Effects of a chitin synthesis inhibitor on spore germination of the decay fungi Gloeophyllum trabeum and Poria tenuis
1986 - IRG/WP 2253
This study sought to determine the effect of a chitin synthesis inhibitor - Polyoxin D, on spore germination and early hyphal development of a brown rot and a white rot fungus in-vitro. Polyoxin D is a competitive, substrate-analogue type of chitin synthtase inhibitor (2). The drawbacks to use of such a compound as a wood preservative tie. cost - $20,000/g, possible leaching or degradation) might ...
E L Schmidt


Biological Durability of Laminated Veneer Lumber from Durable and Non-Durable Wood Species
2005 - IRG/WP 05-10567
Laminated Veneer Lumber (LVL) was laboratory manufactured using veneers from decay and non decay resistant species in order to evaluate changes in the durability as a result of the LVL manufacturing process, and to test if the mixing of decay resistant species and non decay resistant species can improve durability. Laboratory soil block test and field test were conducted. The durability of solid w...
P Nzokou, J Zyskowski, S Boury, D P Kamdem


Wood Preservation in France. A statement of quality control early 1986
1986 - IRG/WP 3389
A statement of quality control in France early 1986 - Summary of new - Standards criteria for preservatives and treated wood - Aptitude of treated wood for use per class of biological hazard...
M Romeis, G Ozanne


Eco-tax - A new threat for wood preservation? The Belgian experience
1993 - IRG/WP 93-50001-32
At the end of January 1993, a bill was put for Belgian Parliament related to the introduction called "Eco-taxes" on a series of products, such as packaging for drinks (especially on PVC-bottles), non-returnable articles (shavers, small cameras), batteries, pesticides for non-agricultural use and paper....
G Van Steertegem, F De Jaeger


Possibility of use of wood species per class of biological risks. Attempt to determine criteria based on Pr EN 350-1/2/3
1992 - IRG/WP 92-2409
M Rayzal


Establishment of a laboratory method to characterise the ecotoxicity of a polluted soil
1998 - IRG/WP 98-50101-23
This method consists in using the underground grub of the Oxythyrea funesta beetle as a bioindicator of the soils pollution. Due to the significant tolerance of the organism, a large type of substrate of different nature and grain size could have been studied. We have tested substances and preparations such as wood preservation products even under powder or liquid form but also some wastes of di...
P Martinet


Selective adsorption of antisapstain actives from two aqueous suspensions, and movement of actives into wood
1996 - IRG/WP 96-30103
Green-off-saw rough sawn Pinus elliottii (slash pine) boards were dipped in aqueous suspensions of two antisapstain formulations, NeXgenâ and Busanâ Sap Stain Preventative (Busan 1009), at three product concentration levels. Concentrations of active ingredients (NeXgen: CTL (chloro-thalonil) and MTC (methylene bisthiocyanate); Busan 1009: TCMTB (2(thiocyanomethylthio)-benzothiazole) and MTC) wer...
M J Kennedy, T L Woods


Studies of the distribution and degradation of tributyltin naphthenate in double-vacuum treated wood
1983 - IRG/WP 3230
The effects of forced solvent evaporation by kilning redwood (Pinus sylvestris) that has been double-vacuum treated with tributyltin naphthenate (TBTN) have been investigated. Contrary to previous studies reported, it has been shown that forced evaporation can have a considerable influence on the losses of the fungicide. It has been found that, whether the solvent is allowed to evaporate slowly or...
J Jermer, M-L Edlund, W Hintze, S V Ohlsson


Rates of emission from CCA-treated wood in the marine environment: measurement, modelling and requirements for further research
2001 - IRG/WP 01-50166-12
Accurate estimates of rates of emission of leachate from preservative treated wood are crucial for realistic predictions of the environmental impact of its use in maritime construction. Estimates are available for some commonly used preservatives, but these vary widely. Though variable, these measurements suggest that emission generally decreases exponentially with time. Part of the variation is d...
S M Cragg, C J Brown, R A Albuquerque, R A Eaton


Dimensional stabilization of wood with dimethylol compounds
1987 - IRG/WP 3412
This study showed that a substantial degree of dimensional stability can be imparted to wood by crosslinking with low concentrations of dimethyloldihydroxyethyleneurea. It was demonstrated that by selecting the right catalyst system the cure temperature can be reduced to the point that strength loss of the treated wood is minimized....
D D Nicholas, A D Williams


Update on lab and field test results for polymeric alkylphenol polysulfide treated wood
2002 - IRG/WP 02-40240
The possibility of using Polymeric Alkylphenol Polysulfide (PXTS) as a wood preservative has been undergoing evaluation in our laboratories for the past four years. Various formulations prepared from this compound have been tested and found to be effective against wood decay fungi and insects in field stakes after 42 months exposure. In accelerated soil bed tests, PXTS has been shown to be consi...
J Goswami, A Abramson, R Buff, D D Nicholas, T Schultz


Corrosion of fasteners in heat-treated wood – progress report after two years’ exposure outdoors
2005 - IRG/WP 05-40296
The corrosion of common fastener materials now in use - mild steel, zinc-coated steel, aluminium and Sanbond Z-coated steel – has been evaluated after two years’ exposure outdoors in untreated and heat-treated spruce (Picea abies) respectively. Spruce from South-western Sweden was used. The heat-treatment was carried out in Finland according to the ThermoWood process at a maximum temperature ...
J Jermer, B-L Andersson


