus (Coriolus versicolor)
2005 - IRG/WP 05-30373
The chemistry analysis of the compounds present in dichloromethane and ethanolic fraction as well as bioassays enables to understand the durability differences of Eperua falcata and Eperua grandiflora. The principal distinction between these two species is the acidic subfraction of diterpenoic extract, which is antifungic in Eperua falcata when tested in in-vitro conditions. This study also enable...
N Amusant, C Moretti, B Richard, E Prost, J M Nuzillard, M-F Thévenon


An attempt to evaluate wood resistance against fungal decay in non-sterile conditions by measuring the variation of resistance to bending test
1988 - IRG/WP 2308
The main object of this work was to determine the variation of strength on large test specimens of wood (800 x 45 x 45 mm³) when exposed to accelerated fungal attacks close to natural conditions, out of test vessels. The modulus of elasticity (MOE) and the modulus of rupture (MOR) have been assessed. Thereby, the natural resistance of the wood species to fungal decay, the efficiency of preservati...
L N Trong


Laboratory tests on natural resistance to Cryptotermes brevis (Walker) attack of native hardwoods for crossarms production
1985 - IRG/WP 1266
Eletropaulo (Eletricidade de Sao Paulo S/A) and IPT (Instituto de Pesquisas Tecnologicas do Estado de Sao Paulo S/A) are carrying on a study to evaluate wood species for crossarms in replacement of Aspidosperma polyneuron - Apocynaceae (Peroba-rosa) traditionally used for this purpose. Nineteen Amazon wood species were elected, with physical and mechanical properties equal or better than those pre...
M D Canedo, A T De Lelis


The effect of sapwood on the rate of deterioration of fence posts
1986 - IRG/WP 1277
In order to evaluate the effect of the presence of sapwood on the rate of deterioration of fence posts, 30 specimens with and without sapwood of Eucalyptus citriodora, Eucalyptus paniculata, Eucalyptus saligna and Eucalyptus tereticornis were exposed in three test sites in the State of São Paulo, Brazil. The results of the inspection carried out in 1985, after 5 years of exposure, are reported in...
M S Cavalcante, G A C Lopez, E S F Mucci, R G Montagna