IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3033 documents. Displaying 25 entries per page.


Decay resistance of resin treated wood
1999 - IRG/WP 99-30206
Selected natural resin systems were evaluated for their potential as wood protecting agents according to standard test procedures. As indicated by the European standard EN 599 both a Basidiomycete test according to EN 113 and a ENV 807 soil bed test were carried out. Six resin treatments were tested using 3 concentration or treatment levels. Using the biocidal activity criteria as usually applied ...
J Van Acker, A J Nurmi, S M Gray, H Militz, C Hill, H Kokko, A O Rapp


An appraisal of methods for environmental testing of leachates from salt-treated wood (2)
1998 - IRG/WP 98-50110
For wood preservatives for use in hazard class 4 information on the ecotoxicity of preservatives and ingredients as well as on the effect of losses from impregnated timber is needed for a proper environmental risk assessment. In the evaluation of a suitable test procedure the leaching behaviour of copper-based formulations was studied using analytical and ecotoxicological test methodology. These ...
H W Wegen, A Platen, G M F Van Eetvelde, M Stevens


Wood decay in Danish buildings
1985 - IRG/WP 1261
At Technological Institute identification of fungi and advisory activity concerning repair of damages has taken place since 1935. Statistical analyses based on material from 1982 and 1983 are compared to earlier investigations worked out by L. Harmsen. The material shows that building traditions influence the diversity and frequency of fungal species. Many fungal damages in the last decade have sh...
A P Koch


Surface coatings for impregnated wood
1992 - IRG/WP 92-3684
The use of proper surface coatings enhances the aesthetic and protective properties of impregnated wood. Good results with especially water-borne coatings have been obtained for class-A impregnated L-joints and claddings in field tests started in 1982....
L Kotama


Ultrastructural observations on wood-degrading erosion bacteria
1986 - IRG/WP 1283
G F Daniel, T Nilsson


CCA Chemistry
1983 - IRG/WP 3268
A Pizzi


Re Questionnaire: The use of computers in wood preservation research
1985 - IRG/WP 2239
A questionnaire (Document No: IRG/WP/2240) concerning the use of computers in wood preservation research is introduced. Completing and returning the questionnaire will allow information to be collated on the usage of computers and computer programmes...
E F Baines


The window joinery test hut
1975 - IRG/WP 257
D F Purslow


Data sheet on wood-boring insects: Ptilinus pectinicornis (Linnaeus)
1987 - IRG/WP 1334
S Cymorek, M-M Serment


Termiticidal effectiveness of synthetic pyrethroids, carbaryl and chlordane in wood-block test
1985 - IRG/WP 3356
The results of some wood-block tests with allethrin, permethrin, fenvalerate, carbaryl and chlordane against Coptotermes formosanus are tabled and compared against some organophosphates, chlorpyrifos, fenitrothion, phoxim, tetrachlorvinphos and acephate. The treatment of the wood blocks was exactly as described in Document No: IRG/WP/3330. Among the pyrethroids tested, permethrin was the most effe...
K Tsunoda


An Australian test of wood preservatives. - Part IV: The condition, after 35 years' exposure, of stakes treated with creosote oils and oilborne preservatives
2000 - IRG/WP 00-30241
This paper contains the first results dealing with creosote oils and oilborne preservatives from this in-ground field trial in Australia. The substrates impregnated with preservative were Pinus radiata D. Don sapwood and Eucalyptus regnans F. Muell. heartwood and sapwood. Data are reported from stakes exposed for 35 years at three Australian sites (Innisfail, Sydney, Walpeup). Comparisons were mad...
G C Johnson, J D Thornton


Biocides - Efficacy assessment and doses for wood preservatives (product type 8). Local/geographical aspects. Termite control as case study
1999 - IRG/WP 99-20181
Currently, the efficacy of a wood preservative, as biocidal product type 8, is assessed as a ‚critical value' (CV), an efficient dose (retention in wood at a given depth of penetration). CVs are planned to be adapted for exposure to basic target organisms (5 hazard classes) and additional requirements concerning the occurrence of local target organisms in relation with climate, building...
G Ozanne


Creosote movement from treated wood immersed in fresh water: Initial PAH migration
2003 - IRG/WP 03-50201
Creosote has a long history of successful use as a wood preservative, but polycyclic aromatic hydrocarbons (PAHs) in this preservative have raised environmental concerns, particularly when creosote-treated wood is used in aquatic environments. A number of models have been developed to predict the risk of creosote use in aquatic environments, but one limitation of these models is a lack of data o...
Sung-Mo Kang, J J Morrell, J Simonsen, S T Lebow