Accelerated ageing of preservatives in treated wood
1988 - IRG/WP 3476
New preservatives are tested in the laboratory and often in field tests before they are used commercially. Some preservatives, however, tested in the laboratory do not show the expected stability when used in service. The differences between laboratory tests and practical use can never be completely eliminated but must be minimized as far as possible by relevant testing methods. Studies of the eff...
M-L Edlund, B Henningsson, B Jensen, C-E Sundman


Rapport sur l'activité du CNE/TC 38 'Méthodes d'essais des produits de préservation du bois'
1980 - IRG/WP 279
G Castan


Wood-destroying insects found in the Eastern Black Sea sub-region of Turkey
1982 - IRG/WP 1153
The Eastern Black Sea subregion has important forest resources. The settlement areas are scattered at the countryside. That's why a good deal of wood and timber is used in the construction of buildings without sufficient protective measures in the rural areas. In the forests and rural buildings 52 wood-destroying insect species have been specified 35 of which are new in this subregion and...
O A Sekendiz


Blue stain in timber in service. Results of co-operative tests to compare different artificial weathering systems 1981-82
1983 - IRG/WP 2193
The paper describes results of the third phase of co-operative laboratory experiments comparing the effects of different artificial weathering systems on chemicals to control blue-stain in service. Atlas, Xenotest and Marr equipments are shown to give essentially the same results for 5 of the 6 chemicals tested....
A F Bravery, D J Dickinson


Decay fungi in Finnish houses on the basis of inspection samples from 1978 to 1988
1989 - IRG/WP 1401
A summary of the causes and sources of fungal damages was made on the basis of decay samples and sample information sent to the Forest Products Laboratory of the Technical Research Centre of Finland (VTT) between 1978 and 1988. About 50-130 decay cases in wood structures were studied annually. In almost 50% of all fungusdamage cases the cause was Serpula lacrymans. The proportion of Coniophora put...
L Paajanen, H Viitanen


Assessment of losses of wood preservatives from treated wood by leaching into the environment
1993 - IRG/WP 93-50001-13
Wood preservative chemicals may be lost from treated timber by leaching into water or soil. The degree to which this might occur and its effect on the environment is difficult to assess quantitatively due to the absence of appropriate test methods. This paper describes work to assess test methodology capable of allowing the rates of loss of wood preservative from treated timber to be quantified. T...
R J Orsler, G E Holland


Proposals for a vermiculite burial soft rot test method
1980 - IRG/WP 283
J G Savory, J K Carey


Production of treated wood in Brazil in 1982 and 1983
1985 - IRG/WP 3327
The data of Brazilian production of treated sleepers, poles, crossarms, fence posts and other commodities are given for the years of 1982 and 1983. This report updates information given to the Group in Document No: IRG/WP/3321 Wood Preservation in Brazil, STU information no 445...
M S Cavalcante


A new ground-contact wide-spectrum organic wood preservative: DNBP
1986 - IRG/WP 3358
A new organic wood preservative, which 25 years field tests have proved to be of efficiency and effectiveness comparable to CCA wood preservatives for ground-contact applications, is presented. Physical and chemical tests, supporting the long term field test results as well as indicating the characteristics of this preservative, are also presented....
W E Conradie, A Pizzi


An in-ground natural durability field test of Australian timbers and exotic reference species. Part 2: Progress report after approximately 13 years' exposure
1983 - IRG/WP 1189
The condition of heartwood specimens of Australian and exotic timber species after approximately 13 years' in-ground exposure is given. Four of the 5 test sites have a termite hazard in addition to the hazard from a range of decay fungi. Values for specimen life are given only where all replicates of a timber species have become unserviceable. Results give evidence leading to doubt about ...
J D Thornton, G C Johnson, I W Saunders


Cytochemical localization of hydrogen peroxide in brown rot fungus Tyromyces palustris by cerium chloride technique
1999 - IRG/WP 99-10299
Cerium chloride (CeCl3) was used to localize H2O2 cytochemically for studying relationship between ultrastructural and functional characteristics of cellulose degradation by brown rot fungi. This technique proved very useful in localizing discrete electron-densereactionproducts at high resolution with minimal nonspecific deposition. The cytochemical localization of extracellular H2O2 by CeCl3 usin...
Yoon Soo Kim, Seung-Gon Wi


A combination of chlorothalonil and chlorpyrifos for more effective wood preservation
1995 - IRG/WP 95-30067
Chlorothalonil (tetrachloroisophthalonitrile) is a highly effective fungicide and wood preservative. Chlorpyrifos (O,O-diethyl O-(3,5,6-trichloro-2-pyridinyl)phosphorothioate) is an insecticide and is not generally considered to possess significant antifungal activity. However, a review of the literature revealed that chlorpyrifos effects in various ways the activity of microorganisms and is even ...
T L Woods, P E Laks, T C Blewett, R D Fears


Changes in the degree of decay of lignocellulosic substrate used in a screening test of fungicidal wood preservatives
1977 - IRG/WP 287
This report contains results of investigations aimed at: a) determination of the effect of the kind of substrate and species of test fungus on quantitative changes in used samples prepared from spruce cardboard, and b) comparison of the threshold fungicidal values of come fungicides determined with accelerated method, with values obtained by block method. During performed investigations, the metho...
K Lutomski