Determination of toxic limits of wood preservatives towards wood-destroying Basidiomycetes. Investigation on the effect of the use of two impregnated wood blocks and of one impregnated and an untreated block respectively in Kolle jars on the toxic limits of wood preservatives
1973 - IRG/WP 225
O Wälchli


300 years water-logged wood: Treatability with CCA-C
1998 - IRG/WP 98-40103
The treatability of 300 years water-logged and recent wood (Abies bornmülleriana M.) was assessed by dip treatment and vacuum and pressure cycling with CCA-C. Treatment runs were evaluated on the basis of weight gain retention and radial and tangential penetration measurements. The preservative penetration and retention levels in the 300 years water-logged wood were higher than in the recent wood...
S N Kartal, N Yilgör


Draft of a mongraphic card for Serpula himantioides (Fr.) Karst. according to the 'Model Questionnaire for preparation of monographic cards for wood-destroying fungi'
1978 - IRG/WP 174
L Harmsen


Copper based water-borne preservatives: The biological performance of wood treated with various formulations
1987 - IRG/WP 3451
Wood samples treated with the various components of CCA preservative singly and in combination were tested against a soft rot organism, a copper tolerant brown rot organism and in soil burial both unleached and after leaching. The results suggest that, of the elements tested, fixed copper is essential for preventing soft rot attack and fixed arsenic is essential for preventing attack by a copper t...
S M Gray, D J Dickinson


Implications for comparability of laboratory experiments revealed in studies on the variability in survival and wood consumption between colonies of Coptotermes acinaciformis (Froggatt) (Isoptera: Rhinotermitidae
1983 - IRG/WP 1196
(Summary of paper 1193) Groups of Coptotermes acinaciformis, originating from six colonies, three taken from each of two localities, 1500 km apart, in northern Australia (Townsville, Darwin) were kept at population densities of 0.005, 0.01 and 0.02 g termites/mL. Survival and wood consumption of the groups after 8 weeks followed a similar pattern in the colonies from both collection areas. Groups were least vigorous at the lowest population density; their performance reached a maximum at a population density of 0.01 g/mL. The subsequent decline in vigour was less marked as the highest population density was approached. However, the actual values for survival and wood consumption varied widely between colonies, irrespective of their origin. It is recommended that in all laboratory experiments which use survival and wood consumption as indicators of termite vigour, controls of a favourable as well as an unfavourable food type are included which would serve to monitor the vigour of the termites. Results from termite sources whose vigour falls below a certain threshold value would have to be treated with caution and could not be used in definative data, as e.g. in defining critical retentions of wood preservatives.
M Lenz


Seasonal effects of the field evaluation on wood preservatives against mold fungi
1996 - IRG/WP 96-20087
For the purpose of the amelioration of field test methods, commercial preservatives against mold fungi were tested under two different seasons, in winter and in summer. The specimens were bundled and set over the water bath and all these systems were covered with plastic film. At top of the system under film, black films for regeneration of sunlight were put in, and windows for changing air were r...
K Suzuki, Y Sugai, K Ryugo, D Watanabe


Estimation of service life of durable timber species by accelerated decay test and fungal cellar test
2002 - IRG/WP 02-20249
Many kinds of durable wood species for outdoor uses has been imported from all over the world to Japan. However information on the natural durability of these species is not sufficient to estimate the service life of them in the climate of Japan. Highly durable species such as Jarrh, Teak, Ipe, Ekki, Selangan batu, Red wood, Western red cedar showed no significant percent mass losses by accelerate...
K Yamamoto, I Momohara


Trends in environmental management in industry. Implications for wood preservation activities
1993 - IRG/WP 93-50001-34
J A De Larderel


Monographic information on Serpula (Poria) incrassata according to the "Model Questionnaire for preparation of monographic cards for wood-destroying fungi"
1980 - IRG/WP 160
J G Palmer, W E Eslyn


Some statistics on the Brazilian Wood Preservation Industry: 1980-81
1982 - IRG/WP 3214
Statistical data on the production of pressure treated wood and on the consumption of wood preservatives are given for the years of 1980 and 1981 in Brazil....
M S Cavalcante, F C Geraldo, A R De Freitas


Programme section 3, Wood protecting chemicals
1996 - IRG/WP 96-30119
IRG Secretariat


Evaluation and approval of wood preservatives in the Nordic countries
1988 - IRG/WP 2311
This paper reviews the system for evaluating and approving the efficacy of wood preservatives for industrial use currently in force in the Nordic countries Denmark, Finland, Iceland, Norway and Sweden....
B Henningsson, J Jermer


Previous Page | Next Page